Part 8 · Chemistry
Hydrochloric Acid
Warm common salt with sulfuric acid and a choking gas comes off; dissolve it in water and you have hydrochloric acid — "spirit of salt". It cleans rust and scale from metal, makes soldering flux and many useful chlorides, and turns bones into gelatin, glue and fertiliser.
- Difficulty
- ●●●●●
- Time
- An afternoon per batch in glass; 1–2 weeks to turn bones into gelatin
- Steps from zero
- 11 prerequisites →
The full path from nothing — 11 steps before this one
- Fire
- Finding and Preparing Clay
- Sulfur
- Pottery
- The Kiln
- Lime
- Salt
- Lye and Potash
- Glass
- Saltpeter
- Sulfuric Acid
- Hydrochloric Acid
Do them roughly in this order. See it on the tech tree →
Why it matters
Hydrochloric acid is the second great acid of industry, after Sulfuric Acid. It is made from the cheapest chemical you have — common Salt — and the acid you already have. Its old names say where it comes from: spirit of salt, and muriatic acid (from the Latin muria, brine).
With it you can:
- clean rust and scale off iron and steel before tinning, soldering, wire-drawing or plating (Soldering and Brazing, Electroplating, Tin and Pewter);
- make soldering flux ("killed spirits") by dissolving zinc in it;
- make chlorides — tin chloride for dyeing, iron chloride for etching copper, calcium chloride for drying air and gases;
- turn bones into gelatin (Gelatin) and glue, and their mineral into phosphate fertiliser (Glues and Adhesives, Chemical Fertilisers);
- make carbon dioxide from limestone and hydrogen from iron, for Hydrogen, Oxygen and Gases;
- make chlorine for bleach (Chlorine and Bleach) and, with Nitric Acid, aqua regia, the classic acid that dissolves gold (Gold and Silver);
- dissolve limescale from kettles, boilers and pipes, and identify carbonate rocks (Rocks and Minerals).
The leftover from making it is saltcake (sodium sulfate), the first step of the Leblanc process for Soda Ash and Baking Soda.
How it works
Sulfuric acid holds on to its hydrogen less tightly than you might think — when it meets salt and is warmed, it hands that hydrogen to the chlorine in salt and pushes it out as a gas, hydrogen chloride:
salt + sulfuric acid → hydrogen chloride gas + sodium bisulfate (gentle heat, 100–200 °C)
salt + sodium bisulfate → more hydrogen chloride gas + saltcake (strong heat, red heat)
Hydrogen chloride is a colourless, choking gas that makes white fog wherever it meets damp air. It dissolves in water astonishingly well: one litre of cold water swallows about 450 litres of the gas. The solution is hydrochloric acid.
Two facts follow from that, and both matter:
- Suck-back. Gas dissolves so fast that if a delivery tube dips into water, the water rushes back up the tube faster than gas can push it out — into the hot flask, which cracks or bursts. Every setup in this chapter is designed to stop that.
- You cannot concentrate it by boiling. The strongest acid that water will hold at room temperature is about 38 %, and it fumes. If you boil acid, it loses gas (if strong) or water (if weak) until it reaches about 20 %, which then boils at about 109 °C without changing. To get strong acid, you must absorb more gas — not boil.
What you need
For a first batch in glass, giving about 200 g of acid at roughly 30 %:
| Item | Amount or details |
|---|---|
| Salt | 100 g, dry; lumps or coarse crystals foam less than fine powder. Rock salt is ideal |
| Sulfuric acid | 90 ml (about 165 g) of concentrated acid, or about 220 g of 75 % "brown" acid (Sulfuric Acid) |
| Generating flask | A round flask or tubulated retort of 500 ml–1 litre (Laboratory Glassware) |
| Thistle funnel (optional) | A long tube with a funnel top, reaching nearly to the bottom of the flask, for adding acid little by little |
| Delivery tubes | Glass tubing with smooth bends, and bored corks or ground joints. Gut sleeves are attacked — keep them short and replace often |
| Safety bottle | An empty bottle between the flask and the water |
| Absorbers | Two bottles, each with 75 ml of cold rainwater or distilled water; one small glass funnel |
| Cooling | A bowl of cold water for the absorbers to stand in |
| Heat | A sand bath over a small charcoal fire or a spirit lamp |
| Neutraliser | A bucket of wood ash or crushed chalk, and two buckets of water |
| Protection | Eye shield, wool or leather over arms and hands, a cloth to tie over nose and mouth. Work outdoors |
Where to find it
- Salt — from seawater, brine springs or rock salt: see Salt. Any salt works. Bitter, damp "sea salt" that still contains magnesium salts works too, but gives a little less gas.
- Sulfuric acid — see Sulfuric Acid. Acid weaker than about 60 % gives little gas, because the water it contains holds the gas back. Boil weak acid down first.
- Manganese ore (for making chlorine, below): black, sooty, heavy lumps of pyrolusite that stain the fingers black, in bogs, streambeds and weathered rocks; see Finding and Identifying Ores.
Method 1: Making acid in glass
- Set up outdoors, on a firm bench, upwind of yourself and downwind of everyone else. Stand the absorbers in a bowl of cold water.
- Charge the flask. Put in the salt. If you use a thistle funnel, fit it and the delivery tube now; otherwise pour in the acid in one go and fit the stopper quickly.
- Connect the train: flask → empty safety bottle → first absorber → second absorber → a short tube venting downwind.
- In the first absorber, the gas tube ends in a small funnel turned upside down, with its rim just touching the water — not under it. If water rises into the funnel, the surface drops away from the rim, air gets in, and the water falls back.
- In the second absorber, the tube may dip 1 cm under the water. It catches what the first misses.
- Add the acid. Pour it through the thistle funnel a little at a time, about a fifth at once. Froth and white fumes start at once, even cold.
- Warm gently on the sand bath — the flask should feel too hot to hold but never boil hard. Bubbles should pass steadily through the second absorber, a few per second. If they race, take away heat.
- Keep the absorbers cold. Water warms as it dissolves the gas, and warm water holds less. Change the cooling water when it gets warm.
- Finish. After 1–2 hours the bubbling slows even with more heat. Before you take the heat away, lift the funnel and tube out of the absorbers. Then let the flask cool.
- Combine the two absorbers' contents in a glass bottle with a glass or waxed stopper. Label it.
- Clean out the flask while still warm: the white cake in it is sodium bisulfate, a dry acid. Dissolve it in water and keep it — it makes a milder pickle for metals, or heat it strongly with more salt to make saltcake for Soda Ash and Baking Soda.
The acid is often pale yellow from a trace of iron. That does not matter for any use in this book. For water-white acid, distil the finished acid gently in glass and keep the middle part.
Method 2: Making it by the litre
For larger amounts, follow the same idea with bigger vessels.
- Use a stoneware jar or a thick clay retort of 10–20 litres, set in a brick furnace (The Kiln), with salt and acid in the same ratio — about 1 part salt to 1.6 parts concentrated acid by weight. Hydrochloric acid does not attack well-fired clay, but the hot bisulfate slowly eats glazes.
- Lead the gas through clay pipes luted with clay and sand into a row of three or four large stoneware bottles half full of water, each joined to the next — the arrangement called Woulfe bottles. The first one has no water; it is the safety bottle.
- Or build an absorption tower: a vertical clay pipe 1.5–2 m tall and 15–20 cm across, packed with broken pottery or coke, with water trickling slowly down from a dish on top. The gas goes in at the bottom and rises through the wet packing; acid drips out of the base into a pot. This is what the soda works of the 1800s used.
How strong is it?
With a balance, fill the same cup to the same mark each time (Measurement from Scratch):
| Cup holds | Strength | Use |
|---|---|---|
| 100 g of water | — | — |
| about 105 g | about 10 % | pickling iron, cleaning |
| about 110 g | about 20 % | bone gelatin (diluted), general use |
| about 115 g | about 30 % | stock acid |
| about 118 g | about 36 % | strongest practical; fumes in air |
For exact work, titrate (Acids, Bases and Testing).
Using it
Pickling metal
Mix 1 part of 30 % acid into 2 parts water (about 10 %). Dip rusty or scaled iron in it — a few minutes for light rust, up to an hour for heavy forge scale — until it is clean grey. Rinse at once in water, then in lime water or wood-ash water to neutralise, and dry it near the fire. Bare pickled iron rusts within hours, so tin, solder, oil or paint it straight away. Brass and copper come bright in a few seconds.
Killed spirits (soldering flux)
In a glass or stoneware pot outdoors, drop scraps of zinc (Zinc and Brass) into strong acid, a few at a time, until it stops fizzing and a little zinc is left over. The gas is hydrogen — no flame nearby. Pour off the clear liquid: zinc chloride. Brushed onto iron, copper or brass, it dissolves the oxide film so solder flows and sticks (Soldering and Brazing). Wash the work afterwards; the flux leaves corrosive salts.
Other useful chlorides
- Calcium chloride. Dissolve limestone or chalk in the acid until it stops fizzing, filter, and boil dry. The white cake drinks water from the air — a dish of it keeps a closed box of tinder, seeds, salts or instruments dry, and a tube of it dries gases (Hydrogen, Oxygen and Gases). When it has turned damp, dry it again over the fire at about 200–250 °C and it can be reused. Do not take it to red heat: it melts at about 770 °C into a glassy lump.
- Tin chloride. Tin dissolved slowly in strong acid gives a mordant that makes red and scarlet dyes brilliant (Dyes and Mordants).
- Iron chloride. Rust or iron filings dissolved in the acid, then left in air to turn from green to brown, give a solution that etches copper — for printing plates and nameplates — far more safely than Nitric Acid.
Gelatin, glue and phosphate from bones
Bone is two things woven together: a hard mineral (calcium phosphate) and a tough protein framework (collagen). Acid dissolves the mineral and leaves the protein.
- Clean the bones. Boil fresh bones for an hour to loosen meat and draw out fat (skim it off for Soap). Crack or saw them into pieces about 2–3 cm.
- Soak in acid diluted to about 5 % (1 part of 30 % acid to 5 parts water), in a glazed or stoneware pot, enough to cover them twice over. It fizzes gently.
- Wait 1–2 weeks, stirring daily. Replace the acid with fresh after the first week. The bones are done when they are soft, translucent and bend like rubber, with no hard core when cut. This is ossein.
- Wash the ossein in many changes of clean water for a day, until a test paper shows the water is no longer acid. (For the clearest gelatin, soak it after that in lime water for 2–4 weeks and wash again.)
- Extract. Cover it with clean water and hold it at about 60–80 °C — steaming, but not boiling — for 3–5 hours. The ossein slowly dissolves. Strain through cloth.
- Set. The liquid sets into a jelly as it cools. Boil it down further for glue; or slice the jelly thin and dry it on nets in a breezy shade for sheet gelatin.
- Recover the phosphate. Stir slaked lime or chalk into the used acid liquor until it no longer turns cabbage indicator pink. A white powder settles — calcium phosphate in a form plants can use. Dry it and spread it on fields (Chemical Fertilisers).
Gelatin is food, glue for wood and paper, the binder of photographic films and plates (Photography), and — set with broth — the first solid medium for growing bacteria (Culturing Microbes), later replaced by Agar and Culture Plates, which does not melt at body heat.
Chlorine (with great care)
Warm strong acid with crushed pyrolusite (manganese dioxide) and a yellow-green gas comes off: chlorine. It bleaches cloth and disinfects water, and it is also a deadly poison gas. Do not try this until you have read Chlorine and Bleach.
How to tell it worked
- White fog. Blow gently across the open neck of strong acid: it fumes white. A rag damped with stale urine (ammonia) held near it makes thick white smoke.
- Fizzes with chalk and turns cabbage indicator red.
- Eats iron with bubbles, and the liquid turns pale green.
- The silver test. If you have silver (Gold and Silver) dissolved in nitric acid, one drop added to a little diluted acid makes a white curd that darkens in sunlight. That curd is the sure sign of chloride.
Note Troubleshooting. Little or no gas → the sulfuric acid is too weak (below about 60 %); boil it down. Or the salt is wet. Flask froths over into the safety bottle → too much acid at once, fine powdered salt, or too much heat. Add acid in portions; use lumps. Water climbs up into the safety bottle → suck-back. That is what the safety bottle is for. Raise the funnel, increase the heat a little, and empty the bottle afterwards. Acid is weak → absorbers got warm, or too much water in them. Use less water, keep it cold, and run a second batch of gas through the same acid. Corks swell and crumble → acid fumes. Use ground joints or clay-and-sand lute, and fresh corks each batch.
Dangers
Danger The gas attacks eyes and lungs. Hydrogen chloride burns the eyes, nose and throat, and a lungful can cause choking, coughing up blood and fluid in the lungs. Work outdoors, upwind, with the vent pointing away from everyone. If you start coughing, walk away into fresh air at once. Anyone who has breathed a lot of it must rest and be watched for a day.
Danger Never mix it with bleach. Hydrochloric acid poured on bleach, or on bleaching powder, releases chlorine gas — a poison that has killed people cleaning a small room. Keep them on different shelves.
- Skin and eyes. Strong acid burns skin and blinds. Flood any splash with lots of water for 20 minutes; for eyes, hold them open under a gentle pour of water for 30 minutes. Keep your eye shield on while pouring.
- Suck-back can crack a flask full of hot sulfuric acid. Always use a safety bottle and never let a tube dip deeply into water. Remove the tubes from the water before you stop heating.
- Hydrogen. Acid on iron or zinc gives off hydrogen, which explodes with a flame. Keep pickling and flux-making away from fire.
- Corrosion. The fumes rust every iron tool in the workshop. Store the acid in glass with a ground or waxed stopper, or in waxed stoneware, in a separate shed — never in metal, and never next to tools.
- Spills. Cover with wood ash or crushed chalk; wait for the fizzing to stop; wash away with plenty of water.
What this unlocks
- Soda Ash and Baking Soda — the saltcake left over is the start of the Leblanc process.
- Soldering and Brazing, Electroplating, Tin and Pewter — clean, pickled metal.
- Glues and Adhesives, Photography, Culturing Microbes — gelatin from bone.
- Chemical Fertilisers — phosphate from bone.
- Chlorine and Bleach — chlorine from acid and manganese ore.
- Gold and Silver — aqua regia, with Nitric Acid.
- Hydrogen, Oxygen and Gases — carbon dioxide and hydrogen generators.
How it was first done
Medieval alchemists probably made impure hydrochloric acid by distilling salt with vitriols or clay, and "spirit of salt" was known in Europe by the 1500s. In 1648 the German-Dutch chemist Johann Rudolf Glauber described the method of this chapter — salt heated with oil of vitriol — and noticed that the residue was a useful new salt, still called Glauber's salt (sodium sulfate). In 1772 Joseph Priestley collected the gas itself over mercury and called it "marine acid air". In 1774 Carl Wilhelm Scheele made chlorine from it with pyrolusite, and in 1810 Humphry Davy showed that chlorine is an element.
The acid became an industrial by-product of the Leblanc soda works in the early 1800s, which at first simply vented the gas — killing crops and trees for miles around. William Gossage's absorption tower of 1836 captured it, and Britain's Alkali Act of 1863, one of the first pollution laws anywhere, made capturing it compulsory. Once captured, the acid was turned into chlorine and bleaching powder, and became a product in its own right.
Source: content/entries/chemistry/hydrochloric-acid.md