Electric light, the honest way — first the carbon arc lamp, blindingly bright and fairly easy to make, then the carbon-filament bulb of Swan and Edison, which needs a vacuum, a glass seal and many patient failures.

Difficulty
●●●●●
Time
A week for an arc lamp once you have a generator; months of trials for a lasting filament bulb
Steps from zero
24 prerequisites →

You need first

GlassThe BatteryCharcoalThe Vacuum Pump

This unlocks

Arc Lamps, Neon and Fluorescent LightsThe Vacuum TubeCinema: Film Cameras and Projectors
The full path from nothing — 24 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Hunting and Trapping
  7. Basic Woodworking
  8. The Kiln
  9. Pottery
  10. Charcoal
  11. Hides and Leather
  12. Lime
  13. Mercury
  14. Lye and Potash
  15. Fermentation
  16. The Wheel and Axle
  17. Glass
  18. Bellows
  19. The Lathe
  20. Copper Smelting
  21. Laboratory Glassware
  22. Pumps
  23. The Battery
  24. The Vacuum Pump
  25. The Light Bulb

Do them roughly in this order. See it on the tech tree →

Why it matters

For all of history, light after dark meant flame: dim, smoky, hungry for fuel, and quick to burn a house down. Electric light is brighter, smokeless, instant, and can go anywhere a wire can reach — into mines, ships and barns full of hay.

Lighting was also the first use of electricity people would pay for. It is why towns built power stations and strung wires through the streets — wires that then carried power for The Electric Motors and everything else. The bulb itself led directly to the The Vacuum Tube, the first electronic device, and so to Radio and the The Computer.

This chapter is honest about difficulty. The arc lamp is the easier first light: simple parts, no vacuum, but it needs a strong supply (a The Generator or a large battery) and it is too bright and fierce for a room. The filament bulb is the gentle household light, but it needs a vacuum far better than any simple pump gives, a glass-to-metal seal that does not leak, and a thread of pure carbon. Expect dozens of failures.

How it works

Anything heated enough glows: dull red at 600 °C, orange at 1,000 °C, yellow-white at 1,500 °C, dazzling white above 2,000 °C. Electricity heats whatever resists it — the thinner and more resistant the path, the hotter it gets (see Copper Wire).

Carbon is the material for the job. It does not melt at any temperature you can reach — it turns straight to vapour only above about 3,600 °C. It conducts electricity, but not too well, so it heats. And you can make it from charcoal, or from plant fibres baked without air. Its one weakness: in air, hot carbon simply burns, as charcoal does.

  • The arc lamp solves this by brute force. Two carbon rods touch, then are drawn a few millimetres apart. The current keeps flowing across the gap through a bridge of glowing, electrified vapour — the arc. The tip of the positive rod is heated to about 3,500 °C and shines brighter than anything else made by people before the 20th century. The rods burn away in the air, and you feed them together as they do.
  • The filament bulb uses a thin thread of carbon (the filament) heated white-hot by the current. To stop it burning, it is sealed inside a glass bulb with almost all the air pumped out — a vacuum. With no oxygen, it can glow for hundreds of hours.

Volts, amps and watts. The power a lamp uses is volts × amps, measured in watts (W). A thin, long filament has high resistance: it needs a high voltage but little current. A short, thick one needs a low voltage and a lot of current. Batteries give low voltage and run out fast, so a lamp that runs from batteries is short, thick and expensive to run. A The Generator is the natural partner of electric light.

What you need

For the arc lamp:

Item Amount Notes
Power supply 45–60 V at 3–10 A A self-exciting dynamo (The Generator). A battery needs 50–70 cells in series, each with large plates: an ordinary Daniell cell gives only about half an amp, so you would need several such strings in parallel (The Battery)
Carbon rods 8–12 mm thick, 20–30 cm long Made below from charcoal or coke
Ballast resistance About 2–5 ohms that can get hot Roughly 20–40 m of iron wire about 1 mm thick, wound on a clay or stone former; adjust the length until the arc burns steadily
Holder Two clamps on insulating wooden arms, one sliding Basic Woodworking, brass or copper (Zinc and Brass)
Dark glass Several layers of smoked glass To look at the arc
Glass globe Optional, to shield people from the arc Glass

For the filament bulb:

Item Amount Notes
Fibre for filaments Bamboo, cotton thread or stiff paper Make dozens
Clay crucible and charcoal powder For carbonising Pottery, Charcoal
Glass Bulbs 6–8 cm across, tube, glass rod Glass; you must be able to blow and join it
Lead-in wires Platinum ideally, or very thin copper See The seal below
A good vacuum pump Mercury pump, reaching a millionth of an atmosphere The Vacuum Pump
Power supply 20–100 V depending on filament The Generator or The Battery

Where to find it

  • Bamboo. Edison's best filaments came from a Japanese bamboo. Any large, mature, woody bamboo will do. Use the dense, hard outer layer just under the shiny skin — it is made of long, straight, even fibres. Bamboo grows in warm, wet regions of Asia, Africa and the Americas.
  • Cotton thread comes from the seed hairs of the cotton plant (Spinning and Weaving Cloth). Linen thread from flax also works. Strips of thick, smooth paper (Paper) or card are a third choice.
  • Carbon for arc rods. The best is dense coke from heating coal without air, or retort carbon — the hard, grey, metallic-looking crust that builds up inside clay or iron vessels used to heat coal or tar. Graphite, a soft, black, greasy mineral that leaves a grey mark on paper, is found in veins in old metamorphic rocks; powdered, it improves rods. Ordinary Charcoal works but is soft and burns away fast.
  • Platinum is a heavy, silvery-grey, untarnishing metal found as small grains with gold in river gravels in a few places — notably Colombia and the Ural Mountains (Platinum and the Platinum Metals). It is much heavier than ordinary gravel; it stays in the pan with gold (Finding and Identifying Ores). Most people will never find enough. See the alternatives below.

Method 1: The carbon arc lamp

Make the carbon rods

  1. Grind dense coke or charcoal to a fine powder — as fine as flour. Sieve it through cloth. If you have graphite, mix in up to a quarter of graphite powder.
  2. Bind it. Knead in thick tar (Tar, Pitch and Glue) or thick sugar syrup (Sugar) — about 1 part binder to 3 parts powder by weight — to make a stiff dough.
  3. Shape rods 10 mm thick and 25 cm long, by rolling the dough on a board or pressing it through a tube. Keep them straight. Dry them slowly for several days.
  4. Bake them without air. Pack the rods side by side in a long clay box or pipe, filling the spaces with sand or charcoal powder, and seal the lid with clay. Heat it in a The Kiln, slowly at first, then to a bright orange-yellow heat (about 1,100 °C) for several hours. Let it cool completely before opening, or the rods will burn.
  5. Densify. Soak the baked rods in thin syrup or tar, and bake them again. Two or three rounds make a harder, denser, longer-lasting rod.

A good rod rings when tapped, barely marks paper, and conducts well (test it on a galvanometer against a known one — The Electromagnet).

Build the lamp

Upper carbon (+) its hollow white-hot crater gives most of the light Arc gap 2–4 mm Lower carbon (−) burns half as fast Feed screw lowers the upper carbon as the rods burn Ballast iron wire coil, 2–5 Ω, gets hot Supply dynamo, 45–60 V positive to the top dry wooden arms insulate
Fig. 1 The carbon arc lamp. Two carbon rods are held in line on insulated arms. They are touched together, then drawn a few millimetres apart; the current jumps the gap as a blinding arc. With direct current the upper, positive rod forms a glowing crater that gives most of the light.
  1. Holder. Fix two brass or copper clamps on wooden arms, one above the other, so that the two rods line up exactly, tip to tip. The upper arm slides up and down in a wooden guide, moved by a screw or a cord over a pulley with a counterweight.
  2. Wiring. With DC, connect the positive side of the supply to the upper rod: the positive tip forms a hollow crater that throws most of the light, and on top it shines downward. Put the ballast — the coil of iron wire — in series with the lamp. Without it, the current rises until something burns out, because an arc lets more current through the hotter it gets.
  3. Strike the arc. Lower the upper rod until the tips touch, then raise it 2–4 mm. A brilliant arc forms with a hiss.
  4. Feed it. The rods burn away — the positive about twice as fast as the negative with DC — and the gap widens until the arc goes out with a snap. Close the gap by hand every few minutes, or build an automatic feed: an electromagnet in series with the lamp lifts the upper rod a few millimetres when current flows, and lets it fall back to re-strike when it stops.
  5. Shield it. Put a globe of glass around the arc (ordinary glass blocks much of the harmful ultraviolet light) and hang the lamp high.

The electric candle. In 1876 Pavel Yablochkov made an arc lamp with no moving parts: two thin carbon rods (4 mm) side by side, separated by a thin wall of plaster or fired clay, with the arc burning across their tips and creeping down as they burned, like a candle. It needs alternating current, so that both rods burn equally fast, and each candle lasts an hour or two.

What to expect. A 10 mm carbon arc at 45–50 V and 5–10 A gives about as much light as several hundred candles — enough to light a big hall, a yard or a street. The rods burn away at a few centimetres an hour. Self-feeding arc lamps, searchlights and the gas-discharge lamps that replaced them are in Arc Lamps, Neon and Fluorescent Lights.

Method 2: The carbon-filament bulb

This is a hard project: it took Joseph Swan nearly thirty years of on-and-off work, and Edison's laboratory tried thousands of materials. You have the advantage of knowing what works.

Tip pumping tube, melted shut Filament carbonised bamboo, cotton or card, about 0.2 mm thick Joints small copper clips covered with carbon paste The seal wire through hot glass: platinum, or very thin copper Base wood or plaster, with two contacts Glass bulb 6–8 cm across Vacuum under 1/100,000 of the air Glass stem melted into the neck To the supply copper wires
Fig. 2 Inside a carbon filament bulb. The filament is a hairpin of carbonised bamboo or cotton, joined to two lead-in wires that pass through a glass seal. The air has been pumped out through a narrow tube, which was then melted shut.

1. Make the filaments

  1. Bamboo: split a section of mature bamboo and shave off the shiny skin. From the dense layer just under it, split thin slivers and scrape them with a sharp blade through a gap set between two pieces of hard steel, until they are even: about 0.2 mm thick and 0.3 mm wide, 12–15 cm long. Leave the two ends wider (2 mm) as "feet" for clamping.
  2. Cotton: use a smooth, even cotton thread. Swan made his threads denser and more even by dipping them for a few seconds in a mixture of about 2 parts strong Sulfuric Acid to 1 part water (acid poured slowly into the water, never the reverse), then washing them thoroughly — this turns the surface to a tough, smooth "parchment".
  3. Paper: cut hairpin shapes from thick, smooth card with a sharp knife against a metal template.
  4. Make dozens. Most will break.

2. Carbonise them

  1. Bend each fibre into a hairpin or loop and lay it in a groove cut in a flat block of fired clay or carbon, so that it keeps its shape.
  2. Pack the blocks in a clay crucible filled with fine charcoal powder, covering every filament. Put a lid on and seal it with clay.
  3. Heat slowly — over an hour — to red, then hold it at a bright orange-yellow heat (about 1,000–1,200 °C) for one to two hours. Slow heating lets the gases escape gently without cracking the fibres.
  4. Let it cool completely, overnight, before opening. Hot carbon meeting air burns instantly.
  5. Lift the filaments out with fine tweezers. They are now black, springy, glassy, and very fragile, and they have shrunk by about a fifth. Check each one by eye for cracks and thin spots, and test it on a battery and galvanometer: it should conduct.

3. The seal: getting wires through the glass

The filament must be connected to the outside through the glass, and the glass must seal tight around the wires. This is the hardest part to improvise.

  • Platinum is the proper answer: it expands with heat almost exactly as much as ordinary soft glass, so a seal made red-hot stays tight when it cools, and it does not tarnish. Swan's and Edison's lamps used short pieces of platinum wire (0.3 mm) for the part inside the glass only, joined to copper outside.
  • Very thin copper. Copper expands much more than glass, so a thick copper wire cracks its seal as it cools. But copper is soft: a wire thinner than about 0.2 mm, or a copper wire hammered at the sealing point into a thin ribbon with knife-sharp edges, can give way to the glass instead of cracking it. This works some of the time; test every seal (below).
  • No seal at all. For your first experiments, put the filament on a stopper of glass ground to fit the neck of the bulb, or set the wires through a plug and cover the joint thickly with a cement of beeswax and pine resin melted together. These seals leak a little, so keep the bulb connected to the pump and pumping while the lamp is lit. This is how many early experimenters first saw a carbon thread glow in a vacuum.

Fix the filament's feet to the lead-in wires by clamping them in tiny folded copper clips and covering the joint with a paste of fine lampblack (soot) in thick syrup, which carbonises in the first heating and makes a good contact.

4. Pump out the air

The filament needs a very good vacuum — less than a hundred-thousandth of the air that was in the bulb. A simple piston pump reaches perhaps a hundredth; a filament in that much air burns through in seconds or minutes. You need a mercury pump of the Sprengel type, described in The Vacuum Pump.

  1. Blow the bulb (6–8 cm across) with a narrow glass tube at its top for pumping. Seal the stem carrying the filament into its neck in the flame (Glass).
  2. Connect the pumping tube to the vacuum pump and pump for a long time — an hour or more.
  3. Drive out the hidden gas. Carbon holds a lot of gas inside it. While still pumping, pass a small current through the filament so that it glows dull red, then gradually brighter. Gas bubbles out of the carbon and the pump removes it. Keep going until the vacuum holds steady with the filament glowing brightly. Swan and Edison both found that this step was the secret to a long life.
  4. Seal it off. Heat the narrow pumping tube with a hot flame until it softens and collapses, and draw it apart into a sealed tip.

What voltage, what current?

A filament's needs depend on its length and thickness. As a rough guide:

Filament Needs roughly Light
Bamboo loop 12 cm long, 0.2 mm thick (like Edison's) 80–110 V, about 0.5 A (about 50 W) 15–20 candles
Cotton or bamboo, 4 cm long 25–35 V, about 1 A 6–10 candles
Thick, short (2 cm) 10–15 V, 1.5–2 A a few candles

Start every new lamp on a low voltage and raise it slowly while watching. A carbon lamp at its right brightness glows a warm yellow-white. Pushed brighter, it lives much shorter.

The light is weak for the power used: a carbon filament turns only about one part in two hundred of its power into light. Running even a few lamps from batteries means a large battery and a lot of zinc; this is why the bulb arrived only once The Generators existed.

Tip Why not just burn the oxygen out? A candle burned inside a sealed jar goes out while about three-quarters of the oxygen is still there — far too much for a hot filament. Filling the bulb with a gas that carbon cannot burn in, such as pure nitrogen, does work, and some later lamps were gas-filled. But making pure, dry nitrogen is a project in itself. The vacuum is the more direct path.

How to tell it worked

  • The arc burns with a steady hiss or hum and an intensely white light. Looking through dark glass, you see a bright hollow crater on the positive rod and a pointed tip on the negative. A flickering, wandering arc that goes out means the gap is too wide, the rods are poor, or the supply voltage is too low.
  • The bulb glows steadily, a little yellow, with no flicker. Over hundreds of hours the inside of the glass slowly darkens with carbon evaporated from the filament; that is normal.
  • Testing a seal. Pump the bulb down, close it off from the pump, and wait a day. Then connect it to the pump again: if the pump labours or you see a gas glow when the filament is lit, the seal leaks.

Note Troubleshooting the bulb. Filament flashes bright and breaks at once → air in the bulb: poor vacuum, or a leaking seal. Faint blue or violet glow fills the bulb when lit → there is still gas inside. Pump longer, and heat the filament more while pumping. White or brown smoke inside → oxygen got in and the filament is burning. Check seals. Filament glows unevenly, with one bright spot, then breaks there → a thin spot. Scrape filaments more evenly, and reject any with visible flaws. Glass cracks round the wire → wire too thick, or glass cooled too fast. Use thinner wire, and cool the seal slowly in warm ash.

Dangers

Danger The arc can blind you. It is brighter than looking near the sun and gives off strong ultraviolet light. Looking at it unprotected, even for a few seconds, can burn the eyes ("arc eye": hours later, intense pain and a feeling of sand in the eyes) and can permanently damage the retina. Never look directly at an arc. View it only through several layers of dark smoked glass, and shield bystanders. Ultraviolet also sunburns bare skin within minutes at close range.

Danger High voltage. Lamps run at 50–110 V. That can kill, especially through wet skin or from hand to hand. Switch off at the supply before touching any part of a lamp, and mount all live parts on dry wood out of reach. See The Generator.

  • Burns and fire. Arc carbons stay red-hot for minutes after switching off and drop glowing fragments. Mount arc lamps over bare earth, stone or sand, away from wood, cloth and hay. Bulbs get hot too.
  • Imploding bulbs. An evacuated bulb is crushed from outside by the air. If cracked it bursts inward and then sprays glass outward. Wear eye protection while pumping, sealing and handling new bulbs.
  • Mercury. Mercury vacuum pumps give off poisonous vapour. Work in a well-aired room and catch every spilled drop. See The Vacuum Pump.
  • Fumes. Arcs make small amounts of irritating gases. Ventilate any indoor room lit by an arc.
  • Acid. Treating cotton with sulfuric acid: see Sulfuric Acid.

Going further

  • The vacuum tube. In 1883 Edison noticed that a small current flowed through the vacuum from the hot filament to a metal plate sealed into the bulb. That "Edison effect" became the vacuum diode (1904) and then the amplifying triode: see The Vacuum Tube.
  • Better filaments. Metal filaments of tungsten, from about 1904–1910, gave three times the light for the same power; filling bulbs with inert gas (from 1913) improved them further.

How it was first done

Humphry Davy showed the brilliant light of an arc between charcoal points at the Royal Institution in London in the first decade of the 1800s, using an enormous battery of some 2,000 pairs of plates. Arc light stayed a laboratory wonder until generators could feed it. Lighthouses began using it in the late 1850s; Pavel Yablochkov's "electric candles" lit the streets of Paris from 1878, and Charles Brush's arc lights lit American cities from 1879.

The incandescent lamp had many inventors. Warren de la Rue made a platinum-coil lamp in a vacuum in 1840, too costly to use. In England, Joseph Swan experimented with carbonised paper filaments from about 1850, but his vacuums were too poor. When Hermann Sprengel's mercury pump (1865) made good vacuums possible, Swan returned to the problem and showed working carbon lamps in Newcastle upon Tyne early in 1879. In New Jersey, Thomas Edison's team made a carbonised cotton thread glow for about 13 hours in October 1879, and by 1880 had carbonised bamboo filaments lasting over 1,000 hours. In 1880 Cragside, the Northumberland house of William Armstrong, became one of the first homes lit by electric bulbs — Swan's lamps, powered by a dynamo driven by water from the estate's lakes. Edison and Swan later joined forces in Britain as the "Ediswan" company.

Source: content/entries/electricity/light-bulb.md