Part 6 · Building
Doors, Hinges, Handles and Latches
The metal and wooden fittings that make a door work — strap and butt hinges, thumb latches and spring latches, bolts, handles and doorknobs, knockers, letterboxes, pull bells and door closers — plus garden gates and the draught-proofing that keeps a closed door warm.
- Difficulty
- ●●●●●
- Time
- An hour to a day for each fitting; a week to equip a house
- Steps from zero
- 18 prerequisites →
This unlocks
—The full path from nothing — 18 steps before this one
- Stone Tools
- Fire
- Cordage and Rope
- Finding and Preparing Clay
- Finding and Identifying Ores
- Basic Woodworking
- Hunting and Trapping
- Charcoal
- Hides and Leather
- Bellows
- Iron (the Bloomery)
- Blacksmithing
- Steel
- Axes, Chisels, Knives and Planes
- Springs
- Timber Framing and Log Building
- Locks and Keys
- Doors, Windows and Joinery
- Doors, Hinges, Handles and Latches
Do them roughly in this order. See it on the tech tree →
Why it matters
Doors, Windows and Joinery shows how to build a door that does not sag. But a door is only as good as its hardware: the hinges it swings on, the latch that holds it shut against the wind, the bolt that keeps it shut at night, the handle you pull it by. Bad hinges let a good door drop and drag; a latch that misses lets it bang open in every gust; a door that does not close itself is left open, and the heat goes out through it.
A house needs dozens of these small objects, and they are among the first things a village smith (Blacksmithing) and founder (Metal Casting) make in quantity. The skills lead straight on to Locks and Keys, cupboard fittings and the standard parts of later industry.
How it works
The hinges carry the door as a lever. The weight hangs from one edge, and its centre is half a door-width away, so it tries to rotate the door about the bottom hinge: the top hinge is pulled out of the frame and the bottom hinge is pushed in.
pull on top hinge = door weight × half the door width ÷ distance between hinges
A 50 kg oak door, 85 cm wide, hinges 160 cm apart: 50 × 42.5 ÷ 160 ≈ 13 kg of steady pull, for ever. Halve the hinge spacing and the pull doubles. So put the top hinge 15–20 cm below the head and the bottom one 20–25 cm above the floor; add a third hinge in the middle of any outside door or any door over about 30 kg; and give the top hinge the longest fixings, into solid timber.
A latch closes itself. Gravity or a spring pushes a bar outward; a slope lets the shutting door push it aside; then it drops or springs into its keeper. A bolt moves only when you slide it, so it holds against a hard push. A closer stores energy as you open the door — lifting a weight, winding a spring, or lifting the door itself — and gives it back to shut it. The hard part is stopping the slam.
What you need
| Item | For | See |
|---|---|---|
| Forge, anvil, tongs, punches, round mandrels 5–20 mm | Hinges, latches, bolts, handles | Blacksmithing |
| Iron or mild steel: bar 25–40 × 4–6 mm and 20 × 5 mm, rod 12–16 mm, plate 1.5–3 mm | Straps, latch parts, butt leaves | Iron (the Bloomery), Steel, Sheet Metal and Rolling |
| Brass or bronze, sand moulds, crucible | Butts, knobs, knockers, letter plates | Zinc and Brass, Metal Casting |
| Files, hacksaw, drill and countersink | Fitting | Files and Saws, Drills and Boring |
| Spring steel wire and strip | Latch, flap and door springs | Springs |
| Lathe | Wooden and brass knobs | The Lathe |
| Nails, wood screws, rivets | Fixing | Nails, Rivets and Wire Fasteners, Screws, Nuts and Bolts |
| Felt, thick leather | Draught strips | Felt, Hides and Leather |
Where to find it: timber, leather and iron as in Doors, Windows and Joinery and Iron (the Bloomery). Oak is acid and rusts iron set into it, so paint or oil every fitting before it goes on oak. For anything handled daily — knobs, latch grips, letter plates — brass repays the effort: it does not rust and stays smooth.
The door itself
Door
Build doors as in Doors, Windows and Joinery: ledged and braced for sheds and cottages, framed and panelled for houses.
| Door | Width | Height | Thickness |
|---|---|---|---|
| Inside room door | 76–83 cm | 198–204 cm | 35–40 mm |
| Front or back door | 81–91 cm | 198–204 cm | 44–50 mm |
| For a wheelchair or stretcher | at least 90 cm clear |
House doors usually open inward against the stop, so the hinges are inside where they cannot be knocked out. Doors of halls, schools and workshops open outward, the way people run in a fire (Firefighting). Hang a door to open against a wall, not across another door.
Good: hangs plumb, even 2–3 mm gap all round, stays where it is left, shuts with one push and a click. Bad: drags at the latch corner, rattles, or sticks every winter.
Panelled door
Framed and panelled construction is in Doors, Windows and Joinery. Four panels (two tall above the lock rail, two short below) is the classic house door; replace the top two with glass (Window Glass) to light a dark hall. Keep the lock rail at 90–100 cm so latch, handle and letterbox go through solid wood. Raised and fielded panels — 18–22 mm thick, planed down to 8–10 mm round the edges to fit the groove — are warmer and quieter than flat ones. A small moulding run along the inner edge of the frame with a moulding plane (Planes, Drawknives and Woodworkers' Tools) hides the hairline gap that opens as a panel shrinks. Judge it by tight, gap-free tenon shoulders and by panels that rattle very slightly in summer: free to move. A glued panel will split.
Gate
An outdoor door that stands in the weather and the wind. Field gates are in Fences and Hedges; a garden or yard gate:
- Size: person gate 90–100 cm wide, 100–120 cm high; cart gate 3–3.6 m, often as a pair.
- Frame: stiles and rails 70–90 mm square, tenoned and wedged through (glue fails outdoors), filled with boards or palings 15–20 mm thick and 2–5 cm apart so wind passes.
- Brace from the bottom of the hinge stile up to the top of the latch stile — always rising away from the hinges.
- Hanging post 15–20 cm square (oak, chestnut, larch heartwood or stone), set a third of its length and at least 75–90 cm into the ground, rammed with stones or set in lime concrete (Mortar and Concrete).
- Hang on strap hinges and pintles with the top pintle pointing down (or capped) so the gate cannot be lifted off. Set the bottom pintle 1–2 cm further out than the top one and the gate falls shut by itself onto a gravity latch.
- Rot: slope or cap the post tops, keep the bottom rail 5–10 cm off the ground, tar the buried wood (Tar, Pitch and Glue), oil yearly.
Hinges
Hinge
Every hinge is a pin with two parts turning round it. The pivot, leather, wooden and strap-and-pintle hinges are in Doors, Windows and Joinery. Three rules for all of them: the pins of all hinges on one door lie on one vertical line (check with a plumb bob); fixings go into solid wood; and the pin fits with almost no play — 0.5 mm of slack drops the latch edge 2–3 mm.
Strap hinge
Forging the strap hinge of Doors, Windows and Joinery from 30 × 5 mm bar: draw the strap to a taper, 30 mm at the eye to 15–20 mm at the tip (the tip can be split and scrolled). Punch 5–7 holes hot, staggered so they do not split one line of grain, the first 5 cm from the eye — it does most of the work. Form the eye: heat the last 8 cm to bright orange, wrap it round a mandrel 1–2 mm bigger than the pintle, and forge-weld the lap shut at white heat with a pinch of sand as flux. A curled eye that is not welded slowly opens under the door's weight. A tee hinge has a short cross-bar instead of a pintle, for screwing to a flat frame.
Butt hinge
The hinge of modern house doors: two flat leaves with interlocking knuckles round a pin, let into the door edge and the frame so only the knuckle shows. Both leaves fold flat, so the door closes tight against its stop.
Sizes: a pair of 75–100 mm butts (the knuckle length) for an inside door, three of 100 mm for a front door. Leaves 2.5–3.5 mm thick and 30–40 mm wide; pin 5–7 mm; five knuckles on a 100 mm hinge.
Forged:
- Cut two blanks of 3 mm plate, 100 mm long and as wide as the leaf plus 3.2 × the pin diameter (enough to wrap round the pin) — for a 6 mm pin, 35 + 19 = 54 mm.
- Mark five knuckles of 20 mm along one edge of each. Keep parts 1, 3, 5 on one leaf and 2, 4 on the other; saw or chisel out the rest, 19 mm deep and 2 mm wider than marked so knuckles clear each other.
- Roll the knuckles hot round a mandrel of the pin's size, then close them in a swage or grooved block. Roll both leaves the same way.
- Fit the leaves together on the mandrel and file the knuckle ends till they turn freely with no gap over 0.5 mm.
- Drill three or four countersunk screw holes per leaf, staggered.
- Pin with a rod 1 mm shorter than the knuckles and peen both ends over; or forge a head on one end for a loose-pin hinge you can knock apart.
Cast: carve a wooden pattern of one leaf, cast both leaves in brass in green sand (Metal Casting), drill the knuckles straight with a jig, file to fit and pin with steel. Industrial: stamped from steel strip in a power press, knuckles curled by dies, thousands an hour (Machine Tools).
Hanging a door on butts:
- Hold each hinge on the door edge with the pin centre 1–2 mm beyond the door face, so the door opens past the frame. Knife round the leaf and chisel a recess exactly as deep as the leaf is thick.
- Wedge the door in the opening on 6–10 mm packers at the bottom and 2–3 mm at the top and latch side; mark the jamb, cut matching recesses, and drive one screw per hinge to test the swing before the rest.
- Closed, the leaves should lie parallel with a 1–3 mm gap. If the door springs back open (hinge-bound), the recesses are too deep: pack them with card.
Good: no rattle when you shake the open door by its latch edge; silent with a drop of oil; screw heads flush. Bad: wobbly knuckles, bent pin, screw heads grinding on each other.
Rising butt hinge
A butt whose knuckles meet on a steep helical slope (about 30°) instead of a flat face. Opening the door lifts it 10–15 mm; let go and its weight slides it down and shut. Cast the two halves in brass or iron with the slope on the pattern, and bevel the door's top edge on the hinge side so it clears the head as it rises. It shuts light doors gently but will not latch a heavy one.
Latches and bolts
Thumb latch
The iron version of the wooden latch in Doors, Windows and Joinery — the Suffolk or Norfolk latch, or sneck. It has no spring.
- Grip: forge a bow of 12 mm bar, 18–25 cm long, ends flattened into leaves with nail holes. Rivet on a thumb-piece, a flat lever 6–8 cm long whose back end passes through a slot 8 × 25 mm in the door.
- Latch bar: 20 × 5 mm, 20–25 cm long, drilled at one end for its pivot (a stud or staple) 10–15 cm back from the door edge, so it lies level.
- Keeper on the frame: a hook with a slope facing the door, so the bar rides up and drops in as the door shuts. A guide staple near the bar's free end keeps it in line and stops it rising more than needed.
- Set the grip at 90–100 cm and cut the slot so the thumb-piece reaches under the bar and lifts it 15–20 mm.
Good: drops in with a clean clack from a gentle push. Bad: the bar lands on top of the keeper (keeper too low) or the thumb-piece cannot lift it clear (slot misplaced). Move the keeper; do not bend the parts.
Spring latch
The latch of modern inside doors. A springbolt with a bevelled face sticks out of the door edge; as the door shuts, the bevel strikes a striking plate on the frame, the bolt is pushed in, and it springs out into a hole in the plate. A handle on a square spindle through the door turns a follower (a small cam) that draws the bolt in.
- Rim latch — the case screws to the inside face of the door. Fold and rivet a box of 1.5 mm sheet iron about 10 × 7 × 2.5 cm (Sheet Metal and Rolling); file a bolt from 10 × 15 mm bar with a 30–40° bevel, sliding in two slots; press it out with a leaf or coil spring (Springs); file a follower from 5 mm plate with a square hole and a tooth that hooks behind a lug on the bolt.
- Mortise latch — the same works in a thin case let into a mortise in the door edge. Neater, but only for doors 35 mm or thicker.
- Spindle 8 mm square; backset (door edge to spindle) at least 60 mm, so knuckles clear the frame when you turn a knob. Make the bolt reversible so the latch fits a door hung either way.
Good: latches with a two-finger push, handle springs back level, no rattle (bend the striking plate's tongue to take up slack). Bad: bolt sticks half-way (burr — file and oil) or misses the plate (the door has dropped — fix the top hinge first). A spring latch with a key-turned deadbolt in the same case is a lock (Locks and Keys).
Door bolt
- Barrel bolt: a round bolt 8–12 mm thick sliding in staples on a back-plate, with a knob that drops into a notch so it cannot rattle back. Roll the edges of a 2–3 mm plate round the bolt (as for a butt knuckle) to make the guides; rivet on the knob.
- Tower bolt: the same, square, 15–30 cm long, for heavy doors. Flush bolt: let into the edge of the second leaf of a double door, shooting into head and floor.
- Keeper: a staple or socket plate screwed into the solid frame (not the stop bead), or a hole in a stone floor lined with a short iron tube.
One bolt at the top and one at the bottom beats one big one in the middle. A good bolt slides with a finger and cannot fall back.
Handles and knobs
Door handle
- Pull handle (D-handle): a bow of 12–16 mm bar, 15–25 cm long, ends flattened and drilled, or forged as spikes clenched through the door.
- Lever handle: a lever 10–13 cm long on a rose (round back-plate over the spindle hole), cast in brass or forged with a turned wooden grip. Curl the end back toward the door so it does not catch sleeves. Levers work with an elbow or a weak hand, so they suit the old, the young and anyone carrying things (Hearing Aids, Braille and Daily-Living Aids).
- Height 90–105 cm.
Doorknob
A knob 50–60 mm across on a spring-latch spindle. Wood: turn it from box, beech, fruitwood or ash on the The Lathe with a neck 25–30 mm thick, bored for the spindle and fixed with a cross pin; wax it. Ceramic: mould it in Stoneware and Porcelain or glazed earthenware (Glazes) round a metal shank set in with sulfur. Brass: cast hollow on a core, turn the outside, and fit a threaded shank. Set it on a rose with at least 60 mm backset. Good: a quarter turn or less draws the latch fully, no wobble on the spindle, and a soapy hand can still turn it.
Knocker, letterbox and bell
Knocker
A ring 12–15 cm across of 12–16 mm bar, forge-welded closed, or a cast brass or The Blast Furnace and Cast Iron hammer of 300–700 g, hinged from a back-plate or hung through an eye bolt nutted inside the door, with its hinge at about 140–150 cm. It falls on a striking stud that goes through the door into a hardwood pad inside, so the stud, not the door, takes the blows. Good: two light knocks are heard at the back of the house. If not, make it heavier rather than larger.
Letterbox
A slot with a hinged flap so post comes in when no one is home (The Post). Make the opening at least 25 × 250 mm, better 40 × 260 mm for newspapers, through the lock or middle rail (never a thin panel), between 75 and 150 cm from the floor. Outside, a brass or iron letter plate about 8 × 32 cm with a flap hinged along its top on a pin and held shut by a strip of spring brass. Line the slot with sheet metal, and fit a second flap or a cloth hood inside against draughts. Good: the flap closes itself with no rattle and no daylight at its edges.
Doorbell
Electric bells are in Electric Bells, Buzzers and Alarms. Before them:
- Pull bell. A knob outside on a rod with a return spring; inside, a wire runs to a small bell (Bronze) hung on a curled spring in the kitchen. At each corner the wire passes round a bell crank — an L-shaped lever pivoted at its corner, which turns a pull in one direction into a pull at right angles. Guide the wire with screw-eyes every 1–2 m. A board of bells, one per door or room, shows which was rung.
- Twist bell. A gong inside the door, its hammer worked by a crank turned from outside by a knob. Only one small hole through the door.
Door closers
Door closer
From simplest to best:
- Tilt the hinges: set the top hinge 3–6 mm nearer the door than the bottom one, and a light door always swings shut.
- Weight and pulley: a cord from the door, 30 cm out from the hinges, over a pulley on the frame to a 1–3 kg weight hanging in a wooden box. Cheap, reliable, very old.
- Rising butts (above).
- Spring: a long coil spring (Springs) from frame to door near the hinges, or a leaf spring on the frame pressing a roller on the door. Firm, but it slams.
- Door check (damped closer): a spring to shut the door and a dashpot to slow it — a piston in a sealed cylinder of oil or air, with a one-way flap that lets the fluid past freely as the door opens, and a small bypass hole, set by a screw, that is the only way back as it closes. Air checks (a leather-cupped piston in a brass tube) are easier; oil is smoother.
Good: closes from fully open in 3–7 seconds, latches every time, and a small child can still push it open.
Draught-proofing
Weatherstripping
The first steps are in Insulation and Keeping Buildings Warm or Cool. In detail:
- Stops: every door closes against a rebate or stop 12–15 mm deep. Pin a strip of Felt or soft leather 3–5 mm thick along the stop on the latch and head sides, so the door squeezes it as it latches; on the hinge side put it on the frame edge, or the door springs open.
- Threshold: an outside door needs an oak sill (Doors, Windows and Joinery) with a water bar — an iron or brass strip 6 × 25 mm set on edge — that the rebated bottom of the door closes against, plus a weatherboard outside. Inside doors: a leather strip on the bottom edge that brushes the floor, or a sausage of sand in cloth.
- Holes: a keyhole escutcheon with a swinging cover, a second flap behind the letterbox, a heavy curtain on a rod.
- Test: a candle flame round the closed door on a windy night does not flicker, and a strip of paper shut in the door pulls out against firm resistance all round.
How to tell it worked
- The door swings freely, stays where it is left (unless you meant it to close), and shows an even 2–3 mm gap.
- The latch catches every time from a gentle push and the door does not rattle in the wind; bolts slide with a finger and cannot fall back.
- A month later, the gap under the latch corner has not closed: the top hinge fixings are holding.
Note Troubleshooting. Door drops at the latch corner → top hinge loose or pin worn. Re-fix with longer screws into solid timber (plug stripped holes with glued hardwood pegs), or add a third hinge. Door springs open after closing → hinge-bound, or draught strip on the hinge side. Pack the hinges out with card; move the strip. Latch does not catch → the door has dropped, or the keeper is misplaced. Fix the hinges first, then move or file the plate. Latch catches but the door rattles → stop too far back. Move it in, or bend the striking plate's tongue. Squeak → dry pin. A drop of oil or tallow, or graphite rubbed on from a pencil (Lubricants and Greases). Knob turns but the latch does not move → spindle or follower worn round. Make a slightly oversize spindle and file it to fit. Closer slams → bypass screw too open or oil leaked. Close it a little; refill.
Dangers
Danger Fingers in the hinge gap. As a door closes, the gap on the hinge side shuts with enough force to cut off a child's fingertip, and closers make it worse. In houses with small children, cover the hinge-side gap with a flap of leather or cloth, and keep closers gentle and few.
Danger Falling gates. A heavy gate lifted off its pintles — by a child swinging on it, by cattle or by wind — falls flat and can crush a child to death. Always turn the top pintle down or cap it, check the hanging post every year, and do not let children swing on gates.
- Escape doors open outward and are never locked or bolted while people are inside (Firefighting).
- Hanging doors: a door weighs 20–60 kg. Lift it with two people. Forge, file and drill dangers are in Blacksmithing; wear eye protection.
Going further
Locks and deadbolts are in Locks and Keys; cupboard hinges and catches in Cupboards, Drawers, Shelves and Desks; windows use the same hinges, latches and stays at small size (Doors, Windows and Joinery, Window Glass). Once hardware is made to drawings (Technical Drawing) and gauges, one maker's parts fit another's doors — the start of Precision and Interchangeable Parts.
How it was first done
Egyptian and Mesopotamian doors of the 3rd millennium BC turned on pivots in stone sockets. Roman doors had bronze pivot sleeves, iron hinges, sliding bolts and bronze ring knockers, some of which survive. Medieval European doors hung on long, often decorated strap hinges, many still in use on church doors, and the Suffolk thumb latch was the common English latch from the 1600s into the 1800s. Cast-iron butt hinges were made in quantity in England from the later 1700s and soon took over house doors. Spring latches with knobs spread through the 1800s, when American makers sold ceramic and glass knobs by the million. The door letterbox became common in Britain after the penny post of 1840 brought daily letters to ordinary houses. Lewis Norton of Boston is generally credited with the first practical damped door closer, an air "door check" of about 1880.
Source: content/entries/building/doors-and-door-hardware.md