Part 3 · Metals
Planes, Drawknives and Woodworkers' Tools
The full kit of a joiner, carpenter and chairmaker — the jack plane and moulding planes, spokeshave, drawknife, froe, gouges, brace and bit, augers and gimlets, crosscut, rip, coping, two-man and hack saws — and the workbench, holdfasts, sawhorses, mallets and marking gauges that hold and mark the work. How each is made, what sizes work, and how to tell a good one.
- Difficulty
- ●●●●●
- Time
- A day for a mallet, froe or holdfast; two to three days for a jack plane or a workbench; a week for a set of moulding planes
- Steps from zero
- 15 prerequisites →
This unlocks
—The full path from nothing — 15 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- Charcoal
- Hides and Leather
- Bellows
- Iron (the Bloomery)
- Blacksmithing
- Steel
- Axes, Chisels, Knives and Planes
- Files and Saws
- Planes, Drawknives and Woodworkers' Tools
Do them roughly in this order. See it on the tech tree →
Why it matters
Axes, Chisels, Knives and Planes gave you the axe, chisels and a basic plane; Files and Saws the file and saw. This chapter fills the rest of the woodworker's chest: tools that make boards flat and square, cut mouldings, shave curves, split, bore and saw cleanly, and hold the work still. Every piece of Furniture, every door and window (Doors, Windows and Joinery), wheel (The Wheel and Axle) and wooden machine (The Watermill, The Loom) depends on them.
How it works
A plane is a chisel held in a jig. The wooden body fixes the blade (the iron) at one angle and lets it project only a fraction of a millimetre, so each stroke takes a thin, even shaving. Three things decide whether it cuts cleanly or tears:
- Bed angle: 45° for general work ("common pitch"); 50–55° for hard or curly wood and moulding planes.
- Mouth: the gap in front of the edge. Tight (under 1 mm) for finishing, wider for coarse work. The sole in front of the mouth presses the wood down so it cannot split out ahead of the edge.
- Cap iron (chip breaker): a second plate fixed on top of the iron, its edge 0.5–2 mm behind the cutting edge. It bends the shaving sharply as it forms, so the shaving breaks before it can lever a split ahead of the edge. This is the biggest single improvement to a plane.
Splitting tools (froe, wedges) follow the grain instead of cutting it. Saws are rows of tiny chisels (rip) or knives (crosscut) — see Files and Saws. And holding the work is half the job: a heavy bench, a vice, a holdfast and a stop let both hands drive the tool.
What you need
| Item | Notes |
|---|---|
| Metal | Steel for irons, blades, saw plates and bits (Steel); soft iron for holdfasts and frames |
| Forge tools | Swage block for gouges, mandrel for the froe eye (Blacksmithing) |
| Files and stones | Saw, round and half-round files; sandstone, whetstone, shaped slipstones (Abrasives and Grinding Stones, Sharpening and Honing) |
| Wood | Beech, hornbeam or boxwood for planes; ash wood for handles; lignum vitae or beech for mallets; oak slabs 8–10 cm thick for the bench |
Where to find it
Beech — tall, smooth, silver-grey trees with pale, even wood — is the classic plane wood. Hornbeam and boxwood are harder still; lignum vitae, a tropical wood that sinks in water, makes the best mallets. Cut plane blocks in winter from the quarter (growth rings upright on the end), rough them out oversize, seal the ends with wax, and season them under cover for two years.
Planes
The jack plane
The body, the iron and the 45° bed are made as in Axes, Chisels, Knives and Planes. A jack plane is 35–45 cm long and about 7 × 7 cm in section, with an iron 50–55 mm wide. What makes a good one:
- Tote: a closed handle of beech or ash mortised in behind the throat, leaning forward about 70°, and a knob in front.
- Cap iron: a plate the width of the iron, 1.5–2 mm thick, its last 1 cm bent down so only its front edge touches the iron. File that edge straight and smooth, or shavings wedge under it. Fix it with a screw through a slot (Screws, Nuts and Bolts), its edge 1.5–2 mm back for a jack, 0.5 mm for a smoother.
- Wedge: hardwood tapering about 10°, split down the middle so shavings escape between its legs, bearing on the cap iron near the edge.
- Edge: bevel 25°, honed at 30°. For a jack, round the edge about 1 mm higher in the middle than the corners, so it takes a thick, scooped shaving without ridges.
- Adjusting: tap the iron to cut deeper; tap the back of the body (on a hardwood strike button) to back off.
- Sole: flatten it on sandstone with the iron wedged in but drawn back, since wedge pressure bends the body slightly. Rub on a little tallow.
Plane with the grain; if it tears, turn the board round. Check twist with two straight sticks across the ends (winding sticks): sighted across, their tops should be parallel.
Moulding planes
A moulding plane has its sole and iron shaped to the reverse of the profile it cuts.
- Hollows and rounds are the basic set: a "hollow" has a concave sole and cuts a convex shape; a "round" the opposite. They come in pairs, each pair a different width and curve. Six pairs, from 6 to 25 mm, will make almost any moulding, worked in steps.
- The rebate plane has an iron as wide as the sole, often skewed about 20°, and an opening in the side for the shavings. It cuts a step along an edge (a rebate) for doors, window frames and boxes.
- The plough plane cuts grooves 3–12 mm wide for panels and drawer bottoms (Doors, Windows and Joinery). Its narrow iron rides on a steel skate (a thin runner forming the sole); a fence slides on two wooden stems through the body and is locked by wedges or wooden screws; a depth stop is a block screwed up and down beside the skate.
Sizes: bodies about 24 cm long and 8–9 cm high, as wide as the profile plus 6–10 mm. Bed the iron at 50–55°. Most are held tilted while cutting — the spring — shown by lines scribed on the front end.
Making a hollow or round:
- Shape the sole of a seasoned beech blank to the profile, checking with a sheet-metal template.
- Chisel the throat at 50–55° and an escapement (an opening up the side) for the shavings.
- Lay a soft iron blank 3–4 mm thick in the bed, scribe the sole's profile on it from below, file to the line, and bevel it 25–30° underneath.
- Harden, temper straw, hone with slipstones. A good one cuts a clean profile and stops cutting by itself when the sole bottoms on the work.
The spokeshave
A spokeshave is a very short plane with a handle on each side, for curves: spokes, chair legs, tool handles, the inside of a curved arm.
The wooden spokeshave has a stock of beech or box about 25–30 cm long. Its blade, 5–7 cm wide and 3 mm thick, has a tang at each end bent up at right angles; the tangs push through two holes in the stock and hold by friction, the blade lying bevel-up at a low angle. Tap the tangs to set the depth; a brass strip in front of the mouth resists wear. Iron spokeshaves are tiny planes with a bevel-down blade under a screwed cap. Skew it slightly across the cut; a sharp one leaves a surface that needs no sanding.
The drawknife
A drawknife is a blade 20–30 cm long, 3–4 cm wide and 5–6 mm thick at the back, with a tang at each end bent toward you at about 90° into a wooden handle 10–12 cm long. Forge it from steel (or iron with a steel edge, Axes, Chisels, Knives and Planes), bend the tangs, grind a single bevel at 25–30°, harden and temper the blade straw-brown, and let the tangs run blue. Used bevel down, it scoops hollows and follows curves; bevel up, it takes long straight cuts. It is the fastest way to shape green wood, used at a shaving horse (Furniture). Keep a leather sheath on it.
Froe and gouges
The froe
A froe splits wood along the grain into boards, shingles (Roofs), laths, staves and chair parts.
- Blade: steel or iron bar 25–40 cm long, 5–6 cm wide, 10–12 mm thick along the back, tapering to a blunt edge of 30–35°. It is not sharpened like a knife: it wedges, it does not cut.
- Eye: at one end, forge an eye at right angles to the blade. The old way: draw the end thin, wrap it round a round mandrel 30–35 mm across, and forge-weld the end back to the blade (Blacksmithing).
- Handle: 30–45 cm of ash or hickory, driven through the eye from the top, perpendicular to the blade — the handle is the lever.
- Heat treatment: none, or a light hardening tempered blue. It is struck only with wood.
Strike the back of the blade with a froe club (a 40 cm length of hardwood, thicker at the striking end) to start the split, then lever the handle to drive it down and steer it, working with the split held in a froe brake — a fork of two logs.
Gouges
A gouge is a chisel with a curved cross-section, for hollows, coves and carving. Its curve is its sweep: from nearly flat to a deep U. A basic set: three or four sweeps in widths of 6, 12, 20 and 30 mm.
- Out-cannel gouges (bevel on the outside) carve and hollow bowls, spoons and mouldings.
- In-cannel gouges (bevel on the inside) pare a concave edge to fit a round — the edge of a chair seat, a round tenon's shoulder.
Making one: forge a flat chisel blank with a tang or socket as in Axes, Chisels, Knives and Planes. At an orange heat, lay the blade over a groove in a swage block and drive it in with a round bar on top, until it takes the sweep. File the inside smooth with a round file, grind the bevel at 25° (outside or inside), harden, temper straw, and hone the inside with a slipstone — a small stone rubbed to fit the curve.
Boring tools
How augers, gimlets and the brace work is in Drills and Boring. A few particulars:
- Auger: 40–60 cm long, 6–50 mm, with an ash cross handle 35–40 cm wide. For a twist auger, heat a flat steel bar 2 × 0.5 cm orange, clamp one end in the vice and twist the other a turn every 3–4 cm; file a tapering screw point (lead screw) and two cutting lips.
- Gimlet: 2–6 mm, 10–15 cm long with a wooden crosspiece and a screw point, for pilot holes.
- Brace: carve it from one piece of beech or a naturally bent branch, with a sweep of 25–30 cm. The head spins on a pin with a leather washer; the pad has a square, tapering socket for the bit's tang and a spring catch or wedge.
- Centre bit: the easiest brace bit. File a flat steel blade with a sharp centre point, a nicker (a spur that scores the circle) on one side and a cutter (a lip that lifts the waste) on the other. It bores clean holes 10–50 mm. Temper purple.
Saws
Making a saw blade, cutting, setting and sharpening teeth, the frame saw and the pit saw are all in Files and Saws.
Crosscut and rip handsaws
The open handsaw has no frame, so its plate must be stiff, springy and flat — much harder to make than a frame saw.
- Plate: 55–66 cm long, 0.8–1 mm thick, tapering from 15–18 cm wide at the handle to 7–9 cm at the toe, tempered evenly blue. A good plate is also tensioned: lightly hammered in the middle on a smooth anvil, which stretches it so it stands stiff.
- Crosscut saw: teeth 3–3.5 mm apart (7–8 points to 25 mm), filed as little knives; saw at about 45° to the board.
- Rip saw: teeth 5–6 mm apart (4–5 points), filed straight across as chisels; saw at about 60°.
- Handle of beech or apple, fixed by three rivets.
A backsaw for joints has a short thin plate stiffened by a folded iron or brass strip along its back, with 10–16 teeth to 25 mm. Use it on a bench hook: a board 25–30 cm long with a cleat on top at the far end and one underneath at the near end, hooked over the bench edge.
The coping saw
For curves and inside cuts: a U-shaped frame of springy steel rod 6–8 mm thick with a 12–15 cm throat, and a blade about 16.5 cm long, 2–3 mm wide and 0.5 mm thick, with 15–18 teeth to 25 mm, tempered blue. Cross-pins at its ends sit in slotted spigots; screwing up the handle tensions it. Unhook one end and pass it through a drilled hole to cut a shape out of the middle of a board. A fret saw has a deeper frame.
The two-man crosscut saw
For felling and cross-cutting big logs (Firewood and Coppicing): a plate 1.2–2 m long and about 1.6–2 mm thick, with a curved (bellied) toothed edge and a vertical wooden handle at each end. Each person only pulls; pushing buckles the plate.
For hardwood and frozen wood, all teeth are knife-like cutters. For softwood and big logs, groups of 2–4 cutters alternate with a pair of chisel-like rakers filed 0.3–0.5 mm shorter: the cutters sever the fibres at each side of the kerf, and the rakers plane out the wood between in long shavings. Teeth are 15–25 mm long, set 0.25–0.4 mm each side. So long a plate needs a water-powered hammer or rolling mill (Sheet Metal and Rolling). Wedge the cut behind the saw so it does not pinch.
The hacksaw
A hacksaw cuts metal. The blade is 25–30 cm between its holes, about 12 mm wide and 0.6 mm thick, with 18–32 teeth to 25 mm (0.8–1.4 mm apart). Cut fine teeth like a file's (Files and Saws), with the teeth pointing away from the handle. Harden the whole blade in oil, then temper only the back blue, leaving the teeth glass-hard. The frame is a bent iron bar with a handle; the blade hangs on pins, one on a threaded rod with a wing nut that tensions it until it rings. Use fine teeth for thin sheet and tube (at least three teeth must be on the metal at once), coarse for thick bar; cut on the push, with slow, full strokes, 40–60 a minute.
Holding the work
The workbench
The bench must not move when you plane: weight is everything.
- First bench: a log 30–40 cm across split lengthways, 2–3 m long, flat face up, on four splayed legs in bored holes. A day's work.
- Joiner's bench: oak or beech top 8–10 cm thick, 50–60 cm wide, 1.8–2.4 m long, on legs 10–12 cm square joined by stretchers. Keep the front legs flush with the top's front edge so long boards can be clamped against both.
- Height: with arms hanging, the top at the base of your palm — about 80–90 cm.
- Planing stop: a 5 × 5 cm hardwood block in a tight mortise near the left end, tapped up 1–2 cm when needed.
- Holdfast holes: 20 mm, straight through, about 30 cm apart.
- Leg vice: a hardwood chop 80 cm tall, 15–20 cm wide and 5–6 cm thick, closed by a screw 40–60 mm across through the front leg; near the floor a bar with a row of holes and a peg (the parallel guide) keeps it parallel.
The holdfast
A holdfast pins work to the bench with a single blow. It is an L-shaped bar of soft iron: a round shank 18–20 mm thick and 25–30 cm long, and an arm 15–20 cm long bent at about 80° to it, so the arm's tip lies lower than its root. The hole is just 1 mm bigger than the shank.
Drop it in the hole with the arm's tip on the work and strike the top of the bend with a mallet. The arm flexes like a spring, the shank tilts and jams in the hole, and the work is locked. A sharp tap on the back of the shank releases it. Do not harden it — it must flex. Roughen the shank with crossed file marks if it slips. The bench top must be at least 7–8 cm thick for the hole walls to grip.
Sawhorses
Each sawhorse is a beam about 10 × 8 cm and 80–100 cm long on four legs splayed about 15° to the sides and 10° to the ends, notched in and pegged, 55–60 cm high — knee height, so you can kneel on a board to rip it. For logs, a sawbuck of two X-shaped trestles holds the log in the crotches.
Mallets
- Joiner's mallet: a head of beech or hornbeam about 14 × 9 × 6 cm, with its two striking faces each angled about 5° inward, so they land square on the chisel when you swing from the elbow. Cut the handle hole tapered, wider at the top, and shape the handle (30–35 cm of ash) to match: the head is driven down onto the swell and is never wedged — every blow and every swing tightens it.
- Round mallet: turned from lignum vitae, boxwood or a root burl, 8–10 cm across, for carving; it strikes the same wherever it lands.
- Beetle: 4–8 kg of elm bound with iron rings, for wedges and pegs (Timber Framing and Log Building).
The marking gauge
Described in Doors, Windows and Joinery: a stem 20–25 cm long and 2 × 2 cm through a fence about 7 × 6 × 2.5 cm, locked by a wedge or wooden thumbscrew, with a hardened steel pin 2 cm from the end, filed to a tiny knife edge and standing out 2–3 mm. Push it away from you, tilted so the pin trails. A mortise gauge has a second pin on a sliding bar, set to the chisel's width.
How to tell it worked
- Plane: a thin, continuous, full-width shaving you can see light through, a shining surface, no chatter.
- Saw: follows a line unsteered, cuts square, does not bind.
- Bench and holdfast: nothing slides when you plane hard; one blow sets the holdfast, one tap frees it.
- Edges: gouge and drawknife pare softwood end grain shiny, not crushed.
Note Troubleshooting. Plane chatters → iron not bedded flat, wedge loose or bearing in the wrong place. Flatten the bed, refit the wedge to bear near the edge. Plane tears the wood → mouth too wide, cap iron too far back, or planing against the grain. Set the cap iron closer, reverse the board, skew the plane. Shavings jam in the throat → cap iron not tight on the iron. Hone its edge flat. Saw drifts to one side → more set on that side. Stone the teeth lightly on that side, or reset. Saw binds → too little set, or green wood closing the cut. Increase set; wedge the kerf. Holdfast will not grip → hole too big or top too thin. Roughen the shank; bend the arm a little more closed. Mallet head loose → the taper in the head or the handle is wrong. Refit the handle to the taper; never wedge it.
Dangers
Warning Drawknives, gouges and froes cut toward the body. Hold the work in a shaving horse or vice, never in your lap or hand. Keep the drawknife's path clear of your knees and belly, and sheath every edge when it is put down. Most woodworking injuries are chisels and gouges slipping into the other hand: keep both hands behind the edge.
Danger Felling with a two-man saw. A falling tree, a kicking butt or a dead branch shaken loose from above kills. Plan the fall, clear an escape path at 45° behind the stump, call before the tree goes, and never work under a hung-up tree (Firewood and Coppicing, Forestry and Tree Nurseries).
- Hacksaw blades are glass-hard and can snap and fly; keep the blade tight and straight, and do not twist it in the cut.
- Dust from some hardwoods irritates lungs and eyes; work in a breeze.
What this unlocks
With these tools a workshop makes Furniture and Cupboards, Drawers, Shelves and Desks, doors and windows (Doors, Windows and Joinery, Doors, Hinges, Handles and Latches), carts (Wagons and Carriages), wooden Gears and mills, boats and Violins, Guitars and Harps. The bench and vice also serve the metalworker (Hammers, Pliers, Wrenches and Screwdrivers, Machine Tools), where the moulding plane's idea — a cutter shaped to its profile — returns in the milling machine. Powered planers, moulders and saws for a joinery shop are in Planers, Thicknessers and Woodworking Machines.
How it was first done
Roman carpenters had almost the whole kit: iron-soled wooden planes have been found at Pompeii (buried in AD 79) and across the empire, with drawknives, augers, gouges and frame saws. The brace appears in Flemish paintings from about the 1420s. Moulding planes became common tools of the joiner in the 17th and 18th centuries, and in 1769–1774 the French joiner André-Jacob Roubo published a great illustrated book on his trade, L'Art du menuisier, whose workbench design is still copied. The cap iron spread in Britain in the second half of the 18th century. Two-man crosscut saws with raker teeth were widely used in 19th-century North American logging. From the late 1850s Leonard Bailey in the United States patented the adjustable iron plane, later made by the Stanley company, which replaced most wooden bench planes.
Source: content/entries/metals/woodworkers-tools.md