How to make the moving and finished woodwork of a house — ledged and framed doors that do not sag, hinges of wood, leather and iron, latches and bolts, window frames, sashes and shutters, and stairs that nobody trips on — and how to mark and cut joints accurately enough for all of it.

Difficulty
●●●●●
Time
A day for a ledged door; three to five days for a framed door or a flight of stairs
Steps from zero
15 prerequisites →

You need first

Timber Framing and Log BuildingAxes, Chisels, Knives and Planes

This unlocks

Doors, Hinges, Handles and LatchesStairs, Floors and Interior FinishesCupboards, Drawers, Shelves and Desks
The full path from nothing — 15 steps before this one
  1. Stone Tools
  2. Fire
  3. Cordage and Rope
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Basic Woodworking
  7. Hunting and Trapping
  8. Charcoal
  9. Hides and Leather
  10. Bellows
  11. Iron (the Bloomery)
  12. Blacksmithing
  13. Steel
  14. Axes, Chisels, Knives and Planes
  15. Timber Framing and Log Building
  16. Doors, Windows and Joinery

Do them roughly in this order. See it on the tech tree →

Why it matters

A frame (Timber Framing and Log Building) or a wall of stone or earth gives you shelter. Joinery — the finer woodwork that fills the openings and connects the floors — makes it a home: doors that keep out wind, animals and thieves, windows that let in light but not cold, stairs that make a second storey usable.

Joinery is also where you learn precision. A barn frame can be a few millimetres out; a door 3 mm out of square jams or rattles. The same habits lead on to Furniture, Barrels and Cooperage, patterns for Metal Casting and, in the end, Machine Tools.

How it works

Wood moves. It swells when damp and shrinks when dry — almost only across the grain. A board 30 cm wide can change width by 3–6 mm between a wet winter and a dry summer, while its length hardly changes. So: never fix a wide board rigidly at both edges (it splits or buckles) — join boards so they can slide past each other, and let panels float loose in grooves. Use seasoned wood (Basic Woodworking): a door of green boards opens gaps you can put a finger in. Seal both faces equally, or the board cups.

A rectangle is not rigid. A door hangs from one edge, so its weight tries to fold it into a parallelogram and drop the far corner. This is sag, the commonest failure in joinery. You stop it with a triangle (a diagonal brace) or with joints stiff enough to resist racking.

Square means equal diagonals. A frame with equal opposite sides is square if its two diagonals are the same length. Measure them with a stick or cord — the most useful test in joinery.

What you need

Tool Use Where to get it
Saws — a rip saw and a finer crosscut saw Cutting along and across the grain Files and Saws
Chisels — 6, 12 and 25 mm, and a 10 mm mortise chisel Mortises, housings, hinge recesses Axes, Chisels, Knives and Planes
Plane — a long one (45–60 cm) for flat edges, a short one for smoothing Flat, straight, square surfaces Axes, Chisels, Knives and Planes
Auger or brace and bits, 10–25 mm Peg holes, rung holes, starting mortises Drills and Boring
Try square Marking and testing right angles Make one (below)
Marking gauge Scribing a line parallel to an edge Make one (below)
Marking knife, mallet, straightedge, measuring rod Layout Measurement from Scratch
Workbench with a stop and a vice or wedges Holding the work Build from heavy planks

Fixings and finishes: Nails, Rivets and Wire Fasteners, split oak pegs, Glues and Adhesives (hide glue indoors only — it fails in damp), linseed oil (Oils and Pressing), beeswax or tallow for sliding parts, thick Hides and Leather, and forged iron (Blacksmithing).

Make your own layout tools. A try square: a 30 cm blade of thin hardwood pegged into a thicker stock. To true it, draw a line along it from a straight edge, flip it over and draw again from the same point; the error is half the gap between the lines — plane and repeat until they coincide. A marking gauge: a hardwood stem sliding through a square block (the fence), locked by a wedge, with a sharpened pin near the end to scribe a line parallel to an edge.

Where to find it

  • Timber, all seasoned: oak heartwood (the dark centre — pale sapwood rots), chestnut or elm for outside doors, frames and sills; pine, spruce or fir indoors or under paint; ash for handrails. Boards 20–25 mm thick for doors and shutters, 45–50 mm stock for frames, stiles and rails, 35–45 mm for sashes, 40–50 mm for stair strings. Straight-grained, knot-free stock for stiles and sashes; knots are fine in ledges.
  • Leather: the thick back of an ox or horse hide, tanned. Iron: bar 25–40 × 4–6 mm for strap hinges, rod 12–16 mm for pintles (Iron (the Bloomery)).

Accurate joints

Accuracy comes from method, not talent.

  1. Prepare a face and an edge. Plane one wide face flat — two straight sticks laid across its ends ("winding sticks") show any twist when you sight over them — then one edge square to it. Mark them. Measure everything from these two surfaces, never from rough ones.
  2. Gauge to thickness and width from them, and plane to the lines.
  3. Mark with a knife, not a pencil: a knife line is 0.2 mm wide, a pencil line 1 mm.
  4. Saw on the waste side of the line, then pare to it with a chisel.
  5. Gauge mortise and tenon with the same setting from the reference faces; they then match even if your measurements were slightly off.
  6. Test-fit before gluing or pegging: hand pressure or light mallet taps, no gaps at the shoulders.

The joints you need, besides the mortise and tenon and drawbore of Timber Framing and Log Building and the basic joints in Basic Woodworking:

Joint What it is Where
Tongue and groove A 6–8 mm tongue on one board's edge fits a groove in the next Door boards, floors, panelling: tight but free to move
Rebate A step cut along an edge Window sashes (for the glass), door frames (for the door to close against), shiplap boards
Haunched mortise and tenon A tenon with a short stub (the haunch) left at its outer edge to fill the groove Corners of framed doors and sashes
Wedged through tenon Tenon passes right through; wedges driven in from outside spread it Door and gate frames, where glue would fail outdoors
Housing A groove across the grain, a third of the wood's thickness deep Stair treads into strings, shelves

Method 1: The ledged and braced door

The simplest strong door: vertical boards held together by horizontal ledges and diagonal braces. Good for houses, barns and sheds.

LEDGED AND BRACED (BACK VIEW) FRAMED AND PANELLED Ledge25–30 mm × 12–15 cm Strap hinge Boardstongue and groove,not glued weight of free edge Bracerises AWAY from thehinges, so it is squeezed two clenched nailsper board per ledge hinge sidelatch side Top rail Panel12–18 mm, loose Stile45 mm × 11 cm Lock rail20 cm, latch height Bottom railwidest, 22–25 cm SECTION: PANEL IN ITS GROOVE Gap 2–3 mmpanel can swell;never glue it stile
Fig. 1 Two kinds of door. Left: a ledged and braced door — the braces must rise away from the hinged edge so they are squeezed, not stretched. Right: a framed and panelled door — the panels float in grooves so they can shrink and swell.

Typical size for a house door: 80–90 cm wide, 190–200 cm high. Check your doorway first and make the door 3 mm narrower and 3 mm shorter than the opening at the top, leaving 6–10 mm at the bottom (more if the floor is uneven).

  1. Boards 20–25 mm thick and 10–15 cm wide (narrow boards move less), joined by tongue and groove or overlapping rebates. Do not glue the edges.
  2. Ledges. Three, 25–30 mm thick and 12–15 cm wide, across the back: 15 cm from the top, at the middle (latch height), and 20 cm from the bottom, stopping 2 cm short of each edge.
  3. Braces. Two braces of the same stock fit between the ledges. The braces must rise from the hinge side at the bottom to the latch side at the top. Then the weight of the free edge pushes down along the brace into the bottom ledge near the hinge, and the brace is squeezed. Put a brace in the other way and it is pulled, does nothing, and the door sags. Cut the brace ends to sit snugly in shallow notches 1 cm deep in the ledges.
  4. Fix it. Lay the boards face down, square them (equal diagonals), and set ledges and braces on top. Drive two nails through each board into each ledge from the front, so their points come 1–2 cm out of the back, then clench them — bend the points over across the grain and hammer them flat. Clenched nails do not pull out (Nails, Rivets and Wire Fasteners). Without nails, use 10–12 mm oak pegs, wedged from the back.
  5. Finish. Plane the edges to fit and oil both sides twice, especially the end grain at the bottom.

Method 2: The framed and panelled door

Heavier work, but stronger, more stable, and it does not need braces: the stiff frame resists sag, and thin panels fill it.

Part Size (for a 85 × 200 cm door)
Stiles (the uprights) 45 mm thick, 11 cm wide, full height
Top rail 45 × 11 cm
Middle (lock) rail 45 × 20 cm, at about 90–100 cm from the floor
Bottom rail 45 × 22–25 cm — wide, because it carries most of the racking
Panels 12–18 mm thick, in grooves 10–12 mm deep
  1. Mark out matching parts together, clamped side by side, so mortises and shoulders line up.
  2. Groove the inner edges of stiles and rails, 10–12 mm deep.
  3. Mortise the stiles, tenon the rails. The tenon is a third of the stile's thickness (15 mm) and haunched — cut back to a stub that just fills the groove, so the mortise does not break out at the end of the stile. Wide rails get two tenons side by side; one wide tenon would shrink loose.
  4. Panels. Make each 2–3 mm narrower at each side than the bottom of the groove (more if made in a damp season), so it can swell without bursting the frame. Oil them before assembly so shrinkage never shows a bare strip.
  5. Assemble. Glue only the tenons, never the panels. Check the diagonals, then drawbore and peg (Timber Framing and Log Building) or wedge through-tenons.

Hinges

STRAP HINGE AND PINTLE LEATHER HINGE WOODEN LATCH (INSIDE) lifts off Pintleiron pin 12–16 mm, drivenor leaded into the post Strap25–40 × 4–6 mm, eyerolled to drop over the pin Leather strip4–5 mm thick, 8–10 cm wide;nailed to the frame, held onthe door by a pegged batten string outthrough a hole lift Pivot peg Keeperhooked blockon the frame Latch barhardwood, 40–50 cm
Fig. 2 Three hinges and a latch. A strap hinge on a pintle lets you lift the door off. A leather hinge needs only a strip of thick hide and some nails. The wooden latch lifts from outside by a string through a hole.
  • The pivot. The oldest hinge, needing no metal: make the hinge-side stile extra thick and long, round its ends into pins, and let them turn in a hole in the threshold stone and a socket in the lintel. Grease with tallow.
  • Leather hinges. Strips 4–5 mm thick and 8–10 cm wide, nailed to the frame and held on the door under a pegged batten. Three on a house door. They wear out in a few years but cost almost nothing.
  • Wooden pin hinges. Interlocking carved knuckles on door and frame with a 15–20 mm hardwood pin through them. Good for shutters and chests.
  • The strap hinge and pintle. The classic forged hinge (Blacksmithing): an iron strap 25–40 mm wide, 4–6 mm thick and 40–60 cm long, nailed along a ledge, with one end rolled into an eye that drops over a pintle — an L-shaped pin 12–16 mm thick driven or leaded into the frame or masonry. The door lifts off, which makes hanging easy.
  • Butt hinges — two leaves knuckled round a pin, let into the door edge — are neater but need accurate forging or Metal Casting.

Hang the door so it stays where you leave it. The hinge pins must lie on one vertical line; check with a plumb bob (a stone on a string). If the top pin stands out further, the door swings shut by itself; if less, it swings open.

Latches and bolts

  • The wooden latch. A hardwood bar 40–50 cm long, pivoted on a peg, drops into a hooked keeper on the frame. A cord tied to it runs out through a small hole so it can be lifted from outside; pull the string in at night and the door is shut to outsiders. The iron thumb latch works the same way.
  • Bolts. A square bar slides in two staples into a socket in the frame. A drop-bar across the whole door, resting in brackets on both sides, makes it very hard to force. For locks and keys, see Locks and Keys; for spring latches, handles, knockers and door closers, see Doors, Hinges, Handles and Latches.

The door frame

Make it of durable wood, 50 × 100–125 mm: two posts (jambs) and a head, tenoned together. Cut a rebate 12–15 mm deep along the inside so the door closes against a step and wind cannot blow straight through. At the bottom, an oak sill slopes outward about 1 in 10, with a groove (a drip) under its front edge so water drops off instead of running back. Build the frame into the wall as you go (Stone Masonry, Cob, Adobe and Rammed Earth) or fix it with iron cramps, and seal the gap with lime mortar. A sloping weatherboard along the bottom of an outside door throws rain clear of the sill.

Windows and shutters

A window is a small door made to hold glass.

  • The frame is built like a door frame, with a sloping sill and drip.
  • The sash (the frame that holds the glass) is 35–45 mm square stock, joined with haunched mortises and tenons, with a rebate about 1 × 1 cm for the glass and thin glazing bars for small panes. Glazing is in Window Glass; before you have glass, the same sash holds oiled paper, horn or skin.
  • Casements are sashes hinged like small doors. Outward-opening ones shed rain best; fit a notched stay to hold them in wind.
  • Sliding sashes run in grooves, sideways (simplest) or up and down — a vertical sash needs counterweights on cords over pulleys, or pegs to hold it.
  • Shutters are small ledged or framed doors. Closed inside shutters cut night heat loss through a single pane by a third or more; outside ones guard against storms and thieves.

Stairs

Bad stairs injure more people than almost any other part of a house. The rule is about the length of a human stride:

twice the rise plus the going = 60–64 cm

The rise is the height of one step; the going is the depth of the tread from the front of one step to the front of the next.

Rise16–20 cm Going22–28 cm Total risefloor to floor 85–100 cm Handrailon at least one side;balusters on an open side String40–50 mm thick, 25–30 cm deep upper floor THE STRIDE RULE 2 × rise + going = 60–64 cm Example: 270 cm floor to floor ÷ 15 rises = 18 cm each 62 − 36 = 26 cm going, 14 treads headroom at least 2 m everywhere TREAD HOUSED IN STRING tread glued wedgedriven in below riser
Fig. 3 Laying out a flight of stairs. Divide the total height into equal rises of 16–20 cm, then choose a going so that twice the rise plus the going is about 62 cm. Treads are housed into the strings on each side.
  1. Measure the total rise, floor to floor, exactly — say 270 cm.
  2. Divide it into equal rises of 16–20 cm: 270 ÷ 15 = 18 cm. All must match within 5 mm; one odd step trips people.
  3. Choose the going: 62 − (2 × 18) = 26 cm.
  4. Count the treads — one fewer than the rises, 14 — so the stair needs 14 × 26 = 364 cm of floor. Short of room, go steeper (up to about 42°) or turn at a landing. For a little-used loft, a ladder stair at 60–70° takes far less space.
  5. Headroom: at least 2 m above every tread.
  6. Strings: two planks 40–50 mm thick, 25–30 cm wide. Step a template (a board triangle of rise and going) along each to mark the treads.
  7. Housings 12–15 mm deep for treads 30–40 mm thick, slightly tapered, with a glued wedge driven under each tread so it never works loose or squeaks.
  8. Fix the strings at the bottom to the floor and at the top to the trimmer (the beam framing the opening), with notches, tenons or iron straps.
  9. Handrail 85–100 cm above the tread noses on at least one side, and balusters on any open side. Landings, banisters and winding stairs are in Stairs, Floors and Interior Finishes.

How to tell it worked

  • Diagonals equal within 2 mm on every door, sash and frame before you fix it.
  • The door hangs still when left half-open, swings freely, and shows an even gap — about the thickness of a coin, 2–3 mm — at the sides and top.
  • No sag. Measure the gap under the latch corner after a month: it should not have shrunk.
  • No light round a closed door or window at night, and no draught on a wet fingertip.
  • Stairs feel natural. Walk up and down with your eyes on something else. You should not have to look at your feet. Measure every rise; none should differ by more than 5 mm.

Note Troubleshooting. Door sags and drags at the latch corner → no brace, brace the wrong way round, or loose joints. Fit a brace rising from the bottom hinge corner, or tighten and re-peg the frame. Door sticks in wet weather → fitted too tight in a dry season, or unsealed bottom edge. Plane 1–2 mm off, then oil the cut. Panel split → it was glued or nailed in. Free it, or make a new panel smaller. Gaps open between boards → wood was not seasoned. Use tongue-and-groove so the gaps do not show daylight, and wait a year before fitting the final trims. Door swings open or shut by itself → the hinge pins are not plumb. Move a pintle in or out. Joints show gaps at the shoulders → marked from rough faces or sawn on the line. Mark from reference faces, saw on the waste side and pare to the knife line. Stair creaks → a tread is loose in its housing. Drive the wedge in again with fresh glue.

Dangers

Danger Falls on stairs kill and cripple, especially the old and small children. Never build uneven risers, treads too shallow for a whole foot, or an open side without a rail. Light every stair at night.

Warning Doors in a fire. A crowd pushing toward an inward-opening door crushes the people at the front against it. Every room where many people gather must have doors that open outward and at least two ways out.

  • Chisels and knives cause most workshop injuries. Keep both hands behind the edge, cut away from your body, and clamp the work instead of holding it.
  • Heavy doors. An oak door weighs 40–60 kg. Hang it with two people, and never stand under one while lifting it onto pintles.
  • Saws and planes slip on knots; keep fingers clear of the line.
  • Fine dust from oak and other hardwoods irritates lungs and is linked to nose cancer after years of exposure; work outdoors or in a draught and sweep up wet.

Going further

A The Lathe turns balusters and knobs (Wood Turning and Treen); planing and moulding machines driven by a The Waterwheel or The Steam Engine (Planers, Thicknessers and Woodworking Machines) make boards and tongue-and-groove in quantity. Frame-and-panel construction makes chests and cupboards (Furniture). Weatherstripping (felt or leather pinned into the rebate) and double windows are in Insulation and Keeping Buildings Warm or Cool.

How it was first done

Doors turning on pivots in stone sockets were used in Mesopotamia and Egypt by the 3rd millennium BC, and Egyptian woodworkers already made dovetails and framed panels. Roman joiners had planes, iron hinges and sliding bolts. Medieval European doors were mostly ledged boards hung on long, often decorated iron strap hinges; framed and panelled work spread in northern Europe from about the 15th century. The counterweighted sliding sash window appeared in England and the Netherlands in the late 1600s. The stair rule of "two rises plus a going" was published by the French architect François Blondel in 1675; builders had probably used something like it long before.

Source: content/entries/building/joinery.md