Part 13 · Electricity
Electric Kettles, Irons, Heaters and Cookers
Push a current through a wire that resists it and the wire gets hot. Wound from nichrome and held on mica, fired clay or packed magnesia, that wire becomes the heating element inside every electric kettle, iron, toaster, room heater, hot plate, cooker, immersion heater and hair dryer. How to size, wind and insulate elements, how to build each appliance, and the earthing and cut-outs that stop them killing anyone.
- Difficulty
- ●●●●●
- Time
- An afternoon to wind and test an element; a few days for an iron, toaster or heater; two to three weeks for a sheathed-element kettle or a cooker
- Steps from zero
- 26 prerequisites →
This unlocks
Electric Kilns and FurnacesThe full path from nothing — 26 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- Charcoal
- Pottery
- Hides and Leather
- Salt
- Fermentation
- The Wheel and Axle
- Bellows
- Gears
- Copper Smelting
- Iron (the Bloomery)
- The Waterwheel
- Blacksmithing
- Magnets
- The Battery
- Copper Wire
- Electrolysis
- Nickel and Cobalt
- The Generator
- Wiring and Electrical Safety
- Electric Kettles, Irons, Heaters and Cookers
Do them roughly in this order. See it on the tech tree →
Why it matters
A The Light Bulb wastes nine-tenths of its power as heat. A heating appliance wastes none: every watt that goes in comes out as heat, exactly where you want it, with no smoke, no ash, no fuel to carry and no fire to tend. A 1,000 W element gives as much heat as a small wood stove, on the turn of a switch, in a room with no chimney.
Boiling water for washing, cooking and Sterilising Instruments and Dressings stops costing an hour of wood-chopping. Ironing stops meaning a row of sad irons heating on a stove. A sick room or a chick brooder stays warm all night. The same elements heat The Kilns, glue pots and soldering irons.
The cost is power: a kettle takes as much as twenty lamps. Be sure your The Generator, Power Lines and Distribution and wiring (Wiring and Electrical Safety) can carry the load.
How it works
Heat from resistance
Every wire resists the current a little, and the resisting turns electric energy into heat (Joule's law):
heat (watts) = volts × amps = volts² ÷ resistance (ohms)
So on a fixed supply, less resistance means more heat: 230 V across 53 Ω gives 1,000 W; across 106 Ω, 500 W. On 110 V, 1,000 W needs only 12 Ω. Work out the resistance first, then cut the wire to length:
resistance needed = volts² ÷ watts → length of wire = resistance needed ÷ ohms per metre
Choosing the wire
A heating wire must have high resistance (so you need metres, not kilometres), must not burn away when hot in air, and must keep the same resistance as it heats.
| Wire | Resistance of 1 m, 1 mm² | Safe working heat in air | Notes |
|---|---|---|---|
| Copper (for comparison) | 0.017 Ω | — | Far too low; used only for the leads |
| Soft iron | 0.10 Ω | about 300 °C; scales fast above | Resistance rises several times as it heats. Usable only sealed or under water |
| Nickel silver (German silver) | about 0.3 Ω | about 250 °C | The first resistance wire of the 1880s (Nickel and Cobalt) |
| Constantan (55 copper, 45 nickel) | 0.49 Ω | about 400–500 °C | Resistance hardly changes with heat. Good for irons, warmers, low-heat jobs (Thermocouples and Thermoelectricity) |
| Nichrome (80 nickel, 20 chromium) | 1.1 Ω | about 1,100 °C | The standard. A tight green-grey oxide skin protects it at bright red |
| Iron–chromium–aluminium | 1.45 Ω | about 1,300 °C | Cheaper than nichrome, but goes brittle after heating; do not bend it once used |
Make nichrome as in Nickel and Cobalt: melt pure nickel with a quarter of its weight of chromium (from chromite ore, Alloy and Stainless Steels) in a covered crucible, and draw it with an anneal every few passes. Without nichrome, build low-heat appliances (irons, warming plates, sealed immersion heaters) from constantan or even iron wire, run well below red heat.
How hot will it run?
A wire's temperature depends on how many watts each square centimetre of its surface must throw off. For nichrome:
| Where the wire sits | Watts per cm² of wire surface | What you see |
|---|---|---|
| Open coil in free air (bar fire, toaster) | 4–6 | Cherry red, about 750–850 °C |
| Bedded in a groove or on mica | 2–3 | Dull red at most |
| Packed in magnesia inside a tube, tube in water | 8–15 (of tube surface) | Tube stays near 100 °C while water covers it |
| Same tube in air, no water | 2–4 (of tube surface) | Tube dull red; any more and it burns out |
"Glowing current" below is roughly what makes an open coil of that wire glow cherry red.
| Nichrome diameter | Ohms per metre | Glowing current |
|---|---|---|
| 0.25 mm | 22 Ω | 1.4 A |
| 0.3 mm | 15.4 Ω | 1.8 A |
| 0.4 mm | 8.7 Ω | 2.7 A |
| 0.5 mm | 5.6 Ω | 3.8 A |
| 0.6 mm | 3.9 Ω | 4.9 A |
| 0.8 mm | 2.2 Ω | 7.6 A |
| 1.0 mm | 1.4 Ω | 10.6 A |
Worked example: a 1,000 W radiant fire on 230 V draws 4.35 A and needs 53 Ω. The 0.6 mm wire glows at 4.9 A, a little above that, so it runs a safe cherry red: length = 53 ÷ 3.9 = 13.6 m, wound into a coil.
What you need
| Item | Notes |
|---|---|
| Resistance wire | Nichrome 0.25–1.0 mm, or ribbon rolled from it (Nickel and Cobalt, Iron and Brass Wire) |
| Mica sheet | Split to 0.1–0.3 mm. Stands 600–700 °C; insulates. (Rocks and Minerals) |
| Fireclay and kaolin | Formers, bars, hot plate discs, fired to stoneware (Firebrick and Refractories, Stoneware and Porcelain) |
| Magnesia | Dead-burnt magnesite, ground (Magnesium) — fills sheathed elements |
| Copper or steel tube | 6–10 mm, for sheathed elements (Metal Pipes and Tubes) |
| Cast iron, sheet steel, sheet copper | Sole plates, kettle bodies, cases (The Blast Furnace and Cast Iron, Sheet Metal and Rolling) |
| Brass or nickel | Terminals and screws, kept away from the hottest part (Zinc and Brass) |
| Bimetal strip | Brass and iron riveted together, for cut-outs (Thermostats and Automatic Control) |
| Flexible cord with earth wire, plug, fuse | Wiring and Electrical Safety |
| Ammeter and voltmeter | Measuring Electricity |
| Soapstone | Carves and drills easily into terminal blocks that stand heat |
Where to find it
Mica comes in "books" of sheets in coarse quartz-and-feldspar veins (pegmatite); peel it with a knife point into sheets as thin as paper. Magnesite is a white, porcelain-like rock in veins in green serpentine; roast it at a white heat (over 1,400 °C) for several hours so it no longer swells with water, then grind it to fine sand. Soapstone is the soft, greasy grey-green rock a fingernail scratches.
The heating element
Every appliance here is an element plus a body that holds it, spreads its heat and keeps fingers off it.
Winding an open coil
- Mandrel. Use a smooth steel rod about 5–6 times the wire diameter — 3 mm for 0.5 mm wire, 4 mm for 0.6–0.8 mm. A thinner mandrel gives a stiff, springy coil; a fatter one gives a floppy coil that sags when hot.
- Wind close-turned by hand or on a The Lathe turning slowly, keeping the wire under steady tension. Leave 15 cm straight at each end.
- Stretch the coil evenly until the gap between turns equals about one wire thickness. Turns that touch short out, and the coil runs too hot there.
- Cold ends. The wire must be cool where it meets the brass terminal, or the joint oxidises and burns. Double or triple the straight end back on itself and twist it tight for 5–8 cm: doubled wire has half the resistance and runs much cooler. Clamp it under a brass or nickel nut with a washer each side. Never try to solder nichrome — solder will not take, and would melt anyway.
- Test before mounting, laid on bricks with an ammeter in circuit. It should glow evenly at the current you designed.
Ribbon on mica
For irons and toasters, where the element must be flat, use ribbon: nichrome wire rolled flat between hardened rollers (Sheet Metal and Rolling) to about 1.5 mm wide and 0.1 mm thick, or simply thin round wire.
- Cut a card of mica 0.3 mm thick to shape. Notch both edges with a file at an even spacing of 2–3 mm.
- Wind the ribbon round the card, flat side down, each turn sitting in a pair of notches so turns cannot slide together.
- Fix the ends through eyelets of brass to terminals. Sandwich the card between two more mica sheets.
The sheathed element
The best element is a coil sealed in a metal tube, held in its centre by packed magnesia powder, which insulates electrically but carries heat well. It can go straight into water, be bent into rings, or bolted under a plate. It is also the hardest to make.
- Tube: copper or steel, 8 mm outside, 0.7 mm wall, 40–80 cm long.
- Coil: nichrome on a 3 mm mandrel, with a straight 2 mm iron or nickel terminal pin welded or tightly twisted to each end. The coil must lie at least 2 mm from the tube wall all round.
- Bake the magnesia at 300 °C or more for an hour, and keep it hot and dry — damp magnesia leaks current.
- Fill: stand the tube upright in a vice, hold the coil in the centre with its top pin, and pour in magnesia a spoonful at a time, tapping the tube constantly with a light hammer and pressing each spoonful down with a thin rod.
- Compact: roll the filled tube between two hard rollers, or hammer it evenly along its length on an anvil, turning it, until its diameter shrinks by about a tenth. This packs the powder rock-hard.
- Bend it slowly round a wooden former into the loop you need, with no bend tighter than three times the tube's diameter.
- Bake again at 300 °C, then seal both ends at once while hot with a plug of Glass fused round the pin, or with Water Glass (Sodium Silicate) and magnesia paste.
- Insulation test (see below). A sheathed element must show no leakage at all.
Making each appliance
Electric kettle
What it is: a pot of sheet metal with a heating element in or under its base. Body: copper sheet 0.6–0.8 mm, tinned inside, or steel enamelled inside (Enamel on Metal), 1–2 litres, with a wooden or fired-clay handle and a spout.
- Simplest version — element under the base. Give the kettle a thick flat bottom (2–3 mm copper) and clamp beneath it a fired-clay plate with a coil in its groove (as for a hot plate), closed by a steel cover. Slow — about 15 minutes for a litre — like the kettles of the 1890s.
- Better version — element in the water. Bend a sheathed element of 1,000–1,500 W into a loop 1 cm above the bottom. Its ends pass out through threaded brass bosses soldered into the wall, sealed with fibre or rubber washers and nuts, inside a porcelain plug socket. 1.5 litres from 15 °C to boiling at 1,200 W takes about 8 minutes.
- Safety: bond the earth pin of the socket to the metal body. Add a dry-boil cut-out: a bimetal disc pressed against the element's mounting boss, which snaps over at about 150 °C and opens a switch, or pushes the plug out of its socket. Never switch on an empty kettle without one.
- Good one: no drips at the bosses after an hour full of water; no tingle on the body; the cut-out trips within a minute when run dry.
Immersion heater
A sheathed element of 1–3 kW with a threaded brass head, screwed into a boss in a hot-water tank (Hot Water and Central Heating), with a rod thermostat set to about 60 °C — hot enough to kill the germs that breed in lukewarm tanks. Water at 60 °C scalds skin within seconds, so mix it with cold at the tap for washing, and especially for bathing children. Mount it low to heat the whole tank, high for a quick small amount. A 3 kW heater warms 100 litres by 45 °C in about 2 hours. Earth tank and heater; add a cut-out at 80–85 °C.
Electric iron
- Sole plate: cast iron 12–15 mm thick, pointed at the front, about 20 × 11 cm, ground flat and polished. Weight 1.5–2.5 kg; heavier irons press better, lighter ones tire the arm less.
- Element: 400–750 W. For 450 W on 230 V you need 117 Ω — about 5.3 m of 0.25 mm nichrome, wound in 40 turns 2.5 mm apart on a mica card cut to the sole's shape.
- Pressure plate: a 3 mm steel plate the same shape, screwed down to the sole by four or five screws so that the mica sandwich is squeezed flat. An element that is not pressed tight overheats and burns out.
- Thermostat: a bimetal strip carrying a silver contact, set by a screw knob (Thermostats and Automatic Control). Mark the knob from trials: silk and wool about 150 °C, cotton 200 °C, linen 230 °C.
- Cover and handle: a sheet steel cover; a hardwood handle on two iron pillars at least 4 cm above the cover. A heel rest so the iron stands up between strokes.
- Cord: rubber-covered flex with a braided cotton or silk outer layer, through a rubber sleeve where it enters, clamped so it cannot pull on the terminals. Earth wire to the sole plate.
Without a thermostat, choose the wattage so the iron stops at about 220 °C standing on its heel, and test with a drop of water: at 100–150 °C it sizzles; at over 200 °C it skates about in balls.
Toaster
Two or three mica cards wound with nichrome ribbon, standing upright 3 cm apart, with the bread held between them in a cage of steel wires so it never touches the element. 600–1,000 W; toast in 2–3 minutes with the bread 1–1.5 cm from the glowing wire. Mount the cards in a sheet steel body with a crumb tray, on feet so the table stays cool. The 1920s pop-up toaster adds a spring-loaded tray held down by a catch, released by a clockwork timer or a bimetal strip, which also opens the switch.
Danger The wires of a toaster are bare and live. Never put a knife or fork into a toaster that is plugged in — pull the plug first. Use a double-pole switch, so the element is dead when off whichever way the supply is wired.
Electric heater
- Radiant (bar) fire: an open nichrome coil laid in a spiral groove on a fired-clay rod 2–3 cm thick and 30–40 cm long, glowing cherry red in front of a polished curved reflector of copper or brass (later chromium-plated). 1 kW per bar. Fireclay rods: roll fireclay with a quarter of grog, cut the spiral groove with a stick while leather-hard, and fire to 1,200 °C. Cover the front with a steel wire guard, meshes no wider than 12 mm. The worked example above designs its coil.
- Convector heater: elements at the bottom of a tall sheet-steel cabinet with louvres at the top. Warmed air rises through it and circulates round the room; the case stays below about 80 °C, safer near children.
- Sizing: in a moderate climate, an ordinary room needs about 60–100 W per square metre of floor if poorly insulated, half that if well insulated (Insulation and Keeping Buildings Warm or Cool).
Hot plate
- Open plate: a fired-clay or porcelain disc 15–20 cm across with a spiral groove on top, holding a coil of 800–1,200 W. Quick, but the bare live wire can be touched and spilt food falls into it.
- Solid plate (better): a cast-iron disc 18 cm across and 12–15 mm thick, flat on top, with spiral grooves cast in the underside. Lay the coil in the grooves, fill them with a paste of magnesia or fine fireclay and water glass, dry slowly, and close the underside with a steel plate. Takes 5–10 minutes to heat; then holds its heat like a stove top. Earth the plate.
- Good one: perfectly flat — lay a straightedge across it — so that a flat-bottomed pan touches all over. A gap of 1 mm halves the heat that reaches the pan.
Electric cooker
A cooker is two to four hot plates on top of an insulated oven: a box of sheet steel about 40 × 40 × 35 cm inside, enamelled, with a second outer box 5 cm away, the space packed with glass or slag wool (Glass Fibre and Glass Wool). A door with the same insulation and a hinge and latch. An element of 1–1.5 kW under the floor and another of about 1 kW under the roof, or one up each side; a rod thermostat with a dial from 100 to 250 °C.
The three-heat switch gives low, medium and high from two equal elements without wasting power in resistors:
| Switch position | Connection | Power (two 1,000 W elements) |
|---|---|---|
| Low | Both in series | 500 W |
| Medium | One alone | 1,000 W |
| High | Both in parallel | 2,000 W |
A full cooker can draw 6–10 kW — 25–40 A on 230 V. It needs its own circuit from the fuse board, wire of 6 mm² or more, its own fuse and a double-pole switch on the wall beside it (Wiring and Electrical Safety).
Hair dryer
A small universal motor of 20–60 W (Fans, Vacuum Cleaners and Washing Machines) turns a fan that blows air through a nichrome coil on a cross-shaped mica former inside a tube. 300–1,000 W. Wire it so the heater cannot be on unless the fan runs; fit a cut-out that opens at about 100 °C at the outlet; put a fine guard over the inlet so hair cannot be sucked in.
Danger A hair dryer or heater dropped into a bath kills. Never use mains appliances where a person is in water, and never put a socket within reach of a bath or basin.
Keeping them from killing
They draw big currents through metal bodies that are often wet. Follow Wiring and Electrical Safety, plus:
- Earth every metal body. A three-core cord, the earth wire screwed to the body itself with a star washer, not to a painted surface. If the element ever touches the body, the fuse blows.
- Fuse to suit: a 1 kW appliance on 230 V draws 4.3 A — use a 5 A fuse in its plug or circuit, not a 30 A one.
- A thermal cut-out in every appliance that can overheat unattended: a bimetal switch set above the normal working heat, or a thermal fuse — two spring contacts held together by a pellet of low-melting metal that melts and lets them spring apart. Tin–lead solder melts at about 183 °C; Rose's metal (half bismuth, a quarter each lead and tin, Antimony and Bismuth) at about 95 °C.
- Double-pole switches on anything with bare elements.
- Heat-proof cord on irons and cookers; never let a cord touch a hot surface.
- Insulation test before first use and every year: unplugged, connect a 100 V battery through a sensitive galvanometer (Measuring Electricity) between the joined element terminals and the metal body. There should be no movement at all. If there is, bake it at 150 °C for a few hours and test again.
How to tell it worked
- Current: measured within 10% of your design (watts ÷ volts). Too high means a short between turns; too low, a bad joint.
- Even glow: open coils glow evenly, with no single bright spot.
- Cool terminals and cord: after an hour at full power, the cord and plug should feel only slightly warm.
- No leakage on the insulation test, no tingle anywhere, and the fuse blows if live is deliberately touched to the body (test as in Wiring and Electrical Safety).
- Cut-outs work: run a kettle dry, block a hair dryer's inlet, stand an iron on full: the cut-out must open before anything smokes.
Note Troubleshooting. Element burns out in the same spot → turns touching, a kink, or the wire thinner there. Stretch the coil evenly; check the wire with a micrometer. Element burns out at the terminal → cold end too short or the joint loose. Double the end back further; tighten the nut. Much less heat than designed → wire too long or too thin, or the supply voltage low under load. Measure volts at the appliance with it running. Tingle from the body, or leakage on test → damp insulation, or a coil touching the tube or plate. Bake dry; if it persists, rebuild. Kettle leaks at the bosses → washers hardened or cracked. Replace them, and do not overtighten.
Dangers
Danger Water and mains electricity together kill. Kettles, immersion heaters and washing-up water are where most household shocks happen. Every metal body must be earthed and fused. Unplug before filling, cleaning or reaching inside. Never run a cord across a sink.
Danger Fire. An appliance left on unattended, a radiant fire near curtains, bedding or clothes drying, or an iron left face-down, will start a fire. Keep 1 m clear in front of radiant fires; always fit a cut-out; switch off at the wall when you leave the room.
- Burns: elements, sole plates and hot plates stay dangerously hot for 10–20 minutes after switching off.
- Asbestos: old appliances used asbestos for heat insulation. Do not use it; its fibres cause fatal lung disease decades later. Use mica, fired clay, magnesia and glass wool instead.
What this unlocks
- Clean, controllable heat for Sterilising Instruments and Dressings, incubators, brooders and laboratory work (Burners, Stands and Laboratory Equipment).
- Electric furnaces and kilns with nichrome windings (Electric Kilns and Furnaces), up to about 1,100 °C, for Glazes, Enamel on Metal and heat-treating Alloy and Stainless Steels; beyond that, the The Electric Arc Furnace.
- With Thermostats and Automatic Control, automatic control of ovens, crystal ovens and water heaters.
- With a fan, the tumble dryer; with bricks heated at night, the storage heater (Storing Energy).
How it was first done
James Prescott Joule of Manchester measured the heat made by a current in 1841 and found it grew with the square of the current. Henry Seely of New York patented an electric flat iron in 1882. In the early 1890s Crompton & Co. in England and the Carpenter Electric Heating Manufacturing Company in Minnesota sold kettles, irons and pans, their iron or nickel-silver wire buried in enamel or cement, and in 1892 Thomas Ahearn cooked a whole meal electrically at the Windsor Hotel in Ottawa. Their elements burned out often.
The breakthrough was nichrome. In 1906 Albert Marsh in Illinois patented nickel–chromium alloy for heating elements, and within a few years General Electric's D-12 toaster (1909) and many others went on sale. Charles Belling in England made radiant fires with wire wound on fireclay bars from 1912. Charles Strite patented the automatic pop-up toaster in 1921. In 1922 Arthur Leslie Large at Bulpitt & Sons in Birmingham sealed the element in a metal tube inside the water, and in 1955 Russell Hobbs's K1 kettle switched itself off with a bimetal strip when it boiled. The French hairdresser Alexandre Godefroy built a seated hair dryer in about 1890; hand-held dryers with small motors followed in the 1920s.
Source: content/entries/electricity/heating-appliances.md