Part 4 · Food and Farming
Oils and Pressing
Squeeze oil out of olives, seeds and nuts with stones, levers and screws, and melt fat out of animal tissue. Oil is concentrated food energy, lamp fuel, the base of soap and paint, and the grease that keeps machines turning.
- Difficulty
- ●●●●●
- Time
- An afternoon for a pot of nut oil or lard; a season to build a beam or screw press
- Steps from zero
- 3 prerequisites →
This unlocks
Pigments, Paints and VarnishToothpaste, Shampoo, Perfume and CosmeticsLinoleum, Oilcloth and FloorclothsLubricants and GreasesRaincoats, Oilskins, Umbrellas and Rubber BootsThe full path from nothing — 3 steps before this one
- Stone Tools
- Simple Machines
- Farming from Seed
- Oils and Pressing
Do them roughly in this order. See it on the tech tree →
Why it matters
Fat is the densest food there is: about 9 kcal per gram, more than twice as much as grain or meat. A litre of oil holds the energy of 2–3 kg of bread. People doing hard physical work in the cold need it, and a diet with almost no fat leaves people hungry no matter how much lean meat they eat (see Nutrition and Deficiency Diseases).
But oil is just as important outside the kitchen:
- Light. A wick in a dish of oil is the oldest lamp (Lamps and Candles).
- Soap. Oil or fat boiled with lye (Lye and Potash) becomes Soap.
- Paint, varnish and ink. Linseed and walnut oil harden in air into a tough film: the base of oil paint (Pigments, Paints and Varnish), printing ink (Printing, Ink) and wood finishes.
- Lubrication. Oil and grease on axles and bearings stop wood and metal grinding themselves away (Lubricants and Greases, Bearings and Lubrication, The Wheel and Axle).
- Leather and waterproofing. Fats keep leather supple and keep rain out (Hides and Leather).
- Preserving. A layer of fat seals pots of food from air (Preserving Food).
How it works
Oil sits inside plant cells as tiny droplets, packed in with protein, fibre and water. To get it out you must:
- Break the cells — crush, grind or pound the seeds or fruit into a paste.
- Free the oil — warm the paste and often add a little water. Heat makes oil runnier and breaks the protein that holds the droplets. Warm paste gives much more oil than cold; cold paste gives less but better-tasting oil that keeps longer.
- Separate it — squeeze the paste hard so the oil runs out, or boil it in water so the oil floats up.
Oil is lighter than water (about 0.92 kg per litre) and does not mix with it. Almost every method ends by letting the liquid stand so the oil rises and the water and dregs sink.
Drying and non-drying oils. Some oils — linseed, walnut, poppy, hemp — slowly react with oxygen in the air and set into a hard, rubbery skin. These drying oils are what you want for paint and varnish, but they go stale fast in food. Non-drying oils — olive, rapeseed, almond, castor, and animal fats — stay liquid; they are best for lamps, lubrication, soap and cooking.
What you need
Oil sources
| Source | Oil content | Climate | Notes |
|---|---|---|---|
| Olive fruit | 15–30 % of fruit weight | Mediterranean: mild wet winters, hot dry summers | Easiest of all to press; trees live for centuries (Fruit Trees and Orchards) |
| Flax seed (linseed) | 35–45 % | Cool temperate | Drying oil; the same plant gives linen (Flax, Hemp and Linen) |
| Sunflower seed | 35–50 % | Warm summers | Shell the seeds first; easy to grow |
| Rapeseed / mustard | 35–45 % | Cool temperate | Old varieties are bitter; good lamp and lubricating oil |
| Walnut kernel | 60–65 % | Temperate | Excellent food and paint oil |
| Hazelnut, beechnut | 40–60 % | Temperate woods | Gather from the wild (Foraging Wild Food) |
| Coconut (dried flesh) | 60–65 % | Wet tropics | Boiling method works well |
| Sesame, peanut | 45–55 % | Warm | Cold-press or roast and press |
| Animal fat | 70–90 % | Anywhere | Render it (below) |
Tools
| Tool | Use |
|---|---|
| Mortar and pestle, or two stones | Crushing small amounts |
| Edge-runner mill | A heavy stone wheel rolling round on a stone bed — crushes olives and seeds in bulk (Ball Mills, Crushers and Grinders) |
| Press bags or mats | Coarse woven cloth of hemp, wool, horsehair or rushes, or flat baskets of grass or palm leaf |
| Press | Lever, wedge or screw (below) |
| Pots | For warming paste, settling oil, and storage |
Where to find it
- Olives grow wild and planted around the Mediterranean, in western Asia, and in similar climates (California, central Chile, South Africa, southern Australia). Trees are grey-green, silvery-leaved and gnarled; fruit ripens green, then purple, then black in late autumn.
- Flax is a slender plant with sky-blue flowers and round seed bolls; it grows wild and escaped from fields in Europe and western Asia. See Flax, Hemp and Linen.
- Sunflowers grow wild across North America; garden and field sunflowers have gone wild near settlements on every continent. Oil types have small, plump black seeds.
- Rapeseed, wild mustard and turnip are yellow-flowered cabbage relatives with long thin pods of round seeds — common weeds of fields everywhere.
- Walnuts, hazelnuts and beech grow in temperate broadleaf woods (Foraging Wild Food).
- Animal fat is thickest around the kidneys and under the skin of the back and belly, and in the tail of fat-tailed sheep. Fish livers and seal and whale blubber are rich in oil.
Method 1: Rendering animal fat
This needs no press and no crop, and it is the quickest way to a supply of fat.
- Cut the fat into pieces 1–2 cm across, or mince it, trimming off meat and blood. Kidney fat (suet) gives the hardest, whitest fat.
- Wet rendering (pale, mild fat): put it in a pot with about 2 cm of water. Heat gently — the water keeps it from scorching at first. Stir often.
- Over 2–4 hours the pieces shrink, turn golden and crisp, and float in clear liquid fat. The water boils away; the bubbling slows almost to nothing.
- Strain through a cloth into clean pots. The crisp leftovers (cracklings) are good food.
- Let it set. Lard (from pigs) is soft and white; tallow (from cattle, sheep and goats) is hard and crumbly and makes better candles and soap.
Keep the fat well below smoking: if it smokes, it is too hot (above about 180–200 °C) and turns bitter. Store it cool, covered and full to the brim; tallow keeps for many months, lard for several.
Method 2: Boiling out oil (nuts, coconut, seeds)
The simplest way to get plant oil without any press.
- Crack and shell nuts, or grate dried coconut flesh. Roast seeds lightly if you like — until they smell toasty, not burnt.
- Pound to a paste in a mortar or between stones — the finer the better. Walnuts and hazelnuts become a smooth, oily butter.
- Boil the paste in 3–4 times its volume of water for 1–2 hours, stirring.
- Let it cool. The oil rises and floats as a layer on top; on cold days it may set into a cake.
- Skim it off with a shell or flat spoon. Reheat the skimmed oil gently in a clean pot until it stops crackling and spitting — that drives out the last water, which would make it go bad.
This gets perhaps a third to a half of the oil. It is how shea butter, coconut oil and palm oil have been made in Africa and Asia for thousands of years.
Method 3: Pressing
Preparing the paste
- Olives. Pick when they are turning from green to purple-black. Press within a day or two — olives that sit get mouldy and give sour, rank oil. Crush them stones and all in an edge-runner mill or with a stone roller on a flat stone, to a thick purple paste. Stir the paste slowly for 30–60 minutes at room temperature; the tiny droplets join into bigger ones.
- Seeds (linseed, rapeseed, sunflower). Shell sunflower seeds. Crush seeds into coarse meal. Then warm the meal in a shallow pan, stirring, sprinkling in water: about a cupful (200 ml) per 2–3 kg, so it feels like damp sand. Heat to about 60–80 °C — too hot to keep your hand in, not hot enough to smoke or scorch. This is how the old Dutch oil mills worked, and it nearly doubles the yield.
- Nuts. Pound to a paste; warm gently.
Loading the press
- Spread paste on a mat or into a cloth bag, 3–5 cm thick, and fold it over. Stack the filled mats one on another, up to 20–30 for olives, on the press bed — a flat stone or thick board with a groove round the edge and a lip to pour the oil out.
- Put a flat board on top. Apply pressure slowly: press, wait for the flow to slow, press harder. Rushing bursts the bags. A good pressing takes 1–2 hours.
- Catch the oil and juice in a pot under the lip.
The beam (lever) press
This is the oldest large press and needs nothing but wood, stone and rope.
- Cut a wall slot or socket — a strong hole in a stone wall or between two deeply buried posts — at about knee height. One end of the beam goes into it as the pivot.
- The beam is a straight hardwood trunk 5–10 m long and as thick as a thigh at the pivot end.
- Put the press bed 1 m from the pivot. Hang stone weights (in a net, or tied on with rope) at the far end, or wind the beam down with a rope round a drum.
- The lever multiplies the force: a beam 6 m long with the bags 1 m from the pivot multiplies the weight six times. Hang 300 kg of stones on the end and the bags feel nearly 2 tonnes. See Simple Machines.
- Lift the beam between pressings with a second lever or a rope over a post.
The screw press
A screw turns a small push on a long handle into a huge squeeze, and the press can be small enough for a room.
- Build a strong frame: two hardwood uprights 15 cm thick, joined at the top by a cross-beam and set into a heavy base.
- Cut a large wooden screw about 10–15 cm across, with a thread of 4–6 cm per turn, and a matching nut in the cross-beam (see Screws, Nuts and Bolts). Hornbeam, oak, apple and walnut take a thread well; grease it with tallow.
- The screw pushes down on a press plate over a basket or cage of slats that holds the paste. Turn the screw with a bar 1–1.5 m long through a hole in the screw head.
- Turn steadily; as the flow slows, put two people on the bar. Two people pushing with 30 kg each on a 1 m bar give the plate a squeeze of roughly 2–3 tonnes.
A wedge press — paste in bags between two wooden blocks, squeezed by driving wedges with a heavy hammer or a water-powered trip hammer — was used in the windmill and watermill oil mills of northern Europe (The Windmill, The Watermill). It gives very high pressure for seeds.
Separating and storing
- Settle. Let the liquid stand in a deep jar for a day. Olive juice separates into oil on top and dark, bitter vegetation water underneath. Dip off the oil, or use a jar with a plugged hole low down to drain the water away.
- Clear. Let the oil stand 1–3 weeks in a cool place; the cloudy sediment sinks. Pour off the clear oil gently.
- Filter if needed through a cone of clean cloth or felt.
- Store in a cool, dark place in full, tightly closed jars. Air and light make oil rancid — sour, sharp and harmful.
What to expect. Hand methods recover roughly two-thirds of the oil: about 15–20 litres of olive oil per 100 kg of olives, or 20–30 kg of oil from 100 kg of linseed or shelled sunflower seed. The pressed cake left behind is rich in protein: excellent winter feed for cattle and pigs (Keeping Animals), or fertiliser (Compost and Manure).
Using the oil
- Cooking. Olive, sunflower, rapeseed, walnut, peanut and sesame oils, lard and tallow. Use linseed oil for food only when fresh.
- Lamps. Olive, rapeseed and fish oils burn well on a wick of twisted flax or cotton. Drying oils gum up wicks.
- Soap. Olive oil and tallow make the best soap (Soap).
- Paint and varnish. For a faster-drying oil, heat linseed oil in a pot outdoors, gently, for a few hours until it thickens a little and darkens ("boiled oil"). Never let it reach smoking. Mixed with ground mineral colours it makes oil paint (Pigments, Paints and Varnish).
- Grease. Tallow mixed with a little oil is axle grease. Castor oil and rapeseed oil stay slippery when hot and are the best plant lubricants (Bearings and Lubrication).
How to tell it worked
- Good oil is clear after settling, smells fresh (fruity, nutty or mild), and leaves no burning in the throat. Rancid oil smells of old paint or crayons and tastes sharp.
- Dry oil — free of water — burns quietly in a lamp. Oil with water in it sputters and crackles on the wick or in a hot pan.
- Spent cake feels dry and crumbly. If it is still greasy when you squeeze it, you need more heat, finer grinding, or more pressure.
Note Troubleshooting. Hardly any oil comes out of seeds → meal not fine enough, not warmed, or too dry. Grind finer, add water and warm it as described. Bags burst → pressure added too fast, or bags too full. Press slowly in stages. Oil is cloudy and goes bad quickly → water left in it. Settle longer, or warm it gently until it stops crackling. Olive oil bitter or rank → olives left too long before pressing, bruised or mouldy, or paste left in contact with vegetation water. Press fresh fruit and separate quickly. Lard brown and strong-smelling → rendered too hot. Use water and low heat.
Dangers
Danger Oily rags catch fire by themselves. Cloth, straw or sawdust soaked in linseed, walnut or other drying oil heats up as the oil hardens. Piled in a heap, it can burst into flame hours later, with nobody near. Spread oily rags flat outdoors to dry, or put them in a pot of water or burn them at once. This has burned down many workshops and barns.
Danger Hot oil fires. Fat and oil heated past smoking can burst into flame. Never throw water on burning oil — the water explodes into steam and throws flaming oil everywhere. Smother it with a lid, a wet (wrung out) cloth, sand or earth, and take it off the heat. Keep children away from rendering pots.
- Burns. Hot fat sticks to skin. Cool burns under running water for 20 minutes (Wound Care and Antiseptics).
- Poisonous seeds. Castor beans contain ricin, one of the deadliest plant poisons; a few chewed seeds can kill a child. Their oil is a fine lubricant, but never eat the seeds, keep the pressed cake away from people and animals, and wash your hands after handling them. Cottonseed oil and cake contain a poison (gossypol) unless cooked and refined; don't eat them unprocessed. Never press seeds you can't identify.
- Old rapeseed. Traditional rapeseed and mustard oils contain a lot of erucic acid, which in large amounts may harm the heart; use them for lamps and machines, or eat them in moderation.
- Crushing injuries. Beams, screws and weights can break bones. Never put a hand under a loaded beam, and stand clear of the end weights when they are lifted.
- Rancid fat upsets the stomach and destroys vitamins.
What this unlocks
With oil and fat you can make Soap, light homes with Lamps and Candles, make paints and varnishes (Pigments, Paints and Varnish) and printing ink (Printing), grease Bearings and Lubrication and axles, dress Hides and Leather, and feed animals on the press cake. The screw press itself is the same machine that presses grapes and apples (Beer, Wine and Cider), paper sheets (Paper) and type (Printing). Large mills driven by water or wind (The Watermill, The Windmill) and later hydraulic presses multiply output many times.
How it was first done
People rendered animal fat as long as they had fire and containers. Olive oil was being extracted in the eastern Mediterranean by at least 5000 BC: at Kfar Samir, a drowned village off the coast near Haifa in Israel, archaeologists found pits full of crushed olive stones from around that time. Beam presses with stone weights were used throughout the Bronze and Iron Ages; the Philistine city of Ekron (in modern Israel) had more than a hundred olive-oil installations in the 7th century BC, one of the largest oil industries of the ancient world.
The screw press appeared in the Greek and Roman world around the 1st century BC. The Roman writer Pliny the Elder, in about AD 77, describes it as a recent improvement. Linseed oil was used for paintings in Afghan cave temples at Bamiyan in the 7th century AD and became the classic painters' oil in Europe from the 15th century. Wind- and water-driven oil mills with stampers and wedge presses spread across the Netherlands in the 17th century. Sunflowers were domesticated in North America at least 4,000 years ago, but large-scale sunflower oil began in Russia in the 1830s.
Source: content/entries/food/oils-and-pressing.md