Part 7 · Home and Daily Life
Mattresses and Upholstery
How to make a bed you can sleep well on — straw ticks, wool and curled-horsehair mattresses with stitched edges and tufting, featherbeds — and how to stuff and spring a chair seat with webbing, hessian, hair and tied coil springs. Comfort is spreading the body's weight; this chapter shows how.
- Difficulty
- ●●●●●
- Time
- A day for a straw tick; two to three days for a wool or hair mattress; a day for a stuffed seat, two for a sprung one
- Steps from zero
- 16 prerequisites →
This unlocks
Cradles, Hammocks, Sofas and Folding ChairsThe full path from nothing — 16 steps before this one
- Stone Tools
- Fire
- Cordage and Rope
- Finding and Preparing Clay
- Finding and Identifying Ores
- Basic Woodworking
- Hunting and Trapping
- Charcoal
- Hides and Leather
- Bellows
- Iron (the Bloomery)
- Blacksmithing
- Steel
- Axes, Chisels, Knives and Planes
- Springs
- Furniture
- Mattresses and Upholstery
Do them roughly in this order. See it on the tech tree →
Why it matters
You spend a third of your life in bed. A hard, lumpy, cold bed means stiff backs, poor sleep and slow healing; a good one restores a tired worker and is part of nursing the sick, who otherwise develop pressure sores from lying still (Nursing the Sick). A padded seat lets the old, the injured and anyone doing long desk work sit for hours without pain.
The Furniture chapter gives you the bed frame — rope or slats — and a first stuffed tick. This chapter goes further: mattresses that keep their shape for decades, stuffed and sprung seats, and the spring mattress.
How it works
A body lying on a board rests on a few small areas — shoulder blade, hip bone, heel. The pressure there squeezes blood out of the skin and wakes you up to turn over. A mattress spreads your weight over a large area by sinking more under the heavy parts and less under the light ones, then springing back when you get up.
How well a filling does this depends on its springiness:
- Straw, leaves and husks are cheap and comfortable at first, but their hollow stems crush and break. A straw tick goes flat and dusty within a year.
- Wool fibres are crimped (wavy), so a mass of carded wool is full of tiny springs. It stays springy for years and is warm.
- Curled horsehair — hair twisted, boiled and set into tight corkscrews — is the springiest natural filling. It lasts generations.
- Feathers and down are the softest, but compress flat under weight; they belong on top as a soft layer, not underneath.
- Steel coil springs do the job best of all, because a spring pushes back in proportion to how far it is squeezed (Springs).
Two other things matter. The cover (ticking) must be woven tightly enough to keep the filling in and dust out. And the filling must be held in place by stitches running through the mattress or seat, or it drifts to the edges and leaves you lying in a hollow.
What you need
| Item | For | Notes |
|---|---|---|
| Ticking | Mattress covers | Dense twill of linen, hemp or cotton (The Loom). A single mattress 90 × 190 × 15 cm needs about 5 m² |
| Filling | Mattress | Single bed: 8–12 kg straw, or 10–12 kg wool or hair, or 4–6 kg feathers for a featherbed |
| Mattress needle | Tufting, stitched edges | Straight steel, 25–30 cm long, pointed at both ends, eye near one end |
| Curved needle | Sewing on springs and covers | 8–12 cm, a half-circle (Sewing, Needles and Thread) |
| Regulator | Moving lumps of stuffing | A steel spike 20–25 cm long, pointed at one end, flat at the other |
| Twine | Tufting, stitching, ties | Strong waxed flax or hemp twine, 1–2 mm (Ropewalks and Sailcloth) |
| Laid cord | Tying springs | Smooth, hard-twisted hemp cord 3–4 mm that does not stretch |
| Webbing | Seat base | Strong woven band 5 cm wide of hemp, flax or jute (Tablet and Band Weaving) |
| Hessian | Over webbing and springs | Coarse, strong plain-weave hemp or jute cloth (burlap) |
| Calico, wadding, top cloth | Seat covers | Plain cotton or linen; a thin sheet of carded wool or cotton; leather or heavy wool for the top |
| Tacks and hammer | Fixing webbing and cloth | Short iron tacks 10–16 mm with wide heads (Nails, Rivets and Wire Fasteners) |
| Webbing stretcher | Pulling webbing tight | A hardwood paddle 20 cm long with a slot or pegs to grip the webbing |
| Coil springs | Sprung seats and beds | Double-cone ("hourglass") springs, 12–20 cm tall, of hardened steel wire 3–4 mm thick (Springs) |
Where to find it
- Straw: oat straw is softest, then barley, wheat and rye (The Great Staple Crops). Maize husks, shredded into strips, are springier and last longer than straw. Dried bracken and heather were long used in hill country.
- Wool: from your own sheep, washed and carded (Wool). Short, coarse wool not good enough for spinning is perfect for stuffing.
- Horsehair: cut from the tails and manes of living horses (it grows back) or saved from slaughtered animals; cattle tail hair is a cheaper second grade.
- Feathers: from ducks and geese (Quilting, Down and Warm Clothing shows how to clean them).
- Coir: coconut husk fibre in the tropics. Kapok: the floss of the kapok tree. Both are springy, rot-resistant stuffings.
- Seaweed and moss: dried eelgrass (sea grass) from sheltered shores, rinsed of salt, and cured Spanish moss in the American south were both used commercially for mattresses.
Method 1: The straw tick (paillasse)
The quickest real mattress.
- Sew a bag of ticking the size of the bed frame and 20 cm deep (Sewing, Needles and Thread). In the middle of the top face leave a slit 40–50 cm long with a deep overlapping flap or a row of ties.
- Fill it through the slit with 8–12 kg of dry, clean straw or shredded maize husks, until it is plump and round — it will settle by a third in the first week.
- Every morning, put your arm through the slit and stir the filling to break up the hollows. This is why the slit is in the middle.
- Replace the filling every year after the harvest. Old straw goes to the compost heap or animal bedding.
Tip Layer your bed. The classic bed is a straw tick underneath for bulk, a wool or hair mattress above it for support, and a featherbed on top in winter for warmth. Each layer does what it is best at.
Method 2: A wool or horsehair mattress
Curling horsehair
Straight hair is only a little springy. Curling makes it permanent springs:
- Wash the hair in hot soapy water, rinse well and dry.
- Spin it into a rope about 2 cm thick, twisting very hard until it kinks back on itself — use the methods in Cordage and Rope or a ropemaking hook.
- Boil the rope for 2–3 hours, or steam it.
- Dry it slowly for several weeks, hanging in an airy, warm place. The longer it rests, the better the curl sets.
- Untwist the rope and pull the hair apart by hand ("picking"), then tease it into a loose, curly mass. Each hair now holds a tight corkscrew.
Making the mattress
- Cut the cover. Two panels the size of the bed (for example 90 × 190 cm) plus 2 cm all round for seams, and a border strip the depth of the mattress (15 cm) plus 4 cm, long enough to go all the way round (about 5.6 m — join pieces as needed). Sew the border to the bottom panel, inside out, then turn it right side out. Mark the tuft positions on both panels with chalk: a grid every 20–25 cm, starting 15 cm from the edges.
- Open the filling. Tease or card the wool or hair into loose, even layers. Lumps put in now stay as lumps.
- Fill in layers. Lay the filling evenly over the bottom panel, pushing extra into the corners and along the edges. Build it to about 25–30 cm loose — roughly twice the finished depth. In a hair mattress, put a 3–4 cm layer of wool on each face so hair does not poke through.
- Close it. Lay the top panel on and sew it to the border all round with a strong, close stitch.
- Make the edges. With the mattress needle, sew a row of blind stitches just above and below the border seams: in through the border, diagonally into the filling, out on the top panel, and back. Pull each stitch tight — it drags filling forward into the edge. Then sew one or two rows of top stitches right through the edge, about 3 cm in, to form a firm roll 3–4 cm thick along every edge. A stitched edge stops the mattress sagging when you sit on its side.
- Tuft. Thread the mattress needle with doubled twine. Push it straight through at a tuft mark, pull it out of the far face, put it back through 1 cm away and out at the start. Thread a tuft — a little pad of wool, a disc of leather or a cloth-covered button — under each loop on each face, so the twine cannot pull through. Tie a slip knot and pull it down until the mattress there is squeezed to about two-thirds of its thickness. Tie off. Work from the middle outwards.
A wool mattress of 10–12 kg should be turned and aired weekly for the first months, then monthly. Every 5–10 years, unpick it, wash the ticking, card the filling fresh and remake it; travelling mattress makers once did exactly this from house to house.
A featherbed
A featherbed is a soft, thick tick of feathers laid on top of the mattress. Feathers work through ordinary cloth, so use the tightest ticking you can weave and wax it inside: rub a cake of beeswax over the inner face, then press it with a warm iron so the wax melts into the weave. Fill with 4–6 kg of cleaned feathers. Shake it up every morning so it lofts again.
Beds that give
Rope and slatted frames are described in Furniture. A rope bed should be retightened every few weeks; a sagging one is the commonest cause of morning backache. For a firmer, springier base without metal, make the slats from ash or birch 6–7 cm wide and 8–10 mm thick, bent while steamed (Steam-Bending Wood) into a gentle upward curve of 2–3 cm, and set them in shallow pockets on the side rails so they flex under weight. Thin bent wood springs back for many years (Springs).
Method 3: A stuffed seat
This is the classic padded seat on a wooden chair or stool frame.
- Webbing. Fold the end of the webbing over 3 cm and fix it to the top of the back rail with five tacks in a W. Run it across to the front rail, lever it tight with the webbing stretcher against the outside of the rail until it rings like a drum when you flick it, and fix it with three tacks. Cut it 3 cm long, fold the end back and fix it with two more. Space the webs about one web-width apart: 4–5 front to back, then 4–5 side to side, woven over and under the first set.
- Hessian. Stretch a piece of hessian over the webbing and tack it every 3–4 cm, folding the raw edge over on top.
- Bridle ties. With the curved needle and twine, sew rows of loose loops onto the hessian 10–12 cm apart, each just loose enough to slide your flat hand under.
- Stuffing. Tease curled hair, wool or coir under the ties until you have an even dome about 8 cm thick, a little higher in the middle. The ties stop it sliding.
- First cover. Pull a sheet of calico down over the stuffing and fix it with temporary tacks (driven halfway) on the rails, compressing the stuffing to about half its loose height. Use the regulator through the cloth to move lumps. When it is smooth and firm, drive the tacks home.
- Wadding. Lay a 1 cm sheet of carded wool or cotton over the calico to stop hair working through.
- Top cover. Leather, heavy wool or woven horsehair cloth, pulled smooth, folded into neat pleats at the corners, and tacked under the rails. Tack a piece of thin cloth underneath to keep dust from falling out.
On a seat stuffed over the edge of the frame, the front edge needs a stitched roll exactly like a mattress edge, sewn through a cover of loose-woven cloth (scrim) before the calico goes on.
Method 4: A sprung seat
- Webbing goes underneath. Fix the webs to the underside of the rails, so the springs have room to stand.
- Place the springs. A dining chair takes 4–5 springs (four in a square, one in the middle); an armchair 9–12 in rows. Space them so their top rings are 2–3 cm apart. Sew each bottom ring to the webbing with three or four stitches of twine with the curved needle, knotting each stitch.
- Tie the springs (eight-way tie). Fix a laid cord with two tacks to the rail opposite each row of springs. Run it across the row, tying a clove hitch round the top ring of each spring as you go, to a tack on the far rail. Pull each spring down 2–4 cm as you tie, so all stand straight and at the same height; tilt the outer springs slightly outwards and tie them a little lower, to give a rounded crown. Tie every row front to back, then every row side to side, then both diagonals: each spring is now held in eight directions and cannot tip, rub or clunk.
- Cover the springs with strong hessian tacked to the rails, and sew each spring's top ring to it at three or four points.
- Finish exactly as for the stuffed seat: bridle ties, stuffing, calico, wadding, cover.
Spring beds
- A box spring is the same thing at bed size: a stout frame of 5 × 10 cm rails with 4–6 cross bars, carrying 40–60 double-cone springs sewn or stapled down and tied eight ways, covered with hessian, a thin layer of hair and ticking. A wool or hair mattress lies on top.
- An innerspring mattress puts the springs inside the mattress itself, joined to each other by spirals of wire, with hair and wool layers above and below.
- Pocket springs — each slender spring sewn into its own cloth pocket, the pockets sewn together in rows — let each spring move separately and need no wire ties. They need only cloth, thread and lots of small springs.
All three require hundreds of identical springs; build them only when you have a steady supply of spring wire and a winding jig (Springs, Iron and Brass Wire).
How to tell it worked
- Mattress: lie on your side. Your hip and shoulder should sink in so that your spine is straight, and you should not feel the frame under your hip. Turn over: the hollow should fill again within a minute.
- After a month, the filling is still even, with no lumps between tufts and no hollow in the middle; the edges stay square when you sit on them.
- Seat: press the middle hard — it gives evenly and comes back. Flick the webbing underneath: it rings. A sprung seat makes no clicking or squeaking.
Note Troubleshooting. Hollows and lumps → filling not teased evenly, or tufts too far apart; open it, re-card the filling and tuft every 20 cm. Edges collapse when you sit → no stitched roll; add blind stitches and top stitches. Feathers or hair poke through → ticking too loose; wax the inside, or add a wool layer under the cover. Seat sags after a few months → webbing not tight enough or too few webs; re-web tighter. Springs click, squeak or lean → ties loose or springs touching; re-tie with the springs further apart. Musty smell, dark spots → damp filling; empty and dry it in the sun, or replace it.
Dangers
Danger Babies can suffocate in soft bedding. A baby under one year must sleep on its back, on a firm, flat mattress, with no pillow, featherbed, loose quilt or soft toys, and not between adults who are drunk, drugged or exhausted. Soft beds that are a luxury for adults are a deadly trap for infants.
Danger Fire. Straw, feathers, kapok, coir and dry hair all burn fast, and a burning mattress fills a room with smoke in a minute. Never take a candle or lamp into the bed, never smoke in bed, and keep beds well away from hearths (Lamps and Candles, Firefighting).
- Tacks in the mouth. Upholsterers traditionally held tacks between their lips to work faster; many swallowed or breathed them in. Keep them in a dish.
- Anthrax has been caught from horsehair and other animal hair. Use hair only from healthy animals; wash it hot. Boiling does not reliably kill anthrax spores. See Horn and Bone Working.
- Dust and mould. Old straw and damp filling grow mould and harbour dust mites, which trigger asthma. Keep bedding dry, air it in the sun, replace straw yearly.
- Pests. Mattresses shelter bed bugs, fleas and moths. See Household Pests.
- Compressed springs can fly loose when a tie is cut. Hold the spring while you cut, and keep your face away.
What this unlocks
With well-made beds and seats, the sick heal better and workers rest properly. The same skills — webbing, stuffing, stitched edges and tied springs — make sofas and armchairs (Cradles, Hammocks, Sofas and Folding Chairs) and upholster carriage and railway seats (Wagons and Carriages, Railways), saddles and padded harness (Draft Animals and Harness). When you can make Rubber into foam or webbing, it replaces springs and hair with something lighter.
How it was first done
People have made beds for a very long time. At Sibudu Cave in South Africa, layers of sedges and rushes laid down as bedding about 77,000 years ago were topped with leaves of a tree whose scent repels insects. Romans stuffed mattresses with reeds, hay, wool or feathers. Through the Middle Ages most Europeans slept on straw ticks, and a featherbed was valuable enough to be left in a will.
Upholstered chairs became common in Europe in the 1600s, stuffed with hair over webbing and tacked with leather or cloth. Coil springs began to appear in seats in England in the 1820s, and spring mattresses spread in the second half of the 1800s. Around 1900 the Canadian engineer James Marshall introduced pocket springs, each sewn in its own cloth bag. Latex foam rubber, invented by the Dunlop company in 1929, began the shift away from springs and hair.
Source: content/entries/home/upholstery-and-mattresses.md