Part 13 · Electricity
The Telegraph
Send words along a wire faster than any horse — a key at one end, a clicking electromagnet at the other, and a code of short and long signals. How to build the key, sounder and relay, string a line on poles with the earth as the return wire, and learn Morse code.
- Difficulty
- ●●●●●
- Time
- A weekend for a bench pair of instruments; weeks to months for a line between villages
- Steps from zero
- 18 prerequisites →
The full path from nothing — 18 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- Charcoal
- Pottery
- Hides and Leather
- Fermentation
- Bellows
- Copper Smelting
- Iron (the Bloomery)
- Blacksmithing
- The Battery
- Copper Wire
- The Electromagnet
- The Telegraph
Do them roughly in this order. See it on the tech tree →
Why it matters
Before the telegraph, no message could travel faster than a rider, a ship or a signal fire on a hilltop. With it, a sentence typed in one town clicks out in the next town a fraction of a second later — and in the town after that, and the town after that. Weather warnings, prices, news of sickness, calls for a doctor, orders for parts, the time of day for setting clocks (The Mechanical Clock), and train movements on a single track (Railways) can all travel at once.
The telegraph is also the simplest useful electrical system. It needs only a The Battery, a switch, a long wire and an The Electromagnet. It works on currents of a few hundredths of an amp, so a few jars of zinc and copper can run a line tens of kilometres long. Everything learned building it — insulating lines, finding faults, relaying weak signals — leads straight on to the The Telephone, Radio and computer networks. A telegraph line can even carry a telephone later.
How it works
The idea is as simple as a doorbell with a very long wire:
- At the sending end, a key — a spring-loaded switch under the operator's finger — closes the circuit.
- Current from a battery flows along the line wire to the far station.
- There it passes through the coil of an electromagnet, which pulls down an iron armature with a sharp click. When the key is let up, the current stops and a spring lifts the armature back with a second, softer click.
- Short presses and long presses make a code. The listener hears the gap between the "down" click and the "up" click: short is a dot, long is a dash.
The earth is the return wire
A circuit needs a path back. You could string two wires, but in 1838 Carl August von Steinheil in Munich found that the ground itself can carry the return current. Connect the far end of the line to a metal plate buried in damp earth, and the battery's other terminal to another buried plate at the home station. The current flows out along the wire and back through the earth. The earth is so enormous that, although soil is a poor conductor, its resistance between two good earth plates is only a few ohms. This halves the cost of wire, and almost every telegraph line ever built used it.
Why a relay is needed
A long line has resistance and leaks a little current at every pole in wet weather. By the time the current reaches the far end it may be too weak to slam down a loud sounder. So the line works a relay (The Electromagnet): a sensitive electromagnet with many turns of thin wire and a light lever, which closes a second, local circuit at the receiving station. That local circuit has its own two or three cells and a heavy, loud sounder. The weak line current only has to flip a feather-light lever; the local battery does the hard work.
If a line is so long that even a relay will not work reliably, cut it into sections. At the junction, the relay of the first section works a key for the second section, with its own battery. This is a repeater, and with repeaters a message can cross a continent.
Closed circuit or open circuit
There are two ways to wire the stations. Choose one and use it on the whole line.
- Closed circuit (the American system, simplest for many stations on one wire). One main battery, all stations' relays and keys in a chain along the line. Each key has a small lever switch (the circuit closer) beside it, which is kept closed when the operator is not sending, so the current flows all the time and every relay is held down. To send, the operator opens his circuit closer; now his key alone makes and breaks the whole line, and every relay along the line follows it. Everyone hears every message, so begin each message with the call letters of the station you want.
- Open circuit (the European system). No current flows while the line is idle. Each station has its own battery, and its key has two contacts: at rest, the key connects the line to the station's own relay to listen; pressed, it connects the line to the station's battery instead. It uses less zinc, but needs a battery at every station.
The closed-circuit system is described below, as it is the easiest to build and extend.
What you need
| Item | For a 20 km line with two stations | Notes |
|---|---|---|
| Line wire | 21 km of iron wire 3–4 mm thick, or copper 1.5–2 mm | Copper Wire; iron is stronger and cheaper |
| Poles | About 500 (every 40 m) | Straight trunks 6–7 m long, 12–20 cm thick at the top |
| Insulators | One per pole, plus spares | Glazed stoneware, porcelain or glass (Stoneware and Porcelain, Glass) |
| Main battery | 15–25 Daniell or gravity cells | The Battery; about 1.1 V each |
| Local batteries | 2–3 cells per station | For the sounders |
| Relay | One per station, 100–200 Ω, many turns of 0.2–0.3 mm wire | The Electromagnet |
| Sounder | One per station, 3–5 Ω | Heavier electromagnet, thicker wire |
| Key | One per station | Brass or bronze lever, springy strip, hardwood base |
| Earth plates | Two, each copper or zinc 60 × 60 cm, or 2 m of iron pipe | Buried in permanently damp soil |
| Hardwood, brass screws, wire for connections | Basic Woodworking, Zinc and Brass |
Where to find it
- Poles: any straight, durable tree. Cedar, larch, chestnut, oak and pine have all been used. Peel the bark; season for a few months if you can. The part that goes into the ground rots first: char the bottom 1.5 m in a fire until it is black all over, then soak it in hot pine tar (Tar, Pitch and Glue). Charring and tarring double or treble the pole's life.
- Insulators: shape them from good stoneware clay (Finding and Preparing Clay) and fire them hard with a glaze (Glazes) so they do not soak up water. Unglazed earthenware is useless: wet, it conducts.
- Gutta-percha (for cables): the latex of the gutta-percha tree of South-East Asia, or balata from South America (see the materials list). Outside the tropics you will not find it; use the alternatives under Cables below.
- Everything electrical comes from Copper Wire, The Battery and The Electromagnet.
Method 1: The instruments
Build and test a pair of instruments on a bench, joined by a few metres of wire, before stringing any line. Learn the code on them at the same time.
The key
- Lever: a bar of brass or hard bronze about 15 cm long, 1.5 cm wide and 0.6 cm thick, or a strip of hardwood with a brass contact. Pivot it on a pin through two brass posts, about one third of the way from the back.
- Knob: a wooden knob 2.5 cm across on the front end, at a comfortable height for the fingertips.
- Contacts: under the lever, just behind the knob, a contact point; below it on the base, a fixed contact. Use silver if you have it (Gold and Silver) — it does not burn and pit as copper does. Otherwise use thick copper and file it clean now and then.
- Spring: a coil or strip spring at the back end, holding the front up.
- Adjusting screws: a screw at the back to set the gap between the contacts — about 1 mm — and a screw to set the spring tension. Light enough to press easily, firm enough to snap back.
- Circuit closer: a small brass lever on the base that can be swung across to touch the fixed contact and short the key.
- Mount everything on a hardwood base 15 × 10 cm, screwed to the table so it does not slide.
The sounder
- Electromagnet: a horseshoe of soft iron, legs 5–6 cm long and 1 cm thick, with a coil on each leg of about 300 turns of 0.5–0.6 mm covered wire (together about 3–5 Ω). Stand it upright on a hardwood base with the poles facing up.
- Armature lever: a brass bar about 12 cm long pivoted at the back end, carrying a soft iron bar across it just above the two poles, with a gap of about 1–2 mm when it is up.
- Two stops: a screw above the front end of the lever (the up stop) and one below it (the down stop). The lever hits the down stop when the magnet pulls and the up stop when the spring lifts it. These two impacts are the sound. Set them so the lever moves only 1–2 mm.
- Spring: from the lever back to an adjustable post, just strong enough to lift the armature as soon as the current stops.
- Sound box: mounting the sounder on a thin wooden box, open at one side, makes it louder.
The down click is crisp and loud; the up click is softer. A dot is "click-clack" almost at once; a dash is "click … clack". You read the spaces between them, not the clicks.
The relay
Build the relay exactly as in The Electromagnet, but sensitive: 2,000–5,000 turns of 0.2–0.3 mm silk-covered wire, giving 100–200 Ω, an armature gap of 0.5 mm, and a very light spring. Its contacts close the local sounder circuit. A good relay of this kind pulls in reliably on 20–30 milliamps (thousandths of an amp). Give it a screw to adjust the spring from the operating table: as the weather changes and the line leaks more or less, the operator adjusts it until the signals are clean.
Test on the bench
Wire up: key → relay coil → back to the key through two cells. Relay contacts → sounder → two more cells. Press the key: the relay clicks faintly, the sounder loudly. Tap out dots as fast as you can: the sounder should follow every one with no sticking.
Method 2: Learn the code
Samuel Morse and Alfred Vail's code was later simplified into International Morse, used across the world from the 1860s. Use it; it is the code every manual and every later radio operator expects.
| Letter | Code | Letter | Code | Figure | Code |
|---|---|---|---|---|---|
| A | · — | N | — · | 1 | · — — — — |
| B | — · · · | O | — — — | 2 | · · — — — |
| C | — · — · | P | · — — · | 3 | · · · — — |
| D | — · · | Q | — — · — | 4 | · · · · — |
| E | · | R | · — · | 5 | · · · · · |
| F | · · — · | S | · · · | 6 | — · · · · |
| G | — — · | T | — | 7 | — — · · · |
| H | · · · · | U | · · — | 8 | — — — · · |
| I | · · | V | · · · — | 9 | — — — — · |
| J | · — — — | W | · — — | 0 | — — — — — |
| K | — · — | X | — · · — | . (full stop) | · — · — · — |
| L | · — · · | Y | — · — — | , (comma) | — — · · — — |
| M | — — | Z | — — · · | ? (question) | · · — — · · |
Useful signals:
| Signal | Code | Meaning |
|---|---|---|
| Error | · · · · · · · · (eight dots) | "I made a mistake; I will repeat the last word" |
| Wait (AS) | · — · · · | "Wait" |
| Over (K) | — · — | "Go ahead, your turn to send" |
| End of message (AR) | · — · — · | "Message ends" |
| Distress (SOS) | · · · — — — · · · | Sent as one run with no gaps: "Emergency, help needed" |
Timing is everything. Take the length of a dot as one unit:
- dot = 1 unit, dash = 3 units;
- gap between dots and dashes inside a letter = 1 unit;
- gap between letters = 3 units; gap between words = 7 units.
Learning it. Learn by sound, not by looking at the table. Have a partner send letters at full speed with long gaps between them, and write each one down; do not count dots. Start with E, T, A, N, I, M, S, O, then add a few letters at a time. Twenty minutes twice a day beats two hours once. Most people can read and send 5 words a minute after two or three weeks, and a working operator manages 20–30. A register — a lever with a blunt point that embosses dots and dashes on a moving paper strip driven by clockwork — helps beginners and keeps a record, but every operator soon reads faster by ear.
Method 3: Build the line
Earths
- At each station, dig down to permanently damp soil — below the summer water table if possible, typically 1.5–2 m. Bury a copper or zinc plate 60 × 60 cm upright, or drive in 2 m of iron pipe, or sink the plate in a well.
- Solder or rivet a thick copper wire to it (3 mm or more) and bring it up to the station.
- Pack round the plate with charcoal mixed with a few handfuls of salt and wet it well. This keeps the soil around it moist and conductive.
A poor earth is the commonest cause of weak signals. The earth should be at least as good a conductor as a kilometre of line wire.
Poles
- Set poles about 40 m apart (about 25 to the kilometre) on straight runs, closer on curves and in country with heavy snow, ice or wind.
- Dig holes 1.2–1.5 m deep — about a fifth of the pole's length — and stamp the soil back hard in layers, with stones packed round the base in soft ground.
- Use poles 6–7 m long, so that the wire runs at least 5 m above the ground, higher at roads, out of reach of carts and riders.
- At corners, brace the pole with a stay: a strong wire or rope to a buried log on the outside of the bend.
Insulators
Every pole is a leak. On a wet day, the film of water on an insulator conducts a little; multiplied by hundreds of poles, the leaks can steal most of the current. The insulator's job is to make the wet path from wire to wood as long and as narrow as possible.
- Shape: a bell 7–10 cm across and 8–10 cm tall, with a groove round the top or the neck for the wire, and a hollow underside — the petticoat — that the rain cannot reach. Two petticoats, one inside the other, are better still.
- Mount it on a hardwood pin screwed or wedged into the top of the pole or into a cross-arm. Wrap the top of the pin with tarred cloth before pushing the insulator on, so it grips.
- Fire hard and glaze all over the outside. Test each one: soak it in water for a day, then dry the outside only; it should not feel cool and damp on the surface after a minute (porous) and should ring, not thud, when tapped (cracked).
- Glass insulators are excellent if you can press them in a mould (Glass); stay away from cracked or bubbled ones.
Stringing the wire
- Joints: overlap the two wire ends by 10 cm, twist each end tightly round the other wire 5–6 times, and solder the joint (Soldering and Brazing). An unsoldered joint rusts and fails within months.
- Run it out from a drum on a cart, lifting it into place on each pole.
- Tension: pull it tight with a block and tackle (Simple Machines) but not hard. Leave a sag of about 40 cm in the middle of each 40 m span in mild weather. Iron wire shrinks in frost and snaps if it was strung tight in summer.
- Tie it to each insulator with a short piece of soft wire wound round the line wire on both sides of the groove.
- Protect iron wire from rust. Zinc-coated (galvanised) wire, dipped in molten zinc (Zinc and Brass), lasts decades. Otherwise paint it with hot boiled linseed oil or tar before stringing, and expect to replace it.
Battery size
The current must push through the whole circuit. Add up the resistances:
| Part | Resistance |
|---|---|
| Iron wire 4 mm, per km | about 10 Ω |
| Iron wire 3 mm, per km | about 17 Ω |
| Copper wire 2 mm, per km | about 5.5 Ω |
| Each relay | 100–200 Ω |
| Two good earths together | 5–20 Ω |
Example: 20 km of 4 mm iron (200 Ω) + two relays (300 Ω) + earths (10 Ω) = about 510 Ω. To push 30 milliamps through 510 Ω takes about 15 volts (volts = amps × ohms; see Measuring Electricity): about 14 Daniell cells in series. Add a third more for wet weather: 18–20 cells. Put the main battery at one end, or half at each end.
Lightning protection
Lightning striking the line, or even nearby, can send thousands of volts into the office. At each station, where the line enters, fit a lightning arrester: two brass plates with saw-toothed edges facing each other 0.5–1 mm apart, one connected to the line and one to the earth plate. Normal signals cannot jump the gap; lightning prefers it to the instruments. Also fit a switch that connects the line straight to earth, and use it whenever a storm comes near. See Static Electricity and the Leyden Jar.
Cables under water and underground
Bare wire on poles cannot cross a river or run under a street. For that it must be covered in something that keeps water out for years.
- Gutta-percha. Soften the gum in water at 60–70 °C, knead it, and press it round a copper wire (better, a strand of seven thin wires, which does not break) in two or three layers, each about 1–2 mm thick, so that a hole in one is covered by the next. Over this wind tarred hemp or jute, and for the sea or a riverbed, an armour of iron wires laid spirally round it. Gutta-percha lasts for decades under water, but in air and sunlight it oxidises and crumbles — keep it wet or buried.
- Without gutta-percha: vulcanised rubber (Rubber) — use tinned copper wire, since the sulfur in rubber blackens bare copper; or cotton-covered wire soaked in hot pitch, beeswax and resin, drawn into a lead pipe (Lead); or wire wrapped in tarred cloth and laid in a fired clay pipe (Tiles and Clay Pipes) filled with hot pitch.
- Short crossings are easier overhead: a tall pole on each bank, and a span of steel or iron wire up to a few hundred metres, sagging high enough to clear boats.
A long cable behaves differently from an overhead line: it soaks up charge like a Leyden jar, so sharp signals come out blurred and slow. Send more slowly over cables, and never raise the battery voltage to "push harder" — high voltage punctures the insulation. The first Atlantic cable of 1858, already weak, was finished off this way after a few weeks.
How to tell it worked
- Bench test: the sounder follows the key crisply at the fastest rate you can tap.
- Line test: with all circuit closers shut, every relay on the line is held down. Open any closer and every relay drops. Key "V" (· · · —) slowly; each station should hear it cleanly.
- Galvanometer test: put a galvanometer (The Electromagnet) in the line at each station. Note the swing on a dry day. On a wet day it is lower at the far end than at the battery end — that difference is the leakage.
Note Troubleshooting. Nothing at the far end, and no current at the home end either → a break: a snapped wire, a failed joint, a dead cell or a loose terminal. Walk the line; a broken wire is usually lying on the ground. Strong current at the home end but weak or none at the far end → an earth fault: the wire is touching a tree, a wet pole, a broken insulator, or the ground. Look for branches and storm damage. Signals fine in dry weather, fading in rain → leaky insulators. Clean or replace them; make sure every one is glazed and has a dry petticoat. Relay sticks down, dots run together → spring too weak or armature too close; adjust. Or the relay's iron is not soft enough (The Electromagnet). Faint ticks and noises on the line → another line or a power wire nearby (keep at least 2–3 m away), or a bad earth. Signals blurred and slow on a cable → send more slowly; that is the cable's nature.
Dangers
Danger Power lines kill linemen. Never string a telegraph wire near or under a power line, and never let the two cross. If a power wire falls on a telegraph line, every metre of it, every instrument and every key becomes live at lethal voltage. In 1889 a lineman named John Feeks was killed in the middle of New York's tangle of telegraph wires, many of which had come into contact with arc-lighting circuits. See Wiring and Electrical Safety.
Danger Lightning. A long wire on poles collects lightning. Operators have been killed at their keys. Fit lightning arresters and an earth switch at every office, earth the line in storms, and never climb poles or handle line wire while thunder is about.
- Falls. Climbing poles with spikes or a ladder is dangerous; use a rope belt round the pole, and never climb a pole whose base has rotted. Push on it hard before climbing.
- Battery voltage. A main battery of 50–100 cells gives a painful and possibly dangerous shock, especially with wet hands. Disconnect it before working on terminals.
- Battery chemicals. See The Battery.
- Falling wire. A dropped wire across a road can catch a rider at the neck. Lift sagging wires at once.
What this unlocks
- Time signals: a single click sent at noon sets every clock along the line (The Mechanical Clock).
- Safe railways: one line per section of track, and no train enters a section until the far station telegraphs that it is clear (Railways, Railway Signalling and Safety).
- The The Telephone, which can run on the same poles and insulators.
- Wireless: the code of this chapter is the code of early Radio.
- Data: a printing telegraph, and later the The Teleprinter, sends letters directly; this leads to relay logic and Networks and the Internet.
How it was first done
People had tried electrical signalling since the 1700s with static electricity and dozens of wires, one per letter. After the The Electromagnet, practical systems came quickly. Pavel Schilling demonstrated a needle telegraph in St Petersburg in 1832, and Carl Friedrich Gauss and Wilhelm Weber strung a wire over the rooftops of Göttingen in 1833. Joseph Henry rang a bell through a mile of wire in 1831 and developed the relay. In 1837 William Cooke and Charles Wheatstone patented a needle telegraph in Britain, and by 1839 it was working on the Great Western Railway out of London. Steinheil discovered the earth return in 1838.
In the United States, the painter Samuel Morse, working with Alfred Vail and helped by Leonard Gale, developed the key, the register and the code of dots and dashes. On 24 May 1844, Morse sent "What hath God wrought" from Washington to Baltimore, about 60 km. Within a few years operators found they could read the code by the sound of the register, and the sounder replaced it. A simplified code, worked out in Germany by Friedrich Gerke in 1848, became International Morse.
Gutta-percha reached Europe in 1843; Werner Siemens built a machine to press it seamlessly round wire in 1847. A cable crossed the English Channel in 1851 after a failed attempt in 1850. The first Atlantic cable (1858) worked for only a few weeks, its failure hastened by the high voltages used to force signals through it; the steamship Great Eastern laid a lasting one in 1866. The first line across North America opened in 1861, and by the 1870s cables and overhead lines linked every continent.
Source: content/entries/electricity/telegraph.md