How to turn plant stems, tree bark and animal tendons into string and rope by twisting — plus braiding and the handful of knots that do almost every job.

Difficulty
●●●●●
Time
An hour to make your first metre; a few minutes per metre with practice
Steps from zero
0 prerequisites →

You need first

Nothing — start here.

This unlocks

Scaffolding and LaddersMusical InstrumentsThe LatheBaskets and ContainersBow and ArrowFishingHunting and TrappingKnots, Lashings and RiggingFlax, Hemp and LinenRopewalks and SailclothSpinning and Weaving ClothBoats and SailsRafts and Canoes

Objects made here

ropetwinecord

Why it matters

String is one of humanity's oldest and most underrated inventions. With it you can tie a shelter frame (Shelter), spin a bow drill (Fire), bind a stone blade to a handle (Stone Tools), set snares (Hunting and Trapping), make fishing lines and nets (Fishing), string a bow (Bow and Arrow), and weave Baskets and Containers and cloth (Spinning and Weaving Cloth). Later, rope raises loads with pulleys (Simple Machines), drives the The Lathe, and rigs Boats and Sails.

All of it comes from one simple trick: twisting short fibres together so they lock.

How it works

A single plant fibre is short and weak. Twist a bundle of fibres and they squeeze against each other; friction then stops them sliding apart, so the bundle is as strong as many fibres together. But a single twisted strand wants to untwist, and will kink and unravel as soon as you let go.

The answer is plying. Twist two strands in one direction, then wrap them around each other in the opposite direction. Each strand's urge to untwist now tightens the wrap instead of loosening it. The two forces lock each other, and the cord holds its shape forever. Almost every rope in history is built this way.

Twist direction has names. If the twist runs like the middle stroke of the letter Z when you hold the cord vertically, it is a Z-twist; like the middle of an S, it is an S-twist. A two-ply cord is made of two Z-twisted strands plied together in S, or the other way round.

What you need

Material Best for Notes
Stinging nettle, dogbane, milkweed stems Fine, strong string, fishing line, snares The best wild fibres in temperate lands
Inner bark of basswood (linden), willow, cedar, elm Thick cord, rope, lashing Fast to gather in quantity
Yucca, agave, flax, hemp leaves or stems All-purpose cord Dry country (yucca, agave); flax and hemp are also crops
Grass, cattail and reed leaves Quick, rough cord Weak, but always to hand
Spruce and pine roots Sewing and lashing bark Use split, whole or peeled
Sinew (animal tendon) Bow strings, hafting, sewing Strongest of all; shrinks tight as it dries
Rawhide Lashings, heavy straps See Hides and Leather

You need no tools, though a sharp stone flake helps (Stone Tools), and a smooth stick or bone helps to scrape fibre.

Where to find it

  • Stinging nettle grows in dense patches on rich, damp soil — along streams, field edges, and around old settlements and dung heaps. Square stems, opposite saw-toothed leaves, covered in stinging hairs. Gather tall stems (1–2 m) in late summer to autumn, when the stem is fully grown and the leaves are starting to drop. Dead, standing stems in early winter also work, and no longer sting.
  • Dogbane (Indian hemp) grows in North American fields and roadsides: reddish stems, opposite smooth leaves, milky sap. Gather the tall dead red-brown stems in autumn. Its sap is poisonous to eat.
  • Milkweed: thick stems, broad leaves, milky sap, big seed pods full of silky fluff. Gather dead stems in autumn.
  • Basswood (linden) has large heart-shaped, lopsided leaves and smooth grey bark when young. Its inner bark is the classic rope fibre of northern forests. Willow grows by water, with long narrow leaves; cedar has flat scale-like leaves and stringy red-brown bark.
  • Yucca and agave are spiky leaf rosettes of dry lands. The fibres run the full length of the leaf.
  • Sinew is the white, silvery tendon along the backbone (the "backstrap" sinew, just over the loin meat) and in the lower legs of deer and similar animals. See Hunting and Trapping.

Preparing the fibres

Plant stems (nettle, dogbane, milkweed, flax)

The fibres lie in a thin layer just under the skin of the stem, around a woody core.

  1. Strip the leaves. For fresh nettles, wear a glove of leaves or stroke upwards from the base: the stinging hairs point upwards.
  2. Crush the stem flat by rolling it under a round stone or squashing it with your fingers along its length. It splits into two to four ribbons.
  3. Break out the core. Snap the woody core every 5 cm by bending it, then peel the fibre-and-skin ribbons away from the core pieces.
  4. Clean the fibre. Rub the ribbons between your palms, or scrape them over a smooth stick with a blunt stone, until the papery outer skin flakes off and soft, silky threads remain.
  5. Dry and store in bundles. Dampen slightly before twisting: damp fibre twists tighter and stays put.

Inner bark (basswood, willow, cedar, elm)

Bark peels easily only when the sap is running, in late spring and early summer.

  1. Choose a straight sapling or branch, 5–10 cm thick. Cut it down. (Stripping bark from a living tree all the way round kills it.)
  2. Score the bark lengthwise and peel it off in long strips. The inner bark is the pale, fibrous, moist layer next to the wood.
  3. Retting. Coil the bark and sink it in a pond or slow stream, weighted with stones, for 2–6 weeks. Bacteria rot the soft glue (pectin) that holds the fibres together. Check every few days: it is ready when the bark separates into many thin, papery layers when you flex it. It smells of swamp.
  4. Pull the layers apart, rinse and dry them. Split into strips 3–10 mm wide.

Willow and cedar bark can be used fresh, without retting, for rough cord.

Flax and hemp are retted the same way, whole stems in water for 1–3 weeks, or laid on grass for 3–6 weeks so dew does the work (dew-retting). Then the dried stems are beaten to break the core out — the start of linen cloth (Flax, Hemp and Linen, Spinning and Weaving Cloth).

Yucca and agave leaves

Pound fresh leaves with a smooth stone on a log, then scrape off the green pulp with a blunt edge until white fibres remain. Roasting leaves in hot ashes first makes the pulp easier to remove.

Sinew

  1. Cut out the backstrap and leg tendons. Scrape off all meat and fat.
  2. Dry them flat in the shade for a few days. They become hard and amber-coloured, like horn.
  3. Pound the dry tendon gently with a smooth stone on a log until it turns white and fluffy, then pull it apart into threads as fine as you need.
  4. To use, chew or soak a thread until soft. Wet sinew contains its own glue: it sticks to itself and shrinks hard as it dries.

Method 1: The reverse wrap (two-ply twist)

1. FOLD AND KINK 2. TWIST THE FAR STRAND 3. WRAP IT TOWARDS YOU Hold the bundle a third of the wayalong, so the ends are uneven.Twist hard until a loop kinks. Pinch the loop. Roll the farstrand away from you betweenfinger and thumb until tight. Bring it over the near strand,towards you. They swap places.Pinch, and repeat from step 2. THE FINISHED CORD splice: 5 cm overlap Each strandtwisted one way The pairwrapped the other way, so the twists lock
Fig. 1 The reverse wrap. Twist the far strand away from you, then bring it over the near strand towards you. Repeat. Each strand is twisted one way and wrapped the other, so the cord locks.

This is the method to learn first. It needs nothing but your hands.

  1. Make a bundle. Take a bundle of fibre about as thick as the finished cord should be — say 2–3 mm for string. Hold it about one-third along its length, not in the middle, so the two ends are uneven (one about twice the length of the other). This makes the joins (splices) fall at different places later.
  2. Make the loop. With both hands, twist the bundle hard at the fold until it kinks into a small loop. Pinch that loop between your left thumb and forefinger. You now have two strands hanging from the loop.
  3. Twist the far strand. With your right thumb and forefinger, grip the strand farther from you about 3 cm below your left fingers, and roll it away from you until it is tight.
  4. Wrap it over. Keep the twist in, and bring that strand towards you, over the near strand, so the two swap places. The wrap goes the opposite way to the twist.
  5. Move your grip. Pinch the new crossing with your left fingers to hold it.
  6. Repeat: twist the (new) far strand away, wrap it towards you. Over and over. Each twist-and-wrap moves you about 1 cm along.
  7. Splice in new fibre. When one strand has about 5 cm left, lay a new bundle of fibre along it, overlapping by 5 cm, with its thin end against the old strand's thin end. Twist the two together as if they were one strand and carry on. Because the ends were uneven at the start, the two strands never need splicing at the same spot — that would be a weak point.
  8. Finish with an overhand knot at the end, or by splicing the cord back into itself.

Thigh rolling is faster. Lay two strands side by side on your bare thigh and roll them down your leg under your palm: this twists both at once in the same direction. Lift your palm at the bottom and let them go: they spring back and ply around each other in the opposite direction. Many peoples have made all their string this way.

Method 2: Rope

A rope is cord made of cord. Make three long lengths of two-ply cord (each with the same final twist direction). Tie them together at one end and hang them from a branch. Twist each one tighter in its own direction, then wrap them around each other in the opposite direction. Tie the bottom end. This is "laying" a rope. A three-strand rope of 5 mm two-ply cords is easily strong enough to haul a log or hang a pack.

For long ropes, two people work together: one at each end, each turning the strands with a crank-handle stick, while a third person walks along feeding the twist. This grows into the ropewalk (Ropewalks and Sailcloth).

Method 3: Braiding

Braiding (plaiting) needs no twisting and works with flat materials — rawhide strips, leaves, inner bark — that don't twist well.

  1. Tie or hold three strands together at one end.
  2. Bring the right strand over the middle one. It becomes the new middle.
  3. Bring the left strand over the (new) middle one.
  4. Repeat, right over middle, left over middle, pulling each tight.

A three-strand braid is flat; braids of four or more strands can be made round. Braids are good for slings, straps, handles and fishing lines.

Knots worth knowing

Overhand knota stopper, and the start of many knots Square (reef) knotjoins two ends of the same cord Clove hitchties a cord to a pole load
Fig. 2 Three basic knots, drawn loose so you can follow the cord. Pull each one tight slowly, and leave a tail at least ten times as long as the cord is thick.
  • Overhand knot — the simplest knot: make a loop and pass the end through it. It stops a cord end from fraying or slipping through a hole, and it is the first half of many other knots.
  • Square knot (reef knot) — joins two ends of the same cord, for bundles, bandages and lashings. Right over left and under, then left over right and under. It can slip with stiff or slippery cord, and must never be trusted to hold a person.
  • Sheet bend — joins two cords of different thickness. Bend the thick one into a hook; pass the thin one up through the hook, round behind both legs, and tuck it under itself.
  • Bowline — a loop that does not slip or tighten, and unties easily even after a heavy load. Make a small overhand loop in the standing part ("the rabbit hole"). Bring the end up through the hole, round behind the standing part ("the tree"), and back down the hole.
  • Clove hitch — ties a cord to a pole, and starts and ends most lashings. Two turns round the pole, the second crossing over the first, with the end tucked under the crossing.
  • Lashing — to join two poles at right angles, start with a clove hitch, wrap three or four times round both poles, then two or three "frapping" turns between the poles to pull the wraps tight, and finish with another clove hitch (more in Knots, Lashings and Rigging).

How to tell it worked

  • Good two-ply cord is even in thickness, and the twists are tight and regular, like a row of grains of wheat. Hold a 30 cm length by its ends and let it go slack: if it stays straight or kinks gently on itself, the twist is good. If it unravels, you wrapped the same way you twisted.
  • Strength test. Tie a loop and hang your weight, or a stone, from it gradually. A well-made 3 mm nettle or dogbane cord should hold a heavy stone of several kilograms easily; a pencil-thick cord of good bark fibre will often take a person's weight — but test it before you trust it.
  • Knots should be tight, neat, and look like the drawings. A knot that looks wrong usually is wrong.

Note Troubleshooting. Cord unravels → you twisted and wrapped the same way; twist away, wrap towards. Lumps at splices → the new bundle was too thick; taper both ends to thin points before overlapping. Breaks at the same place → both strands were spliced at the same point. Fibres snap while twisting → they are too dry; dampen them. Bark won't peel → wrong season; wait for late spring, or ret it longer.

Dangers

  • Stinging nettles cause painful, burning blisters for an hour or so. Rubbing the skin with dock leaves, plantain or cool mud gives some relief. They are harmless otherwise.
  • Poisonous sap. Dogbane and milkweed sap are toxic if eaten and irritate eyes; wash your hands before eating and do not rub your eyes.
  • Rope failure. A rope that breaks under load whips back and can cut skin or injure eyes. Never trust home-made cord with a person's life until you have tested it with at least five times the weight. Rope weakens fast if left wet: it rots. Dry it before storing.
  • Cuts. Stone flakes are sharper than you expect. Cut away from your body.

What this unlocks

Cord leads directly to Baskets and Containers and nets, to Fishing lines, to snares in Hunting and Trapping, to the Bow and Arrow, and to Spinning and Weaving Cloth — which is only cordage made very fine and very long, then woven. Strong rope makes possible Simple Machines such as pulleys, the bow lathe (The Lathe), and Boats and Sails.

How it was first done

The oldest known piece of cord is a tiny fragment of three-ply twisted bark fibre stuck to a stone tool at Abri du Maras in France. It was made by Neanderthals between about 41,000 and 52,000 years ago. Impressions of cord and woven fabric pressed into fired clay at Pavlov and Dolní Věstonice in the Czech Republic date to around 26,000–27,000 years ago. A length of two-ply cord was found in the Lascaux cave in France, about 17,000 years old. The Iceman who died in the Alps 5,300 years ago carried cord of grass and bast, and Ancient Egyptians made rope of papyrus and palm fibre on a large scale. Until about two hundred years ago all rope everywhere was made by twisting natural fibres, exactly as this chapter describes.