Part 8 · Chemistry
Burners, Stands and Laboratory Equipment
The metal, wood and paper hardware that holds, heats, filters, spins and dries the glassware of a laboratory — the Bunsen burner, spirit and paraffin blowlamps, retort stands and clamps, tripods and wire gauze, filter paper, the hand centrifuge, water baths, drying ovens, desiccators and test-tube racks — and how to make each from the materials of a village workshop.
- Difficulty
- ●●●●●
- Time
- An afternoon for a rack, tripod or gauze; a day or two for a burner, stand or oven; a week for a geared centrifuge
- Steps from zero
- 32 prerequisites →
This unlocks
—The full path from nothing — 32 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- The Kiln
- Pottery
- Charcoal
- Hides and Leather
- Lime
- Bricks
- Lye and Potash
- The Wheel and Axle
- Glass
- Firebrick and Refractories
- Bellows
- Gears
- Iron (the Bloomery)
- Copper Smelting
- Laboratory Glassware
- The Waterwheel
- Blacksmithing
- Magnets
- Sheet Metal and Rolling
- Copper Wire
- The Generator
- The Electric Arc Furnace
- Calcium Carbide and Acetylene
- Welding
- Metal Pipes and Tubes
- Burners, Stands and Laboratory Equipment
Do them roughly in this order. See it on the tech tree →
Why it matters
Glassware (Laboratory Glassware) is only half a laboratory. A flask must be held over a flame without being touched; a precipitate must be filtered, dried at a steady temperature, cooled without picking up damp, and weighed; a cloudy liquid must be spun. Plain hardware — iron rods, rings, wire, wood and paper — does all this, and it is what turns the recipes of Identifying Substances, Making Medicines and Culturing Microbes into work that gives the same result twice. The same burners solder and braze (Soldering and Brazing) and lead to gas lamps (Lanterns, Gas Lamps and Lighters).
How it works
Clean, hot flames come from mixing air with the fuel before it burns. A candle burns only where its vapour meets air at the edge of the flame; the starved middle leaves glowing soot — a yellow, smoky flame of about 1,000 °C. Gas mixed with air first burns all at once in a small, roaring blue cone with no soot, at up to about 1,500 °C. In a Bunsen burner or blowlamp, a jet of gas shooting through a tube drags the air in with it.
Even heat comes from heating something in between. Glass cracks where a flame touches one spot; gauze, sand or water spreads the heat, and water never gets hotter than 100 °C. A desiccant — quicklime, calcium chloride, strong sulfuric acid, silica gel — holds water more tightly than the thing you are drying, and in a sealed jar pulls the last moisture out of it. Spinning makes a tube feel a push outwards hundreds of times stronger than gravity, so fine particles that take a day to settle sink in minutes.
What you need
| Item | Use | Where it comes from |
|---|---|---|
| Brass or copper tube 10–12 mm bore, sheet brass | Burner bodies, jets | Metal Pipes and Tubes, Zinc and Brass |
| Iron rod 8–12 mm; iron wire 0.3–2 mm | Stands, rings, tripods, gauze | Blacksmithing, Iron and Brass Wire |
| Cast iron, stone; sheet iron | Bases; ovens, baths | The Blast Furnace and Cast Iron, Sheet Metal and Rolling |
| Hardwood, cork, leather, fireclay | Racks, clamp jaws, triangles | Basic Woodworking, Firebrick and Refractories |
| Cotton or linen rags | Filter paper | Paper |
| Fuel gas, spirit or paraffin | Burners | Coal and Coke, Biogas and Wood Gas, Distillation, Petroleum and Refining |
Where to find it
Almost everything here is made, not found. Fuel gas — coal gas (Coal and Coke), biogas (Biogas and Wood Gas) or producer gas — reaches the burner through a rubber hose (Rubber). Desiccants come from Lime, Hydrochloric Acid, Sulfuric Acid and Water Glass (Sodium Silicate). Cobalt ore, with its pink crusts of cobalt bloom (Nickel and Cobalt), makes the colour-change paper for desiccators.
The Bunsen burner
What it is
A gas burner with an adjustable air inlet at its base: a twist of the collar turns its flame from a soft yellow glow to a roaring blue cone. It is the standard heat of every laboratory.
Making it
- Base. A heavy disc or square, 8–10 cm across and at least 500 g so the hose cannot tip it: cast iron (Metal Casting), a lead-weighted block or a drilled stone.
- Gas inlet and jet. Braze a ridged side tube for the hose into a brass block on the base. The gas turns upwards through a jet: a brass plug drilled with one hole of about 0.8 mm (Drills and Boring). Open it up a little at a time if the flame is too small for your gas.
- Tube. A brass or copper tube of 10–12 mm bore, 10–13 cm long — long enough for gas and air to mix — pushed tightly over the jet block.
- Air holes and collar. Drill two opposite holes of 6–8 mm in the tube, level with the jet. A snug sleeve of sheet brass with matching holes opens or closes them as it turns.
- Test. Light the gas with the collar closed, then slowly open it.
Using it
Collar closed: a sooty yellow flame, about 1,000 °C — leave it like this while idle, because it is easy to see. Collar open: a pale outer flame with a sharp blue inner cone 1–3 cm tall. The hottest point is just above the tip of the inner cone, about 1,500 °C; a thin iron wire there glows bright orange at once. Inside the cone is unburnt gas that pulls oxygen from hot metal oxides (a reducing flame — see Identifying Substances).
The Meker burner has a wider tube (18–20 mm), a bigger jet and a wire-mesh grid across the top that splits the flame into many small cones: a broad, even heat of about 1,600 °C for crucibles and borax fusions (Borax and Boric Acid).
How to tell a good one
A steady roar; a sharp blue cone with no yellow tips; the flame sits on the tube mouth and stays lit with the gas turned down by half. If it strikes back — burns down at the jet with a small green flame and a whistle — turn off the gas, let it cool, close the collar a little and relight. If it lifts off and blows out, there is too much gas or air.
Blowlamps and blowtorches
Without piped gas, liquid fuel can be turned into vapour and burned the same way. Here a blowlamp is a small self-heating spirit lamp for the bench; a blowtorch is a pressurised paraffin torch for soldering and plumbing.
The spirit blowlamp
- Make a closed copper boiler about 6 cm across and 4 cm deep, every seam brazed — never soft-soldered, which melts if it boils dry. Fit a filler plug with a safety valve: a cone seat held down by a light spring.
- From the top, lead a 3 mm copper tube over and down to a nozzle with a 0.5 mm hole, aimed sideways.
- Under the boiler set a wide-wicked spirit lamp (Laboratory Glassware) whose flame both heats the boiler and sits in front of the nozzle.
- Fill the boiler no more than half full of strong spirit and light the lamp. In a minute vapour jets from the nozzle, catches in the lamp flame, and roars out as a blue flame 10–15 cm long, hot enough to melt thin glass rod and silver solder.
Test a new lamp with water first: steam should hiss from the valve long before the boiler swells.
The paraffin blowtorch
A brazed brass tank of 0.5–1 litre carries a filler cap, a small hand pump with a cup-leather piston and non-return valve (Pumps), and a pressure release. A riser from the bottom of the tank leads fuel to a vaporiser loop lying in the flame, then back to a nipple drilled 0.3–0.4 mm, aimed down a short burner tube with air holes at its back. A priming cup sits under the vaporiser.
Fill the tank three-quarters full — the air space keeps the pressure steady. Burn a spoonful of spirit in the priming cup; when the vaporiser is hot, pump five to ten strokes and open the valve. Fuel turns to vapour in the hot loop and roars out as a blue flame. A yellow, spitting flame means the loop was not hot enough: shut off, release pressure, prime again.
Danger A blowtorch tank holds a flammable liquid under pressure next to a flame. Never open the filler of a hot or burning torch, over-pump it, or use one that leaks. Release the pressure before putting it away. If the tank becomes too hot to hold, back away and let it burn out; keep sand, not water, at hand.
Retort stands, clamps and rings
A retort stand is a vertical iron rod on a heavy base. On it slide boss heads — small blocks with two holes at right angles and a thumbscrew in each — that hold clamps (jaws for flask necks, tubes and condensers) and rings (iron circles for funnels, dishes and gauzes). Two stands hold a whole distillation train.
- Base: a cast-iron plate about 15 × 25 cm and 2–3 kg, or a board weighted with stone or lead, tapped or socketed near one end for the rod.
- Rod: smooth round iron 10–12 mm thick and 50–75 cm long.
- Boss head: a block of iron or brass about 3 cm square with two offset holes at right angles, each with a thumbscrew — a screw with a wing head that fingers can turn (Screws, Nuts and Bolts). A wooden block locked with wedges works too.
- Clamp: two curved jaws of flat iron riveted on a pivot and closed by a thumbscrew, on a 15 cm rod. Line the jaws with cork or leather — never let bare metal grip glass — and clamp the neck of a flask, never its body.
- Ring: a circle of 6 mm iron rod, 7–12 cm across, forge-welded to a short rod.
A stand is good when a filled 1-litre flask clamped at the top of the rod can be tilted 15° without the stand tipping, and the clamps hold without creeping down over an hour.
Tripod, wire gauze and pipeclay triangle
- Tripod: a ring of 8 mm iron rod about 10–12 cm across, with three legs of the same rod 18–22 cm long, splayed slightly. Match its height to your burner: the gauze should sit about 1 cm above the tip of the blue inner cone.
- Wire gauze: a square 12–15 cm of iron wire mesh — wire about 0.4–0.5 mm thick with openings of about 1 mm — woven on a small frame like cloth (Spinning and Weaving Cloth), as for sieves, with the edges bound in thicker wire. It spreads the flame over a wide patch so glass on it heats evenly and does not crack. A dab of fireclay dried into the centre spreads it further; never use asbestos.
- Pipeclay triangle: three short pieces of clay pipe stem (Tiles and Clay Pipes) or fired fireclay tube, threaded on iron wire twisted into a triangle about 6 cm on a side. It rests on the tripod ring and holds a small crucible directly in the flame.
Filter paper
Filter paper is a soft, thick, porous paper of pure cellulose with no size (no glue, starch or alum), so liquids run through and fine solids do not. Make it as rag Paper, but: use only white cotton or linen rag boiled in weak lye; beat the pulp less, so the long fibres leave an open, fast sheet (beat longer for a slow, fine one); and press thick sheets only lightly and add no size. For ashless paper, to be burnt with its precipitate and weighed, soak the sheets a day in water with a few drops of Hydrochloric Acid per litre and wash well.
Cut circles 9, 11 and 15 cm across. Fold in half and in half again, open into a cone, set it in a 60° funnel and wet it so it clings; for speed, pleat it like a fan.
A good paper passes 100 ml of water in one minute (fast) to five or more (fine), turns muddy clay water perfectly clear, and holds together wet when lifted by a corner. Without paper, use a plug of cotton wool, tight linen or felt.
The hand centrifuge
A centrifuge whirls tubes so that solids, cells or droplets are flung to the bottom in minutes. It collects fine precipitates, clears cloudy liquids, and separates blood and urine (Examining a Patient, The Medical Laboratory) and microbes (Culturing Microbes).
- Drive. A hand crank and gears or a belt (Gears, Belts, Chains and Power Transmission) with a step-up of 12 to 20 times, so 1½ turns of the crank a second give 1,000–1,800 turns a minute. A geared hand drill or egg beater has the right parts.
- Head. On a vertical spindle in two good Bearings and Lubrication, fix a cross of flat iron carrying two or four swinging buckets — metal cups hanging on pins, padded with cork, that swing out flat as the head speeds up.
- Radius about 10–15 cm to the bottom of a swung-out tube. At 1,500 turns a minute and 10 cm, the tube feels about 250 times gravity — enough for nearly any precipitate or blood cells.
- Guard. Bolt it to the bench inside a strong drum with a lid: a breaking tube becomes a projectile.
Always balance it: tubes in opposite pairs, weighed equal to within 1 g. An unbalanced head shakes and can tear loose. Never stop it by hand.
Without gears, a card disc 10 cm across on a loop of string through two holes near the centre — a button whirligig — spins very fast as the string is pulled and relaxed, and separates blood in sealed capillary tubes taped to it in a few minutes.
Water baths and sand baths
A water bath is a covered pot of water, heated from below, with holes in its lid. Over each hole sits a set of loose, nesting concentric rings of sheet metal, so you can fit the opening to any dish, flask or beaker. It heats glass evenly up to 100 °C and never higher, and evaporates solutions without spitting or scorching. Make it of copper or tinned sheet iron, 15–20 cm across. For long evaporations, keep the level constant with a bottle of water stood upside-down in a side cup joined to the bath at the water line: as the level falls, air bubbles in and water runs out. For a steady lower temperature — 37 °C for cultures, 70 °C for creams — keep the flame small and watch a The Thermometer in the bath.
A sand bath — an iron dish of fine dry sand over the fire — goes to 300 °C and more.
The drying oven
A drying oven is a small box held at a steady temperature, usually 100–110 °C, to dry precipitates, salts and glassware completely before weighing.
- Water-jacketed oven. A box of tinned sheet iron or copper with double walls 2–3 cm apart, the gap part-filled with water and vented so steam escapes. Heated from below, the boiling jacket holds the chamber at about 98–100 °C with no attention at all. Fit wire-mesh shelves, a door, and small vents top and bottom.
- Air oven (105–200 °C). A sheet-iron box about 30 cm each way, its double walls packed with ash or glass wool, over a burner or on the back of a stove, with a bottom vent for fresh air, a top vent with a slide, and a thermometer through a cork in the top. Adjust the flame until the reading holds.
A good oven holds its thermometer within ±5 °C for half an hour untouched, and dries a wet filter paper in 20 minutes without browning it; browning means a hot spot — add a baffle plate above the flame.
The desiccator
A desiccator is a sealed jar with a desiccant in the bottom and a perforated shelf above. A hot crucible cooling on the bench gains weight from the damp air; one cooled in a desiccator does not. It also stores things that soak up water, such as caustic soda.
- Jar: a heavy glass jar or glazed stoneware pot, 15–20 cm across, with rim and lid ground flat with emery (Laboratory Glassware). Grease the rim thinly with tallow and beeswax, 4 to 1: the lid should look clear all round and slide sideways with a firm push.
- Shelf: a perforated disc of glazed clay or sheet metal a third of the way up.
- Desiccant in a dish beneath:
| Desiccant | How to make it | Notes |
|---|---|---|
| Quicklime | Fresh lumps from the kiln (Lime) | Cheap; replace when it crumbles |
| Fused calcium chloride | Limestone dissolved in hydrochloric acid, boiled down, the crust heated to about 250 °C | Strong; reheat when it turns liquid |
| Strong sulfuric acid | Sulfuric Acid | Strongest; dangerous to carry |
| Silica gel | Water Glass (Sodium Silicate) | Clean, reusable: dry at 150 °C |
- Indicator: dip a strip of filter paper in a weak solution of cobalt chloride (roasted cobalt oxide dissolved in hydrochloric acid — Nickel and Cobalt; never raw cobalt bloom, which carries arsenic) and dry it in the oven: it turns blue. Kept in the desiccator, it stays blue while the air is dry and turns pink when the desiccant is spent.
Let a red-hot crucible cool a minute in air before it goes in, and after a few seconds open the lid a crack to let out the expanded air, or it may stick fast.
Test-tube racks
A test-tube rack holds tubes upright and in order, with pegs to dry them upside-down. Make it of hardwood: two boards about 25 × 8 cm, held 6–8 cm apart by end pieces. Bore the top board with six or twelve holes a few millimetres wider than your tubes (about 20 mm for 16 mm tubes) at 30 mm centres. Bore the lower board with shallow sockets directly beneath, so tubes stand straight. Along the back of the top board fix a row of wooden pegs 6–8 cm long to hang washed tubes on. Wax the wood against spills and burn numbers beside the holes. A good rack stands steady when full and holds tubes upright without leaning.
Dangers
Danger Gas, flame and pressure. Coal gas, producer gas and biogas can poison (carbon monoxide) and explode. Light the match before turning on the gas, never the other way round. Check hoses for cracks by brushing them with soapy water and watching for bubbles. Turn off at the supply tap, not just the burner. Pressurised blowtorches and closed spirit boilers can burst: use brazed seams, safety valves and never overfill.
- Burns. Hot iron and hot glass look exactly like cold iron and glass. Handle anything that has been near a flame with tongs, and put hot things down only on a tile or stone.
- Centrifuges fling glass if a tube breaks or the head is unbalanced: guard, balance and never touch the moving head.
- Desiccators can implode if pumped out or cooled too fast with a hot item inside; wrap them in cloth tape when new. Strong sulfuric acid in them burns.
- Cobalt chloride is poisonous and can cause skin allergy. Handle the paper with tongs, keep it away from food, and wash your hands after making it.
- Spilled spirit near a burner flashes into flame across the bench: keep fuel bottles away from flames and stoppered.
How to tell it worked
Each section above gives a test. The sign of a working laboratory: you can set up a flask over a flame, hold a condenser, filter, dry and weigh a precipitate, all without anyone holding anything by hand, and get the same weight twice.
Note Troubleshooting.
- Bunsen flame yellow even with the collar open → jet too large or collar holes too small; fit a smaller jet or widen the holes.
- Flame strikes back when turned down → jet too small for the gas, or too much air; close the collar a little at low settings.
- Blowtorch spits liquid fuel → coil not hot enough; shut off, release pressure, prime longer.
- Filter paper clogs at once → pulp beaten too much, or the precipitate too fine; let it settle, pour the clear liquid through first, or use the centrifuge.
- Precipitate keeps gaining weight → not cooled in the desiccator, or the desiccant is spent (pink cobalt paper).
- Centrifuge shakes → tubes unbalanced, or a bucket not swinging freely.
Going further
With a steady gas supply, a laboratory can add blast lamps — a Bunsen-type burner fed with air from a foot bellows for glassworking (Laboratory Glassware, Scientific Glassblowing and Glass-to-Metal Seals) — and, with Hydrogen, Oxygen and Gases, an oxy-hydrogen flame hot enough to melt platinum and quartz. A thermostat (Thermostats and Automatic Control) — a bimetal strip or a mercury contact that turns the gas down — holds ovens and incubators within a degree. A motor-driven centrifuge (The Electric Motor) reaches several thousand turns a minute. And the same careful hardware, scaled up, becomes the stills, filters and driers of chemical works.
How it was first done
Alchemists and apothecaries used sand baths, water baths (bain-marie), furnaces, funnels and filters of cloth for two thousand years. Swedish chemist Jöns Jacob Berzelius, in the early 1800s, set the standard for careful analytical work, with fine Swedish filter paper and an improved spirit lamp still called the Berzelius lamp. Early gas burners gave a smoky, luminous flame; Robert Bunsen and his instrument maker Peter Desaga at Heidelberg perfected the burner with its adjustable air inlet in 1855, for the new town gas, and used its clean flame for the flame spectroscopy that found new elements (The Spectroscope). Carl Richard Nyberg in Sweden made the paraffin blowlamp in 1882. The French chemist Georges Méker introduced his wide, gridded burner early in the 1900s. Hand centrifuges came from the dairy — Gustaf de Laval's cream separator of 1878 — and were soon used for blood and urine; in 2017, Manu Prakash's group at Stanford showed that a paper whirligig on strings, the "paperfuge", can spin blood samples for diagnosis with no electricity at all.
Source: content/entries/chemistry/laboratory-equipment.md