How to make carrying, gathering and storage containers from plants — plaited mats and bags, twined and coiled baskets, willow baskets, folded bark boxes and gourd bottles — how to seal them with pitch to hold water, and how to build a frame for carrying heavy loads.
- Difficulty
- ●●●●●
- Time
- An hour for a plaited mat or bark box; a day for a willow basket; a season to grow and cure gourds
- Steps from zero
- 1 prerequisite →
You need first
Cordage and RopeThis unlocks
—The full path from nothing — 1 step before this one
- Cordage and Rope
- Baskets and Containers
Do them roughly in this order. See it on the tech tree →
Why it matters
Before pottery, before metal, there were baskets. A person with bare hands can carry only what fits in their arms. With a basket they can gather a day's nuts, berries and shellfish (Foraging Wild Food), carry firewood, store grain away from mice (Granaries and Food Storage), sieve flour, trap fish (Hunting and Trapping, Fishing), and with a sealed basket or a gourd, carry water (Finding and Purifying Water). Woven mats make floors, walls, beds and sails.
Basketry is also the root of other crafts. The same over-and-under that makes a basket makes cloth on a The Loom (Spinning and Weaving Cloth), a wattle wall (Shelter), a fence, and the frame of a coracle boat (Rafts and Canoes). Clay smeared inside baskets may even have helped lead people to Pottery.
How it works
Every basket is a structure of stiff parts and flexible parts, held together by friction. There are four basic ways to build one:
- Plaiting — flat strips of equal stiffness (leaves, bark, split cane) cross each other over-and-under. Fast; good for mats, bags and trays.
- Twining — stiff spokes (warps) are held by pairs of flexible strands (wefts) that twist around each other between every spoke, locking it in place. Strong and flexible; the method of bags, fish traps and the finest watertight baskets.
- Coiling — a thick bundle of grass, needles or rods is wound in a spiral and stitched to the coil below it. Slow, but very strong, rigid and tight — it can be made watertight.
- Wicker (stake-and-strand) — stiff stakes are woven with long flexible rods, like a little wattle fence. The everyday basket of Europe and Asia.
Fresh plant material is flexible; dry material is brittle. Work everything damp. Material shrinks as it dries, so pack each row tight, and tighten again as you go.
What you need
| Material | Best for | Notes |
|---|---|---|
| Willow withies, hazel, dogwood shoots | Wicker, frames, rims, fish traps | One-year shoots, 60–200 cm long, pencil- to finger-thick |
| Cattail leaves, rushes, sedges, palm leaves | Plaiting, twining wefts | Cut green, dry, then re-dampen |
| Long pine needles, grass, split rods | Coiling bundles | Longleaf pines give needles 20–45 cm long |
| Inner bark of basswood (linden), elm, cedar, willow | Twining wefts, stitching, straps | Strip in spring or early summer (Cordage and Rope) |
| Split spruce or pine roots | Stitching bark and coiled baskets | Very strong and flexible when fresh |
| Birch bark, elm, cherry, tulip-tree, cedar bark | Folded boxes, trays, buckets | Sheets peeled in early summer |
| Gourds | Bottles, bowls, ladles, floats | Grown, then dried for months |
| Pine resin + charcoal + fat or beeswax | Waterproof pitch | See below |
| Tools | — | A sharp flake or knife (Stone Tools), a bone awl (a polished point of bone), a smooth stone or wooden beater to pack rows |
Where to find it
- Willow grows along streams, lakes and wet ground. Its long, flexible, smooth shoots spring up in dozens from cut stumps. Cut them in winter, when the leaves have fallen, and either use them fresh within a week or two, or tie them in bundles to dry and soak them later — roughly one day of soaking for every 30 cm of length, then wrap them overnight in damp grass or cloth to "mellow" before weaving.
- Cattails and rushes fill marshes and pond edges (Foraging Wild Food). Cut leaves in late summer, dry them in the shade for a week, and dampen them before use.
- Spruce and pine roots run just under the moss and leaf litter around the trunk. Pull them up in long lengths (a metre or more), thumb-thick or less; roast them briefly in hot ashes and the bark slips off, then split them in half with your thumbnails.
- Birch bark comes off in large sheets in early summer, when the sap is running. Take it from trees you are felling anyway, or cut only the papery outer bark carefully without cutting into the green inner layer beneath — cutting the inner bark all round a tree kills it.
- Gourds — the bottle gourd (calabash) is a vine of warm climates with white flowers and hard-shelled fruit. Where it doesn't grow wild, grow it (Farming from Seed).
Method 1: A plaited mat or tray
- Cut 20–30 strips of cattail leaf, palm leaf or bark, all the same width (2–3 cm) and about 60 cm long. Dampen them.
- Lay half the strips side by side on the ground, touching, pointing away from you.
- Weave the first crossing strip over one, under one, all the way across. Push it up to the top.
- Weave the next strip under one, over one — the opposite of the row before — and push it tight against the first. Repeat until the square is full. That is a checkerboard plait. (Over two, under two, shifting one each row, gives a stronger twill.)
- For a tray or box, stop weaving 10 cm from each edge, fold the loose ends up at each side to make walls, and weave more strips around the walls.
- Finish the edge by folding each strip end back and tucking it under two or three strips on the inside.
Method 2: A twined basket
- Make the spokes. Cut 8 stiff spokes 50 cm long (willow shoots, split rods or thick rush stems). Lay 4 side by side, and lay the other 4 across them at right angles, making a cross.
- Start the weaver. Take a long, soft weft — cattail leaf, inner bark or cord — fold it in half around one arm of the cross, so you have two ends.
- Twine round the cross. Bring the back strand over the front strand and in front of the next arm of the cross, then the new back strand over the front strand, and so on. Each half-twist locks one arm. Go round twice, pulling tight.
- Split the spokes. On the third round, twine round pairs of spokes; on the fifth, round single spokes, so they spread out like the spokes of a wheel. Keep them evenly spaced.
- Add a new weft when one runs short by laying the new end alongside the old one for two or three spokes and twining both together.
- Turn up the sides. When the base is the size you want (15–20 cm across for a gathering basket), bend all the spokes upward and keep twining. Pull the wefts tighter to narrow the basket, looser to widen it. If spokes get too far apart (over 3 cm), push a new spoke in beside an old one.
- Finish the rim. Bend each spoke down beside the next one and tuck it inside the weaving, or bind a hoop of willow around the rim with a spiral of bark.
Method 3: A coiled basket
Coiling is slow but makes the strongest, tightest baskets — some peoples made coiled baskets so tight they could cook in them by stone boiling (Cooking Without Pots).
- Make the bundle. A bundle of long pine needles, grass, or thin split rods, about 1 cm thick (a pencil to a finger). Dampen it.
- Make the stitching strand. A long strip of split root, yucca leaf, raffia or inner bark, 2–3 mm wide, damp and pointed at the end.
- Start the centre. Bend the end of the bundle into a tight spiral 1–2 cm across, and wrap it round and round with the stitching strand to hold it.
- Coil and stitch. Lay the bundle around the outside of the centre. With the bone awl, pierce a hole through the top of the coil underneath, push the stitching strand through, and wrap it over the new bundle. Repeat every 0.5–1 cm. Each stitch binds the new coil to the old one.
- Keep the bundle even. As the needles or grass run out, push new ones into the middle of the bundle so the thickness never changes.
- Build the walls. For a flat base, lay each coil beside the last. For walls, lay each coil on top of the outer edge of the one below.
- Finish by tapering the bundle to nothing over the last 10 cm and binding it down tightly.
Method 4: A willow (wicker) basket
- Base sticks. Cut 8 thick rods (finger-thick), 25 cm long. With a sharp flake, slit 4 of them through the middle for 4 cm. Push the other 4 through the slits to make a cross of 4 by 4.
- Tie in the cross. Take two thin, long willow rods. Push their tips into the slit beside the cross, and weave them around the four arms with pairing: each rod in turn goes in front of one arm and behind the next, crossing over the other rod between arms. Go round twice.
- Open the spokes. Now pair round each spoke singly, pressing them apart until they are evenly spaced like a wheel. Keep pairing until the base is 20–25 cm across, then cut the base sticks off flush. Press the base slightly domed (higher in the middle) so it stands steady.
- Stake up. Push a long, stout rod (the stakes, 80–100 cm long) into the weaving beside each base spoke, one on each side — 32 stakes for 16 spokes. Kink each one where it leaves the base by pressing it with a thumbnail or the back of a knife, bend it upward, and gather all their tips together in a hoop or tie them at the top.
- Upset (the first rows of the wall). Weave three rows of waling: three rods together, each in turn going in front of two stakes and behind one. This is the strongest weave and sets the shape.
- Weave the sides. Weave single rods in and out of the stakes (randing). With an even number of stakes, use two rods, one starting a stake ahead of the other, so they alternate. Press each row down hard with your fingers or a beater. Keep the stakes evenly spaced; the shape follows them.
- Finish with a border. When the wall is high enough (25–30 cm), soak the tops of the stakes again. Bend each stake down to the right, behind the next stake and in front of the following one, and leave it lying outside. Go round; tuck the last ones in. Trim the ends to 2 cm on the outside.
- Handle. Push a thick rod 15 cm into the weave on each side, beside a stake, to make an arch. Wrap it tightly with four or five thin rods spiralled round and round, and tuck their ends through the border.
A 30 cm willow basket takes a beginner a full day. It will carry 10–15 kg and last for years if kept dry when not in use.
Method 5: A folded bark box
Bark folds without cracking if it is fresh, or if it is gently warmed over a fire (never in the flame) until it becomes supple.
- Cut a rectangle of birch (or elm, cherry or cedar) bark, for example 40 × 60 cm. The grain lines on birch bark (the dark streaks) should run along the long side.
- Mark the base — a rectangle in the middle, say 20 × 30 cm. Score its outline lightly on the inside of the bark with the back of a blade, so it folds cleanly. Don't cut through.
- Fold up the sides. At each corner, the extra bark folds into a triangle that you press flat against the side wall — like wrapping a parcel. No cut means no leak.
- Make a rim. Bend a thin willow rod into a hoop that fits the top, inside or outside the walls. Stitch the bark to it with split spruce root or bast, using an awl, every 1–2 cm.
- Seal the corners and any cracks with hot pitch (below). A good birch-bark box holds water, and can even be used to boil water over gentle coals (Cooking Without Pots).
A quick bark bucket can be made in ten minutes: fold a long rectangle of bark in half like a book, fold each end up into a pleat, and pin the pleats with a split stick clamped over them.
Method 6: Gourd containers
- Grow bottle gourds like squash (Farming from Seed): plant seeds in warm soil after the last frost and give them 100–180 frost-free days and a fence or tree to climb.
- Harvest when the vine and the stem near the gourd are brown and dry.
- Cure them in an airy, shaded, dry place for one to six months, until they are light and the seeds rattle when shaken. A black or grey mould on the skin is normal; scrub it off with sand and water.
- Cut an opening: a small round hole near the stem for a water bottle, a lengthwise cut for a bowl or ladle.
- Clean out the dry pith and seeds with a stick. Fill with water, gravel and sand and shake hard to scour the inside, then rinse.
- Seal the inside with melted beeswax or a little pitch to stop it tasting bitter. Plug a bottle with a carved wooden stopper or a corn cob wrapped in leaf.
Gourds also make dippers, floats for nets (Fishing) and rattles (Musical Instruments).
Sealing baskets with pitch
A tightly woven basket swells and nearly stops leaking when soaked, but to hold water for days it needs a lining of pitch — a hard, waterproof resin glue.
- Gather pine or spruce resin from wounds on the trunks. Melt it gently in a shell, bark tray or stone hollow beside the fire — never in the flame; it catches fire easily and smokes when too hot. Strain out bark and grit through a twist of grass.
- Stir in finely powdered Charcoal, about 1 part charcoal to 3–4 parts resin, and a little fat or beeswax (about 1 part in 10) so it is less brittle. Hardened, it should dent under a thumbnail without shattering. More fat makes it softer; more charcoal makes it harder. See Tar, Pitch and Glue and Glues and Adhesives.
- Coat the inside of the basket with hot pitch using a stick, working it into every gap. A trick used in the American Great Basin: drop hot, pitch-coated pebbles into the basket and swirl them around, which spreads the melted pitch evenly over the inside.
- Coat the outside too for a bottle that will stay wet. Let it harden for a day.
Pitch softens in strong sun and in hot liquids, and taints hot food. Use pitched baskets for cold water; stone-boil in unpitched, tightly woven baskets, wooden bowls or hide (Cooking Without Pots).
Carrying frames
- Cut two side poles of straight, light, strong wood (ash, hazel, willow), thumb-thick, about 70–80 cm long — from your waist to the top of your shoulders.
- Lash on three or four crossbars 35–40 cm long with cord or wet rawhide (Hides and Leather), which shrinks tight as it dries. Make the frame slightly curved to fit your back.
- Shoulder straps: two straps of rawhide, woven bark or braided cord, at least 5 cm wide — narrow straps cut into the shoulders. Pad them with moss or fur.
- Tumpline: a band 5–8 cm wide, tied to the bottom of the frame or load and passed over the top of the head. It takes much of the weight on the spine. Many porters carried loads with the tumpline alone.
- Pack it right: heavy things close to your back and high up, light things outside and low. A fit adult can carry about a fifth to a quarter of their body weight all day; more for short distances.
A conical burden basket worn on the back with a tumpline does the same job for loose loads such as nuts, roots or firewood.
How to tell it worked
- Strength test: fill a basket with stones and carry it for 10 minutes. The bottom should not sag, the rim should not twist, and nothing should pull loose.
- Water test: fill a sealed basket or gourd with water and leave it on a dry stone overnight. No damp patch underneath in the morning means it works.
- Shape: a good basket sits flat without rocking, and its walls are evenly spaced.
Note Troubleshooting. Material cracks when bent → it is too dry; soak longer and mellow overnight. Old willow (two years or more) is too stiff; use one-year shoots. Weaving gaps open as it dries → material shrinks; pack rows tighter, and re-tighten the next day. Basket leans or twists → stakes unevenly spaced, or one side woven tighter. Keep stakes evenly spaced and turn the basket as you work. Coils separate → stitches too far apart or not pierced deep enough into the coil below. Pitch cracks and flakes → too much charcoal or too little fat; add fat. Pitch stays sticky → too much fat; add resin and charcoal. Gourd rots instead of drying → it was picked unripe or kept in a damp, still place.
Dangers
Danger Hot pitch burns. Melted resin sticks to skin and keeps burning. Keep cold water at hand and plunge a burn into it at once for 20 minutes; don't try to peel the pitch off (Wound Care and Antiseptics). Resin catches fire easily — melt it beside the fire, not in it, and keep a lid or a handful of earth ready to smother flames.
- Cuts and eye injuries. Willow rods spring back and can whip into an eye; keep your face back and point rod tips away. Splitting with a flake cuts fingers — cut away from yourself.
- Poison ivy climbs like a basket vine; its hairy-rooted stems cause a rash. Learn it before you gather vines (Dangerous Plants and Animals).
- Gourd dust and mould. Scraping dried gourds raises a fine dust and mould spores that irritate the lungs. Work outdoors, wet the inside first, and cover your nose and mouth with a cloth.
- Killing trees. Stripping bark all the way round a living tree kills it. Take bark from trees you fell, or only the outer layer.
- Overloading. Heavy loads carried badly injure backs and knees. Build up slowly.
What this unlocks
Baskets let you gather, carry and store food in quantity — the foundation of Farming from Seed and Granaries and Food Storage. Twining and plaiting lead directly to cloth (Spinning and Weaving Cloth, The Loom); wicker leads to wattle walls (Shelter), hurdles, fish traps (Fishing), sieves for Grain, Flour and Bread and Paper-making, and the frames of coracles (Rafts and Canoes). Pitch-sealed vessels are a step towards Barrels and Cooperage, and towards the boxes, sacks and jars of Sacks, Boxes, Crates and Packaging.
How it was first done
Baskets and mats rot quickly, so their history is mostly lost. The oldest known traces are impressions of woven fibres pressed into fired clay at Pavlov and Dolní Věstonice in the Czech Republic, made about 26,000–27,000 years ago. Fragments of real twined baskets and mats survive from dry caves in the American West and Peru from about 10,000 years ago. At Nahal Hemar cave near the Dead Sea, people about 9,000 years ago coated baskets with natural asphalt to make them waterproof. The bottle gourd was one of the first plants people grew — probably in Asia and Africa — and it reached the Americas by at least 10,000 years ago, possibly floating across the ocean on its own. Indigenous Californian peoples such as the Pomo made coiled and twined baskets so fine and tight that they held water and were used for cooking with hot stones.