◆ Rebuild

Part 8 · Chemistry

Fermentation

Let invisible living things do chemistry for you — turning sugar into alcohol, and alcohol into vinegar. Fermentation preserves food, raises bread, and is the starting point for distilled alcohol and antiseptics.

Difficulty
●●●●●
Time
2–6 weeks for wine or mead; about 10 days for simple beer; 1–2 months for vinegar
Steps from zero
3 prerequisites →

You need first

Pottery

This unlocks

Acids, Bases and TestingDistillationCitric and Tartaric AcidThe BatteryBiogas and Wood GasBeer, Wine and CiderStarter Cultures and Food MicrobiologyVinegar and PicklingAntibiotics Beyond Penicillin
The full path from nothing — 3 steps before this one
  1. Fire
  2. Finding and Preparing Clay
  3. Pottery
  4. Fermentation

Do them roughly in this order. See it on the tech tree →

Why it matters

Fermentation is chemistry done by living things too small to see. You provide sugar, water, a clean pot and the right temperature; they do the rest. With it you can make:

  • Alcohol — wine, mead, cider and beer. Beyond drinking, alcohol is the raw material for Distillation, which concentrates it into a strong spirit that kills germs on hands, instruments and wounds (Wound Care and Antiseptics), dissolves resins and medicines, and burns as a clean fuel.
  • Vinegar — a mild acid that preserves vegetables, fish and meat for months (Preserving Food), cleans, dissolves minerals, sets dyes (Dyes and Mordants) and can serve as the liquid in a simple The Battery.
  • Risen bread — the same yeast that makes alcohol makes dough rise (Grain, Flour and Bread).
  • Soured foods — sauerkraut, yoghurt and cheese keep far longer than fresh food (Dairy and Cheese); moulds and salt turn soybeans into soy sauce and miso (Soy Sauce, Miso and Koji).

Learning to grow the microbes you want, and keep out the ones you don't, is also your first step towards growing medicines like Penicillin (Culturing Microbes). This chapter gives the basic methods; Beer, Wine and Cider, Vinegar and Pickling and Starter Cultures and Food Microbiology take each further.

How it works

Everywhere — on fruit skins, in the air, on your hands — live microbes: living things made of a single cell, far too small to see. Three kinds matter here.

  1. Yeasts are tiny fungi. When they have sugar but no air, they turn the sugar into alcohol and carbon dioxide gas (the bubbles). About half the weight of the sugar becomes alcohol. Yeasts work best at 18–25 °C (pleasantly cool room temperature), slow down below 10 °C, and die above about 40 °C. They also poison themselves: most stop when the alcohol reaches 10–15 %.
  2. Lactic acid bacteria turn sugar into lactic acid, the sourness of sauerkraut, yoghurt and sourdough. They also prefer no air and tolerate salt, which is how salted vegetables sour safely (see Preserving Food).
  3. Vinegar bacteria (acetic acid bacteria) turn alcohol into vinegar (acetic acid). Unlike the other two, they need air. They are the enemy of the winemaker and the friend of the vinegar maker.
YEASTno air · 18–25 °C VINEGAR BACTERIAneeds air · 25–30 °C SUGARfruit juice, honey, malt ALCOHOL + GASwine, mead, cider, beer VINEGARsour, under a skin of "mother" LACTIC BACTERIAno air · salt keeps rivals out SOUR FOODSsauerkraut, pickles, yoghurt, sourdough —vegetables held under brine by a stone airlock air, through cloth
Fig. 1 The three useful fermentations. Yeast turns sugar into alcohol without air; vinegar bacteria turn alcohol into vinegar with air; lactic bacteria sour sugary food without air.

The whole art is controlling air, temperature and cleanliness so that the microbe you want wins.

Sugar first. Yeast can only eat sugar. Fruit juice and honey are already sugary. Grain is mostly starch, which yeast cannot eat until it is broken into sugar. Sprouting grain makes its own starch-cutting substances (called enzymes); that is what malting does. (Some peoples of the Americas did the same job by chewing maize — saliva contains the same kind of enzyme.)

What you need

Item Details
Fermenting pots Glazed pottery, or unglazed pottery sealed inside with beeswax or pine pitch (see Tar, Pitch and Glue). Wooden barrels, gourds and leather bags also work. Size: 5–20 litres
Something sweet Ripe fruit, honey, or malted grain (quantities in each method)
Water Clean, boiled and cooled (Finding and Purifying Water)
Airlock A water-sealed lid or a bent tube into water (below)
Cloth Tightly woven, to keep out flies and dust
Tube A hollow reed, elder stem or bamboo, for drawing clear liquid off the sediment
Sanitising Boiling water, soap or wood-ash lye (Soap, Lye and Potash)

Which pots. Avoid any pot with a lead glaze (shiny, smooth, often yellow-green or amber glaze made with lead ore — see Glazes). Wine and vinegar are acids and dissolve lead into the drink. Unglazed clay is porous: it lets in air and soaks up microbes from batch to batch. Line it with melted beeswax (Beekeeping) or pitch, as ancient people lined their wine jars.

Where to find it

  • Fruit. Grapes are the easiest: they have plenty of sugar (about 20 % of their juice) and carry their own yeast in the dusty white "bloom" on their skins. Apples, pears, plums, cherries, elderberries, blackberries, figs and dates all work. Pick them fully ripe — sugar rises sharply in the last weeks.
  • Honey. From wild bee nests in hollow trees or rock crevices, or from your own hives (Beekeeping). Honey is about 80 % sugar.
  • Grain. Barley malts best; wheat, rye, maize, sorghum and millet also work. See Farming from Seed and Foraging Wild Food.
  • Tree sap. Birch and maple sap in early spring, and the sap of palms in the tropics (palm wine), are sweet enough to ferment directly.
  • Wild yeast. On the skins of ripe fruit (especially grapes and plums with a powdery bloom), in flowers, in honey, and in any sourdough. You never need to buy it.

Method 1: Capture wild yeast

  1. Put a handful of unwashed ripe grapes, plums, berries or dried fruit into a clean jar with about 500 ml of water and two spoonfuls of honey (or a cup of fruit juice).
  2. Cover with cloth and keep somewhere at 20–25 °C. Stir with a clean stick twice a day.
  3. In 2–5 days it should fizz when stirred, form a light foam, and smell fresh, fruity and bready. This is your starter.
  4. If instead it grows fuzzy coloured mould, smells rotten or like nail-polish remover, throw it out, scald the jar and start again with different fruit.
  5. Keep your yeast. After every good batch, save a cup of the creamy sediment at the bottom (the lees) in a covered pot in a cool place and feed it a spoonful of honey every week or two. Or spread the foam from an active brew thinly on a clean board, dry it in the shade, and store the flakes — the old way of keeping yeast between seasons.

Method 2: Wine, cider and mead

  1. Clean everything (see Keeping it clean, below).
  2. Make the sweet liquid.
    • Wine: crush ripe grapes by hand or foot in a clean tub. Leave juice, skins and seeds together for 3–7 days (stirring the floating skins down twice a day), then squeeze the juice out through a cloth or basket and discard the skins.
    • Cider: crush apples or pears to a pulp with a club and squeeze the juice out through cloth.
    • Mead: stir 1 kg of honey into 3–4 litres of warm (not hot) boiled water. One part honey to three of water gives a strong, sweet mead of about 12–14 %; one to four gives a lighter, drier one that finishes sooner.
  3. Add yeast. Grape juice usually starts on its own. For cider and especially mead, stir in a cupful of starter.
  4. Fill the pot about four-fifths full and cover with cloth. Keep it at 18–25 °C.
  5. Vigorous stage (3–7 days). It foams and fizzes, and smells strongly. The foam keeps air off the surface. Keep it covered.
  6. Quiet stage (2–6 weeks). When the foaming calms, top the pot up nearly to the neck with similar juice or boiled water, and fit an airlock. From now on, air is the enemy: it lets vinegar bacteria in.
  7. It is finished when the airlock bubbles less than once a minute, the liquid starts to clear from the top down, and a thick layer of sediment has settled. Dry wine tastes not sweet at all.
  8. Draw it off. Put the full pot on a table and the empty one on the floor. Suck on a hollow reed placed in the liquid (keeping its end above the sediment) until liquid comes, then let it run downhill into the clean pot. This is called racking. Seal the new pot and keep it cool.

Method 3: Malting grain and simple beer

whole grain shoot = ¾ of the grain roots 1 · STEEPabout 2 days,fresh water twice a day 2 · SPROUT4–6 days at 12–18 °C,turn twice a day 3 · DRYbelow 50 °C — warm,never hot 4 · MASHcrushed malt in waterat 63–68 °C for 1 hour
Fig. 2 Malting and mashing. Soaked grain sprouts until the shoot inside is three-quarters of its length, is dried gently, then crushed and steeped in water at about 65 °C, where its starch turns to sugar.
  1. Steep. Soak barley in clean water for about 2 days, draining and replacing the water every 12 hours and leaving it to drain in the air for a few hours each time. It is ready when a grain squashed between your fingernails is soft right through.
  2. Sprout. Spread the wet grain 5–10 cm deep on a clean floor or cloth in a cool, shaded place (12–18 °C). Turn it twice a day so it doesn't mat together or heat up, and sprinkle on water if it dries. In 4–6 days little roots appear and the pale shoot growing inside the husk reaches about three-quarters of the grain's length. Stop here — any longer and the plant starts eating the sugar you want.
  3. Dry. Spread it in the sun or on a warm (never hot) surface. Keep it below about 50 °C — no hotter than a sun-warmed rock you can rest your hand on comfortably — or you will kill the enzymes. When dry and crunchy, rub off the roots. This is malt. It stores for months, dry.
  4. Crush the malt coarsely between stones (see Grain, Flour and Bread) — crack every grain, but do not grind to flour.
  5. Mash. For every kilogram of crushed malt, prepare 3 litres of water at about 70 °C: two parts boiling water mixed with one part cold water gives about this temperature, and stirring in the cool grain brings it down to the ideal 63–68 °C. At 65 °C you can dip a finger in for only a second. Cover the pot and wrap it in straw, hides or blankets to hold the heat for 1 hour. Add a ladle of boiling water if it cools.
  6. Taste it. The liquid (now called wort) should taste clearly sweet. Drain it off through a basket lined with straw, and pour a few litres of hot water over the grain to rinse out more sugar.
  7. Boil the wort for an hour, with bittering herbs if you like (hops; or yarrow, heather or bog myrtle as in old northern European ales). Boiling kills wild microbes.
  8. Cool it, covered, until it feels cool to your wrist (below 25 °C). Add a cup of yeast starter or lees. Ferment as for wine, under cloth then an airlock, for 5–10 days. Simple ales of this kind are weak (3–6 % alcohol) and best drunk within a few weeks.

Airlocks

An airlock lets the gas out but keeps air, flies and dust from getting in. You can make one without any glass or metal.

Upturned bowl Water-filled moatgas bubbles outunder the rim Wine or mead Leesyeast sediment Wax-sealed plug Bent reed or clay tube Cup of watergas bubbles out,air can't get in Wine or mead WATER-MOAT JAR BENT-TUBE AIRLOCK
Fig. 3 Two airlocks made from pottery. Left: a jar with a water-filled moat around its neck and an upturned cup as a lid. Right: a plugged jar with a bent tube leading into a cup of water.
  • Water-moat jar. Shape a jar with a deep gutter around its neck, about 3 cm wide and 4 cm deep. Fill the gutter with water and set an upturned bowl over the neck so its rim stands in the water. Gas pushes out under the rim as bubbles; nothing can get in. Pickling jars of this kind have been used in China and Korea for centuries.
  • Bent tube. Seal the jar's mouth with a wooden or clay plug made airtight with beeswax or clay. Push through it a hollow reed or a fired clay tube that bends over (two straight pieces joined at an angle with wax or clay will do) and dips 1–2 cm into a cup of water.
  • Bladder. In a pinch, a cleaned animal bladder or a sheet of leather tied tightly over the mouth swells with gas. Prick a pinhole when it gets tight.

Method 4: Vinegar

  1. Start with alcohol. Wine, cider, mead or beer. Strong wine (over about 10 %) slows vinegar bacteria — dilute it with one part boiled water to one part wine.
  2. Give it air. Use a wide-mouthed pot and fill it only half full, so the surface is large. Cover with cloth tied tightly against vinegar flies. Keep it warm — 25–30 °C is ideal — and in the dark.
  3. Add a mother. Mother of vinegar is the pale, slimy, rubbery skin that vinegar bacteria build on the surface. Add a piece from a previous batch, or a cup of living (unboiled) vinegar. Without either, it still works: wild bacteria arrive on their own within 1–3 weeks.
  4. Leave it alone. Don't stir or sink the mother. Over 3–8 weeks a skin forms and thickens, and the smell changes from wine to sharp vinegar.
  5. It is done when it smells and tastes sharply sour with no alcohol warmth left.
  6. Keep it going. Draw off two-thirds through a spigot or tube near the bottom, leaving the mother undisturbed, and gently pour in fresh wine to replace it. This is the old Orléans method, used in France since the Middle Ages, and gives vinegar every few weeks.
  7. To stop it changing further, fill bottles or pots right to the top and seal them, or heat the vinegar to about 70 °C first.

How to tell it worked

  • Alcohol: bubbles rising, a fizz on the tongue, a warming feeling in the throat, a winey or beery smell. The sweetness falls day by day.
  • Vinegar: sharply sour. Drop a pinch of crushed chalk, limestone or eggshell into a spoonful — it fizzes strongly. A purple red-cabbage or berry juice turns red in it. Homemade vinegar is usually 4–6 % acid; for pickling, use it undiluted, since you cannot know its exact strength.

Note Troubleshooting. Nothing happens after 3 days → too cold, too little yeast, or the liquid was still hot when the yeast went in. Warm it and add more starter. It stops while still sweet → too much sugar for the yeast (it poisoned itself), or it got cold. Accept a sweet wine, or add water and fresh starter. Your wine turned to vinegar → air got in. Keep pots full, airlocks topped up. Smells of nail-polish remover or rotten eggs → wild bacteria or stressed yeast. Clean better, ferment cooler. Slimy, ropy liquid → bacterial infection. Throw it away and scald everything. A flat, white, wrinkled skin on wine → film yeast from air. Skim it off and top up the pot. Fuzzy, coloured (green, black, pink) mould means throw it away.

Keeping it clean

Most failures are dirty pots. Before every batch:

  1. Scrub pots, lids, spoons and tubes with hot water and soap or a little weak lye. Rinse well.
  2. Scald them with boiling water, or fill them with boiling water and leave them covered for 10 minutes.
  3. Dry them upside down in the sun. Sunlight kills many microbes.
  4. Barrels can be fumigated by burning a small strip of cloth dipped in melted Sulfur inside them, then closing the bung for a few hours — a winemakers' practice since Roman times. The fumes are poisonous (see Sulfur); air the barrel well and rinse it before use.
  5. Never use a pot that has held lye, oil or rotten food for fermenting. Keep separate pots for vinegar — vinegar bacteria linger and will sour your next wine.

Dangers

Danger Fermentation gas can kill. Carbon dioxide has no smell or colour, is heavier than air and pools in cellars, pits and the bottoms of large vats. People die every year climbing into fermenting tanks or going down into closed wine cellars. Before entering a cellar or leaning into a large vat, lower a burning candle or splinter: if the flame dims or goes out, get out at once and ventilate it for hours. A flame that keeps burning does not prove the air is safe: carbon dioxide can knock you out at levels a candle survives. Ventilate first, go in only with a rope tied to you and a helper outside, and come out at the first headache, dizziness or panting. Never go in after someone who has collapsed; haul them out by their rope.

Warning Sealed pots burst. Never seal a pot tightly while it is still fermenting. The gas pressure can shatter pottery and bottles and throw shards like a bomb. Use an airlock.

  • Lead poisoning. Never ferment, store or boil wine, vinegar or fruit juice in lead pots or lead-glazed ware. The Romans boiled grape juice in lead pans to sweeten it, and many were slowly poisoned.
  • Mouldy grain. Never brew with grain that is mouldy, or rye that carries ergot — hard, purple-black, horn-shaped growths replacing some grains in the ear. Ergot poisoning causes hallucinations, convulsions and gangrene.
  • Alcohol itself. Fermented drinks are drugs. They impair judgement around fire, water and tools, and are addictive. Children should not drink them. Ordinary fermentation does not make dangerous amounts of methanol; that danger appears in Distillation.

What this unlocks

How it was first done

People were fermenting long before they understood it. Pottery jars from Jiahu in northern China, about 9,000 years old (around 7000 BC), hold the residue of a drink of rice, honey and fruit. Grape wine was being made in the Caucasus, in what is now Georgia, by about 6000 BC, and residues of wine and beer have been found in jars at Godin Tepe in Iran from around 3500 BC. A Sumerian hymn to the beer goddess Ninkasi, written down about 1800 BC, is partly a brewing recipe. Egyptian workers building the pyramids were paid partly in beer.

Nobody knew what caused fermentation until the 1850s–1860s, when the French scientist Louis Pasteur showed that it is the work of living yeast, and that other microbes — not bad luck — spoil wine and turn it into vinegar. In 1883 Emil Christian Hansen at the Carlsberg brewery in Copenhagen grew the first pure yeast from a single cell, making brewing reliable for the first time.

Source: content/entries/chemistry/fermentation.md