◆ Rebuild

Part 15 · Knowledge and Science

Measuring Angles: Theodolite and Sextant

How to divide a circle into degrees, read it to a single minute with a vernier, and build the two great angle-measuring instruments — the theodolite, which maps land and lays out roads and tunnels, and the sextant, which finds a ship's latitude from the sun and the horizon.

Difficulty
●●●●●
Time
Two to three weeks for a wooden sighting theodolite or octant; months for a brass instrument with telescope and verniers
Steps from zero
29 prerequisites →

You need first

Geometry and TrigonometryThe Telescope

This unlocks

—
The full path from nothing — 29 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Sulfur
  7. Writing and Numbers
  8. Hunting and Trapping
  9. Basic Woodworking
  10. The Kiln
  11. Pottery
  12. Charcoal
  13. Arithmetic and Fractions
  14. Hides and Leather
  15. Lime
  16. Lye and Potash
  17. Geometry and Trigonometry
  18. Glass
  19. Bellows
  20. Saltpeter
  21. Copper Smelting
  22. Lead
  23. Sulfuric Acid
  24. Lenses
  25. Gold and Silver
  26. Nitric Acid
  27. Silver Nitrate and Silver Salts
  28. Mirrors
  29. The Telescope
  30. Measuring Angles: Theodolite and Sextant

Do them roughly in this order. See it on the tech tree →

Why it matters

Distances are slow and hard to measure across rough country, rivers and sea. Angles can be measured from one spot, in seconds, to things far out of reach. With a good angle and one measured line, Geometry and Trigonometry gives you every other length. That is how whole countries were mapped (Maps and Mapmaking), how tunnels started from both ends meet in the middle, how railways and canals keep their gradients, and how a ship out of sight of land knows how far north it is (Navigation).

The simple instruments in Surveying and Levelling and Navigation — the plane table, the quadrant with its plumb line, the cross-staff — read to a quarter or half a degree. This chapter takes you to one minute of angle (a sixtieth of a degree) and better. At sea, one minute of latitude is one nautical mile (1,852 m); on land, a minute is 3 cm at 100 m. That is the difference between "somewhere on this coast" and "this harbour mouth".

How it works

Every angle instrument has three parts:

  1. A divided circle or arc — a ring marked in degrees.
  2. A sight that points at the object — two vanes with slits and hairs, or a small telescope with a crosshair (The Telescope).
  3. A way to read exactly where the sight's pointer falls on the circle — a vernier.

Two tricks turn crude work into fine work:

  • Measure everything twice in ways whose errors are opposite, and average. Read two pointers on opposite sides of the circle; measure an angle with the telescope one way up and then flipped over. Most errors in making the instrument cancel.
  • Check against things that must be true. The three angles of a triangle add to 180°; a level must read the same when turned end for end; a sextant must read zero when looking at the horizon twice.

What you need

Item Details
Wood for frames Well-seasoned, straight-grained hardwood or boxwood; oak, pear, mahogany. Seasoned at least two years, or it warps
Brass or bronze For arcs, pivots, clamps and screws, if you have it (Zinc and Brass, Bronze)
Dividers and a beam compass Two hard steel points on a bar, with a fine adjusting screw (Scientific Instrument Making)
A scriber A hard steel needle, ground to a fine point
A magnifier f = 3–5 cm (Lenses)
Mirrors Flat, small; silvered glass or polished speculum metal (Mirrors)
Spirit level vials Glass tube 8–10 mm bore, 8–12 cm long (Laboratory Glassware), filled with strong alcohol (Distillation)
Crosshair Fine silk fibre or spider thread
Small telescopes Keplerian, focused on infinity, with crosshair (The Telescope)
Fine screws For clamps and slow-motion (Screws, Nuts and Bolts)
Dark glass Several pieces of deeply coloured glass, for looking at the sun

Dividing a circle

radius 0° 60° 120° 180° 30° 15° Bisect Step the radius round: exactly six steps, 60° each 1. Construct 60°, 30°, 15° 2. Divide 15° into three by trial 0° 15° Too wide: overshoots close the dividers by a third of the overshoot and try again 0° 5° 10° 15° Just right: lands exactly then divide each 5° into five the same way
Fig. 1 Dividing a circle by construction. The radius steps round the circle exactly six times, giving 60°. Bisect to get 30° and 15°. Divide each 15° by trial into three, then each 5° into five, opening and closing the dividers until their steps fit exactly.
  1. Choose the size. A bigger circle reads finer. On a circle of radius 15 cm, one degree is 2.6 mm along the edge; on 30 cm, 5.2 mm. For a first theodolite, 12–15 cm radius; for an octant, an arc of 25–30 cm radius.
  2. Scribe the circle with a beam compass round a fine centre punch mark. Do not move the centre again; everything depends on it.
  3. 60° by stepping the radius. With the dividers set exactly to the radius, step round: they cut the circle into six equal parts.
  4. Bisect each 60° to make 30°, and again to make 15°: from two marks, swing equal arcs that cross outside the circle, and lay a straightedge from the centre through the crossing (Geometry and Trigonometry).
  5. Thirds by trial. Set the dividers by eye to a third of 15°. Step three times from one mark. If you overshoot the next mark, close the dividers by one third of the overshoot, and try again. Five or six tries get it exact. Now you have 5°.
  6. Fifths by trial in the same way gives single degrees; then halves or thirds of a degree (30' or 20') if the circle is large enough.
  7. Cut the lines. Lay a thin, straight steel edge from the centre pin to each mark and draw the scriber along it once, firmly. Make every 5th line longer and every 10th longer still. Number every 10°.
  8. Fill the lines with black wax or soot in oil, and wipe the surface clean.

Tip Check the division by stepping the dividers set to, say, 37° from several different starting points round the circle. They should land on a line every time. Note any line that is off and correct it before you go finer.

Later, a dividing engine — a large wheel turned by a fine screw — divides circles to a few seconds of angle with no trial at all (Scientific Instrument Making).

The vernier

You cannot cut and read lines much closer than about half a millimetre. The vernier reads ten or thirty times finer than the lines on the circle, with no extra lines on it at all.

The idea. Beside the main scale, a short sliding scale (the vernier) has n divisions that together span exactly n − 1 divisions of the main scale. Each vernier division is therefore a little shorter than a main division — short by one nth of a main division. When the vernier's zero sits a little past a main line, exactly one vernier line lines up with a main line, and its number tells you how far past.

47° 48° 49° 50° 51° 52° 53° 54° 55° 56° 57° 58° 59° 60° 61° 62° 0 5 10 15 20 25 30 Main scaledivided in half degrees (30') Vernier30 divisions span 29 half degrees, so it reads to 1' 47°30' line Vernier zerojust past 47°30' The 17th line lines up exactlywith a main-scale line Reading: 47°30' + 17' = 47°47'
Fig. 2 Reading a vernier. The main scale is divided in half degrees. The vernier has 30 divisions that span 29 half-degrees, so it reads to one minute. Its zero lies just past 47°30'; the 17th vernier line lines up exactly with a main line, so the reading is 47°30' + 17' = 47°47'.

Worked example. The circle is divided in half degrees (30'). The vernier has 30 divisions occupying 29 half-degrees. It reads to 30' ÷ 30 = 1'.

  1. Find the vernier's zero. It lies between 47°30' and 48°00'. Write down 47°30'.
  2. Run your magnifier along the vernier and find the one line that lines up exactly with a main-scale line. It is the 17th.
  3. Add: 47°30' + 17' = 47°47'.

Making one. Scribe the vernier on its own small arc of the same radius as the main circle. Step out 29 main divisions on it with the dividers, then divide that length by trial into 30 equal parts. A straight vernier for a ruler works the same way: 10 vernier divisions over 9 mm read to 0.1 mm — the principle of the vernier caliper (Measurement from Scratch, Machine Tools).

The spirit level

Every angle instrument must be set level. A spirit level vial is a glass tube very slightly curved along its length, almost filled with alcohol, leaving one bubble. The bubble always seeks the highest point of the curve.

  1. Close one end of a glass tube in the flame. Warm the middle and let it sag very slightly — a curve of 2–5 m radius — or, better, grind the inside to a gentle barrel shape with a rod and fine emery.
  2. Fill with strong alcohol through a drawn-out end, leaving a bubble about a third of the tube's length. Seal the end in the flame.
  3. Mount it in a wooden or brass holder with an adjusting screw at one end.
  4. Mark lines 2 mm apart on the glass either side of the middle.

Testing a level. Set it on a flat surface and note the bubble. Turn it end for end on the same spot. If the bubble moves, adjust the holder screw to take out half the movement and level the surface for the other half. Repeat until the bubble stays still when reversed. This reversal trick, used everywhere below, finds errors in any instrument without needing a perfect standard.

Sensitivity. If the tube's curve has radius R, tilting it by a small angle moves the bubble R × angle (in radians). For R = 3 m, a 2 mm movement means a tilt of about 2 minutes of angle.

Method 1: The theodolite

Objective telescope 10–20× Eyepiece and crosshair Vertical circle reads the tilt up or down Trunnion axis telescope can turn right over Standard A-frame, one each side Plate levels two, at right angles Upper plate two verniers 180° apart, clamp Horizontal circle on the lower plate Three foot screws for levelling Tripod seasoned wood, iron points Plumb bob over the station mark
Fig. 3 The theodolite. The lower plate carries the horizontal circle; the upper plate turns on it, carrying two verniers, two levels and the standards. The telescope turns up and down on the trunnion axis, with a vertical circle to read its tilt. Three foot screws level the whole, over a plumb bob hanging above the station mark.

Building it

  1. Tripod. Three straight legs 1.4–1.5 m long of seasoned wood, with iron points, hinged to a solid wooden head. A hook under the centre carries a plumb bob.
  2. Levelling head. A plate on three foot screws (or, more simply, a ball-and-socket joint you can lock).
  3. Lower plate. A disc carrying the horizontal circle, divided in half degrees, on a central upright spindle. A clamp locks it to the head.
  4. Upper plate (the alidade), turning on the same spindle, carrying two verniers 180° apart, two levels at right angles to each other, and two upright standards shaped like the letter A.
  5. Telescope. A Keplerian telescope with a crosshair, 20–30 cm long, magnifying 10–20× (The Telescope). Fix it to a horizontal trunnion axis resting in notches at the top of the standards, so it can tip up and down and even turn right over.
  6. Vertical circle fixed to the trunnion axis, with a vernier on the standard, to read the telescope's tilt above or below level.
  7. Clamps and slow-motion screws on the upper plate and the trunnion: clamp roughly, then turn the fine screw to put the crosshair exactly on the target.

A first instrument can use open sights — a vane with a slit at one end, a vane with a fine thread at the other — instead of a telescope. It will read to about 5–10 minutes. The telescope and crosshair bring it to 1 minute or better.

Setting up over a station

  1. Plant the tripod over the mark (a nail in a peg) with the head roughly level. Hang the plumb bob; shift the legs until it hangs within 3 mm of the nail.
  2. Level. Turn the upper plate so one level lies along two of the foot screws. Turn those two screws in opposite directions — thumbs moving towards each other or apart — until the bubble is central. Turn the plate 90° and centre the bubble with the third screw. Repeat both steps. Turn the plate 180°: if the bubble moves, take out half with the level's own screw and half with the foot screws.

Measuring a horizontal angle

  1. Clamp the lower plate. Unclamp the upper plate and sight the left target. Clamp and use the slow-motion screw to set the vertical crosshair exactly on it — on the foot of a pole, never its top, which may lean.
  2. Read both verniers; average their minutes. (This cancels any error in centring the circle on its spindle.)
  3. Unclamp the upper plate, swing right to the second target, set it exactly, and read again.
  4. The angle is the difference of the two readings.
  5. Change face. Turn the telescope right over on its trunnions and swing the plate round 180°. Repeat steps 1–4. Average the two results. This cancels a crosshair that is a little off centre or a trunnion axis that is not quite square.

Vertical angles. Level carefully, sight the target, and read the vertical circle. Measure face left and face right; the average removes any error in the circle's zero.

Worked example: a triangle

You measured a baseline AB = 412.36 m with great care (Surveying and Levelling). From A, B and C you measure the three angles of triangle ABC:

Station Angle measured Correction Corrected
A 62°18' −1' 62°17'
B 54°41' −1' 54°40'
C 63°04' −1' 63°03'
Sum 180°03' −3' 180°00'

The sum should be exactly 180°. The error of 3' is shared equally. An error larger than about 1' per angle with a good theodolite means a mistake — measure again.

By the sine rule, each side ÷ sine of the opposite angle is the same:

  • BC = AB × sin A ÷ sin C = 412.36 × 0.8853 ÷ 0.8914 = 409.5 m
  • AC = AB × sin B ÷ sin C = 412.36 × 0.8158 ÷ 0.8914 = 377.4 m

(You need a sine table to minutes — calculate one as in Geometry and Trigonometry and print it once for everyone.) Each new side becomes the base of the next triangle, and so a chain of triangles crosses a valley or a country.

Height by vertical angle. From a point 850 m (measured on the map) from a hilltop beacon, the telescope, 1.45 m above the ground, tilts up 4°12' to the top of a 2.00 m pole on the summit. Height difference = 850 × tan 4°12' + 1.45 − 2.00 = 62.42 + 1.45 − 2.00 = 61.9 m.

Method 2: The sextant

How it works

The sextant uses two mirrors to bring two things together in one view: the horizon seen straight ahead, and the sun or a star reflected down onto it. Because turning a mirror by some angle turns its reflection by twice that angle, an arc of only 60° (a sixth of a circle — hence the name) measures angles up to 120°. The arc is marked in double degrees, so you read the true angle directly.

The beauty of it at sea: the two images move together as the ship rolls, so you can hold them in contact. A plumb-line quadrant cannot do this.

0 20 40 60 80 100 Index mirror on the arm, over the pivot Sighting telescope 2–4×, looks at the horizon glass Horizon glass one half silvered, one half clear Shades dark glass for the sun Index arm swings across the arc Vernier, clamp and slow-motion screw Arc of 60° marked 0–120 Sun Horizon seen straight through
Fig. 4 The sextant. The index mirror on the swinging arm reflects the sun onto the horizon glass, which is silvered on one half only; through the clear half you see the horizon directly. Move the arm until the sun's lower edge just touches the horizon, and read the angle on the arc.

Building it

  1. Frame. A rigid triangle of seasoned hardwood or brass with a 60° arc of radius 15–20 cm at the bottom, carrying a strip of boxwood, ivory or brass for the divisions. (An octant — a 45° arc reading to 90° — is easier in wood and enough for the noon sun at most latitudes.)
  2. Index arm. A straight bar pivoted at the top of the frame, its lower end sliding over the arc and carrying the vernier, a clamp and a slow-motion screw.
  3. Index mirror. A flat mirror about 5 × 4 cm fixed on the arm, directly over the pivot, standing square to the frame.
  4. Horizon glass. A small flat glass about 3 × 3 cm fixed to the frame, square to it, with one half silvered and the other half clear. Set it so that it is parallel to the index mirror when the arm reads zero.
  5. Sight. A small tube, or a small Galilean telescope of 2–4×, on the frame, aimed at the horizon glass.
  6. Shades. Hinged frames holding dark glasses between the index mirror and the horizon glass, and others in front of the horizon glass. Make at least three of different darkness.
  7. Divide the arc as above, but number every half-degree of arc as one degree, because the mirror doubles the angle. Split each of these again into two, so each line stands for 30' of reading (a quarter-degree of real arc, about 0.7 mm on a 16 cm radius). A vernier of 30 divisions spanning 29 of these lines reads to 1', just as on the theodolite.

Adjusting it

  1. Index mirror square to the frame. Hold the sextant flat, arc away from you, and look into the index mirror at a slant. The arc seen directly and its reflection must form one unbroken curve. If they step, adjust the mirror's screws.
  2. Horizon glass square to the frame. Set the arm near zero and look at the horizon or a star. Rock the arm slowly: the reflected image should pass exactly over the direct one, not beside it.
  3. Index error. Set the arm near zero and look at the sea horizon (or a distant level roofline). Turn the slow-motion screw until the reflected horizon and the direct horizon make one straight line. Read the scale. If it reads above zero — "on the arc" — subtract that much from every reading. If below — "off the arc" — add it. Check every time you use it.

A noon sight for latitude

  1. Shades down — all of them — before you look.
  2. Aim the sight at the horizon directly under the sun. Swing the arm forward from zero until the sun's image appears in the silvered half. Clamp.
  3. With the slow-motion screw, bring the sun's lower edge down to just touch the horizon.
  4. Swing the arc: rock the sextant gently side to side about the line of sight. The sun swings in a little curve; it should just kiss the horizon at the bottom of each swing.
  5. As noon approaches, the sun climbs; keep it touching. When it stops rising and starts to dip, the highest reading is the noon altitude.

Corrections (to turn the reading into the true height of the sun's centre):

Correction Size Why
Index error As found The instrument's own zero
Dip −1.76' × √(height of your eye above the sea, in metres) You see over the curve of the sea, so the horizon lies below true level
Refraction −10' at 5° altitude, −5' at 10°, −2' at 25°, −1' at 45°, almost 0 overhead Air bends light, lifting low objects
Semi-diameter +16' for the lower edge You measured the edge, not the centre

Worked example. On 21 March, from a deck 4 m above the sea, the noon reading of the sun's lower edge is 52°36'. Index error is 2' on the arc.

  • 52°36' − 2' (index) = 52°34'
  • Dip: 1.76 × √4 = 3.5' → 52°30.5'
  • Refraction at 52°: about −0.8' → 52°29.7'
  • Semi-diameter: +16' → 52°45.7', call it 52°46'

The sun's declination on 21 March is close to 0° (look up the exact figure for the day and hour in the Almanacs and Astronomical Tables), and it is to the south, so latitude = 90° − 52°46' + 0° = 37°14' north (Navigation).

On land, with no sea horizon, use an artificial horizon: a shallow dish of dark oil or water, sheltered from wind under a small glass roof. Measure the angle between the sun (or a star) and its reflection in the liquid. The true altitude is half that angle, after the index correction. There is no dip. (Old surveyors used a pool of mercury; it is poisonous — see Mercury.)

Other uses. Held flat, a sextant measures the angle between two landmarks from a boat; two such angles to three charted landmarks fix the boat's position exactly. With a good almanac (Almanacs and Astronomical Tables), the angle between the moon and a star gives the time at home, and so longitude — the "lunar distance" method, accurate but long to calculate.

How to tell it worked

  • Theodolite: the angles of a triangle close within 1' per angle; the bubble stays central when the plate turns; face-left and face-right readings agree within 1–2'.
  • Sextant: index error found three times in a row agrees within half a minute; the noon latitude at a place of known latitude comes out within 2–3'.
  • Repeat a measurement on another day. Differences show your real accuracy.

Note Troubleshooting. Angles of triangles never close → the circle is badly divided or off-centre; always read both verniers; recheck the division by stepping the dividers. Bubble wanders as the plate turns → the level is out of adjustment; use the reversal method; check the spindle is not loose. Readings change through the day → the tripod is settling or the wood is moving with sun and damp; drive the legs in firmly, shade the instrument, use seasoned wood. Sextant index error keeps changing → loose mirror mounts or a warping frame; tighten, and keep the sextant out of the sun when not in use. Two sun images, or a ghostly double horizon → the mirrors are not flat, or the glass is too thin and bends in its frame.

Dangers

Danger The sun through a sextant or theodolite telescope blinds in an instant, painlessly and for ever. Put all the shades in place before you look towards the sun, starting with the darkest, and open them one at a time only if the sun looks dim. Never point a theodolite telescope at the sun at all. Teach every new user this before they touch the instrument.

  • Lightning. A metal-tipped tripod on a hilltop in a thunderstorm is a lightning rod. Leave the summit when thunder is heard (Reading the Weather).
  • Falls. Surveyors look through instruments, not at their feet; check the ground before you step back, especially on cliffs and quays.
  • Mercury for an artificial horizon gives off poisonous vapour; use oil or water.
  • Tripod points are sharp; carry the tripod upright, points down.

What this unlocks

With a theodolite you can run a triangulation over a whole region and draw true Maps and Mapmaking; set out Railways, Canals and Locks, Roads and Bridges and tunnels (Tunnels and Rock Drilling) so that both ends meet; and measure the height of mountains. With a telescope fixed to point only north–south, the same parts make a transit instrument for exact time from the stars (Astronomy, Building an Observatory, The Mechanical Clock). With a sextant and a good sea clock (Chronometers and Stopwatches), a ship can find its place anywhere on the ocean (Navigation).

How it was first done

Greek astronomers such as Hipparchus (2nd century BC) measured star positions with large divided rings. Around 1533 the Dutch mathematician Gemma Frisius described triangulation from a measured baseline. In 1571 the English surveyor Leonard Digges's book Pantometria, published by his son, described an instrument he called the "theodelitus". The Portuguese mathematician Pedro Nunes devised a way to read fractions of a degree in 1542, and the Frenchman Pierre Vernier published the simpler scale that bears his name in 1631. In the 1640s William Gascoigne in England put crosshairs — reputedly a spider's thread — in a telescope. In 1731 John Hadley in London and, independently, Thomas Godfrey in Philadelphia made the reflecting octant; in 1757 Captain John Campbell extended it to the sextant. Jesse Ramsden built a dividing engine in the 1770s that divided circles quickly and accurately, and in 1787 a great theodolite with a 90 cm circle that linked the observatories of Greenwich and Paris by triangulation. Instruments of this kind measured India in the Great Trigonometrical Survey through the 1800s and found Mount Everest to be the highest mountain on Earth.

Source: content/entries/knowledge/angle-instruments.md