◆ Rebuild

Part 3 · Metals

Arsenic

Arsenic is the hidden poison in many copper, tin, gold, cobalt and silver ores, and in some well water. This chapter teaches you to recognise arsenic minerals and contaminated ore, explains why roasting them is deadly, and shows how to protect workers, children and water. It also covers arsenic's long history of use — and why you should not repeat it.

Difficulty
●●●●●
Time
Seconds to test a rock; a day to lay out a safe roasting site; a lifetime of good habits
Steps from zero
1 prerequisite →

You need first

Finding and Identifying Ores

This unlocks

—
The full path from nothing — 1 step before this one
  1. Finding and Identifying Ores
  2. Arsenic

Do them roughly in this order. See it on the tech tree →

Why it matters

You will probably never want arsenic. But you will meet it, because it hides inside the ores of metals you do want. Many copper ores carry it. So do many tin ores, most cobalt ores, a lot of gold-bearing rock, and some lead, silver and nickel ores. When those ores are roasted or smelted, the arsenic does not stay in the furnace: it rises as a white smoke, drifts downwind and settles as a fine white dust on everything — plants, water, roofs, food, skin.

The smoke can kill quickly. The dust and contaminated water kill slowly, over years. Whole mining districts in history were poisoned this way, and in our own time tens of millions of people in South and South-East Asia have drunk arsenic in well water without knowing it.

This chapter is about recognition and protection. Learn to spot arsenic in a rock in a few seconds, sort it out of your ore, lay out your works so the smoke never reaches homes or water, and know the signs of poisoning. Read it before you roast any ore in Finding and Identifying Ores, Copper Smelting, Tin and Pewter, Gold and Silver or cobalt for glazes.

How it works

Arsenic is an element that behaves halfway between a metal and a non-metal. In rocks it is almost always combined with sulfur, iron, copper, cobalt or nickel. Three facts make it dangerous:

  1. It turns to vapour easily. When arsenic-bearing ore is heated in air, the arsenic burns to arsenic oxide ("white arsenic"). This oxide goes off as a vapour well below red heat, and condenses again into a fine white powder as soon as the smoke cools. It does not stay in your furnace; it stays in your lungs, your fields and your water.
  2. It is very poisonous. About a tenth to a quarter of a gram of white arsenic — less than a pinch of salt — can kill an adult. Much smaller amounts, swallowed or breathed day after day, cause skin disease, nerve damage, cancers and heart disease after years.
  3. It has no taste and no colour in water or food. The only warning you get is in the rock itself, and in the smoke: a smell of garlic.

Arsenic also dissolves slowly out of mine waste, slag heaps and roasting ash when rain soaks through them, and it occurs naturally in the groundwater of some regions, especially deep wells in the young muddy sediments of great river deltas.

What you need

Nothing has to be made for this chapter. For safe prospecting and roasting you need:

Item Why
A steel hammer or a steel striker For the strike test (Blacksmithing)
A flat stone and a small fire, or a hot iron plate For the heat test, outdoors
A long-handled iron spoon or tongs, 60 cm or more To hold a sample at arm's length
Separate work clothes and a head cloth Kept at the works, never worn home
Water, soap, a basin Washing hands and face before eating (Soap)
Damp cloth masks Against dust only — they do not stop fumes
Stakes, paint or carved signs To mark poisoned ground and water

Where to find it

Arsenic minerals form in hydrothermal veins (where hot water once rose through cracks), often with quartz, and in the same districts as copper, tin, gold, silver, cobalt and antimony. Learn these:

Mineral What it looks like Key tests
Arsenopyrite (mispickel) Silver-white to steel-grey, bright metallic, in sharp wedge or diamond-shaped crystals or grainy masses, often in quartz Hard: scratches glass, a knife barely marks it. Struck with steel it smells of garlic. Streak dark grey-black. Whiter than pyrite, which is brassy yellow
Realgar Bright red to orange-red, resinous (like glossy toffee), soft Scratched by a fingernail. Orange-red streak. Crumbles to yellow-orange powder after months in daylight
Orpiment Lemon to golden yellow, pearly, in flexible flakes or crusts, often with realgar Very soft, flakes bend like mica. Yellow streak
Grey copper ore (tetrahedrite, tennantite) Steel-grey to iron-black metallic masses, sometimes small three-sided pyramids, in copper and silver veins Brittle; streak black to reddish-brown. Often with chalcopyrite. Gives garlic smoke when heated
Cobalt and nickel ores (skutterudite, cobaltite, nickeline) Tin-white, silver-grey or pale copper-red metallic masses Heated, give garlic smoke. Weather to pink or green crusts (below)
Weathering signs Pink to purple crusts (erythrite, "cobalt bloom"); apple-green crusts (annabergite, "nickel bloom"); pale green to blue-green or brownish crusts and nodules (scorodite) in rusty gossan All mean arsenic in the rock beneath

Where else arsenic hides:

  • Gold-bearing quartz with fine grey metallic grains: very often arsenopyrite.
  • Tin gravels and lodes in some districts; check the black heavy concentrate for silvery grains (Tin and Pewter).
  • Old mine dumps and roasting sites: grey, yellow or rusty spoil where nothing grows.
  • Hot-spring deposits: yellow and red crusts around vents.
  • Salvaged materials (if you are rebuilding among ruins): greenish-tinted treated timber from fences, decks and poles (CCA — copper, chromium and arsenic); old rat and insect poisons, sheep dips and weedkillers; bright green paints and wallpapers from the 1800s; some old glass and stuffed animals. Never burn treated timber. Its ash and smoke carry arsenic.
Arsenopyrite silver-white crystals, about as hard as steel; struck with steel it smells of garlic Realgar red-orange, glossy, soft as a fingernail; crumbles yellow in daylight Orpiment lemon-gold, pearly flakes that bend; often with realgar Grey copper ore steel-grey to black, in copper and silver veins; garlic smoke when heated Blooms pink-purple crust: cobalt + arsenic; pale green crust: nickel or scorodite The garlic rule Any rock that smells of garlic when struck or heated carries arsenic. Treat the whole heap as poisonous.
Fig. 1 Five warning signs. Learn these and you will catch most arsenic-bearing rock before it reaches the fire.

Method 1: Testing a rock

Test every new ore, from every new place. Do it outdoors.

  1. Look. Silver-white crystals that are whiter than pyrite and harder than galena; red or yellow soft minerals; pink or apple-green crusts. Any of these is a warning.
  2. The strike test. Strike the rock sharply with a steel hammer, or strike the hammer's edge across it, and sniff gently — from 30 cm, not with your nose on the rock. A smell of garlic (sometimes described as like hot onions) means arsenopyrite. It is faint and lasts a second; try a few blows.
  3. The heat test. Put a chip the size of a rice grain — no bigger — on a stone or iron plate on a small fire, or hold it in a long iron spoon in the flame, and step back upwind at once, at least 3 m. White smoke with a garlic smell, perhaps a white bloom forming on a cool surface nearby, means arsenic. Let the fire burn out, and bury the stone. Do not scrape up or keep the white deposit: it is the poison itself.
  4. Record it. Mark that outcrop and that ore heap as arsenic-bearing, in writing and with a sign.

Warning Sulfur-bearing ores also smoke when heated, but sulfur smoke is choking and sharp, like a struck match, and blue-grey. Arsenic smoke is white and smells of garlic. Many ores give both. Either way, stay out of it.

Method 2: Getting arsenic out of your ore before the fire

The best protection is never to heat arsenic in the first place.

  1. Choose clean ore. If one copper or tin outcrop smells of garlic and another does not, work the clean one, even if it is farther away or poorer. Oxidised copper ores (green malachite, blue azurite — Finding and Identifying Ores) are usually far cleaner than grey sulfide and grey copper ores.
  2. Hand-pick. Break the ore to walnut size on a sorting floor and pick out every piece with silvery arsenopyrite or grey copper ore. Work in good daylight, wearing gloves or with hands washed often.
  3. Wash it. Arsenopyrite is heavy (about 6 times water), so it concentrates with tin and gold in panning — washing does not remove it, but it does let you see it. Look at your heavy concentrate in sunlight for silvery-white grains.
  4. Keep the rejects safe. Pile the picked-out arsenic rock in one place, on a clay floor, under a roof or covered with clay, well away from water. Do not throw it in a stream or spread it on paths.

Method 3: If you must roast arsenic-bearing ore

Sometimes there is no other ore. Then treat roasting as the dangerous industry it is.

Usual wind directionroast only when it blows from the village toward the works Village, gardens, wells Wellupstream and uphill at least 500 m ground slopes down this way No homes, food or grazing Long flue to chimneydust settles inside;never open unprotected Stream flows away from the villageno drinking or fishing below the works Roasting hearthsmoke goes into the flue Settling pondfor ore-wash water Waste on clay padditch round it
Fig. 2 Laying out a roasting site. The prevailing wind carries smoke away from homes, fields and water; the hearth stands below the wells and above nothing anyone drinks; waste is stored on a clay pad with a ditch round it.
  1. Place it right. At least 500 m downwind (in the usual wind) of any home, school, animal pen, vegetable garden or grain store. Downhill and downstream of every well and spring, and not on ground that drains toward a stream anyone drinks from or fishes in. Never in a valley bottom where smoke pools on still evenings.
  2. Watch the weather. Roast only on days with a steady breeze blowing from the village toward the works. Never on still, foggy or rainy days, when the smoke hangs low.
  3. Use a long flue. Build the roasting hearth at the foot of a slope and lead its smoke through a long, covered clay or stone flue running uphill to a chimney (Chimneys, Stoves and Heating). The longer the flue, the more of the white dust settles inside it instead of on the countryside. Historic works ran flues hundreds of metres long. Never open a flue to clean it without full protection: the deposit in it is nearly pure poison. If you cannot protect the cleaners, seal and bury the flue when the works close.
  4. Few people, short shifts. Only adults, never children or pregnant or nursing women. Stand upwind. Rotate workers so no one does it day after day for months.
  5. Contain the waste. Roasted ore, ash and slag go on a pad of rammed clay with a ditch round it, covered with more clay at the end of each season. Do not use roasting ash or slag for bricks, paths, fill, fertiliser or children's play.
  6. Close it properly. When a site is finished, cap it with 30–50 cm of clay and soil, plant grass (not food), and mark it with stones that will last.

Protecting workers

These habits matter more than any equipment:

  • Wash before you eat, drink or smoke, every time. Arsenic on the hands goes into the mouth.
  • Never eat, drink or keep food at the works.
  • Work clothes stay at the works and are washed there, not at home with the children's clothes.
  • Damp methods. Sprinkle ore and sorting floors with water to keep dust down. Sweep only when damp.
  • Damp cloth over nose and mouth for dusty work. Be honest about what it does: it stops some dust, and nothing of the fumes.
  • No children at mines, sorting floors, roasting sites or waste heaps, ever. They breathe more for their size, put their hands in their mouths, and are harmed most.

Protecting water

  • Do not draw drinking water downstream of mines, ore-washing floors, roasting sites or waste heaps, or from water flowing out of old mine tunnels, however clear it looks. Orange-stained, very clear water from old workings is a warning, not a recommendation.
  • Wash ore in a separate channel whose water soaks into a settling pond, not straight back into the stream.
  • Be wary of deep wells in great river deltas and low muddy plains. Some regions — Bangladesh and West Bengal, parts of Vietnam, Cambodia, China, Argentina, Chile, Mexico and the United States among them — have natural arsenic in groundwater. Without chemical testing you cannot know. Prefer rainwater from clean roofs (Wells and Cisterns), treated surface water (Water Treatment for a Town), and shallow dug wells, which in those regions are often lower in arsenic than deep tube wells.
  • Iron helps. Arsenic sticks to rust. Where you must use doubtful water, a simple filter of coarse sand mixed with iron filings or rusty nails, above a layer of sand and charcoal, removes much of it. Use two or three stacked clay pots with small holes, the top one holding the iron and sand, the middle one sand and charcoal, the bottom one collecting. Change the iron and sand every few months. This reduces arsenic; it is not proof of safety.
  • Testing water for arsenic needs chemistry, not eyesight — see Identifying Substances. Until you can test, choose sources by where they come from.

How to tell you are safe — and when you are not

There is no instrument-free test for arsenic in a person. Watch for these signs:

Acute poisoning (a large dose, within minutes to hours): burning throat, vomiting, severe watery diarrhoea (sometimes like rice water), stomach cramps, garlic smell on the breath, cold sweat, then collapse. This needs immediate care: get the person out of the smoke, give water and oral rehydration fluids (Oral Rehydration), keep them warm, and get help (Emergencies). Many people die of the fluid loss; replacing it saves some.

Slow poisoning (small doses over months or years):

  • Skin: dark freckling or "raindrop" spots on the chest and back, alternating with pale spots; hard, warty, thickened patches on the palms and soles.
  • Nails: white bands running across all the fingernails.
  • Nerves: tingling, burning or numbness in the hands and feet, then weakness.
  • Tiredness, anaemia, stomach upsets; years later, cancers of the skin, lung and bladder, and heart disease.

If anyone at the works shows these, stop the exposure at once. Many of the skin and nerve signs slowly improve once the arsenic stops.

Note Troubleshooting. The garlic smell is faint and you are not sure → assume arsenic. Test more pieces from the same ore; if any smell, treat the whole heap as arsenic-bearing. Your only copper ore is grey and smells of garlic → look harder for green oxidised copper ore in the upper weathered zone of the same deposit, or a different deposit. Use the arsenic ore only with the roasting rules above. Plants die and animals sicken downwind of the works → the smoke is reaching them. Stop, move the works or lengthen the flue. Workers have tingling hands or rough palms → stop their exposure, check their hand-washing, and check what water they drink. Copper from your ore is brittle and greyish → it may carry arsenic. Fire-refine it outdoors (Copper Wire) and stand upwind.

Dangers

Danger Arsenic smoke kills. The white smoke from roasting or smelting arsenic-bearing ore, and the white dust it leaves, is among the deadliest poisons in this book. Never roast or smelt ore in a closed building, a valley bottom or near homes. Stand upwind. Keep children far away.

Danger Arsine gas. When metal or ore containing arsenic meets acid that is giving off hydrogen — for example zinc, iron or scrap being dissolved in acid to make hydrogen (Hydrogen, Oxygen and Gases) — it can release arsine, a colourless gas with a faint garlic smell. A few breaths can destroy the blood; the urine turns red-brown hours later, and many victims die of kidney failure. Make hydrogen only from clean metal, outdoors or with strong ventilation, and stop at once at any garlic smell.

  • Do not make or keep arsenic compounds. In the past they were used as pesticides, wood preservatives, pigments and medicines, and they poisoned users, makers and children for centuries. Every job they did in a rebuilt world has a safer route (below).
  • Do not eat anything grown on or below a roasting site or mine dump, and do not graze animals there.
  • Old green paint and wallpaper, treated timber and old pesticide stores: do not burn, sand or scrape them. Bury them under clay and mark the place.

What this unlocks — and what to use instead

Knowing arsenic lets you use the ores you need safely: Copper Smelting, Tin and Pewter, Gold and Silver, cobalt for Glazes, and the sulfide ores of Lead and antimony. It also guides where to dig wells (Wells and Cisterns) and site a Mining and Tunnelling camp.

Safer substitutes for arsenic's old jobs:

Old use Use instead
Hardening copper ("arsenical bronze") Tin bronze (Bronze) or brass (Zinc and Brass)
Yellow and red pigments (orpiment, realgar) Yellow and red ochres, lead-free yellows (Pigments, Paints and Varnish)
Green pigments (Scheele's green, Paris green) Green earth, malachite, copper-free greens mixed from blue and yellow
Wood preservation Tar and creosote (Tar, Pitch and Glue), good design that keeps wood dry
Rat and insect poison Traps, cats, sealed stores (Granaries and Food Storage, Pests and Plant Diseases)
Medicines Proper medicines (Making Medicines)
Preserving animal skins Salt and tanning (Hides and Leather)

How it was first done

Arsenic was in use long before anyone knew it as a substance. The first copper alloys of the Near East, from about 4000 BC, were often arsenical copper, made — perhaps by accident — from arsenic-rich ores; it is harder than plain copper and was widely used for a thousand years or more before tin bronze replaced it. Orpiment and realgar were prized pigments in Egypt, Mesopotamia, China and medieval Europe, and arsenic compounds appear in Greek, Chinese and Indian medicine.

White arsenic became notorious as a poison in Renaissance Europe — tasteless, easy to buy, and with symptoms like cholera. In 1836 the English chemist James Marsh devised the first reliable test for arsenic in a body, and poisoning trials changed for ever. The 1800s brought arsenic everywhere: Scheele's green (1775) and Paris green in wallpapers, paints and sweets; arsenical sheep dips and pesticides; Fowler's solution as a tonic. Paul Ehrlich's Salvarsan (1909), an arsenic drug against syphilis, was the first modern targeted medicine, and an arsenic compound is still used today in hospitals against one kind of leukaemia — under careful medical control. The groundwater disaster of Bangladesh and West Bengal, discovered in the 1980s and 1990s after millions of tube wells had been sunk to avoid germ-laden surface water, is the reminder that arsenic can be in the water as well as the rock.

Source: content/entries/metals/arsenic.md