Part 8 · Chemistry
Iodine
Burn kelp to ash, wash out its salts, and add acid and an oxidiser to the dark liquor that is left — violet vapour rises and settles as black shining crystals of iodine. Dissolved in alcohol it is one of the best skin antiseptics; a trace added to salt prevents goitre and the brain damage it brings to unborn children.
- Difficulty
- ●●●●●
- Time
- Two weeks to gather and dry the seaweed; two or three days to burn, leach, concentrate and liberate the iodine
- Steps from zero
- 10 prerequisites →
This unlocks
—The full path from nothing — 10 steps before this one
- Fire
- Finding and Preparing Clay
- Sulfur
- Pottery
- The Kiln
- Lime
- Lye and Potash
- Glass
- Saltpeter
- Sulfuric Acid
- Iodine
Do them roughly in this order. See it on the tech tree →
Why it matters
Iodine is a dark, shining, violet-black solid that turns straight into a purple vapour when warmed. It is needed in tiny amounts, but it does three jobs nothing else in this book does as well.
- It prevents goitre and cretinism. The thyroid gland in the neck needs about 150 micrograms of iodine a day (a pregnant or nursing woman about 250) — a speck too small to see. Far from the sea, soils and food lack it. The neck swells (goitre), adults become slow and cold, and babies born to iodine-starved mothers can be deaf, stunted and mentally disabled for life (see Nutrition and Deficiency Diseases). This is the most common preventable cause of mental disability in the world. About 50 grams of potassium iodide mixed evenly into a tonne of salt prevents it entirely.
- It kills germs. Iodine dissolved in alcohol — tincture of iodine — kills bacteria, fungi and many viruses on skin within a minute or two (bacterial spores take much longer). It cleans the skin before surgery, around wounds and before injections (Wound Care and Antiseptics, Basic Surgery, Sterilising Instruments and Dressings), and a few drops make clear drinking water safe (Finding and Purifying Water).
- It is a test. Iodine turns starch a deep blue-black, even in a dilution of a few parts per million. You can see whether a brewer's mash has turned to sugar (Beer, Wine and Cider), find flour hidden in milk, follow the starch in a potato, and stain bacteria for the microscope (Culturing Microbes). Silver iodide is one of the light-sensitive salts of Photography (Silver Nitrate and Silver Salts).
The raw material is free: the brown kelp that storms throw up on rocky coasts.
How it works
Seawater holds only about 0.06 grams of iodine per tonne. Brown kelps pull it out of the sea and concentrate it thousands of times: dried oarweed and tangle (the big strap-leaved kelps, Laminaria) hold roughly 0.2–0.5% of their dry weight as iodine. In the plant and its ash it is present as iodide — iodine combined with sodium or potassium, a salt that dissolves in water and has no colour.
So the work has three stages:
- Burn the dried weed to ash (gently, because iodide is partly lost as vapour in a fierce fire) and leach the ash with hot water. The water carries away all the soluble salts: much common salt, potassium chloride and sulfate, soda, and the iodide.
- Concentrate. Boil the liquor down. The common salts crystallise out first and are raked away. Iodides are far more soluble than the others, so they stay behind in the last dark syrup — the mother liquor ("the liquid the crystals were born from").
- Liberate. An oxidiser — a substance that pulls electrons away from others; here manganese ore with Sulfuric Acid, or bleach — turns colourless iodide into free iodine. Iodine hardly dissolves in water, so it either falls out as a black sludge or, if you heat the mixture, rises as violet vapour and settles on a cool surface as crystals. Going straight from solid to vapour and back is called sublimation, and it is also how you purify iodine.
What you need
| Item | Amount | Notes |
|---|---|---|
| Brown kelp, fresh | 100 kg wet | Dries to about 15–20 kg. Expect a few tens of grams of iodine at the end — enough for several litres of tincture or a tonne of iodised salt. |
| Large clay pots or iron pans | 2–3 | For leaching and boiling down. Iron is fine until the acid step. |
| Glass or glazed vessels | A flask or retort, a wide jar as receiver | Iodine eats iron, copper and cork. See Laboratory Glassware. |
| Sulfuric acid | 100–300 ml concentrated | Diluted for acidifying and liberating. See Sulfuric Acid. |
| Manganese ore (black oxide) | 50–100 g, powdered | Or bleach solution (Chlorine and Bleach) |
| Red-cabbage indicator, starch, cloth filters | See Acids, Bases and Testing | |
| For tincture: strong alcohol | 90% or better | From Distillation |
| For potassium iodide: iron filings and potash | See Iron (the Bloomery), Lye and Potash |
Where to find it
- Kelp grows on rocky coasts of cool and temperate seas, attached to stones below low tide. After autumn and winter gales it lies in thick banks on the beach. Look for long, flat, leathery brown straps (1–3 m) on a stiff, woody stalk as thick as a thumb, with a branched root-like holdfast. The stalks ("tangles") are especially rich. Gather it fresh, still smelling of the sea: weed rotting high on the beach, or soaked by rain for days, has lost much of its iodine.
- Wracks — the smaller brown weeds of the upper shore with air bladders that pop — hold only about a fifth as much. Use them only if there is no kelp.
- Inland there is no practical source. Trade for dried kelp, kelp ash, or the finished iodine; one coastal village can supply a whole region's salt.
- Manganese ore — soft, sooty black lumps and crusts that blacken the fingers; see Glazes.
Step by step: iodine from kelp
1. Dry and burn
- Spread the kelp on racks or clean stones above the tide, in sun and wind, and cover it against rain. Turn it daily. In 1–2 weeks it is dark, shrunken and brittle enough to snap.
- Burn it slowly. Use a shallow pit or a stone-lined trench about 1 m long and 30 cm deep. Light a little brushwood, then feed the dry weed on a little at a time so it smoulders with thick white smoke rather than roaring. Rake it over. The old kelp-burners let the ash fuse into a hard glassy slab; that drives off much of the iodine. A black, crumbly char keeps more. Better still, char the weed in a closed pot with a small vent, like making Charcoal.
- Expect about one-fifth to one-quarter of the dry weight as ash or char: 3–5 kg from 100 kg of wet weed.
2. Leach
- Crush the ash or char to coarse powder. Soak it in hot water, 2–3 litres per kilogram, stir well, and let it stand a few hours. Pour off the clear liquid. Repeat with fresh hot water twice more and combine the liquids. Strain through cloth and a layer of sand, as for lye (Lye and Potash).
- Check for iodide: put a drop of the liquor on a white plate with a drop of starch water (below), a drop of vinegar or dilute acid and a tiny drop of bleach. Blue-black means iodide is there.
3. Concentrate
- Boil the liquor down in an iron pan. As it thickens, white crystals form and sink (common salt, potassium chloride and sulfate). Rake them out with a perforated ladle and drain them back over the pan. Keep them: they are a good potash fertiliser (Chemical Fertilisers).
- Stop when only about one-twentieth of the starting volume is left and the liquor is dark brown and oily. Let it cool overnight; more crystals come out. Pour off the mother liquor and keep it in a glass or glazed jar. This is where the iodine is.
4. Acidify — outdoors
- Outdoors, upwind, stir in dilute sulfuric acid (1 part acid poured into 4 parts water, never the other way — see Sulfuric Acid) a little at a time. It fizzes and gives off stinking gases — rotten-egg hydrogen sulfide and choking sulfur dioxide from sulfur compounds in the ash. Keep adding until it stops fizzing and a drop turns red-cabbage juice red.
- Let it stand overnight. A pale yellow mud of sulfur settles; pour the liquor off it.
5. Liberate the iodine
Method A — heat with manganese ore (gives crystals directly). Put the acidified liquor in a glass flask or glazed retort no more than half full, with 10–20 g of finely powdered manganese ore per litre and a little more dilute acid. Fit a wide glass tube or the retort neck into a cool receiver — a wide glass jar or glazed pot wrapped in a wet cloth, loosely covered. Heat gently in a pan of sand. Violet vapour rises and settles in the receiver as black, shining, metallic-looking scales. Keep the heat low; when no more violet colour appears, stop.
Method B — bleach in the cold (simpler, no heating). To the acidified liquor in a glass jar, add bleach (Chlorine and Bleach) a spoonful at a time, stirring. The liquor turns brown, then black specks and sludge appear. After each addition, test a drop of the clear liquid with starch and one more drop of bleach: when it no longer darkens, stop. Too much bleach turns the iodine back into a colourless compound and you lose it. Let it settle, pour off the liquid, and collect the black sludge on a cloth. Dry it on a glass or glazed dish at room temperature.
6. Purify by sublimation
- Put the crude iodine in a shallow glazed or glass dish on a pan of warm sand. Cover it with an inverted glass funnel or a flask filled with cold water. At a gentle heat (a pan you can just bear to touch for a moment) the iodine rises and grows as clean violet-black crystals on the cool glass. Scrape them into a glass bottle.
- Store in glass with a glass stopper, or a cork sealed with wax. Iodine slowly eats through cork, metal lids and paper labels.
Making the useful forms
Starch test water
Stir 1 g of starch (a level teaspoon of flour or the white sediment from washing grated potato) into a little cold water, pour it into 100 ml of boiling water, and boil 1 minute. Use it cold, within a day or two. Strips of paper dipped in it and dried make starch papers.
Free iodine turns it blue-black at once. Iodide (in salt or liquor) does not — until you add a drop of acid and a tiny drop of bleach.
Potassium iodide
Iodine dissolves poorly in water but very well in a solution of potassium iodide, which you need for iodised salt and good tinctures.
- In a glass jar, cover 1 part of clean iron filings with 4 parts water and add 3 parts of iodine a little at a time, stirring. It warms and turns to a green solution of iron iodide. Leave the excess iron in.
- Strain. Stir in a strong solution of potash (Lye and Potash) until no more brownish-green precipitate forms (about half the iodine's weight of dry potash). The iron settles out as rust-coloured mud.
- Filter, boil down to a small volume, and let it cool. White cubic crystals of potassium iodide form. Dry them and keep them in a closed jar.
Tincture of iodine (2%)
Dissolve 2.5 g of potassium iodide in 5 ml of water, add 2 g of iodine and stir until dissolved, then add 50 ml of strong alcohol and water to make 100 ml. It is a dark red-brown liquid. Without iodide, 2 g of iodine dissolves in 100 ml of 70–90% alcohol alone; it works the same but stings more.
Using it on skin: paint it on clean, unbroken skin — around a wound, over an operation or injection site, on the hands — and let it dry for 2 minutes before cutting or covering. It kills as it dries. Small cuts and scratches can be painted directly. Do not pour it into large raw wounds or burns (it damages living tissue and is very painful); clean those with boiled water and soap (Wound Care and Antiseptics). Do not bandage tightly over wet tincture, which can blister.
Disinfecting water: to clear water add 5 drops of 2% tincture per litre (10 drops if cloudy or very cold), stir and wait 30 minutes. Boiling is better if you have the fuel; iodine is for travel and emergencies, not for months of daily drinking.
Iodised salt
- Dissolve 1 g of potassium iodide in 100 ml of boiled water.
- Spread dry salt (Salt) on a clean cloth or in a wide bowl. For every kilogram of salt, sprinkle 5 ml (a teaspoon) of the solution evenly over it while turning and mixing with a wooden paddle, as you would knead dough. This gives about 35–40 mg of iodine per kilogram when made: the top of the 20–40 mg/kg range long recommended by the World Health Organization for salt as it leaves the works, which leaves room for losses in storage. (The WHO's 2014 guideline aims for about 20 mg/kg actually reaching people who eat 10 g of salt a day.)
- Dry it in the shade and store in closed, dry pots away from sunlight. Damp salt in the sun loses half its iodine in months. Make it fresh every few months if you can.
At 10 g of salt a day, a person gets about twice their daily need, with room for losses. Do not add more. Too much iodine also upsets the thyroid.
How to tell it worked
- Iodine: black-violet, shining flakes that stain fingers brown; warmed in a test tube, it fills the tube with unmistakable violet vapour; a crystal dropped in starch water turns it blue-black at once.
- Potassium iodide: white crystals that dissolve easily in water; the solution turns iodine crystals into a brown solution quickly.
- Tincture: dark brown; a drop on a cut potato turns black-blue; it dissolves completely with no grains at the bottom.
- Iodised salt: dissolve a spoonful in a little water, add a drop of vinegar, a drop of starch water and a tiny drop of bleach — a faint blue shows the iodide is there. Untreated salt stays colourless. Test a batch from the bottom of the pot as well as the top.
Note Troubleshooting. No blue with the starch test on the liquor → weed rotten or rain-washed, burned too fiercely, or wracks instead of kelp. Use fresh kelp and burn it to a black char. Blue colour appears, then fades → too much bleach. Add more liquor or start again with smaller additions. Brown liquid but no black sludge → too dilute; boil the liquor down further before acidifying. Little iodine from Method A → too little acid or manganese, or heat too high so vapour escaped; seal the receiver better and heat more gently. Crystals damp and sticky → acid carried over. Sublime again. Starch test gives brown, not blue → the starch water is old or was not boiled; make it fresh.
Dangers
Danger Iodine is a poison and a corrosive. Swallowing 2–4 g of iodine can kill; tincture must never be drunk. Signs are burning in the mouth, vomiting, bloody diarrhoea and shock. Give starch — a few spoons of flour or mashed potato in water — which binds iodine, and get whatever help exists (Emergencies). Solid iodine on the skin causes brown stains and then blistered burns; wash at once with plenty of water.
Danger The acid step gives off hydrogen sulfide, a gas that smells of rotten eggs at first and then kills the sense of smell before it kills you. Acidify only outdoors, upwind, a little at a time, and never lean over the pot.
- Iodine vapour stings the eyes and nose and damages the lungs. Heat it only in the open air or a strong draught, gently, in glass.
- Never mix iodine with ammonia or ammonia water. It forms a dark solid that explodes at a touch when dry (Ammonia).
- Too much iodine is also harmful. Do not eat iodine "to be safe", and do not use iodine-treated drinking water for months on end, especially in pregnancy or for anyone with a thyroid disease. Some people are allergic to iodine and get a red, itchy rash; for them use alcohol instead.
- Stains on cloth and skin come out with a solution of "hypo" (sodium thiosulfate, see Photography) or crushed vitamin-C-rich fruit; on a bench, cover with starch paste and wipe.
What this unlocks
Healthier children inland and far from the sea (Nutrition and Deficiency Diseases, Safe Childbirth); clean skin before every operation (Basic Surgery, The First Aid Kit); safe water for travellers; the starch test for brewers, cooks and analysts (Identifying Substances); Gram staining of bacteria (Biological Stains, Culturing Microbes, The Microscope); silver iodide plates for Photography; and sodium iodide crystals that flash when gamma rays strike them (Photomultipliers and Scintillation Counters). The kelp salts left over are potash fertiliser, and the ash once made soap and glass (Soda Ash and Baking Soda).
How it was first done
People in China treated goitre with burnt seaweed and sea sponge by the 4th century AD, without knowing why it worked. In 1811 the French saltpeter maker Bernard Courtois in Paris was making Saltpeter for the Napoleonic wars, using kelp ash from Normandy and Brittany as a source of potash. Cleaning his vats with too much sulfuric acid, he saw a violet vapour rise that condensed into dark crystals. His colleagues Charles Desormes and Nicolas Clément announced it in 1813; Joseph Gay-Lussac named it iode, from the Greek for violet, and he and Humphry Davy showed it was a new element.
In 1820 the Swiss doctor Jean-François Coindet of Geneva treated goitre with iodine, and in 1829 Jean Lugol in Paris made the iodine–potassium iodide solution still named after him. Tincture of iodine was used on the battlefields of the American Civil War. A Scottish industry extracted iodine from kelp in Glasgow from the 1840s, until cheaper iodine from the waste of the Chilean nitrate mines took over after the 1870s. In 1917–1922 David Marine showed in Akron, Ohio, that small doses of iodide prevented goitre in schoolgirls; Switzerland began iodising salt in 1922 and Michigan in 1924, and goitre all but vanished wherever it was done.