◆ Rebuild

Part 15 · Knowledge and Science

Lithography and Offset Printing

Printing from a flat surface instead of a raised or sunken one. Draw on fine limestone with a greasy crayon, treat the stone with gum and a little acid, keep it damp, and ink sticks only to the drawing. The same trick works on zinc and aluminium plates, in many colours, and on the offset press that prints most of the world's paper.

Difficulty
●●●●●
Time
An afternoon to grain a stone; a day to draw, etch and print a first image; weeks to build a press
Steps from zero
16 prerequisites →

You need first

PrintingPigments, Paints and Varnish

This unlocks

—
The full path from nothing — 16 steps before this one
  1. Fire
  2. Stone Tools
  3. Finding and Preparing Clay
  4. Simple Machines
  5. Basic Woodworking
  6. Pottery
  7. Charcoal
  8. The Kiln
  9. Farming from Seed
  10. Lime
  11. Oils and Pressing
  12. Lye and Potash
  13. Ink
  14. Pigments, Paints and Varnish
  15. Paper
  16. Printing
  17. Lithography and Offset Printing

Do them roughly in this order. See it on the tech tree →

Why it matters

Letterpress needs type or carved blocks. Engraving, Seals and Etching needs hours of skilled cutting into copper. Lithography needs neither: an artist, a mapmaker or a clerk simply draws or writes on a flat stone with a greasy crayon or ink, and after a short chemical treatment the stone prints that drawing hundreds or thousands of times, with every soft shade of the crayon kept.

That makes it the cheapest way to print maps, diagrams, music, posters, labels, forms and pictures — anything that is easier to draw than to set in type. With several stones it prints in full colour. And the same principle, moved onto thin metal plates wrapped round a cylinder, became the offset press, which since the mid-1900s has printed most books, newspapers and packaging.

How it works

Lithography is planographic: the printing surface is flat. Nothing is raised or sunk. It works because grease and water repel each other.

  1. Draw with grease. Fatty crayon or ink soaks a little way into the fine pores of limestone. Where it lies, the stone now holds grease firmly.
  2. Etch with gum and acid. A solution of gum arabic with a few drops of Nitric Acid is spread over the whole stone. The acid lightly attacks the bare stone, and the gum fixes there as a thin film that loves water and refuses grease. Where the drawing is, the gum cannot reach.
  3. Damp and ink. Wipe the stone with a wet sponge: water clings to the gummed areas but runs off the greasy drawing. Roll greasy ink over it: the ink sticks to the drawing and is pushed away by the wet stone.
  4. Print. Lay paper on and press it under a sliding scraper. The ink transfers. Damp again, ink again, print again.

The image is reversed on the stone, as in all direct printing. Drawing in mirror image is hard, so lithographers use transfer paper (below) or the offset principle, where the image goes first onto a rubber blanket and from there onto the paper — reversed twice, so right-reading on the plate.

1. Draw 2. Gum etch 3. Damp and ink 4. Print greasy crayon on stone gum film on bare stone water here, ink there paper takes the ink grease soaks in gum holds water, refuses grease ink on drawing water on gum paper with the print The stone is flat throughout. Only grease and water decide where ink goes.
Fig. 1 How a stone prints. The crayon's grease enters the stone; the gum etch makes the rest of the surface hold water; when damped and rolled, ink stays only on the drawing and is pressed onto paper.

What you need

Item Amount / size Notes
Litho stone 25 × 35 cm, 6–8 cm thick, for a start Fine, even limestone (below); weighs about 15–20 kg
Graining sand A few kilograms, three grades Clean quartz sand, sieved coarse, medium, fine (Abrasives and Grinding Stones)
Gum arabic 250–500 g Or cherry, plum or apricot gum; see Glues and Adhesives
Nitric acid A few millilitres per print run See Nitric Acid
Crayon and tusche A few sticks Wax, tallow, soap, shellac, lampblack (below)
Rosin and talc or chalk A handful Dusted over the drawing to protect it
Turpentine, asphaltum 100 ml each Turpentine; bitumen dissolved in it
Litho ink 100–200 g Stiff boiled-linseed ink (Ink, Pigments, Paints and Varnish)
Leather roller 30–40 cm long Calf leather on a wooden core
Press — Scraper press (below); for small work, a burnisher

Where to find it

  • Lithographic limestone. The best comes from Solnhofen in Bavaria: a pale cream to blue-grey limestone in perfectly even layers, so fine-grained that no grain shows even under a magnifier. Look for any dense, fine, uniform limestone that breaks with a smooth, shell-like surface, rings when struck, and has no veins, cracks, fossils or iron spots in the area you need. Test as for all limestone (Lime): it fizzes with vinegar. Grey-blue stones are harder and take finer detail than yellow ones. See Quarrying and Cutting Stone for splitting slabs.
  • Gum arabic oozes from the bark of acacia trees in dry country as pale amber lumps. The clear gum from cherry, plum and apricot trees is a fair substitute.
  • Fats, wax, shellac, rosin and bitumen: beeswax, tallow from Butchery and Meat, lac from lac insects (Glues and Adhesives), rosin from pine resin (Tar, Pitch and Glue), and natural bitumen seeps (Tar, Pitch and Glue, Petroleum and Refining).

The litho stone

The stone is the heart of the craft and lasts a lifetime. Each print run is ground away afterwards and the same stone is used again, losing about 0.2–0.5 mm per graining.

Size. The bigger the stone, the thicker it must be, and never less than 5 cm, or it cracks under the press. Common sizes: 25 × 35 cm at 6 cm, 40 × 55 cm at 8 cm (about 45 kg), 60 × 80 cm at 9–10 cm (over 100 kg — lift with two people or a tackle). Both faces must be parallel so the press bears evenly.

The levigator is the grinding tool: a cast-iron disc about 25–30 cm across and 3–4 cm thick with an upright handle near the rim, so it can be spun round. Without iron, grind one stone against another of the same size, face to face.

Graining a stone

  1. Wash the old image off with turpentine. Sprinkle a spoonful of coarse sand and enough water to make a slurry. Lay the levigator on and push it in figure-of-eight loops over the whole stone, turning it as you go, for 5–10 minutes. Wash off. Repeat until the old image is completely gone — a ghost of an old drawing will print again.
  2. Check flatness with a straight steel or hardwood edge laid across and diagonally. No light should show under it. Grind more at the edges if the middle is low.
  3. Grain again with medium then fine sand, washing thoroughly between grades — one coarse grain left behind scratches the stone.
  4. Finish to suit the work. For crayon drawing, stop at a fine, even, velvety grain: the crayon catches on the tips and gives soft tone. For pen and ink or writing, go further and polish with pumice and then a rag and water until it is smooth and dull-shiny.
  5. Bevel all edges with a file or coarse stone, 3–4 mm wide, so they do not take ink or cut the paper.
  6. Let it dry fully and do not touch the face — the grease from one fingerprint prints as a smudge.

Drawing materials

Lithographic crayon and tusche

Litho crayon is a hard grease made black so you can see what you draw. A workable recipe by weight:

Ingredient Parts Job
Beeswax 4 Body
Hard soap (Soap) 4 Makes it mix with water later; holds it in the stone
Tallow 1 Softness
Shellac 2 Hardness
Lampblack (Lampblack and Carbon Black) 1 Colour only
  1. Melt the wax and tallow together in an iron pot over a low fire. Shave in the soap and stir until dissolved.
  2. Add the shellac little by little. Raise the heat until the mixture smokes and will catch fire from a burning splint; let it burn for half a minute, then smother it with the lid. This burning drives off water and makes the crayon hard. (Do it outdoors, see Dangers.)
  3. Stir in the lampblack, pour into a greased mould of grooves about 1 cm square, and cut into sticks when cold.

More soap and tallow gives a soft crayon for dark, rich tones; more shellac gives a hard crayon for pale greys and fine lines.

Tusche (liquid litho ink for pen and brush) is the same mixture, cast into a cake, then rubbed up in a saucer with a few drops of rain water, like Chinese ink. Dilute it to a wash for greys.

Drawing

Hold the crayon lightly. Tone comes from pressure and from the grain, not from rubbing — the crayon touches only the tops of the grain, leaving tiny white gaps. Rest your hand on a bridge (a plank raised on two blocks) so it never touches the stone. Scrape mistakes away with a sharp blade, which also gives clean white highlights. Remember the image prints reversed: write lettering in a mirror, or use transfer paper.

Transfer paper

Transfer paper lets you draw or write the right way round and lets you move a print from type or a copper plate onto stone.

  1. Make a coating of starch paste (3 parts) with a little glue (1 part) and a pinch of chalk or plaster (Gypsum and Plaster of Paris), as thin as cream.
  2. Brush it evenly on strong, smooth Paper, two thin coats, and dry. Rub smooth.
  3. Write or draw on the coated side with tusche, or take an impression of inked type or an engraving with transfer ink (litho ink softened with extra tallow and wax).
  4. Lay the sheet face down on a clean, slightly warm stone. Damp the back with a sponge and pass it through the press 4–6 times, increasing pressure.
  5. Soak the paper until it lifts off. The grease stays on the stone, now mirror-reversed, ready to etch. It will print the right way round.

Step by step: printing from stone

  1. Protect the drawing. Dust it with powdered rosin, then with talc or fine chalk, and brush off the excess. The rosin makes the drawing resist acid.
  2. Make the gum. Soak 1 part gum arabic in 2 parts water overnight and strain through cloth. It should pour like thin cream.
  3. Mix the etch. To 30 ml of gum add 6–10 drops of strong nitric acid for a light crayon drawing, 12–20 for a heavy ink drawing. Test a drop on the stone's margin: it should start to fizz with fine bubbles after 10–15 seconds. Instant violent fizzing is too strong.
  4. Etch. Brush the etch over the whole stone, working it into the bare areas and lightly over the drawing, for 3–5 minutes. Blot it, then buff the remaining gum to a thin, even film with a soft rag.
  5. Rest. Leave the gummed stone at least 2 hours, better overnight. The gum film sets and the grease settles into the stone.
  6. Wash out. With the dry gum still on, wipe the drawing away with turpentine on a rag. It looks as if it is gone. Rub in a thin film of asphaltum (bitumen dissolved in turpentine) and fan it dry; it gives the image a strong greasy base.
  7. Roll up. Wash the gum off with water. Keep the stone evenly damp with the sponge — never puddled, never dry. Roll ink on with the leather roller, slowly and with firm pressure, in several directions. The drawing reappears, black, as the ink finds it. Damp, roll, damp, roll, until it is fully back.
  8. Second etch (optional). Dust with rosin and talc again and etch once more for 2–3 minutes. This makes the whites cleaner for a long run.
  9. Print. Damp; roll on ink (4–6 passes); lay the paper; put the tympan down; crank the stone under the scraper; lift the tympan and peel the print. Repeat.
  10. Store between runs by gumming the inked stone and letting it dry. It keeps for months.

The litho press

Lithography needs very heavy pressure but no impression into the paper, so the press drags a smooth edge over the back of the paper instead of squeezing it under a platen.

Pressure screwsets the scraper height Scraper boxslides up and down scraper, leather edge tympan over paper Stoneon the bed Sliding bed Rollerunder the scraper Crank wheel Pressure lever pull down bed and stone travel
Fig. 2 The scraper press. The stone sits on a sliding bed. The pressure lever brings the leather-faced scraper down on the greased tympan, and the crank winds the bed and stone underneath it.
  1. Frame. Two oak side cheeks about 1 m high and 1.2–1.5 m long, 8–10 cm thick, joined by cross rails (Doors, Windows and Joinery, Timber Framing and Log Building).
  2. Bed. A strong plank carriage as long as two stones, running on a large hardwood or iron roller set in the frame under the scraper, and on smaller guide rollers at the ends. It must run level.
  3. Scraper. A bar of boxwood or other dense hardwood, 3–4 cm thick, about 8–10 cm deep, slightly shorter than the stone's narrow side, its lower edge planed to a blunt V and rounded to about 3 mm radius. Cover the edge with a strip of leather. Hold it in a scraper box that slides up and down in a heavy crossbeam, and make several scrapers for different stone widths.
  4. Pressure. A long lever with a cam or toggle pushes the scraper box down. A screw above it sets the height so that, with the lever pulled, the scraper bears down with great force — a press of this size may exert several tonnes.
  5. Drive. A crank or star wheel turns the roller under the bed, often through a pair of Gears or a strap wound on a drum. One full movement carries the stone right under the scraper.
  6. Tympan. A sheet of leather, thin zinc or stiff pressboard on a hinged frame, laid over the paper. Grease its back with tallow every few prints so the scraper slides.

The litho roller. Turn a wooden core about 10 cm across and as long as the stone's width, with a handle at each end (Wood Turning and Treen). Wrap it with a layer of flannel, then a sleeve of calf leather, rough side out, sewn tight with the seam flush. Break a new roller in by rolling it for several days in thin varnish, scraping it back each time, until the nap is smooth and even. Scrape it clean with a blunt knife; never wash it in solvent. For colour work, a smooth roller of glue and glycerine composition or rubber is better.

For small proofs without a press, rub the back of the paper hard with a bone burnisher or wooden spoon.

Lithographic plates: zinc and aluminium

Stones are heavy, slow and break. From the 1830s, printers drew on zinc, and from the 1890s on aluminium. A metal lithographic plate is light, cheap, can be bent round a cylinder, and is the only kind an offset press can use.

  1. Metal. Sheet zinc about 0.5–1 mm thick (Zinc and Brass, Sheet Metal and Rolling), or aluminium 0.3–0.6 mm (Aluminium). Cut it 2–3 cm larger all round than the image.
  2. Grain. Lay the plate in a shallow tray, cover it with a layer of glass, porcelain or steel marbles 1–2 cm across, fine sand and water, and rock the tray in small circles for 30–60 minutes. A box hung from a crank on a water wheel or treadle does this all day. The plate comes out with an even, matt, grey grain that holds water and crayon. Wash it well and use it within a day or two; an old grain oxidises and takes ink badly.
  3. Draw exactly as on stone, with crayon and tusche, or transfer onto it.
  4. Etch. Metal needs a different etch from stone: gum arabic with a little phosphoric acid (Phosphoric Acid and Phosphates) or with tannin or gallic acid from oak galls steeped in water (Ink). Brush it on for 1–2 minutes, buff dry, and proceed as for stone.
  5. Print on the scraper press (on a flat iron or stone backing) or on an offset press.

Photolithography (in outline). Coat a grained plate with egg albumen containing a little ammonium dichromate (obtained by trade or from a chromate works, Chromium and Its Compounds). Dry it in the dark, expose it in sunlight for a few minutes under a photographic negative (Photography), roll it thinly with ink, then wash it in water. Where light passed, the albumen hardened and holds the ink; elsewhere it washes away. Maps, drawings and halftone pictures go onto plates this way without hand drawing.

Colour lithography

Chromolithography prints one colour from each stone or plate, one after another on the same sheet.

  1. Draw a key drawing in outline on one stone. Print it in a non-drying powder (or thin ink) onto sheets, and offset each sheet onto a fresh stone, so every stone carries the same faint guide.
  2. On each stone draw only what that colour prints. Light colours first, dark last. Simple pictures use 4–6 colours, posters 15 or more.
  3. Register — getting every colour exactly in place — with two needle holes pierced through the paper at marks printed on the key. Drop needles through the holes onto the marks on each stone before lowering the sheet. Print dry, in one session, because damp paper stretches.
  4. Let each colour dry a day before the next.

The offset press

The offset press prints from a metal lithographic plate, but never lets the plate touch the paper. The plate inks a rubber blanket, and the blanket prints the paper. The soft blanket presses ink into rough paper, card, cloth and even tin far better than a hard plate could, and the plate barely wears: a good plate gives 50,000–100,000 prints.

Proofing press (buildable first). A long flat bed holds the plate at one end and the paper at the other, level with each other. A single heavy cylinder about 20–25 cm across, covered in a rubber blanket (rubberised cloth, Rubber, 2–3 mm thick), runs on toothed racks along both sides of the bed so it rolls without slipping. Damp and ink the plate by hand, roll the cylinder over the plate (it picks up the image) and on over the paper (it prints it). A few hundred clean sheets a day is easy.

Rotary offset press. Three cylinders of equal diameter, geared together:

  • the plate cylinder, with the plate clamped round it; above it, damping rollers covered in cotton flannel, fed from a water trough, and a train of three or four ink rollers fed from an ink duct;
  • the blanket cylinder, which takes the image off the plate;
  • the impression cylinder, whose grippers carry the sheet between it and the blanket.
Plate cylindermetal plate wrapped round Image on platereads the right way round Blanket cylinderrubber blanket,image reversed Impression cylindergrippers carry the sheet Damping rollerswater first Water trough Ink duct and rollersink second Paper in Printed sheets
Fig. 3 The offset press. The plate is damped, then inked, and passes its image to the rubber blanket, which prints it onto paper held by the impression cylinder.

Driven by an The Electric Motor or line shaft (Belts, Chains and Power Transmission), it prints 3,000–10,000 sheets an hour. The art is the balance of water and ink: too much water gives pale prints, too little lets ink scum the whites.

How to tell it worked

  • Clean whites. The bare paper between lines and tones shows no grey film or speckle.
  • Full tones. The darkest crayon areas print solid; the palest still show as grey, not lost.
  • Sharp lines. Under a magnifier, fine pen lines have clean edges, not spreading halos.

Note Troubleshooting. Whites grey or speckled (scumming) → stone too dry, ink too soft, or etch too weak. Damp more often; stiffen the ink with a little more pigment; re-etch. Pale tones disappearing → etch too strong, or too much water. Use a weaker etch on light work. Image fills in and goes blotchy → too much ink, or the roller too greasy. Roll on a slab to thin it. Old drawing showing through → stone not ground deep enough. Regrain. Stone cracked in the press → too thin, uneven backing, or pressure too high. Bed it on a sheet of damp blotting paper; use thicker stones. Colours out of register → paper stretched; print dry and in one session.

Dangers

Danger Nitric acid burns skin and eyes and gives off choking brown fumes. Measure it with a glass dropper, add acid to gum (never the reverse), wear eye protection, and keep plenty of water at hand. See Nitric Acid.

Warning Burning crayon mix. Making crayon involves deliberately setting hot wax and fat alight. Do it outdoors, away from buildings, with a close-fitting lid ready. Never pour water on burning fat — it explodes into a fireball. Smother it.

  • Dichromates used in photolithography are poisonous, cause skin ulcers and cancer, and must never be breathed as dust or handled with bare hands (Chromium and Its Compounds).
  • Heavy stones crush fingers and backs. Lift with two people or a tackle, and keep feet clear.
  • Turpentine is flammable and its vapour causes headaches; work with open windows. Oily rags can catch fire by themselves; spread them flat outdoors.
  • Presses trap fingers. Keep hands clear while cranking.

What this unlocks

Lithography prints Maps and Mapmaking, technical drawings, sheet music, labels for Sacks, Boxes, Crates and Packaging and posters for Teaching and Schools and public health. Photographic plates plus the offset press give halftone pictures in books and newspapers. The idea of drawing a pattern in a resist and etching what is bare leads straight to photolithography on silicon. Offset presses also print on sheet tin for cans (Tins, Cans, Drums and Tanks).

How it was first done

Alois Senefelder, a struggling playwright in Munich, began experimenting in 1796 with ways to print his own plays cheaply. Having jotted a laundry list on a slab of Solnhofen limestone in a greasy ink of wax, soap and lampblack, he found that the stone could be etched and inked so that only the writing printed. By 1798 he had the full chemical process, and he took out a Bavarian privilege in 1799. His Complete Course of Lithography (1818) remains a good manual. Godefroy Engelmann in France patented "chromolithography" in 1837. Zinc plates came into use from the 1830s, and aluminium plates in the 1890s. Alphonse Poitevin found the light-hardened dichromate coating in 1855, the basis of photolithography. Robert Barclay in England printed onto tin sheets from a rubber-covered cylinder in 1875, and in 1903–1904 the American printer Ira Washington Rubel noticed that a sheet accidentally printed from the rubber blanket of his press was sharper than one printed from the stone — the start of offset printing on paper, which by the late 1900s had replaced letterpress for most printing.

Source: content/entries/knowledge/lithography.md