The Generator

How to turn motion into electricity by moving magnets past coils of wire — first a hand-cranked magneto, then a self-exciting dynamo driven by a waterwheel. This is how almost all the world's electricity is made.

Difficulty
●●●●●
Time
Two to four weeks for a hand magneto; months for a waterwheel-driven dynamo
Steps from zero
19 prerequisites →

You need first

MagnetsCopper WireThe Waterwheel

This unlocks

Synchronous Motors and ConvertersThe TransformerWiring and Electrical SafetyWater Turbines and Hydroelectric PowerWind TurbinesThe Electric Arc Furnace

Raw materials

hardwoodbeeswaxlac
The full path from nothing — 19 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Hunting and Trapping
  7. Basic Woodworking
  8. Charcoal
  9. Pottery
  10. Hides and Leather
  11. The Wheel and Axle
  12. Bellows
  13. Gears
  14. Iron (the Bloomery)
  15. Copper Smelting
  16. The Waterwheel
  17. Blacksmithing
  18. Magnets
  19. Copper Wire
  20. The Generator

Do them roughly in this order. See it on the tech tree →

Why it matters

A The Battery makes electricity by slowly eating zinc, and zinc is hard to make. A generator makes electricity from motion — a turning crank, a The Waterwheel, a The Windmill, a The Steam Engine — and uses up nothing but the wear on its bearings. A small battery bank might give you a few watts for a few days; a dynamo on a good stream can give hundreds of watts, day and night, for years.

That is the difference between electricity as a laboratory curiosity and electricity as a tool. With a generator you can light a workshop with arc and filament lamps, run Electrolysis to make Aluminium, chlorine (Chlorine and Bleach) and pure copper, charge storage batteries, and drive The Electric Motors at the far end of a wire — carrying the power of a river to where it is needed.

How it works

In 1831 Michael Faraday discovered the reverse of the The Electromagnet: if a current makes magnetism, then changing magnetism makes a current.

Push a magnet into a coil of wire whose ends are joined through a galvanometer, and the needle kicks. Hold the magnet still inside the coil — nothing. Pull it out — the needle kicks the other way. It is not the magnet that makes electricity; it is the movement. This is called induction.

SN Push inneedle kicks one way SN Hold stillnothing SN Pull outneedle kicks the other way galvanometer (far from the magnet)
Fig. 1 Induction. Moving a magnet into a coil pushes a current one way; holding it still gives nothing; pulling it out pushes current the other way. Only change makes electricity.

How much voltage you get depends on three things, multiplied together:

  • How many turns of wire the coil has. Twice the turns, twice the volts.
  • How strong the magnet is.
  • How fast the magnetism through the coil changes. Twice the speed, twice the volts.

A generator is simply a machine that moves magnets past coils (or coils past magnets) over and over, as fast as possible. Each time a north pole approaches a coil, current is pushed one way; as it leaves, or as a south pole approaches, current is pushed the other way. So the natural output of every generator is alternating current (AC) — a current that flows forward and back, forward and back.

AC or DC?

  • Alternating current is fine for lamps and heaters. To collect it from a spinning coil, use slip rings: two continuous copper rings on the shaft, one for each end of the coil, each with a brush (a springy copper strip) pressing on it. If the magnets spin and the coils stay still, you need no sliding contacts at all.
  • Direct current (DC) — current that always flows the same way — is needed to charge batteries, for Electrolysis, for plating, and to feed electromagnets. To get it, use a commutator: a copper ring split into two halves, insulated from each other, turning with the shaft. Each half connects to one end of the coil. Two brushes press on opposite sides. Every half-turn, just as the current in the coil reverses, the halves swap brushes — so the current in the outside wire always flows the same way.
SLIP RINGS → AC COMMUTATOR → DC Two whole rings one for each end of the coil Brushes springy copper strips coil coil Brushes swap halves every half-turn Split ringtwo halves, insulated output flows forward, then back output always flows one way (in pulses)
Fig. 2 Slip rings and the commutator. Slip rings (left) pass on the alternating current as it is. The split-ring commutator (right) swaps the connections every half-turn, so the output always flows the same way — though it still pulses.

What you need

Item For the hand magneto Notes
Permanent magnets 4 hardened steel bars, 10 × 2.5 × 1 cm, strongly magnetised Magnets; magnetise with an electromagnet if you can
Soft iron 4 rods 1.5 cm thick, 6 cm long, for coil cores; strip for a back ring Iron (the Bloomery), annealed
Insulated copper wire About 150 m of 0.5 mm Copper Wire
Hardwood Disc 30 cm across, 4 cm thick; frame and bearing blocks Basic Woodworking; oak, beech, maple
Iron axle 2 cm thick, 50 cm long Blacksmithing
Copper strip For commutator and brushes, 1 mm thick Copper Smelting
Gears or pulleys and belt Step-up of 1:5 to 1:10 Gears, Hides and Leather
Shellac or wax To varnish coils Copper Wire
Galvanometer For testing The Electromagnet

Where to find it

Everything here is made in other chapters: steel magnets in Magnets, wire in Copper Wire, soft iron in Iron (the Bloomery), gearing in Gears and The Wheel and Axle, and water power in The Waterwheel. Good, dense, seasoned hardwood for the rotor and frame comes from oak, beech, maple, ash or hornbeam; it must be dry, or it will warp and the gaps between magnets and coils will close up and rub.

Method 1: Faraday's first test

Before building a machine, convince yourself that induction works and learn what affects it.

  1. Wind a coil of 200–300 turns of 0.4–0.5 mm covered wire on a paper tube just wide enough for your bar magnet to slide in.
  2. Connect its ends to the thin-wire coil of a galvanometer (The Electromagnet). Put the galvanometer at least 1 m away, so the magnet itself does not swing its needle.
  3. Thrust the magnet into the coil quickly. The needle kicks. Pull it out: it kicks the other way. Do it slowly: smaller kick. Use the other end of the magnet: everything reverses.
  4. Put a soft iron rod in the coil and bring the magnet up to the rod's end quickly: the kick is bigger. Iron cores gather the magnetism through the coil.

Method 2: A hand-cranked magneto

This machine spins four magnets past four fixed coils. Because the coils do not move, the AC version needs no brushes at all.

NSNS Coil (one of four) 400 turns of 0.5 mm wire on a soft iron core Back iron ring joins the outer ends of the cores Steel bar magnets alternate poles outward: N, S, N, S; inner ends joined by an iron ring Gap 1–2 mm as small as you can without rubbing Rotor hardwood disc 30 cm across, 4 cm thick Axle driven by a crank through a 1:5–1:10 step-up
Fig. 3 A hand magneto seen from the front. Four steel magnets, set in a hardwood rotor with alternate poles outward, sweep past four iron-cored coils fixed to the frame. A gear or belt step-up makes the rotor spin five to ten times faster than the crank.

The rotor

  1. Turn or carve a hardwood disc 30 cm across and 4 cm thick, with a square hole at its centre for the axle. It must run true: spin it and watch the rim; it should not wobble more than 1 mm.
  2. Cut four slots running from the rim towards the centre, at 90° to each other, each fitting one bar magnet snugly. Set the magnets in with their ends flush with the rim (or 1 mm proud), alternating: north outward, then south outward, then north, then south. Glue and wedge them hard; at speed a loose magnet will fly out.
  3. Better still: join the inner ends of the magnets with a ring of soft iron. This closes their magnetic loop behind them and makes the outer poles noticeably stronger.

The coils

  1. Make four soft iron cores, 1.5 cm thick and 6 cm long, with their outer ends joined by a soft iron ring or bar (the back iron) that is fixed to the frame.
  2. On each core wind about 400 turns of 0.5 mm covered wire — four or five layers, with paper between layers (see Copper Wire). Varnish.
  3. Mount the coils on the frame, pointing in at the rotor at 90° spacings, with their core ends 1–2 mm from the rotor's rim. The smaller the gap, the more output; but nothing may touch when the rotor spins.

Connecting the coils

  1. When coil 1 faces a north pole, coil 2 faces a south pole, so their currents are opposite. Connect them so that they add: join all four in a chain, but with every second coil's ends swapped. Check it: turn the rotor by hand through a short distance with the galvanometer connected across first one coil, then two in series. Two coils in series must kick more than one. If they kick less, swap one coil's connections.

Speed

  1. Fit a crank on a separate shaft with a large pulley or gear, driving a small one on the rotor shaft at a ratio of 1:5 to 1:10. Turning the crank once a second then spins the rotor 5–10 times a second (300–600 turns per minute). Mount the shafts in greased hardwood or bronze bearings (Bronze), or in iron bushes.

What to expect

Each coil sees a north pole and then a south pole twice per turn. With strongly magnetised steel bars, 400 turns per coil, and the rotor at about 10 turns a second, expect a few volts of AC — roughly 2–6 V from four coils in series — and a current of a few tenths of an amp into a thick, short wire. That is about as much as a small cup battery: enough to swing a galvanometer hard, bubble salt water, glow a very thin wire, ring a bell or give a tingle.

To get more voltage, use more turns of thinner wire (19th-century medical "shocking machines" and telephone ringer magnetos, with thousands of turns, gave 50–100 V at very small currents). To get more current, use fewer turns of thicker wire. To get more of both, you need stronger magnets, more of them, more speed — or Method 3.

For direct current

To get DC from a magneto, add a commutator to the shaft. Because in this machine the coils stand still and the shaft turns, the commutator here works as a rotating reversing switch:

  1. Turn a hardwood or bone hub on the axle. Wrap it with a ring of copper strip and saw the ring into four equal segments, leaving gaps of 2–3 mm filled with shellac-soaked paper or wood. Join opposite segments together (1 with 3, 2 with 4) with wire on the hub.
  2. Beside the commutator, fit two slip rings — whole copper rings, insulated from each other and from the shaft. Connect segments 1 and 3 to one slip ring, segments 2 and 4 to the other.
  3. Connect the two ends of the coil chain to two brushes — springy copper strips — pressing on the commutator 90° apart. Take the output from two more brushes on the slip rings.
  4. With the galvanometer on the output, shift the pair of commutator brushes round the ring (keeping them 90° apart) until the current is strongest and flows one way only, and fix them there.

Every quarter-turn, just as the coils' current reverses, the commutator swaps which coil end goes to which slip ring, so the output always flows the same way.

Method 3: The self-exciting dynamo

The weakness of every magneto is its steel magnets. The answer, found in 1866–67 by Werner von Siemens and others at the same time, is to replace the permanent magnets with electromagnets, fed by the generator's own current.

How it starts by itself: soft iron always keeps a little leftover magnetism. When the machine first turns, this faint magnetism makes a faint current. That current, sent through the field coils, makes the magnets a little stronger, which makes more current, which makes the magnets stronger still. Within a few seconds the machine "builds up" to full strength, limited only by how much magnetism the iron can carry. A self-exciting dynamo can be many times more powerful than a magneto of the same size.

To build one:

  1. The field. Forge a heavy soft iron frame with two pole pieces facing each other across a round hole, like a horseshoe whose ends are hollowed to wrap around the armature. Pole pieces about 10 cm long (along the shaft) and a bore of about 10 cm suit a machine of a few hundred watts. Wind a field coil on each limb: many turns (500–1,000 each) of 0.8–1 mm wire, wound so that one pole is north and the other south (check with a compass, as in The Electromagnet).
  2. The armature. Build an iron core that spins in the bore with 1–2 mm clearance. The simplest is Siemens' shuttle armature: an iron cylinder with two deep slots cut along its length, so that its cross-section looks like an H. Wind a coil lengthways into the slots — 50–150 turns of 1.5–2 mm wire, depending on the voltage you want — and bring the two ends to a two-segment commutator on the shaft. Lay the iron up from thin plates of soft iron with paper between them if you can: a solid core gets hot from currents swirling inside it (Transformer Steel, Ferrite and Magnetic Shielding).
  3. Connect the field coils across the brushes (this is called shunt winding).
  4. Drive it at the design speed: about 1,000–1,500 turns per minute.
  5. If it does not build up: reverse the two field connections (the current was weakening the leftover magnetism instead of helping it); or touch a battery to the field coils for a second to "flash" them; or check that the brushes are on the commutator at the right places; or disconnect the load until it has built up.

A machine of this size, well made and turned fast, can give something like 50–100 V at a few amps — a few hundred watts. Expect to rebuild it at least once. The 19th-century improvement was the ring armature of Zénobe Gramme (1871): many small coils round an iron ring, each to its own commutator segment, giving a smooth, almost steady current.

Driving it with a waterwheel

A The Waterwheel turns slowly — perhaps 5–15 times a minute for a large overshot wheel. A dynamo wants 1,000 or more. You must step the speed up 100 times or more:

× 10 × 10 Water in at the top overshot waterwheel Wheel shaft 10 turns a minute; 2 m pulley Countershaft 100 turns a minute; 20 cm and 1 m pulleys, flywheel Dynamo 1,000 turns a minute; 10 cm pulley leather belt
Fig. 4 Stepping up the speed. A slow waterwheel drives the dynamo through two belt stages, each multiplying the speed about ten times. Belts slip rather than break if the dynamo jams.
  1. First stage: a large wooden pulley or gear on the waterwheel shaft — say 2 m across — drives a small one 20 cm across on a countershaft (×10). Gears (Gears) are stronger here, where the force is greatest.
  2. Second stage: a pulley 1 m across on the countershaft drives a 10 cm pulley on the dynamo (×10). Use a flat leather belt (Hides and Leather) on slightly crowned (barrel-shaped) wooden pulleys; the crown keeps the belt centred.
  3. Steady speed. The voltage rises and falls with speed. Add a heavy flywheel on the countershaft, and adjust the water gate by hand to keep the lamps steady. Later, a centrifugal governor (two weights on swinging arms that close the gate as they fly out) can do it automatically (Governors and Speed Control).

How much power is in your stream? Measure the flow (litres per second — time how long it takes to fill a barrel from the race) and the height the water falls in metres. Then:

power in watts ≈ flow (L/s) × fall (m) × 10 × 0.6

The 10 is gravity; the 0.6 is a good overshot wheel's efficiency. Example: 50 L/s falling 3 m gives about 900 W at the shaft. A home-built dynamo might turn half of that into electricity — 400–500 W, enough for one arc lamp or eight to ten carbon filament lamps.

How to tell it worked

  • Galvanometer. Connected through the thin-wire coil, the needle swings back and forth with AC (if you turn slowly enough to see it), or to one side with DC.
  • Bubbles. Two wires in salt water: bubbles at both wires with AC; steadily from the negative wire with DC.
  • Hot wire. A short length of thin iron wire across the output glows dull red at a few amps.
  • Lamps. A The Light Bulb glows. Its brightness rising and falling as you crank faster and slower shows the dynamo is working.
  • Measuring power without meters. Put a coil of iron wire in exactly 1 litre of water in a wooden or clay vessel and run the dynamo through it for a few minutes, stirring. Every degree Celsius per minute that the water warms is about 70 W (use a The Thermometer).

Note Troubleshooting. Nothing at all → a broken wire or coils connected so that they cancel. Test each coil separately with the galvanometer, then add them one at a time. Brushes spark heavily → brushes in the wrong position, rough commutator, or too much load. Turn the brushes a little round the ring until sparking is least; smooth the copper with fine sand. Output dies as it warms up → wax insulation softening and turns shorting. Use shellac. Self-exciter will not build up → see step 5 of Method 3. Rotor hits the coils → shaft flexing or bearings worn. Thicker shaft, tighter bearings, wider gap.

Dangers

Danger Belts, gears and shafts. Turning machinery catches loose clothing, hair and fingers and does not stop. Fence off belts and gears, tie back hair and sleeves, and never reach over a running belt. Have a way to stop the waterwheel quickly — a gate you can drop — before you work on anything.

Danger High voltage. A dynamo of 50–100 V can kill, especially through wet skin or from hand to hand across the chest. Dynamos for lighting in the 1880s killed workers. Switch off and stop the machine before touching any wire; work with one hand behind your back on live gear; stand on dry wood.

  • The field coils' kick. Opening the circuit of a dynamo's field coils while running gives a high-voltage spark that can shock you badly and burn the insulation. Slow the machine down before disconnecting the field.
  • Flying magnets and rotors. A wooden rotor spun too fast can burst; magnets work loose. Never stand in line with a spinning rotor, and build guards.
  • Fire. Overloaded windings get hot enough to char wood and ignite wax. Never leave a loaded dynamo unattended until you know how warm it runs.
  • Working at the water. Wheel races are deep and fast. See The Waterwheel.

What this unlocks

How it was first done

On 29 August 1831 Michael Faraday, at the Royal Institution in London, wound two coils on an iron ring and saw a galvanometer on one coil kick each time he connected or disconnected a battery to the other. Weeks later he generated a current by moving magnets in and out of coils, and by spinning a copper disc between the poles of a magnet — the first generator. In 1832 the Parisian instrument maker Hippolyte Pixii built a hand-cranked machine in which a horseshoe magnet spun beneath two coils; at André-Marie Ampère's suggestion he added a commutator to turn its alternating current into direct current.

Through the mid-1800s, magnetos with banks of steel magnets lit lighthouses, beginning with Frederick Holmes's machines at South Foreland in England in 1858. In 1866–67 Werner von Siemens in Berlin, Charles Wheatstone and Samuel Varley in England each announced the self-exciting dynamo (Ányos Jedlik in Hungary had built one earlier but not published). Zénobe Gramme's ring dynamo of 1871 made steady currents practical, and in 1881 the English town of Godalming became one of the first places to have a public electricity supply — driven by a waterwheel on the River Wey. The next year, hydroelectric plants opened in Appleton, Wisconsin, and Thomas Edison's steam-powered Pearl Street station began supplying New York.

Source: content/entries/electricity/generator.md