If remains of the old world survive, what to take first, how to judge what still works, how to strip cars, machines and buildings for parts, which hazards of ruins kill, and why salvage runs out so that real production must start at once.

Difficulty
●●●●●
Time
Hours to search a house; a day to strip a car; a season to work through a town. The useful stock lasts years, not generations.
Steps from zero
2 prerequisites →

You need first

Stone ToolsDangerous Plants and Animals

This unlocks

—

Objects made here

salvage cache

Raw materials

scrap metal
The full path from nothing — 2 steps before this one
  1. Stone Tools
  2. Dangerous Plants and Animals
  3. Salvaging from Ruins

Do them roughly in this order. See it on the tech tree →

Note This chapter only applies if ruins of the old world survive. The rest of this book assumes you start with nothing at all, and every other chapter gives the route from raw nature. If you find no ruins, skip this chapter. If you do, it can save you years, but only if you use it to start making things, not to put off making them.

Why it matters

A ruined town is a mine that has already been dug, smelted and shaped for you. One car holds roughly 800 kg to a tonne of iron and steel, including springs of better steel than a beginner's bloomery will make for years (Iron (the Bloomery), Steel), plus about 8–22 kg of copper. A modern house can hold well over 100 kg of copper in its wires and pipes. A school library holds more knowledge than a lifetime of experiment. A packet of seeds can carry a crop that took thousands of years to breed (Saving Seed and Breeding Plants).

But salvage is a gift that shrinks every year. Steel rusts, rubber perishes, fuel goes stale, seeds die, medicines weaken and paper rots. The right use of salvage is to buy time and build the means of production: use salvaged files to make tools, salvaged books to teach, salvaged seed to start fields, salvaged magnets and wire to start making electricity. Then make your own.

How it works: what lasts and what does not

Take first what dies fastest and matters most.

Item How long it stays useful (roughly) What to do
Seeds in packets or sacks 1–5 years for most crops kept cool and dry; onion and parsnip die fastest (1–2 years); beans and squash keep 3–6 Collect at once. Test them. Plant this season and save your own seed (Farming from Seed)
Medicines Tablets kept dry often keep most of their strength years past the date; liquids, injections, insulin and eye drops spoil fast Collect, sort, label; let a trained person decide (Pharmacy: Tablets, Capsules, Ointments and Inhalers)
Petrol (gasoline) 3–6 months; ethanol blends less Treat as a fire danger, not a fuel
Diesel, kerosene 6 months to 2 years if sealed Settle and filter; use for lamps, rust-proofing, lubricating (Lubricants and Greases)
Canned food Usually safe as long as the can is sound; quality falls after 2–5 years (1–1.5 years for acid foods like fruit and tomatoes) Check every can (below)
Rubber, tyres, hoses, belts 5–10 years outdoors before cracking Take seals and belts early (Rubber, Packing, Gaskets and Seals)
Batteries Lead-acid dies within months if left flat; lithium cells fade Mostly scrap for lead; see Dangers
Paper and books Centuries if dry; weeks if wet Move dry books to a dry store first; dry damp ones at once
Timber, thin steel sheet Decades under a roof; years where roofs leak Check for rot and rust-through (Rot, Woodworm and Termites)
Glass, stone, brick, pottery, copper, brass, stainless steel, aluminium, lead Centuries Take when you need it

So the order of a first salvage season is: seeds, medicines and food; then books, tools and cloth; then metal, glass and building materials as you need them.

What you need

  • A partner, always, to go for help, hold the rope and watch the roof.
  • Strong boots, thick gloves, long sleeves against glass, nails and torn sheet metal, and a wetted cloth mask (or a real dust mask, if found) against dust, mould and droppings.
  • Rope of 15–20 m for safety lines and lowering loads (Knots, Lashings and Rigging), and a 2–3 m pole to test floors and ceilings from a distance.
  • Pry bar, hammer, saw, screwdrivers and spanners, usually found in the first garage you search; bags, baskets or a handcart (Baskets and Containers, The Wheel and Axle).
  • Charcoal or paint to mark searched buildings, a tally board or notebook to list what was found (Records, Bookkeeping and Accounts), water, and a small first-aid kit (Wound Care and Antiseptics).

Where to find it

Looking for Best places
Seeds Garden stores, farm sheds, silos and barns (grain is seed), kitchens (dried beans, peas, lentils and whole grains sprout)
Books Libraries, schools, hospitals, workshops. Textbooks of chemistry, physics, medicine, farming and engineering; dictionaries; maps (Libraries and Preserving Knowledge, Maps and Mapmaking)
Hand tools Garages, sheds, workshops, building sites, farms, hardware stores
Steel Car and lorry springs, files, saw blades, chisels, drill bits, axles, shafts, chains, wire rope, fence wire, reinforcing bar in concrete
Copper Electric cable and wiring, motor windings, transformers, water pipes, hot-water tanks, car radiators of older vehicles
Bearings and gears Car wheel hubs, gearboxes, bicycles, washing machines, fans, pumps, factory machines (Bearings and Lubrication, Gears)
Magnets Loudspeakers, computer hard drives, motors of cordless tools and treadmills, bicycle dynamos, some washing machines (Permanent Magnets)
Glass and lenses Jars and bottles, windows, mirrors, cameras, binoculars, spectacles, projectors, microscopes in schools (Lenses)
Cloth, containers Houses, shops, hospitals; pots, pans, buckets, drums and water tanks (Tins, Cans, Drums and Tanks)
Medical supplies Pharmacies, clinics, hospitals, vets, first-aid boxes in vehicles and workplaces

Before you go in, look. Walk round the outside. Look for leaning walls, sagging roofs, cracks wider than a finger, missing floor sections seen through windows, and signs of animals. Mark each searched building at the door with a cross, the date and any danger ("ROOF BAD").

Step by step

1. Judge what still works

  • Hand tools. Surface rust is fine; deep pits on a cutting edge are not. A file that still "bites" a nail with a clean scratch is good. Tap a hammer or axe head with metal: a clear ring means sound; a dull clunk means a crack. Reject mushroomed or cracked heads, which throw splinters. Clean with sand and oil; re-handle as in Hammers, Pliers, Wrenches and Screwdrivers.
  • Steel for toolmaking. Car leaf and coil springs are spring steel of roughly 0.5–0.9% carbon; files are about 1% carbon. Grind a corner and look at the sparks: bright, bursting, branching sparks mean high-carbon steel; long plain streaks mean mild steel (Rubbish, Recycling and Reuse, Axes, Chisels, Knives and Planes).
  • Rope and webbing. Fibres that are powdery or snap between your fingers mean rotten rope, however whole it looks. Never trust it to hold a person until a length has held twice the load it must carry (Knots, Lashings and Rigging).
  • Rubber. Bend it double. Fine cracks on the bend mean it is perished.
  • Bearings. Spin by hand: smooth and quiet is good; grinding, rough spots or play means worn. Wash out old grease with kerosene and repack (Lubricants and Greases).
  • Electric motors. Turn the shaft: it should spin freely with no grinding. Blackened, burnt-smelling windings are scrap copper. A permanent-magnet motor (from cordless tools, treadmills and some fans) makes electricity when you spin it; test it with a small bulb across its terminals (The Generator, The Electric Motor).
  • Seeds. Do a germination test now, not at planting: sprout 10 (or better 100) seeds on a damp cloth, kept warm, moist and covered, and count after 1–2 weeks. Over 85 in 100 is good; under 70, sow thickly and test again; none at all means dead (Granaries and Food Storage).
  • Canned food. Discard any can that is bulging, leaking, deeply rusted, dented on the seam, that spurts when opened, or that smells wrong. Never taste food to test it (Canning and Bottling). For medicines, see Dangers.

2. Strip a car

Gas strut high pressure: never cut or heat Side windows toughened: use whole, cannot be cut Airbags and belt reels (SRS) small explosive charges: leave alone Windscreen laminated: lifts out Battery 10 kg lead, acid Alternator 14 V generator Coil springs spring steel Fuel tank vapour explodes: no saw, no heat Wiring harness copper wire Wheel bearings one in each hub; axles too Take Take with great care Leave alone
Fig. 1 Useful parts of a car, and the parts to leave alone. Springs, bearings, glass, wire, alternator and seat belts are prizes. Airbags, gas struts, the fuel tank and the battery acid can kill or maim.

Work on level ground, with the car on its wheels or on solid blocks, never on a jack alone.

  1. Make it safe first. Remove the battery (below). Do not touch the airbags (marked "SRS" or "AIRBAG" on the steering wheel centre, dashboard, seat sides and roof pillars) or the seat-belt reels: both contain small explosive charges that can fire if heated, cut or hit. Take everything around them.
  2. Battery. A 12-volt lead-acid battery holds about 10 kg of lead and strong sulfuric acid. Keep it upright and put it in the hazard store (The Rechargeable Battery, Rubbish, Recycling and Reuse).
  3. Wiring harness. Cut and pull every bundle of wires. (Copper Wire).
  4. Alternator. The belt-driven generator on the front of the engine. It makes about 14 volts DC when turned fast, roughly 1,500–2,000 turns a minute or more, and most need a battery connected to excite their field. It is the quickest route to charging batteries from a The Waterwheel or Wind Turbines (Storing Energy).
  5. Springs. Leaf springs (stacks of curved steel plates on older cars and lorries) and coil springs. A coil spring under a car is still compressed when the car is on its wheels: only remove it with the suspension fully hanging, or leave it.
  6. Wheels, hubs and bearings. Each hub holds a sealed bearing. Axles and driveshafts are good, tough steel.
  7. Glass. The windscreen is laminated (two layers of glass with plastic between) and comes out whole if you cut round the rubber or glue. Side and rear windows are toughened glass that bursts into small cubes if scratched hard or cut; they cannot be cut to size, only used whole.
  8. Seat belts (cut the webbing, leave the reels), seat fabric and foam, mirrors, lamps and lenses, hoses, tools, the jack.
  9. Body and small motors. Sheet steel for roofing and pans (Sheet Metal and Rolling); starter, wiper and window motors for copper and magnets. Leave the fuel tank and everything joined to it; see Dangers.

3. Strip machines and appliances

  • Washing machines: motor, bearings, a stainless steel drum, springs, belts, hoses.
  • Refrigerators and freezers: the cabinet is a ready insulated box (Cooking Ranges, Iceboxes and Vacuum Flasks); the copper or aluminium tubing and compressor can be cut out outdoors, away from any flame, letting the gas escape. Some old ones used ammonia: if you smell it, stand back upwind.
  • Bicycles: take whole. A bicycle is transport, a store of chain, bearings and wheels, and a pedal drive for a grindstone or generator (The Bicycle).
  • Electronics: hard drives hold two very strong magnets; loudspeakers have magnets and copper; power supplies have transformers (Resistors, Capacitors and Coils).
  • Clocks, scales and instruments: keep working ones whole as patterns for your own (The Mechanical Clock, Balances, Steelyards and Weighing Machines).

4. Strip buildings

Work from the top down and the outside in, and only in buildings that pass the look test above.

  1. Contents first: books, tools, cloth, containers, glassware.
  2. Wiring: switch nothing on. Assume any cable could be live if it connects to solar panels or a battery bank (see Dangers). Pull wire from walls and ceilings.
  3. Pipes: copper pipe (red metal) and old lead pipe (dull grey, soft, bends easily, scratched bright with a knife). Lead is useful but poisonous; wash hands after handling (Lead).
  4. Windows and doors: lift out glass whole by cutting or chipping the putty or seal round the edge. Hinges, locks and handles.
  5. Roof sheets, gutters and timber: from the ground or a sound scaffold, never by walking on a fragile roof (Scaffolding and Ladders).
  6. Bricks and stone: bricks laid in soft lime mortar knock clean; bricks in hard cement mortar mostly break (Stone Masonry).

5. Build a salvage cache

Roof overhang 50 cm or more Seeds + medicines, sealed Books wrapped, off floor Metals sorted one bin per metal Raised floor 30 cm, air below Tools cleaned, oiled, on pegs Inventory board every item, in and out Hazard store batteries, fuel, chemicals Fe Cu Pb Al at least 20 m away
Fig. 2 A salvage cache. Raised off the ground, roofed and dry, with seeds and medicines high and sealed, books wrapped, tools oiled, metals sorted low, and dangerous things kept in a separate store well away.
  1. Site: high, well-drained ground above any flood, close to home; a sound room or a new hut (Shelter, Cob, Adobe and Rammed Earth).
  2. Floor: raised at least 30 cm on stones or posts, with an air gap below, so damp and rats stay out (Granaries and Food Storage).
  3. Roof with an overhang of at least 50 cm, and walls that keep out rain and animals.
  4. Seeds: in sealed glass jars or tins, each labelled with crop, place found, date and germination result, on the highest, coolest shelf, out of sun.
  5. Medicines: sealed, labelled, dry and dark, in a locked box, away from children.
  6. Books and papers: wrapped in cloth or oiled paper, on shelves off the floor and away from walls.
  7. Tools: cleaned and wiped with oil or fat, hung on pegs so every gap shows what is missing.
  8. Metals: sorted into separate bins by type (iron and steel, spring steel, copper, brass, aluminium, lead, stainless) (Rubbish, Recycling and Reuse).
  9. Inventory: a written list of every item, where it came from and who took it out (Records, Bookkeeping and Accounts, Organising a Community).
  10. Hazard store: a separate small shed at least 20 m away, for batteries, fuel, old chemicals and anything you are unsure of, with a raised lip at the door so spills stay inside, as in Rubbish, Recycling and Reuse.

How to tell it worked

  • Within the first season the seeds are tested and stored, the medical supplies sorted, and the best books dry.
  • Every item is on the list and can be found in a minute; nothing is rusting, mouldy or chewed; nobody has been badly hurt.
  • You have started making things yourself: a garden from your own seed, fire without matches, pots, cordage, a forge using salvaged steel.

Note Troubleshooting. Seeds did not come up → dead with age, or eaten; check the germination test, sow thicker, and look for grain in barns and silos. Tools rust in the store → damp: raise the floor, mend the roof, oil them again, add ventilation under the eaves. Rats in the store → seal gaps with sheet metal, raise the floor on posts with metal collars (Household Pests). People take from the store without telling → write rules, keep the list at the door, and have two keepers check it (Laws, Courts and Settling Disputes). Salvaged motor will not make power → it is an induction motor (most mains appliance motors), which needs outside excitation; look for permanent-magnet motors or a car alternator instead.

Dangers

Danger Radiation symbol: leave it alone. The three-bladed trefoil, often on yellow, marks a radioactive source: in hospitals (Radiotherapy (Overview)), laboratories, factories, and the gauges used on building sites and pipelines (often in small yellow carrying cases). Never open, break, carry or keep one. Some are metal capsules no bigger than a pen top that burn the skin within minutes and give a deadly dose within hours if handled or carried in a pocket. In 1987 in Goiânia, Brazil, scrap collectors opened such a capsule from an abandoned clinic; the glowing powder inside was passed around as a curiosity, and four people died. Also leave alone smoke detectors (do not open them; they contain a small radioactive source), luminous dials on old watches and aircraft instruments, and anything from a ruined power station (Nuclear Energy (Overview)). Back away, wash, change clothes, mark the place with a clear warning that a stranger will understand, record it on your map, and tell everyone. See Detecting Radiation.

Danger Bad air in sealed spaces. Cellars, tanks, sewers, wells, silos and closed garages fill with carbon dioxide, carbon monoxide or hydrogen sulfide (rotten-egg smell that soon stops being noticed), or simply lack oxygen. A person can collapse in a few breaths. A burning candle does not prove the air is safe: these gases can kill while a flame still burns. Never go down into a well, pit, tank or cellar on a held breath to rescue someone: the rescuer dies too. Ventilate for a long time first, go in only on a rope with people at the top able to haul you out, and stay out if in any doubt (Mining and Tunnelling, Wells and Cisterns).

Danger Collapse. Old roofs, floors and walls fail without warning. Stay out of buildings with sagging roofs, leaning or bulging walls or cracks wider than a finger. Walk close to walls where floor joists are supported, test floors ahead with a pole, never stand under a hanging load, and never walk on roof sheets or skylights: you will fall through. Work in pairs, one person outside.

Danger Fuel and gas: no heat, no sparks. A fuel tank, drum or can that has held petrol is most dangerous when nearly empty: the vapour inside explodes if a saw, grinder, hot tool or spark touches it. Never cut or heat a fuel tank, drum, gas bottle or aerosol can. Leave gas bottles where they are; corroded ones can burst. Gas struts (the cylinders that hold up car bonnets and tailgates) and shock absorbers hold high pressure: never cut or heat them.

Warning Asbestos. Any building built or refurbished before about 2000 may contain asbestos: grey corrugated cement roof sheets on garages and sheds, pipe lagging, boiler insulation, insulating boards, old floor tiles, textured ceilings, and the brake pads of old cars. Its dust causes lung disease and cancers 20–40 years later. Do not break, saw, drill or sweep it dry. Leave it in place, or wet it, wrap it and bury it whole in a marked place (Rubbish, Recycling and Reuse).

Warning Lead paint, arsenic timber and poisons. Paint on buildings from before about 1980 often contains lead. Never sand or burn painted wood, and keep children away from paint flakes. Greenish treated fence posts and decking contain arsenic and chromium: never burn them (Arsenic). Farm stores, garden sheds and pool rooms hold pesticides, weedkillers and pool chlorine: some poison through the skin, and pool chlorine mixed with acid or ammonia gives off poisonous gas (chlorine or chloramine) (Chlorine and Bleach). Never mix, sniff or taste unknown chemicals, or reuse their containers for food or water. Mercury is in old thermometers, switches and fluorescent tubes (Mercury).

Warning Old medicines. Tablets kept dry and cool often keep most of their strength for years after the date printed on them, but not always, and some are dangerous. Throw away any medicine that is discoloured, damp, crumbly, stuck together or smells odd; all liquids, injections, insulin and eye drops past their date; and any tetracycline-family antibiotic that has turned brown (old breakdown products were reported to damage the kidneys). Never guess a dose from a label you cannot read. If a trained health worker exists, let them decide; see Pharmacy: Tablets, Capsules, Ointments and Inhalers and Antibiotics Beyond Penicillin.

Warning Electrical stored energy. Solar panels make electricity whenever light falls on them, and battery banks stay charged for years: treat any cable connected to them as live (Solar Cells, Wiring and Electrical Safety). Microwave ovens contain a capacitor that can hold a lethal charge for a long time after power is gone; leave the inside of a microwave alone, and do not break the ceramic in its magnetron (some contain beryllium oxide, whose dust is very toxic). Lithium batteries that are swollen, crushed or shorted can burst into flame (Lithium Batteries).

  • Cuts and tetanus. Torn sheet metal and broken glass cause deep, dirty wounds. Wear gloves and boots, clean every wound well, and know the signs of tetanus (Wound Care and Antiseptics).
  • Animals and disease. Ruins shelter rats, feral dogs, snakes, bats and wasps (Dangerous Plants and Animals). Do not sweep up droppings dry: soak them with 0.5% bleach solution or hot soapy water first, as in Household Pests. Floodwater in basements is sewage.
  • The dead. Handle bodies with gloves and bury them downhill and well away from water (Caring for the Dead).

Why salvage runs out

Salvage is a store, not a source: nothing refills it. Three traps catch groups that live on it:

  1. The stock runs out. Seeds die within a few years, fuel within months, rubber within a decade. Steel lasts, but tools wear out and the best pieces go first.
  2. The skills never come. If everyone scavenges, nobody learns to make fire without matches, fire pottery, smelt iron or save seed. When the last matches are gone, the group is worse off than one that started from nothing.
  3. The wrong things are kept. A car without fuel is a store of steel, glass and copper, not a vehicle.

So start real production at once, alongside salvage:

What this unlocks

Sorted scrap feeds Metal Casting, Axes, Chisels, Knives and Planes and Rubbish, Recycling and Reuse; salvaged lenses start Spectacles and the The Microscope. See Where to Start: The First 100 Days, Year and Decade for the order in which to rebuild once the salvage is safely stored.

How it was first done

In Late Bronze Age Europe, around 1000 BC, smiths gathered broken axes, swords and scrap into hoards for remelting; one such hoard at Isleham in England held more than 6,000 pieces of bronze. In Britain after the Romans left, people took stone from abandoned forts and towns, and an Old English poem known as The Ruin (copied in the 10th century AD) marvels at broken Roman buildings as "the work of giants". In Rome itself, the Colosseum served as a quarry for centuries after an earthquake in 1349 brought down part of its outer wall. In the world wars of the 20th century whole nations collected scrap metal, rags and paper, and the Goiânia accident of 1987 showed the cost of salvage done blindly.