Part 4 · Food and Farming
Fruit Trees and Orchards
How to raise apples, pears, plums, cherries, figs, olives and nut trees — from seed, from cuttings, and above all by grafting a good variety onto a hardy wild root — then prune, pollinate and keep an orchard that feeds people for fifty years or more.
- Difficulty
- ●●●●●
- Time
- A morning to graft a dozen trees; three to eight years to the first real crop
- Steps from zero
- 15 prerequisites →
This unlocks
Forestry and Tree NurseriesThe full path from nothing — 15 steps before this one
- Stone Tools
- Fire
- Cordage and Rope
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- Charcoal
- Farming from Seed
- Hides and Leather
- Bellows
- Iron (the Bloomery)
- Blacksmithing
- Steel
- Axes, Chisels, Knives and Planes
- Fruit Trees and Orchards
Do them roughly in this order. See it on the tech tree →
Why it matters
A field of grain must be dug, sown, weeded and harvested every single year. A fruit or nut tree is planted once and then crops for 30, 50, sometimes 300 years with a little pruning. A mature apple tree on a full-size root gives 100–300 kg of fruit a year; a mature walnut or chestnut gives 20–100 kg of nuts, as rich in calories as grain. Trees also grow where the plough cannot go — on steep slopes, in rocky ground, around the edges of fields — and their roots hold the soil against erosion (see Understanding Soil).
Fruit gives vitamins through the winter (dried apples, figs and plums keep for a year — see Preserving Food) and sugar for cider and wine (Beer, Wine and Cider); olives and walnuts give oil (Oils and Pressing). The catch is time: plant trees in your first year, before you need them.
How it works
Why seeds don't give you the fruit you ate
A wheat or bean seed grows into a plant much like its parent (see Saving Seed and Breeding Plants). An apple seed does not. Apples, pears, sweet cherries and most plums cannot fertilise themselves, so every seed is a cross between two trees. Plant 100 pips from a good apple and you get 100 different trees, most with small, sour fruit fit for cider; perhaps one is excellent.
So to get more of the same good tree, you must copy it without seed:
- Cuttings — a pencil-thick piece of last year's shoot, 20–30 cm long, pushed two-thirds into the ground in winter, grows its own roots. Easy for figs, olives, pomegranates, grapes, quinces, mulberries and currants; almost impossible for apples, pears, cherries and nut trees.
- Grafting — a piece of the good tree (the scion) is joined onto a young rooted plant of a related kind (the rootstock). They grow into one tree: the roots are the stock, everything above the join is a perfect copy of the good tree.
Why grafting works
Just under the bark lies a thin, slimy, bright green layer called the cambium. It is the only part of a trunk that grows, making new wood inside and new bark outside. Press two cut cambium layers together and their cells grow into the gap and knit into one living join within 3–6 weeks. Matching cambium to cambium is the whole secret of grafting. The cuts, binding and wax only hold the layers tight and stop them drying out until they fuse.
Grafts only take between close relatives: apple on apple or crab apple; pear on pear (or quince); plum, peach, apricot and almond on plum or peach; cherry on wild cherry. Apple will not take on pear for long, and nothing takes on an oak except another oak.
What the rootstock does
The rootstock decides how big the tree grows and how hardy it is. A wild seedling root gives a full-size tree 6–10 m tall that lives a century but takes 5–8 years to fruit. Dwarfing stocks (from old dwarf apple trees, or quince for pears) give trees 2–4 m tall that fruit in 2–3 years but need staking and good soil.
What you need
| Item | Notes |
|---|---|
| Grafting knife | A short, stiff blade sharpened on one side only, so it cuts dead flat, and sharp enough to shave hair. Flint works for a few cuts (Stone Tools); steel is far better (Axes, Chisels, Knives and Planes). |
| Saw, mallet, hardwood wedge | For cutting back old trees and cleft grafting (Files and Saws). Pruning shears are in Scissors, Shears and Folding Knives. |
| Rootstocks | Wild seedlings; pencil-thick (6–12 mm) for whip grafts and budding, thumb- to wrist-thick for cleft grafts. |
| Scion wood | Last season's shoots from the tree you want to copy, pencil-thick, cut in midwinter while dormant. |
| Binding | Strips of soft inner bark (lime, willow) or thin yarn, 30–40 cm long (Cordage and Rope). |
| Grafting wax | 4 parts pine resin, 2 parts beeswax, 1 part tallow by weight. Or "grafting clay" (below). |
| Stakes and guards | A 1.5 m stake per tree; thorny brush or woven withies against browsing animals. |
Where to find it
- Good scions come from any surviving fruit tree whose fruit you like: old orchards, farmyards, roadside trees. Taste the fruit in autumn, mark the tree with a cord, and come back in midwinter for the wood.
- Rootstocks. Crab apples grow in hedges and woodland edges — small thorny trees with sour fruit 2–4 cm across; their seedlings make tough, full-size apple stocks. Wild pears, wild cherries and wild plums do the same for their kinds. Seedlings springing up under old orchard trees are perfect: dig them in autumn.
- Raising rootstocks from seed. Most temperate tree seeds sprout only after a winter cold and damp (stratification). Mix pips or stones with damp sand in a mouse-proof pot at 1–5 °C — outdoors in shade, or buried — for 60–90 days (apples, pears) or 90–120 days (cherries, plums, peaches). Sow 2–3 cm deep in spring. In one or two years they reach pencil thickness, ready to graft.
- Nuts. Walnuts, chestnuts, hazelnuts, almonds and acorns grow well from seed and come reasonably close to the parent. Plant fresh nuts at once, 5 cm deep (they die if they dry out), in a cage of thorny twigs against mice.
Method 1: Whip-and-tongue graft
The best graft for stock and scion of the same thickness (6–12 mm). With practice, 80–95% take.
When: late winter to early spring, as the rootstock's buds begin to swell. Cut scions in midwinter (buds tight) and keep them dormant until then, buried in damp sand in the coldest shady place you have.
- Practise first on 20 willow twigs. Each cut must be one smooth, flat stroke; a wavy cut will not take.
- Cut the rootstock straight across about 15–20 cm above the ground, at a smooth place between buds.
- The slope. In one stroke, make a slanting cut 3–4 cm long (about four times the stem's thickness) across the top. The face should be a flat, smooth oval.
- The tongue. A third of the way down from the tip, cut into the wood almost parallel to the face, 1–1.5 cm deep.
- Cut the scion — a piece with 3 buds — with an identical slope and tongue at its base.
- Fit them together. Slide the tongues into each other until the faces sit flat. If the scion is thinner, push it to one side so the bark edges line up exactly there.
- Bind firmly from below the join to above it, so the scion cannot wobble, then wax the whole join and the scion's tip. Label the tree.
Method 2: Cleft graft
For stocks that are much thicker than the scion — 2.5 to 10 cm across. This is how you top-work a whole tree: cut off the branches of a poor or wild tree and turn it into a good variety in 2–3 years, using its big root system.
- In early spring, saw the stock off square at a smooth, knot-free place (on an old tree, each main branch 30–60 cm from the trunk).
- With a heavy knife and mallet, split the stump across its centre 5 cm deep. Drive a wedge into the split to hold it open.
- Cut two scions (3 buds each) with a wedge-shaped base 3–4 cm long, the outer edge slightly thicker than the inner.
- Push one scion into each end of the cleft so its inner bark lines up with the stock's inner bark — the scion sits slightly inside the stock's thicker outer bark. A very slight tilt makes sure the cambium layers cross somewhere.
- Pull out the wedge; the split clamps the scions hard.
- Wax everything thoroughly: the top of the stump, down the split, and the scion tips.
- If both scions grow, cut the weaker one back next year and remove it the year after.
Method 3: Budding (T-budding)
Budding uses a single bud, so one good shoot gives 10–15 new trees. Do it in mid to late summer (July–August in the northern temperate zone), when the bark "slips" — peels easily from the wood.
- Cut a strong shoot of this year's growth. Snip off the leaves, leaving 1 cm of each stalk as a handle.
- On the rootstock, 15–20 cm above the ground, make a T-shaped cut through the bark only: a vertical slit 2.5 cm long and a cross-cut 1 cm wide at the top.
- Slice a bud off the shoot: start 1.5 cm below the bud and cut upwards under it, taking a shield of bark 2–2.5 cm long with a thin sliver of wood.
- Lift the bark flaps of the T and slide the shield down into it, bud facing up. Trim the top flush with the cross-cut.
- Bind tightly above and below, leaving the bud uncovered. No wax is needed.
- After 2–3 weeks, touch the leaf stalk. If it falls off at a touch, the bud has taken. If it is shrivelled and stuck, it failed — try again on the other side of the stock.
- Loosen the binding after a month. The bud sleeps over winter; next spring, cut the stock off just above it.
Grafting wax and grafting clay
Wax: melt 4 parts pine resin, 2 parts beeswax and 1 part tallow together slowly over embers, and stir. It should be firm when cold and soften in a warm hand. If it cracks in the cold, add tallow; if it runs in the sun, add resin and beeswax. Apply it warm, like thick honey, with a stick.
Grafting clay, the oldest method: knead 2 parts sticky clay with 1 part fresh cow dung and chopped hay. Pack an egg-sized ball round the join and tie cloth or moss over it.
Planting and spacing
Plant trees in late autumn or early spring while they are leafless.
- Dig a hole 1 m wide and 40–50 cm deep; mix the soil with a bucket of rotted dung or compost (Compost and Manure). Drive the stake in first, on the windward side.
- Set the tree so the graft join is 5–10 cm above the soil — a buried scion roots on its own and the rootstock's control is lost.
- Firm the soil, water with 20–30 litres, and mulch a 1 m circle (keep mulch a hand's width from the trunk, or mice hide there and eat the bark). Tie the tree to the stake with a soft figure-of-eight loop.
- Guard every trunk. Deer, goats, rabbits and mice kill more young trees than anything else.
| Tree | Spacing | Years to first crop |
|---|---|---|
| Apple or pear, grafted on wild seedling | 7–10 m | 4–7 |
| Apple on dwarfing stock | 2–4 m | 2–3 |
| Apple from seed (ungrafted) | 8–10 m | 6–10 |
| Plum, cherry plum | 5–6 m | 3–5 |
| Sweet cherry on wild cherry | 8–10 m | 4–7 |
| Peach, apricot, almond | 4–6 m | 2–4 |
| Fig, quince, pomegranate (cuttings) | 4–6 m | 2–3 |
| Olive (cuttings) | 7–10 m | 4–8 |
| Hazel (seed or layers) | 4–5 m | 3–5 |
| Walnut, pecan (seed) | 12–18 m | 8–15 |
| Sweet chestnut (seed) | 10–12 m | 5–8 |
Pruning
Pruning lets light reach every branch and stops the tree breaking under its crop.
- When: apples and pears in winter, while leafless. Plums, cherries, peaches and apricots in summer, on a dry day — winter cuts on stone fruit let in a deadly fungus (silver leaf) and make them weep gum.
- First cut out anything dead, diseased or damaged; then crossing branches, and shoots growing straight up (water shoots) or down.
- Shape. For most fruit trees, an open centre (vase): in the first winter cut the young tree to 70–90 cm; keep 3–4 strong branches spaced evenly round the trunk, growing out at a wide angle (45–60° from upright — narrow forks split under fruit). In the next 2–3 winters, shorten each new branch by about a third to an outward-facing bud, so the tree spreads out, not in.
- How to cut. Cut a shoot 5 mm above a bud, sloping away from it. Cut a whole branch just outside the slight swelling where it joins the trunk (the branch collar): a stub rots back; a flush cut leaves a wound the tree cannot close.
- Heavy limbs: first undercut a third through, 30 cm out; then cut from the top just beyond it to drop the limb; then make the final cut at the collar. This stops the bark tearing down the trunk.
- Never remove more than a quarter of a tree in one year. Hard pruning makes a forest of water shoots instead of fruit.
- Thin the fruit. When young apples are hazelnut-sized, leave one or two per cluster, 15 cm apart: bigger fruit, and a crop every year instead of every other year.
Pollination
Most fruit needs pollen carried from flower to flower by bees (Beekeeping) or wind.
- Need a partner: most apples, pears and sweet cherries set fruit only with pollen from a different variety flowering at the same time within about 100 m. Plant two or three varieties; a crab apple pollinates almost any apple.
- Self-fertile: peaches, apricots, sour cherries, quinces, most citrus and many plums. Common figs need no pollination.
- Wind-pollinated nut trees — walnut, hazel, chestnut, pecan — need two or more trees, ideally from different parents, within 30–50 m.
- Late frost kills blossom: plant on a slope, not in a hollow where cold air settles.
How to tell it worked
- Grafts: within 3–6 weeks the scion buds open into leaves. Scratch the scion with a thumbnail: green underneath is alive, brown is dead. By midsummer a good graft has grown 30–100 cm.
- Buds: the leaf stalk drops at a touch after 2–3 weeks; the bud stays plump and green.
- The orchard: 20–50 cm of new shoot a year on young trees, and blossom by year 3–6.
Note Troubleshooting. Scion leafs out, then wilts in early summer → it opened on stored sap but the cambium never joined. Line up one edge exactly and bind tighter. Scion shrivelled before leafing → it dried out, or was already growing when cut. Store scions colder; wax every cut. Shoots grow from below the graft → that is the rootstock. Rub them off at once, or they take over. Tree grows hugely but never fruits → over-pruned, over-fed with dung, or no pollinator. Prune less, stop dunging, plant a partner variety. Good crop one year, nothing the next → thin the fruit hard in the heavy year.
Dangers
Danger Falls from trees and ladders cripple and kill farmers every harvest. Never climb a wet tree or stand on a dead branch (bare, budless). Set a ladder (Scaffolding and Ladders) on firm ground with its foot one step out for every four steps up, and have someone hold it. Never stand on the limb you are cutting.
Danger Bitter almonds and the kernels inside apricot, peach and plum stones contain amygdalin, which releases cyanide when chewed. A handful of bitter almonds can kill a child. Sweet almonds are safe; if an almond or kernel tastes bitter, spit it out. Apple pips contain a little of the same poison — harmless swallowed whole, but do not grind and eat them.
- The grafting knife. Its edge is razor-sharp and you cut towards yourself. Keep your thumb behind the blade, not in front of it. Deep cuts to the thumb are the classic grafting wound — see Wound Care and Antiseptics.
- Hot wax sticks to skin and burns deeply; resin is flammable. Melt it over embers, never a flame.
- Walnut trees poison the soil around them (a chemical called juglone): tomatoes, potatoes and apples planted under them wilt and die. Keep vegetables 15–20 m away.
- Spreading disease. Cutting a diseased tree and then a healthy one carries infection on the blade. After cutting cankered or blighted wood, scald the knife in boiling water or pass it through a flame. See Pests and Plant Diseases.
Going further
- Multiplying rootstocks (stooling). Cut a rootstock tree to the ground in winter. When its new shoots are 15 cm long, heap fine soil round their bases, and keep heaping until the mound is 20–30 cm high. By autumn each shoot has roots: cut them off for a dozen identical rootstocks a year. This is how dwarfing stocks are kept.
- Top-working a hedgerow of wild crab apples with cleft grafts gives a working orchard in three years.
- New varieties: grow seeds of your best fruit for 6–10 years and graft the rare outstanding one. See Saving Seed and Breeding Plants.
- Uses: cider (Beer, Wine and Cider), syrups (Sugar), and coppiced hazel and chestnut for poles and fuel (Firewood and Coppicing). Codling moth, scab, canker and fire blight are covered in Pests and Plant Diseases.
How it was first done
The first fruit trees domesticated were those that grow easily from cuttings — olives, figs, grapes, dates and pomegranates — in the Near East and eastern Mediterranean, mostly 7,000–5,000 years ago. Carbonised figs from Gilgal in the Jordan Valley, about 11,400 years old, are of a seedless type that only people planting cuttings could have kept going.
Grafting was invented later, probably in the Near East or China, perhaps 4,000 years ago; letters from the city of Mari in Mesopotamia, around 1800 BC, appear to mention grafted grapevines, and Chinese texts describe grafting well before the common era. The Greek botanist Theophrastus described grafting and budding around 300 BC, and Roman writers such as Cato and Pliny gave recipes for grafting clay.
The apple comes from the wild apple forests of the Tian Shan mountains in Kazakhstan (Malus sieversii), carried west along the Silk Road and crossed with crab apples on the way; grafting is what made it a crop. In the 1910s–1920s, researchers at East Malling in England sorted the old dwarfing rootstocks into numbered types (such as M9), which made the small modern orchard possible.
Source: content/entries/food/fruit-trees.md