Part 6 · Building
Timber Framing and Log Building
How to turn standing trees into houses and barns — stacking notched logs into a cabin, or hewing square beams and joining them with pegged mortise-and-tenon joints into a frame that is raised in a day and stands for centuries.
- Difficulty
- ●●●●●
- Time
- A log cabin in one summer for three people; a timber frame takes weeks of cutting and one day to raise
- Steps from zero
- 14 prerequisites →
This unlocks
Building Against Earthquakes and StormsDoors, Windows and JoineryRoofsScaffolding and LaddersStairs, Floors and Interior FinishesTrusses and FramesRot, Woodworm and TermitesPlaygrounds and Outdoor PlayThe full path from nothing — 14 steps before this one
- Stone Tools
- Fire
- Cordage and Rope
- Finding and Preparing Clay
- Finding and Identifying Ores
- Basic Woodworking
- Hunting and Trapping
- Charcoal
- Hides and Leather
- Bellows
- Iron (the Bloomery)
- Blacksmithing
- Steel
- Axes, Chisels, Knives and Planes
- Timber Framing and Log Building
Do them roughly in this order. See it on the tech tree →
Why it matters
Wood is strong, light for its strength, easy to cut, and grows back. With a sharp axe you can turn a forest into houses, barns, mills, bridges and ships. A wooden building goes up much faster than stone and stands well in earthquakes, because its joints flex instead of cracking. Many timber-framed buildings in Europe and Japan are over 500 years old.
There are two main ways to build with timber. Log building stacks whole logs into walls, notched at the corners — the quickest way to a warm, solid house where straight conifers grow. Timber framing makes a skeleton of squared beams locked together with wooden joints and pegs, then fills the walls with something else: wattle and daub or cob (Cob, Adobe and Rammed Earth), brick, or boards. A frame uses far less wood than log walls and can be much larger — big enough for a barn or a The Watermill.
This chapter assumes the basics of felling, splitting and seasoning from Basic Woodworking, and iron tools from Axes, Chisels, Knives and Planes.
How it works
- Wood is strong along the grain and weak across it. A post standing upright carries enormous weight. A beam lying across a gap bends, and its strength grows with the square of its depth and its stiffness with the cube: a beam twice as deep is four times as strong and eight times as stiff. Always set beams on edge, deep rather than wide.
- Triangles do not change shape; rectangles do. A box of posts and beams will fold sideways like a matchbox in a strong wind. A short diagonal brace in each corner turns it into triangles, and the frame becomes rigid.
- Wet wood rots; dry wood lasts. Rot fungi need water and air (Rot, Woodworm and Termites). Wood kept dry, or kept wholly underwater, can last a thousand years. Keep every timber off the ground and under a roof.
- Green wood shrinks as it dries — hardly at all along its length, but 5–10% across. A log wall gets shorter as it dries; a frame's joints shrink tight onto their pegs.
What you need
| Tool | Use | Notes |
|---|---|---|
| Felling axe | Felling, notching, scoring | 1.5–2 kg head. See Axes, Chisels, Knives and Planes |
| Broadaxe | Hewing flat faces | Wide (20–30 cm) blade, bevelled on one side only, handle bent away from the work |
| Adze | Flattening, trimming | Blade across the handle, like a hoe |
| Auger | Boring holes for mortises and pegs | 2.5 cm and 5 cm bits. See Drills and Boring |
| Chisels | Cleaning mortises, cutting tenons | A heavy 5 cm framing chisel; see Axes, Chisels, Knives and Planes |
| Saw | Cutting to length, tenon shoulders | See Files and Saws; an axe can do it, slowly |
| Wooden mallet (beetle) | Driving chisels, pegs and joints home | A big one, 5–10 kg, for joints |
| Chalk line | Marking long straight lines | Cord rubbed with charcoal or wet ochre, snapped onto the wood |
| Square, plumb line, level, measuring rod | Layout | See Measurement from Scratch |
| Rope, pike poles, cant hook | Moving and raising | See Cordage and Rope and Cranes and Lifting |
Timber. Choose durable, straight trees. Oak heartwood is the classic framing timber; chestnut, larch, black locust, cedar and Douglas fir are also excellent. For log walls, straight conifers (pine, spruce, fir, larch, cedar) are best: light, straight and even. The pale sapwood under the bark rots quickly in most trees; the darker heartwood lasts. Fell in winter, when sap is down; the wood dries with fewer cracks and less insect attack.
A small log cabin 5 × 6 m needs about 40–50 logs 20–30 cm thick and 6–7 m long. A timber frame for the same house needs perhaps 15–20 trees.
Method 1: Log building
The logs
- Fell and peel. Strip the bark the same season you fell, with an axe or a drawknife. Bark left on traps moisture and feeds beetles.
- Match them. Use logs of similar thickness for each wall. Logs taper, so alternate butts and tops — thick end of one log over the thin end of the one below — to keep the walls level.
- Season if you can. Logs left a few months to a year under a roof shrink less in the wall. Green logs work, but the wall will settle more (below).
The foundation
Lay the first logs (the sills) on stone: a continuous stone wall or large flat stones at each corner and every 2 m, with their tops at least 30 cm above the ground (Foundations and Floors). A layer of birch bark or slate between stone and wood stops moisture rising.
Notching the corners
- Saddle notch (for round logs). Roll the next log into place across the one below. Set a pair of dividers — or two sticks tied in a V — to the gap between the logs, and scribe the curve of the lower log onto the upper one. Roll the upper log over and chop out a rounded notch on its underside to the scribed line, about a third of its thickness deep. Roll it back. It should sit snugly. Always notch the underside: a notch on top holds rainwater and rots.
- Dovetail notch (for logs hewn flat on two faces). Each end is cut with sloping faces that lock the logs in both directions, with no peg. Slow to cut, but very strong and it sheds water.
- Scribed fit. In Scandinavia, each log has a long groove scooped along its underside to fit over the log below, with dry moss packed in the groove. It makes a tight, almost draught-free wall.
Building up
- Lay the logs course by course, ends sticking out 20–30 cm past each corner.
- Check the walls are plumb with a plumb line every course.
- At about every fourth course, drive dowels — 2.5–3 cm pegs of dry hardwood — down through holes bored in the logs, every 1.5 m, to stop them bowing. Bore the holes a little longer than the dowels so the logs can settle.
- Openings. Build the wall solid, then saw out doors and windows. Peg a thick plank (a jamb) to the cut log ends on each side, using slots, not fixed nails, so the logs can slide down past it as they settle.
- Settling. A wall of green logs can sink 3–6% as it dries — 10–15 cm on a 2.5 m wall. Leave a gap that size above every door and window frame and stuff it loosely with moss or wool.
- Chinking. Fill gaps between round logs with split wood wedges, then pack them with daub: clay, sand and chopped straw, or lime mortar with hair (Lime). Redo cracks after the first year.
Wood insulates several times better than earth or stone: a 25 cm log wall keeps out more cold than a cob wall a metre thick, though it stores far less heat.
Method 2: Hewing square beams
A frame needs squared timbers. Before sawmills (Sawmills and Lumber), they were hewn with axes.
- Set the log on two short cross logs and fix it with iron dogs (big staples) or wedges so it cannot roll.
- Mark the ends. On each end draw the square of the finished beam inside the circle of the log, using a plumb line to make the sides vertical.
- Snap the lines. Stretch a charcoal-rubbed cord along the log from corner mark to corner mark, lift it, and let it snap against the bark (scrape a strip of bark off first).
- Score. Standing on the log, chop V-cuts with the felling axe every 10–15 cm, down to just short of the line.
- Juggle. Split off the chunks between the score cuts with the axe. This takes off most of the wood quickly.
- Hew. Standing beside the log, chop down with the broadaxe along the line, its flat face toward the finished face, taking off thin slices. Work from one end to the other.
- Roll the log and repeat for the other faces. Two faces flat is enough for log walls and floor joists; four for frames.
A practised hewer squares several metres of beam a day; a beginner, much less. Hew green wood — it is far softer than dry.
Method 3: The timber frame
The parts
| Part | What it does | Typical oak size for a small house |
|---|---|---|
| Sill | Beam lying on the foundation; posts stand in it | 20 × 20 cm |
| Post | Upright, carries the load down | 15–20 cm square |
| Girt | Horizontal beam between posts at floor or mid height | 15 × 20 cm |
| Plate | Beam along the tops of the posts; rafters sit on it | 15 × 20 cm |
| Tie beam | Crosses the building at the post tops, stops the roof pushing the walls apart | 20 × 25 cm for a 6 m span |
| Brace | Diagonal in the corners, at about 45° | 10 × 12 cm, 90–120 cm long |
| Rafter | Pairs meeting at the ridge | 10 × 12 cm, every 40–60 cm |
| Peg (treenail) | Locks each joint | 2.5 cm, split from dry oak |
A bent is one cross-section of the frame: two posts, a tie beam and their braces. A house has bents every 3–5 m; the spaces between are bays.
The pegged mortise and tenon
The mortise and tenon (introduced in Basic Woodworking) is the joint that holds a frame together.
- Lay out from one face. Choose the straightest face and edge of each timber as the reference faces, and measure every joint from them, not from the rough faces.
- Mortise. Usually 5 cm wide and 10–12 cm deep in a 15–20 cm post. Bore a row of overlapping holes with a 5 cm auger, then chop the sides straight with a chisel.
- Tenon. Saw the shoulders across the beam, then split and chisel off the waste to leave a tongue 5 cm thick and 1 cm shorter than the mortise is deep (so it bottoms on the shoulder, not its tip).
- Test. It should go in with firm mallet blows — not loose, not split the mortise.
- Drawbore. Bore the 2.5 cm peg hole through the mortise cheeks, 4–5 cm from the face that the shoulder will meet. Put the tenon in, mark the hole on it, take it out, and bore the tenon hole 2–3 mm closer to the shoulder. When the peg is driven through the offset holes it bends slightly and pulls the shoulder hard against the post. Such joints stay tight for centuries without glue or metal.
- Pegs. Split them from straight-grained, dry oak, shave them roughly octagonal, slightly tapered, 2–3 cm longer than the joint. Split pegs are far stronger than sawn ones.
Fit each joint and number it with marks cut by a chisel (Roman numerals are traditional) so the frame goes together the same way on raising day. Do not peg until the raising.
Green or dry?
Frames have usually been cut from green oak — it is soft and quick to work — and left to dry standing. The frame shrinks onto its drawbored pegs and stays tight, but cracks (checks) will open along the beams; these are normal if they are not at a joint. Use seasoned wood for pegs, floorboards, doors and anything that must keep its shape (see Basic Woodworking).
Raising the frame
- Build the foundation and the sills first, level and square. Check the diagonals are equal (Measurement from Scratch).
- Assemble each bent flat on the sill platform, joints pegged, its post feet lined up with their mortises in the sill.
- Raise. Many hands lift the top end; as it rises, people with pike poles (straight poles 4–6 m long with an iron spike) push higher, while two ropes run back to people on the far side to stop it going over. A gin pole (a single tall pole with a pulley at the top, see Cranes and Lifting) helps with heavy bents. A bent of green oak for a 6 m house weighs 500–700 kg: allow a person for every 25–30 kg.
- Brace it. As soon as it is upright, plumb it and nail or tie temporary diagonal poles from it to stakes in the ground.
- Join the bents with girts and plates, peg everything, then fit rafters in pairs, starting from the ends.
Raising days were community festivals: a barn that took weeks to cut went up in one day with twenty or forty neighbours.
How to tell it worked
- Push hard on a corner post at head height: a braced frame does not move.
- Every joint is tight — no daylight around the shoulders.
- Posts are plumb and the plate is level along its length; diagonals across the floor are equal.
- Log walls settle evenly; doors and windows still open after the first winter.
- After rain, the sills and log ends are dry within a day.
Note Troubleshooting. The frame racks (sways) sideways → braces missing, loose or too small. Add braces in every corner of every wall. A tenon will not go in → mortise sides not square. Pare them with the chisel; never force it so hard the mortise splits. Pegs snap while driving → drawbore offset too big (keep it under 3 mm), pegs sawn or cross-grained, or not dry. Log walls bow outward → no dowels. Add internal posts bolted or pegged through the logs. Doors jam in a log house → no settling gap. Cut one. Sills rot → too close to the ground or splash. Raise the plinth, add a damp-proof layer, drain the site.
Dangers
Danger Falling timbers kill. A bent of green oak weighs over half a tonne and can go over the top while being raised. Never stand under a timber being lifted, keep everyone out of the line it could fall in, have rope crews on both sides, and brace each bent the moment it stands. Stop the raising if the wind rises.
Danger Felling is one of the most dangerous jobs in this book: trees kick back off the stump, drop dead branches and fall the wrong way. Read the dangers in Basic Woodworking before felling a building tree.
- Axes glance off knots into legs and feet. When hewing, keep your feet behind the line of the cut, and keep tools sharp: a blunt axe bounces.
- Rolling logs crush legs. Move them with levers and cant hooks, never by hand from the downhill side.
- Falls from frames and roofs: work from scaffolds, not from beams, whenever you can (Scaffolding and Ladders).
- Fire. A wooden building burns. Keep chimneys sound and well clear of timber (Chimneys, Stoves and Heating).
Going further
- A roof to keep it all dry: Roofs. Floors on joists: Foundations and Floors; stairs, boarded floors and ceilings: Stairs, Floors and Interior Finishes.
- Saw pits and water-powered saws turn logs into boards far faster than hewing (Files and Saws, Sawmills and Lumber), and powered planers and moulders finish them (Planers, Thicknessers and Woodworking Machines).
- Nails and bolts (Nails, Rivets and Wire Fasteners) make lighter, quicker frames possible: the "balloon frame" of thin sawn studs, invented in Chicago in the 1830s, built much of North America.
- Large spans need trusses (Trusses and Frames, Roofs) and cranes (Cranes and Lifting); timber also builds bridges (Roads and Bridges).
How it was first done
The first farmers of Europe, about 7,500 years ago, built long houses on frames of oak posts set in the ground. Posts in the ground rot, so builders later learned to set them on stone or on sill beams — a change that made frames last centuries rather than decades. In Japan, the wooden halls of Hōryū-ji temple, built around AD 700, are among the oldest wooden buildings in the world. Norway's stave churches (Urnes, about 1130) and England's great barns from the 1200s show how far pegged oak frames could go. Log building developed in the conifer forests of Scandinavia, Russia and the Alps; Swedish and Finnish settlers brought the log cabin to North America in 1638, and it spread across the continent with the settlers who followed.