Part 8 · Chemistry
Borax and Boric Acid
Borax is a white salt from desert lake beds that melts into a glass which dissolves rust and scale — the flux of every smith, jeweller and brazier. Refined by crystallising and turned into boric acid with sulfuric acid, it also makes tough, heat-proof glass and low-firing glazes, protects timber, kills ants and cockroaches, fireproofs cloth and feeds crops short of boron.
- Difficulty
- ●●●●●
- Time
- A day to dissolve, settle and set crude borax crystallising; a week for the crystals to grow; an afternoon for a batch of boric acid
- Steps from zero
- 10 prerequisites →
This unlocks
—The full path from nothing — 10 steps before this one
- Fire
- Finding and Preparing Clay
- Sulfur
- Pottery
- The Kiln
- Lime
- Lye and Potash
- Glass
- Saltpeter
- Sulfuric Acid
- Borax and Boric Acid
Do them roughly in this order. See it on the tech tree →
Why it matters
Heat a crystal of borax and it swells into a white froth, then melts into a clear, runny glass. That glass dissolves metal oxides — the scale and rust that stop metals joining. Painted on a joint before brazing, sprinkled on steel before forge welding, thrown on gold and silver in the crucible, it keeps the metal clean so it can flow and stick (Soldering and Brazing, Welding, Gold and Silver). The same property makes the borax bead of the analyst (Identifying Substances).
Borax and its acid do a surprising number of other jobs:
- Glass and glazes. A little boron oxide in glass makes it melt lower and expand less when heated, so it survives hot liquids and flames — the basis of heat-proof laboratory and kitchen glass (Laboratory Glassware). Borax lets glazes and enamels melt at low temperatures (Glazes, Enamel on Metal).
- Timber protection against rot and woodworm, safe enough for houses (Rot, Woodworm and Termites).
- A mild antiseptic, and a slow poison for ants and cockroaches (Household Pests).
- Fireproofing for cloth, paper and loose-fill Insulation and Keeping Buildings Warm or Cool.
- A trace food for crops: beets, turnips, cabbages, celery and fruit trees fail on boron-poor soils.
- Electrical uses: the electrolyte of aluminium rectifiers and capacitors (Rectifiers: Turning AC into DC, Resistors, Capacitors and Coils).
How it works
Borax is sodium borate — sodium, boron and oxygen — with ten molecules of water locked into every unit of the crystal (about 47 % water by weight). That water explains its behaviour in the fire:
- From about 60 °C the crystal starts to lose water; on a hot iron it boils inside itself and puffs up into a white, crumbly foam several times its first size.
- By about 400 °C the water is gone: a light white powder, burnt borax.
- At about 740 °C (dull red heat) it melts into a clear, sticky glass — fused borax. Molten, it dissolves iron, copper and other metal oxides, taking on their colours (blue from cobalt, green from chromium or copper, violet from manganese).
Boric acid is the weak acid inside borax. Add a strong acid such as Sulfuric Acid to hot borax solution, and the sodium goes off with the sulfuric acid while boric acid is left free. Boric acid is only slightly soluble in cold water — about 5 g in 100 ml — but more than five times as soluble in boiling water, so it crystallises out as the liquid cools, as shiny, white, slippery-feeling flakes. Heated, it too loses water and melts into a glass (boron oxide).
Both are refined by the same trick: they dissolve far better in hot water than in cold. Borax dissolves only about 5 g in 100 ml of cold water but more than ten times as much near boiling. Dissolve the crude salt hot, let the mud settle, pour off the clear liquid and let it cool slowly: pure crystals grow, and most impurities stay dissolved.
What you need
| Item | Use | Notes |
|---|---|---|
| Crude borax or borate mineral | Raw material | See below |
| Boiling pan of iron or copper, 20–100 litres | Dissolving | Pots, Pans and Kettles, Sheet Metal and Rolling |
| Settling tub and crystallising pans — wooden, lead-lined or glazed, deeper than wide | Refining | Barrels and Cooperage, Lead |
| Soda ash | Converting borate minerals; clearing iron and lime | Soda Ash and Baking Soda |
| Strong sulfuric acid or hydrochloric acid | Making boric acid | Sulfuric Acid, Hydrochloric Acid |
| Litmus or red-cabbage paper | Judging acid | Acids, Bases and Testing |
| Linen strainer, wooden paddles, sticks or strings | Filtering, growing crystals | |
| Fire and plenty of fuel | Boiling |
Where to find it
Boron is rare in ordinary rocks, but where volcanic steam and hot springs have fed it into closed desert basins, the lakes dry and leave it behind as salt.
- Borax (tincal). White crusts, puffy mounds and beds of colourless to white crystals on the dried floors and edges of salt lakes in deserts and high plateaus — Tibet and Ladakh, the Andes of Chile, Argentina and Bolivia, Death Valley and the Mojave in California, Nevada, central Turkey, Iran. Crystals are short, glassy prisms that turn chalky white on the surface as they lose water in dry air. Taste: faintly sweetish and alkaline.
- Ulexite ("cotton balls"). Soft, white, rounded lumps of silky fibres, like wads of cotton, in playa muds. A polished slice of the fibrous kind transmits images like a bundle of glass threads ("television stone").
- Colemanite. Hard, glassy, colourless to white crystals and nodules in old lake-bed clays — the chief ore in Turkey. It does not dissolve readily in water.
- Sassolite (natural boric acid). In a few volcanic fields — most famously Larderello in Tuscany — jets of steam carry boric acid out of the ground. It collects as white pearly flakes round the vents and dissolves in the hot pools.
Tests for boron:
- Puffing. A crumb heated on a red-hot iron or charcoal swells into white froth, then melts to a clear glass bead. Salt crackles and does not swell; soda melts without much frothing; gypsum goes white and opaque but does not melt to glass.
- Green flame. Wet a pinch of the powder with a few drops of strong sulfuric acid, add a spoonful of spirit (Distillation), and light it in a dark place. The flame is edged with a vivid green. Nothing else common does this.
- Turmeric paper. Acidify a little dissolved sample with hydrochloric acid, dip in a strip of paper stained with turmeric, and let it dry in warmth: boron turns it rose-red. A drop of ammonia or lye then turns that patch blue-black.
- No fizz. Borax does not fizz in vinegar or acid; soda does. Playa crusts are often a mixture: the fizzing part is soda, the puffing part borax.
Method 1: Refining crude borax
Crude lake borax is mixed with mud, salt, soda and sulfates. Traders once smeared it with fat to stop it drying out; Venetian and Dutch refiners made fortunes cleaning it. The process is simple.
- Pick and wash. Pick out stones and lumps of mud. Rinse the crude salt quickly in a little cold water: salt and soda wash off faster than borax.
- Dissolve. Bring water to the boil in the pan and add crude borax until no more dissolves — roughly 1 kg for every 2 litres of boiling water. Stir in about 1 % of its weight of soda ash. The soda throws down iron, lime and magnesia as a fine mud, and turns any free boric acid back to borax.
- Settle. Ladle or siphon the boiling liquid into a deep, covered, wooden settling tub wrapped in straw or sacks so it cools slowly. Leave it 2–4 hours: the mud sinks.
- Crystallise. Draw off the clear, hot liquid into the crystallising pans — deep wooden or lead-lined tanks, kept covered and insulated. Hang clean sticks or strings in it. Cooling must be slow: over 4–8 days large, clear crystals grow on the walls and strings. Fast cooling gives a mush of small crystals that holds dirty liquid.
- Harvest. Pour off the mother liquor (the liquid left over). Break out the crystals, rinse them with a little cold water, and dry them in shade — in hot sun or a warm room they lose water and go chalky. Store in closed jars.
- Second crop. Boil the mother liquor down by a third and crystallise again. The crystals are less pure; use them for flux or wood preservative, and redissolve them with the next batch for anything better.
One recrystallisation turns grey, earthy tincal into white, glassy borax. Two give a product pure enough for glass and medicine.
The crystallising pan
Any deep vessel works, but a good one makes big, clean crystals. Make it at least 40 cm deep, wider at the top than the bottom so the crop knocks out, of hardwood staves (Barrels and Cooperage) or a wooden box lined with thin sheet lead soldered at the seams. Fit a loose lid and pack straw around it so that a 50-litre batch takes several days to cool. Lay sticks across the top with strings hanging into the liquid. Iron rusts and stains the crystals; avoid it.
Method 2: Borax from ulexite and colemanite
Where the land gives ulexite or colemanite instead of borax, boil them with soda ash. The soda takes the boron; the lime of the mineral drops out as chalk.
- Grind the mineral to a fine powder (Mining and Tunnelling, The Watermill).
- For ulexite, use about 1 part soda ash to 4 parts mineral; for colemanite, about 1 part soda ash to 2 parts. Boil in four or five times their weight of water for 2–4 hours, stirring, topping up the water.
- The white mud that forms is chalk (calcium carbonate). Let it settle, draw off the hot liquid, and crystallise as in Method 1. Wash the mud with a little boiling water to recover the rest.
- If the liquid stings the fingers and turns turmeric red-brown strongly, there is spare caustic soda in it; bubbling furnace gas or the carbon dioxide from a fermenting vat through it softens it (Soda Ash and Baking Soda describes this). Too little soda leaves undissolved mineral: add more and boil again.
Yields are roughly 1 kg of borax crystals per 1 kg of ulexite and a little more from colemanite.
Method 3: Boric acid
- Dissolve 100 g of borax in about 250 ml of boiling water in a glass, glazed or lead vessel.
- Measure 14 ml of strong sulfuric acid (or 50–60 ml of strong hydrochloric acid). Always pour acid into water, slowly, never the reverse. Add it a little at a time to the hot borax solution, stirring with a glass rod, until a drop of the liquid turns blue litmus red and keeps it red.
- Let it cool slowly, then stand it in cold water or snow. Shiny white flakes of boric acid crystallise.
- Filter or strain off the flakes; rinse them twice with a little ice-cold water (it dissolves them only slowly). The liquid left holds Glauber's salt (sodium sulfate) and a little boric acid; boil it down by half for a second, dirtier crop.
- For pure boric acid, redissolve the flakes in the least boiling water and crystallise again. Dry at no more than about 80 °C.
From 100 g of borax expect 45–55 g of boric acid in the first crop; 65 g is the most possible.
From volcanic steam. At Larderello the boric acid steam was led into stone-walled pools, where the water slowly gathered a fraction of one percent of boric acid. The weak liquid was run through a chain of pools and evaporated in lead pans heated by the volcanic steam itself. Where hot springs or fumaroles carry boric acid, the same idea works: collect, evaporate with free heat, crystallise.
Fused borax and flux
For brazing and welding, crystal borax is a nuisance: its water boils and pushes the flux off the joint. Make fused borax:
- Heat crystals in a clay or iron pot. They froth and swell — use a pot five times bigger than the charge.
- Keep heating to bright red until the froth has melted to a clear, quiet glass.
- Pour onto a cold iron plate, break up the glass when cool, and grind it to powder. Store it dry in a closed jar: it slowly takes up water from the air.
Use it dry, or mix it with water or spirit to a paste for brazing (Soldering and Brazing). For forge welding steel (Blacksmithing), sprinkle fused borax on the joint at a bright red heat; many smiths stretch it with clean sand or a little iron filing. For melting gold and silver, a spoonful per crucible keeps the metal bright (Gold and Silver). The flux is good if it melts on the work at dull red to a thin, clear, glassy film that spreads and wets the metal, and black scale disappears into it.
Uses with numbers
| Use | How | See |
|---|---|---|
| Heat-resistant glass | Add borax or boric acid to the batch: even 5–10 % boron oxide makes glass that stands sudden heat far better and resists water and acids. True borosilicate glass (about 13 % boron oxide, 80 % silica) needs over 1,600 °C — beyond a wood-fired pot, but a goal for a later furnace | Glass, Laboratory Glassware, Optical Glass and Achromatic Lenses |
| Low-firing glazes and enamels | Borax melts silica at 750–1,000 °C. Because it dissolves in water, melt it into a frit first, quench and grind | Glazes, Enamel on Metal |
| Wood preservative | About 150 g borax and 100 g boric acid per litre of hot water, brushed or soaked into dry, covered timber | Rot, Woodworm and Termites |
| Ant bait | 5 g boric acid (1 level teaspoon) and 100 g sugar in 250 ml warm water (about 1.5 %); soak cotton wool and set it in a lid near the trail. Weak enough that workers carry it home to the nest; ants vanish in one to three weeks | Household Pests |
| Cockroach powder | Fine boric acid dusted thinly in cracks, behind stoves and under sinks; roaches walk through it and lick it off. Heaps are avoided | Household Pests |
| Fire-retardant cloth and paper | 70 g borax and 30 g boric acid per litre of warm water (the mixture dissolves better than either alone). Soak, wring and dry. Treated cotton chars instead of flaming. Washes out: re-treat after washing | Insulation and Keeping Buildings Warm or Cool, Firefighting |
| Boron for crops | About 1 g of borax per square metre (10 kg per hectare) dissolved in a watering can, once every two or three years, only where beet hearts rot, cabbage stems are hollow, or celery stems crack. Ten times that dose poisons the crop | Understanding Soil, Chemical Fertilisers |
| Laundry | A spoonful per bucket softens hard water and helps soap | Laundry and Bleaching Cloth |
| Glue and starch | A little borax thickens starch paste and makes it tackier; it dissolves casein for glue and paper coatings | Glues and Adhesives |
| Electrolytic rectifier and capacitor | Aluminium plates in borax solution | Rectifiers: Turning AC into DC, Resistors, Capacitors and Coils |
| Ointment and cold cream | About 1 % borax emulsifies beeswax creams | Toothpaste, Shampoo, Perfume and Cosmetics |
As an antiseptic. Boric acid is a weak antiseptic. A 2–3 % solution in boiled water (2–3 g in 100 ml) was the standard eye bath and wash for minor skin irritations, and dried lint soaked in it was an early surgical dressing. It is far weaker than alcohol, iodine or carbolic (Wound Care and Antiseptics, Iodine). Use it only on small areas of unbroken or lightly irritated skin, and never on babies, burns or large raw wounds, through which enough is absorbed to poison.
How to tell it worked
- Refined borax: clear, glassy prisms (or white where the surface has dried), dissolving completely in hot water to a clear liquid with no mud; a fragment puffs and melts to a colourless bead. A yellow or brown bead means iron is still there — recrystallise.
- Boric acid: white, pearly flakes that feel greasy-slippery between the fingers; a pinch in a spoonful of burning spirit gives a green-edged flame; its solution turns blue litmus only faintly red (it is a very weak acid).
- Fused borax: a clear, glassy cake, not cloudy; on hot metal it spreads as a thin film.
Note Troubleshooting.
- Crystals tiny and muddy → cooled too fast, or not settled long enough. Redissolve, settle longer, and insulate the crystallising pan.
- Nothing crystallises → too much water. Boil down by a quarter and try again.
- Crystals turn white and crumbly in store → kept too warm and dry; they lost water. Still good for flux; for weighing recipes, store in closed jars.
- Few boric acid flakes → not enough acid (litmus not red), or too much water. Add acid to red, boil down, cool in snow or cold water.
- Boric acid tastes salty or leaves a crust on drying → Glauber's salt still in it; rinse with ice-cold water and recrystallise.
- Flux bubbles and lifts off the joint → crystal borax used; fuse it first.
Dangers
Danger Borax and boric acid are poisons if swallowed, though they look like sugar or salt and taste of almost nothing. A few grams can kill a baby; children have died when boric acid was mistaken for sugar or milk powder, or put on nappy rash and burns. Signs: vomiting and diarrhoea (often blue-green), a bright red, peeling skin rash like a boiled lobster, then fits. Label every jar, keep baits where children and animals cannot reach, and never store borates near food.
- Strong acid. Making boric acid uses strong sulfuric or hydrochloric acid: goggles, gloves, acid into water, and a bucket of water and soda nearby (Sulfuric Acid).
- Boiling solutions in deep pans scald. Fill pans only two-thirds, and ladle with long handles.
- Molten borax at red heat spits if wet: preheat tools and moulds.
- Fertiliser overdose. Boron is good for plants in grams and poison in tens of grams. Weigh, and spread evenly.
- Long, heavy exposure to borates is suspected of harming fertility; wear a cloth over the mouth when grinding or dusting, and wash hands after work.
What this unlocks
With borax in hand, every metalworker can braze, forge-weld and melt precious metals cleanly. Glassmakers can move from soft, easily cracked glass towards heat-proof Laboratory Glassware and Optical Glass and Achromatic Lenses; potters and enamellers gain low-firing glazes. Houses last longer under borax-treated roofs; homes are freer of cockroaches; root crops yield again on poor soils. Later, pure boron compounds absorb neutrons in reactors (Nuclear Energy (Overview)) and boron is the "p-type" impurity added to silicon in Semiconductors and the Transistor.
How it was first done
Borax was traded along the Silk Road from Tibet and western China at least a thousand years ago; Arab and Persian goldsmiths called it būraq, and medieval European goldsmiths bought it, as tincal, by way of India and Venice. For centuries the Venetians and later the Dutch kept the refining secret. In 1777 the German apothecary Hubert Höfer found boric acid in the hot pools of Tuscany; from 1818 the French businessman François de Larderel extracted it there, and in 1827 began using the volcanic steam itself to evaporate the liquor — a first use of underground heat for industry. In 1904 the same steam field lit the world's first geothermal electric bulbs. In America, borax was found in the Nevada and California deserts from the 1860s, and from 1883 to 1889 the "twenty-mule teams" hauled it 270 km across Death Valley. Colemanite and kernite later replaced lake borax, and Otto Schott in Jena (1880s–90s) and Corning in New York (Pyrex, 1915) made boron the key to heat-proof glass.
Source: content/entries/chemistry/borax-and-boric-acid.md