◆ Rebuild

Part 8 · Chemistry

Ether, Acetone and Solvents

Liquids that dissolve what water cannot — resins, fats, rubber, waxes and paints. Wood spirit and acetone come from the smoke of a charcoal retort, ether from alcohol and sulfuric acid, turpentine from pine resin. All of them burn fiercely, and some are poisons.

Difficulty
●●●●●
Time
A charcoal burn plus a week to settle and work up the wood vinegar; a day per acetone retort run; half a day for a batch of ether
Steps from zero
12 prerequisites →

You need first

DistillationSulfuric Acid

This unlocks

Methanol and FormaldehydeAnaesthesia
The full path from nothing — 12 steps before this one
  1. Fire
  2. Finding and Preparing Clay
  3. Sulfur
  4. Pottery
  5. The Kiln
  6. Lime
  7. Fermentation
  8. Lye and Potash
  9. Glass
  10. Distillation
  11. Saltpeter
  12. Sulfuric Acid
  13. Ether, Acetone and Solvents

Do them roughly in this order. See it on the tech tree →

Why it matters

Water dissolves salt and sugar, but not grease, resin, wax, rubber or paint. For those you need a solvent — a liquid that dissolves them and then evaporates away, leaving the dissolved thing behind as a film or a clean residue. With a small set of solvents you can:

You already have two solvents: strong alcohol (ethanol) from Distillation and turpentine from pine resin (the same chapter). This chapter adds wood spirit (methanol), acetone and ether, and shows how to choose among them.

How it works

Like dissolves like. Water molecules are strongly "sticky" at their ends (chemists say polar); they hold on to salts and sugars, which are sticky too, and push away oils, which are not. Oily substances dissolve in oily, non-sticky liquids. Alcohol and acetone are halfway between: they mix with water and dissolve many resins. Ether and turpentine are almost entirely oily.

Volatile means flammable. A useful solvent must evaporate quickly, and anything that evaporates quickly fills the air with vapour that burns. The lower the boiling point, the more dangerous.

Solvent Boils at Dissolves well Mixes with water? Main hazard
Water 100 °C Salts, sugars, gums, glue — —
Ethanol (strong alcohol) 78 °C Shellac, many resins, iodine, plant oils and medicines Yes Flammable; drunk
Methanol (wood spirit) 65 °C Shellac, some resins; a fuel Yes Poison: blinds and kills
Acetone 56 °C Most resins, celluloid, nail varnish, fats; acetylene gas Yes Very flammable
Ether 35 °C Fats, oils, waxes; extracting plants Hardly (floats on it) Extremely flammable; anaesthetic
Ethyl acetate 77 °C Lacquers, glues; smells of pear drops Slightly Flammable
Turpentine 150–180 °C Oils, waxes, varnish resins, rubber (slowly) No Flammable, irritant

Where they come from. When hardwood is heated without air to make Charcoal, its smoke contains a sour watery liquid, wood vinegar (pyroligneous acid — "fire-wood acid"). It holds 5–10% acetic acid (the acid of vinegar), 1–3% methanol and a little acetone. Distilled, it gives wood spirit. Its acid, neutralised with lime, gives calcium acetate, and calcium acetate heated to a dull red heat splits into acetone and chalk. Ether is made by a different trick: hot sulfuric acid pulls a molecule of water out of every two molecules of alcohol and joins what is left.

Hardwood in a sealed retort Charcoal 30–35 kg Condensed smoke wood vinegar Tar 5–8 kg Distil, add lime, distil again Wood spirit methanol, 1.5–2 L Calcium acetate boil down and dry or: vinegar neutralised with chalk Iron retort dull red, 400–500 °C Acetone redistil at 56 °C chalk left in the retort neutralises the next batch From 100 kg of dry hardwood
Fig. 1 Solvents from the charcoal retort. The smoke of the retort condenses to tar and wood vinegar; the vinegar is distilled for wood spirit, and its acid, neutralised with lime, is dried and baked into acetone. The chalk left in the retort neutralises the next batch.

What you need

Item For Notes
A charcoal retort with a condenser pipe Wood vinegar See Charcoal (Method 3) and Tar, Pitch and Glue. An iron drum or large clay pot.
Dry hardwood Wood vinegar Beech, birch, maple, oak, hornbeam. About 100 kg gives 40–50 litres of wood vinegar. Softwoods give much less acid and methanol, more tar.
A pot still or glass retort with a water-cooled condenser All methods See Distillation and Laboratory Glassware
Slaked lime or powdered chalk / limestone Acetone See Lime
A small iron retort Acetone An iron pot with a tight lid and an outlet pipe, or a short piece of thick iron pipe capped at one end (Sheet Metal and Rolling, Metal Casting)
Strong alcohol, 90–95% Ether From Distillation — redistilled twice
Concentrated sulfuric acid Ether See Sulfuric Acid
Glass flask with a side tube, a dropping funnel or tap, a long condenser Ether Glass only — see Laboratory Glassware
Ice or snow, or the coldest spring water you can get Ether The condenser must be very cold
A thermometer reading to 200 °C Ether, redistilling Strongly advised. See The Thermometer.
Dark glass bottles with ground stoppers or tight corks Storage Label everything

Where to find it

  • Hardwood: broad-leaved trees. Beech and birch are classic for wood distillation. Use the wood dry (seasoned a year), cut into pieces no thicker than a wrist.
  • Alcohol: from fermenting grain, fruit, honey or sugar (Fermentation) and distilling (Distillation).
  • Vinegar for the gentle acetone route: let wine or cider sour (Fermentation). The strongest homemade vinegar holds about 5–7% acid.
  • Lime and chalk: burn limestone or seashells into quicklime and slake it (Lime); or simply grind chalk, limestone or shells to flour.
  • Pine resin for turpentine: wounds on pines, spruces and larches (Distillation).

Method 1: Wood spirit (methanol) and wood vinegar

  1. Run a charcoal retort with a pipe leading the smoke into a cooled pot (Charcoal, Tar, Pitch and Glue). A watery brown liquid collects, with tar below it.
  2. Settle. Leave the liquid in a covered pot for a week. Tar sinks; the clear brown liquid on top is wood vinegar. Draw it off.
  3. First distillation. Distil the wood vinegar in a pot still (Distillation). Collect everything until only thick tar remains in the pot. The distillate is lighter yellow and contains the methanol, acetone and acetic acid; the dirty tar stays behind.
  4. Neutralise. Stir slaked lime into the distillate, a handful at a time, until a drop of the liquid no longer turns red-cabbage juice pink (it should stay blue-purple or just turn greenish — see Acids, Bases and Testing), or until a little added lime stays undissolved on the bottom. Never taste it — it contains methanol. Lime holds the acid as calcium acetate, which cannot boil away.
  5. Second distillation. Distil again, gently. The first tenth or so that comes over, while the still head is only just warm, is crude wood spirit: methanol with some acetone, smelling sharp and slightly fishy. Stop when the distillate no longer burns when a spoonful is lit. What stays in the pot is a solution of calcium acetate — keep it for Method 2.
  6. Rectify. Distil the crude spirit once or twice more, slowly, keeping only the part that comes over at the lowest heat. You get a liquid of perhaps 80–95% methanol, the old "wood naphtha".

Tip Yields. 100 kg of dry hardwood gives roughly 30–35 kg of charcoal, 5–8 kg of tar, 1.5–2 litres of crude wood spirit and 4–5 kg of crude calcium acetate. Small, but it comes free with charcoal you were making anyway.

Warning Mark and colour wood spirit at once. Methanol looks, smells and burns almost exactly like drinking alcohol, and there is no simple test to tell them apart. Stir in a little bitter, coloured plant extract (wormwood, or a dye from Dyes and Mordants) so nobody can mistake it for something to drink, and label the bottle with a skull.

Method 2: Acetone from acetate of lime

  1. Make the acetate.
    • From Method 1: boil down the calcium acetate solution left in the still until it is a thick paste, then dry it on an iron sheet over a low fire, stirring, until it crumbles. This is grey acetate of lime.
    • From vinegar (cleaner): stir powdered chalk or limestone into strong vinegar. It fizzes. Keep adding until fresh chalk no longer fizzes and some lies unchanged on the bottom — about 40–45 g of chalk per litre of 5% vinegar. Filter, boil down, and dry as above. 10 litres of vinegar give about 650 g of acetate.
  2. Load the iron retort no more than half full with the dry acetate, broken into pea-sized lumps. Any water left in it ends up in your acetone.
  3. Fit the condenser: an iron or copper pipe 1–2 m long running down through a trough of cold water, into a closed receiving jar with a small vent. Seal the lid joint with clay mixed with a little sand.
  4. Heat slowly to a dull red (about 400–500 °C — the iron glows dull cherry red in a shaded place). Pale vapour comes over and condenses to a yellow-brown liquid with a sweet, sharp smell. Keep the heat steady until no more comes, usually 2–4 hours for a few kilograms.
  5. Redistil the crude liquid from a pot set in a bath of hot water (not on the fire). Acetone boils at 56 °C, so it comes over freely while the bath is well short of boiling. Stop when the flow slows to drops — what is left is water and heavy oils.
  6. The chalk left in the retort is calcium carbonate again. Grind it and use it to neutralise the next batch of vinegar.

A kilogram of good grey acetate gives about 200 g (a quarter of a litre) of acetone; 10 litres of vinegar, about 150 g.

Note Another route: bacteria. Certain bacteria (Clostridium acetobutylicum) ferment mashed maize or potatoes into acetone, butanol and ethanol. This fed Britain's acetone needs in the First World War, but it needs pure cultures kept free of other microbes for days — see Culturing Microbes.

Method 3: Ether from alcohol and sulfuric acid

wind: fire upwind, vapour downwind Alcohol feeddrip in as fast as ether drips out Thermometer135–145 °C Sulfuric acid+ alcohol Sand bathover a small charcoal fire Long condenserpacked with ice and water Receiverin ice Vent tubeto the ground,far downwind
Fig. 2 Making ether. Alcohol drips steadily into hot sulfuric acid at about 140 °C; ether vapour passes into a long ice-cold condenser and collects in an iced receiver. Any vapour that escapes is led far away and downwind of the fire, which burns only under the sand bath, upwind.

Ether is the most dangerous liquid in this book to make. Its vapour catches fire from a flame several metres away, and even from a hot surface without any flame at all. Make it outdoors, in small batches, with the fire upwind and everything that might hold vapour downwind.

  1. Mix the acid. In a heat-proof glass flask of about 1 litre, put 100 ml of 95% alcohol. Stand it in cold water. Pour in 100 ml of concentrated sulfuric acid slowly, a little at a time, swirling — never the other way round. It gets very hot.
  2. Set up. Bed the flask in a sand bath (an iron dish of sand) over a small charcoal fire. Fit the flask with a stopper carrying a thermometer whose bulb dips into the liquid, a dropping funnel or tap for more alcohol, and an outlet to the condenser. The condenser should be 60 cm or longer and packed with ice and water. The receiver sits in a bucket of ice. From the receiver's vent, run a long tube down to the ground and away downwind: ether vapour is heavier than air and flows along the ground like water.
  3. Heat to 135–145 °C. Ether begins to come over and drips into the receiver.
  4. Feed alcohol from the funnel at the same rate as liquid drips into the receiver, keeping the temperature at 135–145 °C. The acid is not used up; a small amount converts several times its own volume of alcohol before it grows too black and weak.
  5. Judge the temperature without a thermometer (only if you must): below about 130 °C, mostly alcohol distils, and the distillate mixes completely with water. Above about 150–160 °C, the acid froths and blackens, a choking sulfur smell appears, and a gas comes over that does not condense (it is ethylene). Aim between the two.
  6. Wash. The crude ether contains water, alcohol and acid. Shake it gently in a stoppered bottle with half its volume of weak lye (Lye and Potash), releasing the pressure often. Let it settle: ether floats as a clear upper layer. Draw off the lower layer. Repeat with clean water.
  7. Dry and redistil. Stand the ether over lumps of fresh quicklime (Lime) for a day in a stoppered bottle, then pour it off and redistil it from a flask set in water that you have heated elsewhere and carried over — water at about 50 °C is plenty. No flame anywhere near.

From each litre of alcohol fed, expect roughly half a litre of ether.

Danger Ether for anaesthesia must be pure: washed, dried, redistilled, and free of the sharp smell of sulfur dioxide. Giving an anaesthetic is a skill of its own and can kill — see Anaesthesia before using ether on any person.

Method 4: Turpentine and other solvents

  • Turpentine: distil pine resin, or resinous wood chips, with water, and collect the oil that floats on the distillate — Distillation (Method 4). Redistil it once for a clean, water-white spirit.
  • Ethyl acetate: warm equal volumes of strong alcohol and the strongest acetic acid you can make (redistilled wood vinegar), with a little sulfuric acid as a helper, and distil. The pear-drop-smelling liquid that floats when the distillate is shaken with salt water is ethyl acetate — a good lacquer solvent.
  • Naphtha: the light oil from distilling crude oil or coal tar — see Petroleum and Refining and Coal and Coke. It dissolves rubber and grease and was the solvent of the first waterproof cloth.

Avoid making the chlorinated solvents (chloroform, carbon tetrachloride), benzene and carbon disulfide without real chemical training: they are strong poisons with long-term effects on the liver, blood and nerves.

How to tell it worked

  • Ether boils in the warmth of your hand: a few drops on the back of your hand vanish in seconds with an icy chill and a sweet, heavy smell. Shaken with water it separates and floats. A drop on paper leaves no stain.
  • Acetone evaporates almost as fast, mixes completely with water, and dissolves a scrap of shellac, pine resin or a smear of old paint almost at once. Clean acetone is colourless and smells sweet-sharp; yellow means it needs redistilling.
  • Wood spirit burns with a pale blue, almost invisible flame and mixes completely with water. It dissolves shellac flakes into a clear amber varnish overnight.
  • Purity: a good solvent evaporates from a clean glass or a white plate leaving no ring behind.

Note Troubleshooting. Acetone yellow, smelly, with an oily layer → the retort was too hot, or the acetate held tar. Heat more slowly, use acetate from clean vinegar, redistil from a water bath. Very little acetone → the acetate was wet, or the retort leaked; seal the lid better. Your "ether" mixes completely with water → the acid was too cool; you distilled alcohol. Raise the temperature. Black froth and choking fumes from the ether flask → too hot. Lower the fire and add alcohol a little faster. Wood spirit won't burn → too much water; distil it again and keep only the first part.

Dangers

Danger Ether fires and explosions. Ether boils at 35 °C, its vapour is heavier than air, it creeps along floors and benches to a flame many metres away, and it can be lit by a hot stove top or steam pipe without any flame (it ignites at about 160–180 °C). Mixed with air in a closed space it explodes. Work outdoors, upwind of nothing, with no fire downwind. Never distil old ether to dryness: stored in air and light it slowly forms explosive peroxides that collect in the last drops. Store it cool, in a full, dark, tightly closed bottle, and use it within a few months.

Danger Methanol poisoning. As little as 15–30 ml of methanol can kill or blind, and even 10 ml has caused permanent blindness. Symptoms start 12–24 hours after drinking — headache, vomiting, blurred "snowstorm" vision, then coma. The breath may smell normal. Breathing heavy vapour or long skin contact also poisons. Ordinary drinking alcohol (ethanol) given early slows the poisoning; seek whatever medical help exists (Emergencies).

  • Acetone and turpentine fires. Both catch from a spark or a candle; acetone vapour flashes back along its trail. Keep only small amounts open, and never near fire.
  • Breathing vapours causes headache, dizziness and drunkenness, and in closed rooms unconsciousness. Ether in particular is an anaesthetic: a person can be overcome by its fumes. Ventilate.
  • Sulfuric acid in the ether flask: see Sulfuric Acid. Always add acid to alcohol slowly with cooling.
  • Hot retorts and tar: see Charcoal and Tar, Pitch and Glue.

What this unlocks

How it was first done

The German physician Valerius Cordus described making "sweet oil of vitriol" from alcohol and sulfuric acid around 1540; in 1730 August Frobenius named it ether. In 1842 the Georgia doctor Crawford Long removed a growth from a patient's neck under ether, and in October 1846 the dentist William Morton gave the famous public demonstration of ether anaesthesia at Massachusetts General Hospital in Boston. Within months it was used across Europe.

Robert Boyle noted a spirit among the products of distilling wood in 1661, and in 1834 Jean-Baptiste Dumas and Eugène Péligot in Paris showed that wood spirit was a distinct alcohol, methanol. Acetone from heating acetates was known to alchemists by around 1600. Through the nineteenth century, "wood distillation" plants beside charcoal works in Europe and North America sold charcoal, acetate of lime and wood spirit together; they supplied nearly all the world's methanol and acetone until fermentation (1915) and then synthesis from coal and natural gas (1920s) took over.