Part 5 · Cloth and Clothing
Sewing, Needles and Thread
How to make needles from bone and metal, prepare thread, and join cloth and leather with the handful of stitches and seams that do every job — plus mending, buttons and buttonholes. Sewing turns cloth and hides into clothes, bags, sails and tents.
- Difficulty
- ●●●●●
- Time
- A bone needle in 2–4 hours; basic stitches in an afternoon; a shirt in 2–3 days by hand
- Steps from zero
- 2 prerequisites →
You need first
Spinning and Weaving ClothThis unlocks
Nappies, Feeding Bottles and Baby GearSacks, Boxes, Crates and PackagingToysThe Sewing MachineBags, Backpacks, Wallets and LuggageButtons, Buckles, Hooks and ZipsFootwearLeatherwork and Harness-MakingMaking ClothesQuilting, Down and Warm ClothingBlankets, Curtains, Rugs and TowelsTailoring and Pattern DraftingTents, Sleeping Bags and Camping GearKites and ParachutesThe full path from nothing — 2 steps before this one
- Cordage and Rope
- Spinning and Weaving Cloth
- Sewing, Needles and Thread
Do them roughly in this order. See it on the tech tree →
Why it matters
Cloth from the loom (Spinning and Weaving Cloth) and leather from the tanning pit (Hides and Leather) are flat sheets. Bodies, bags, tents and sails are not. Sewing is how flat material becomes a shape: a shirt, a pair of trousers (Making Clothes), a shoe (Footwear), a water bag, the cover of a book (Bookbinding), a sail (Boats and Sails), a tent, the bag of a Bellows or a Balloons, the closing stitch of a wound (Wound Care and Antiseptics, Basic Surgery).
The eyed needle is one of the most important inventions in human history. It let people of the last Ice Age make close-fitting, layered, sewn clothing — and with it, survive and spread into the coldest parts of the world (Surviving Cold and Heat).
Sewing is also mending. In a world without shops, a torn shirt patched today is a shirt you do not have to spin, weave and sew from scratch next month.
How it works
A stitch is a short length of thread that passes through two layers and holds them together. A seam is a row of stitches. Three things decide how good it is:
- Thread strength. The seam is only as strong as the thread. Plied thread (Cordage and Rope, Spinning and Weaving Cloth) is far stronger than a single strand. Waxing the thread with beeswax binds the fibres, stops it fraying and tangling, and makes it slide through the material.
- Stitch length. Short stitches (2–3 mm) make a strong, tight seam that does not gape; long stitches (5–10 mm) are quick and are used for tacking pieces in place before the real seam.
- The edge. Woven cloth frays at a cut edge, so the seam is made 1–1.5 cm in from the edge (the seam allowance), and the raw edge is folded in or overcast. Leather and felt do not fray, so they can be sewn close to the edge.
What you need
| Item | Size | Made from |
|---|---|---|
| Needles | Fine cloth: 3–5 cm, 0.6–1 mm thick. Coarse cloth and wool: 5–7 cm, 1–2 mm. Sailmaker's and leather: 6–10 cm, 2–3 mm, three-sided point | Bone, antler, copper, bronze, iron, steel |
| Awl | A sharp spike 4–8 cm long in a handle | Bone, hardwood, or metal; for punching holes in leather |
| Thread | Arm's length (60–75 cm) at a time | Linen, hemp, nettle, silk, cotton, wool, sinew |
| Beeswax | A lump the size of a walnut | Beekeeping |
| Cutting tool | A sharp knife; shears or scissors (Scissors, Shears and Folding Knives) | |
| Thimble | Fits the middle finger | A ring of thick leather, or bone, horn or metal with dimples |
| Pins | 3–4 cm | Thorns, fish bones, wood splinters, or bent wire |
| Marking | Chalk, charcoal, or a dull point to crease the cloth |
Where to find it
- Bone from the leg bones of deer, sheep, goats or cattle (Hunting and Trapping): the long, straight, thick-walled metapodials (lower leg bones, below the knee and hock) are ideal. Bird leg bones make fine, hollow needles.
- Antler for awls and heavier needles: shed antlers in late winter forests.
- Sinew — dried tendons from the back and legs of deer and cattle — makes the strongest thread for leather (Cordage and Rope).
- Plant thread: flax and hemp (Flax, Hemp and Linen) make the best linen and hemp thread; nettle and the inner bark of lime (basswood) also work. Cotton (Cotton) and silk (Silk) make fine thread for cloth.
- Sandstone for grinding needles: any gritty, even-grained stone. A fine-grained piece (it feels like flour, not sugar) for polishing.
- Horn, shell, antler, hard wood and bone for buttons.
Making needles
Bone needles
- Clean the bone. Boil it for an hour, scrape off all the meat and membrane, and let it dry for a day. Fresh bone works more easily than very old, dry bone; if it is dry, soak it in water overnight.
- Cut grooves. With the sharp corner of a flint flake (a burin — a stone tool with a narrow chisel point, see Stone Tools), scratch two parallel grooves 3–4 mm apart down the length of the bone, 8–12 cm long. Keep scoring the same lines over and over until they cut right through the bone wall. This takes an hour or two. A thin flint saw, or later a metal file (Files and Saws), is faster.
- Remove the splinter. Lever the strip out with a wedge or the tip of a knife. You now have a stick of bone about 3 × 3 × 100 mm.
- Grind it round. Rub it lengthways on a sandstone slab, turning it constantly, until it is round and about 1.5–2.5 mm thick. Wet the stone. Taper one end to a fine, smooth point over the last 1–2 cm. Put a groove in the stone with practice: rubbing the needle back and forth in a groove keeps it round.
- Drill the eye. Flatten the blunt end slightly on the stone. With a fine flint point — a tiny chip mounted in a split stick, twirled between your palms, or a bow drill (Fire, Drills and Boring) — drill a hole about 1 mm across, 3–5 mm from the end. Drill halfway from one side, then turn the needle over and drill from the other side to meet it. This makes an hourglass-shaped hole with no sharp edges to cut the thread.
- Polish. Rub the needle with fine sand on leather, then with a scrap of leather alone, until it is glossy. A rough needle drags and tears cloth.
Tip No eye at all. Long before eyed needles, people sewed by punching a hole with an awl and pushing the thread through, its end stiffened with wax, glue or a twist of sinew that had been wetted and dried hard. This still works for leather, and it is quicker than making a needle when you are learning.
Metal needles
Metal needles are thinner, stronger and last far longer. Copper and bronze ones can be made as soon as you can make wire (Copper Wire, Bronze); steel ones are best of all. The method below makes a few at a time; Needles and Pins covers making them by the hundred.
- Make wire of the right thickness (1–1.5 mm for a general needle) by drawing it through a draw plate (Copper Wire). Iron must be low in carbon to draw well; it is hardened later.
- Cut lengths of 4–7 cm.
- Form the eye. Either: hammer one end flat and thin on an anvil, then punch a slot through it with a hardened steel punch, from both sides; or (the oldest metal method) flatten the end, split it with a chisel, and bend and hammer the two halves back together around a thin wire mandrel, leaving a hole. Copper and bronze needles can simply have the end bent over into a tiny loop and hammered flat.
- Point the other end with a file and then a fine whetstone (Abrasives and Grinding Stones).
- Harden steel needles (Steel): heat them to cherry red in a small charcoal fire (a few at a time, in a clay tube or iron pipe so they don't burn) and drop them into water or oil. Then temper them: warm them gently on a hot iron plate until they turn straw-yellow to light brown, and tip them off to cool. Untempered needles are hard but snap like glass.
- Polish by rolling handfuls of needles in a bag of fine sand and oil for hours.
Thread
- Linen thread for sewing is usually 2- or 3-ply (Spinning and Weaving Cloth). Make it hard-spun and fine.
- Wax it: draw the thread across a lump of beeswax 2–3 times, then run it through your fingers to melt the wax in. Always wax linen and hemp thread for leather work.
- Use a length from your fingertips to your elbow and back again — about 60–75 cm. Longer threads tangle and wear out by being pulled through so many times.
- Sinew thread: split dried sinew into fine strands, moisten them in your mouth, and twist. Sew with it damp; it shrinks and grips as it dries.
- For leather and sails, use heavy thread: 4–6-ply linen or hemp, well waxed.
The stitches
Start every seam with a knot in the end of the thread, or (better) with two small backstitches on the spot. Finish with two or three tiny backstitches on top of each other, then run the thread under the last few stitches and cut it.
- Running stitch. Push the needle in and out along the line, taking several stitches onto the needle before pulling through. Stitches 3–5 mm long. Quick, but weak. Use for tacking, gathering and light seams.
- Backstitch. Bring the needle up one stitch length ahead, go down at the end of the previous stitch, and come up one stitch length ahead again. On the front it looks like a continuous line, like machine sewing. Stitch length 2–3 mm. This is the strongest hand seam; use it for every seam that takes strain — crotch, armholes, shoulders.
- Whipstitch (overcast). Hold two edges together and pass the needle through both, always from the same side, so the thread wraps over the edge. Stitches 2–4 mm apart. Joins leather and fur edges, and stops cut cloth from fraying.
- Blanket stitch. Go in 4–6 mm from the edge, and bring the needle out under the edge, through the loop of thread before pulling it tight. It makes a row of little L's with a corded edge. Binds the edges of blankets, felt and buttonholes (the buttonhole stitch is a tighter version of it).
- Hemming stitch (slip stitch). Fold the edge under twice. Pick up just one or two threads of the main cloth, then slip the needle along inside the fold for 5–8 mm, and repeat. Almost invisible from outside.
- Saddle stitch — for leather. Punch a row of holes with an awl, 3–5 mm apart and 3–5 mm from the edge (mark them with a fork-like spacer or a notched stick). Put a needle on each end of a waxed thread. Pass one needle through the first hole and centre the thread. Then for every hole, pass the left needle through to the right and the right needle through to the left. It is like two running stitches filling each other's gaps. If one stitch breaks, the seam does not unravel.
Seams
- Plain seam. Put the two pieces face to face, edges together, and backstitch along a line 1–1.5 cm in from the edge. Open the seam out and press the two allowances flat (finger-press, or press with a smooth warm stone). Overcast each raw edge so it doesn't fray.
- Flat-felled seam — the strongest seam for working clothes, the seam of jeans and of linen shirts for a thousand years. Sew a plain seam with a 1.5 cm allowance. Trim one allowance to 5 mm. Fold the wider one over the narrow one, turn the fold under, and lay it flat on the cloth. Hem it down along its folded edge. Every raw edge is now enclosed and there are two lines of stitches.
- French seam — for fine cloth. Sew the pieces back to back 5 mm from the edge; trim close; turn them face to face, and sew again 7 mm in, enclosing the raw edges inside.
- Hem. Fold the edge under 1 cm, then again 1.5–2 cm, and hem-stitch it down.
- Seams in leather: butt the edges and whipstitch or saddle stitch, or overlap them by 1 cm and saddle stitch through both.
Mending
- Darning (holes in knitted or woven wool): with matching yarn, run lines of running stitch across the hole and 1 cm beyond on each side, close together like a warp. Then weave across them at right angles, over one and under one, like a tiny loom (Spinning and Weaving Cloth). A smooth, rounded object inside — a gourd, a wooden egg — holds the cloth taut.
- Patching: cut a patch 2 cm bigger than the hole all round, on the same grain (thread direction) as the garment. Fold its edges under 5 mm and hem it down over the hole. Then turn the garment inside out, trim the worn edges of the hole, fold them under and hem them to the patch.
- Reinforcing: patch knees, elbows and seat before they wear through. Rows of running stitch through a patch and the cloth (as in the Japanese sashiko) make it far stronger.
- Seams that split should be mended at once with backstitch, overlapping 2 cm into the good stitching at each end.
Fastenings: buttons, buttonholes and others
- Toggles: a stick of wood, antler or bone 3–5 cm long with a groove round its middle, sewn on by a cord, passed through a loop. The simplest fastening, and easy to use with cold hands.
- Buttons: discs of bone, horn, antler, shell, hardwood or fired clay (Pottery), 1.5–2.5 cm across and 3–4 mm thick, with 2 or 4 holes drilled 3–4 mm apart. Grind them smooth so they don't cut the thread. A knot of cord (the Chinese knot button) or a ball of cloth stuffed with scraps also works.
- Sewing on a button: put a matchstick across the top of the button and sew over it 6–8 times through the cloth. Remove the stick, lift the button, and wind the thread 5–6 times round the stitches under it to make a stiff shank. The shank leaves room for the cloth of the buttonhole. Fasten off underneath.
- Buttonholes: mark a line as long as the button's width plus its thickness (plus 2–3 mm), at right angles to the edge, 1.5 cm in from it. Sew a row of small running stitches round the line, 2 mm out from it, then cut the slit. Bind the edges with buttonhole stitch: like blanket stitch, but with the stitches touching each other, so the knots form a hard ridge on the cut edge. Make a bar of 4–5 stitches across each end.
- Loops: a loop of cord or a tube of cloth sewn on the edge, over a button. Easier than buttonholes.
- Lacing and eyelets: holes punched with an awl and bound round with buttonhole stitch, laced with a cord. Good for shoes and fitted bodices.
- Hooks and eyes: bent wire (Copper Wire). Buttons, Buckles, Hooks and Zips covers all of these in more depth, and buckles and press studs too.
How to tell it worked
- The pull test. Pull hard on each side of a seam. A good seam does not open into gaps between stitches ("grin"). If it does, the stitches are too long or loose.
- The thread does not cut the cloth. If the thread tears through when pulled, the stitches are too near the edge or the thread is too thick for the cloth.
- It lies flat. Puckering means the thread was pulled too tight. Gentle, even tension.
- The needle passes easily. If you must force it, the needle is too blunt or too thick, or the leather needs awl holes.
Note Troubleshooting. Thread tangles and knots itself → it is too long, or twisted too hard. Use a shorter length, wax it, and let the needle hang down and untwist every so often. Thread keeps fraying and breaking at the eye → the eye has sharp edges. Polish it with a strand of thread rubbed with fine sand; shift the thread through the eye from time to time. Bone needle snaps → it is too thin for the cloth, or you are levering with it. Make a thicker needle for coarse cloth, and push it straight with a thimble. Seam puckers → stitches pulled too tight, or the two layers were stretched unequally. Pin or tack the pieces first, and stroke the seam flat as you go. Buttonhole frays open → the stitches are too far apart. They must touch.
Dangers
- Puncture wounds. Needles and awls go into hands. Always push away from your body and fingers, use a thimble, and keep the awl's path clear of the hand holding the work. A puncture from a dirty awl into a hand can become badly infected; wash it and watch it (Wound Care and Antiseptics).
- Swallowed or lost needles. Keep needles in a case — a hollow bone or reed with a stopper, or stuck in a pad of felt — and count them. A needle in bedding or a floor rush can go deep into a foot.
- Eyes. Chips fly when grinding and drilling bone and when snapping hardened steel. Look away or shield your eyes.
- Strain. Sewing in poor light ruins eyes and causes headaches. Sew by daylight or a good lamp (Lamps and Candles); later, Spectacles help.
Going further
- Making Clothes — measuring, patterns and cutting; Tailoring and Pattern Drafting for fitted coats and suits.
- Footwear — the turnshoe and moccasin, sewn with awl and saddle stitch.
- Quilting: two layers of cloth with wool, down or cotton between, held by rows of running stitch — a warm, light coat or bedcover (Quilting, Down and Warm Clothing).
- Embroidery with coloured thread (Dyes and Mordants) decorates and strengthens.
- The Sewing Machine — the lockstitch machine that ended thousands of years of hand sewing.
How it was first done
People probably sewed skins with awls long before needles existed. Eyed bone needles appear at least 40,000 years ago in Siberia and are common in Europe by about 25,000 years ago, at the coldest part of the last Ice Age. Bronze needles followed metal-working, and the Romans used bronze and iron ones. Steel needles were made in the Islamic world and Moorish Spain and spread through Europe from the 1300s; by the 1700s the town of Redditch in England had become the world's needle-maker. Buttons used as fastenings with buttonholes seem to have spread in Europe in the 1200s, making close-fitting clothes possible. The first practical sewing machines (Elias Howe, 1846; Isaac Singer, 1851) used an eye at the point of the needle — a reversal of the oldest design in this chapter.
Source: content/entries/textiles/sewing.md