◆ Rebuild

Part 3 · Metals

The Blast Furnace and Cast Iron

A tall stone furnace blown day and night by water-powered bellows gets hot enough to melt iron. It pours liquid iron by the tonne — to be cast into pots, stoves, gears and engine cylinders, or refined into wrought iron at a scale the bloomery could never reach.

Difficulty
●●●●●
Time
A season to build; a week to blow in; then it runs day and night for months
Steps from zero
17 prerequisites →

You need first

Iron (the Bloomery)The WaterwheelFirebrick and Refractories

This unlocks

Chimneys, Stoves and HeatingBoilers and Pressure VesselsStirling and Hot-Air EnginesWater Turbines and Hydroelectric PowerPots, Pans and KettlesCooking Ranges, Iceboxes and Vacuum FlasksBalances, Steelyards and Weighing MachinesBellows to Air CompressorsHydraulic Presses and RamsAnvils, Trip Hammers and Power HammersSteel in Quantity
The full path from nothing — 17 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Hunting and Trapping
  7. Basic Woodworking
  8. Charcoal
  9. The Kiln
  10. Hides and Leather
  11. Bricks
  12. The Wheel and Axle
  13. Firebrick and Refractories
  14. Bellows
  15. Gears
  16. Iron (the Bloomery)
  17. The Waterwheel
  18. The Blast Furnace and Cast Iron

Do them roughly in this order. See it on the tech tree →

Why it matters

A good bloomery smelt gives you 2 or 3 kg of iron after a long day's work (see Iron (the Bloomery)). A modest charcoal blast furnace of the 1700s, 8 m tall, made 1–2 tonnes a day, every day, for months on end. That is the difference between iron as a precious metal and iron as a building material.

The blast furnace makes iron liquid. Liquid iron can be poured into moulds to make things the hammer cannot: cooking pots, kettles and stoves, firebacks and grates, water pipes, gear wheels, rollers, anvils, machine frames, and the great cylinders of the The Steam Engine. The same iron, refined in a finery or puddling furnace, becomes wrought iron in quantity for bars, rails, chain and plate; blown with air in a converter, it becomes steel by the tonne. Every industrial society has been built on the blast furnace.

Be honest about what it takes. A blast furnace needs water power, a mountain of ore, a forest's worth of Charcoal, fireclay and good stone, and a crew working in shifts around the clock. It is the work of a whole community, and the first ones will fail.

How it works

The bloomery stays below the melting point of iron on purpose. The blast furnace does the opposite.

  1. Taller and hotter. The shaft is several times taller than a bloomery, and a powered blast drives far more air through it. The charcoal in front of the tuyeres burns at 1,500 °C or more.
  2. Carbon soaks in. The ore is reduced to solid iron high in the shaft, as in a bloomery. But it then sinks slowly through metres of glowing charcoal, and the hot iron absorbs carbon — up to 3–4.5%. This lowers its melting point from 1,538 °C to about 1,150–1,200 °C.
  3. It melts. The high-carbon iron melts, trickles down through the charcoal, and collects as liquid in the hearth at the bottom, under a layer of liquid slag.
  4. Limestone makes the slag. In a bloomery, the sand in the ore makes slag by stealing iron from the ore, so half or more of the iron is lost. In a blast furnace, limestone is added. It burns to lime, and the lime combines with the sand and charcoal ash to make a slag of calcium silicate instead. Almost all of the iron in the ore ends up in the metal.
  5. It never stops. Ore, charcoal and limestone are tipped in at the top; liquid slag and iron are drawn off at the bottom. The furnace runs continuously for a campaign of months, until its lining wears out.
Gas burns at the topcarbon monoxide: deadly Stackkept full of charcoal, oreand limestone; ore reducesand soaks up carbon Boshwidest part Fireclay lininginside a stone stack Slag Liquid iron pig bed in dry sandwaterwheel Tap holeopened every8–12 hours Charging bridgefrom the hillside Bellows seen from above: the sow and the pigs
Fig. 1 The blast furnace in cross-section. Charges go in at the top; the blast from water-powered bellows enters through the tuyere; iron melts and collects in the hearth, under the slag, and is tapped into a bed of sand.

What cast iron is like

The iron that comes out is pig iron — so called because the channels of sand it was run into looked like a sow suckling piglets. It is very different from wrought iron:

Property Cast iron Wrought iron (from the bloomery)
Carbon 2–4.5% under 0.1%
Melts 1,150–1,200 °C — can be cast 1,538 °C — cannot be melted in a simple furnace
Under the hammer Crumbles at any heat — cannot be forged Forges and welds beautifully
Strength Strong in compression, weak and brittle in pulling and bending Tough; bends before it breaks
Hardness Grey iron: can be filed and cut. White iron: glass-hard Soft

There are two kinds, and you can tell them by breaking a pig:

  • Grey iron: the carbon has formed tiny flakes of graphite; the broken face is dark grey and grainy. It can be filed, drilled and turned on the The Lathe, casts into thin, detailed shapes, and damps vibration — ideal for pots, stoves, gears and machine frames. It comes from a hot-running furnace and slow cooling.
  • White iron: the carbon stays combined with the iron; the broken face is silvery white and crystalline. It is glass-hard and brittle. It comes from a cooler furnace or fast cooling, and is the best iron for fining into wrought iron. Casting against an iron mould (chilling) makes a white, wear-proof skin on rolls.

Cast iron shrinks by about 1% as it cools — 10 mm in every metre. Patterns must be made that much oversize (see Metal Casting).

What you need

Item Amount Notes
Iron ore, roasted and broken About 2–2½ tonnes per tonne of iron, for ore with 40–50% iron See Finding and Identifying Ores
Charcoal Roughly 1½–3 tonnes per tonne of iron 3–10 cm pieces, strong and dry. See Charcoal
Limestone, broken Roughly 1 part to every 4–8 parts of ore, adjusted by watching the slag See Lime
Stone Hundreds of tonnes For the outer stack
Refractory lining Fireclay bricks, or blocks of fine quartz sandstone See Firebrick and Refractories
Water power A wheel of 5–15 kW Driving two bellows. See The Waterwheel
Bellows Two great bellows 4–6 m long, worked alternately by cams See Bellows
Tuyere Iron or copper nozzle, or fireclay; spares
Casting floor A level bed of dry sand in front of the hearth
Tools Long iron tapping bars, rakes, clay plugs on sticks, ladles, shovels, charging baskets
People Two or three per shift at the furnace, around the clock; many more cutting wood, burning charcoal, mining and carting

The forest problem. Charcoal is about one-fifth of the weight of the wood it is made from, so each tonne of iron needs roughly 8–15 tonnes of wood. A furnace making a few hundred tonnes a year needs thousands of tonnes of wood every year — the sustainable yield of a very large area of managed woodland (see Firewood and Coppicing). Plan the forest before the furnace. This is exactly why ironmasters later turned to Coal and Coke, made into coke.

Where to find it

  • Ore: as for the bloomery — red hematite, black magnetite, brown bog iron and grey siderite (see Finding and Identifying Ores). The blast furnace can use poorer, sandier ores than the bloomery, because the limestone, not the iron, takes up the sand. Roast it and break it to 2–5 cm lumps; screen out the fines.
  • Limestone: pale rock that fizzes with vinegar (see Lime). Break it to the size of the ore.
  • Lining: fireclay for bricks (pale clay that stays pale when fired), or a fine-grained, almost pure quartz sandstone that does not crack in the fire — early ironmasters searched for good "firestone" quarries. Test a block by heating it to a white heat in the forge: it must not crack apart, melt or slump.
  • The site: a steep bank beside a stream. Build the furnace against the foot of the bank, so you can wheel charges across a short bridge from the top of the bank to the top of the furnace, and the stream can turn the bellows wheel at the bottom.

Building the furnace

Part First, small furnace Full-size charcoal furnace
Height, hearth floor to top 4–5 m 7–9 m
Widest inside diameter (the bosh) 1–1.2 m 2–2.5 m
Inside diameter at the top (the throat) 0.5 m 0.7–1 m
Hearth, inside 40 × 40 cm, 80 cm deep 50–60 cm square, 1–1.5 m deep
Tuyeres 1 1–2
  1. Foundation. A solid stone platform on firm ground, with drains underneath. Damp under the hearth turns to steam and can wreck it — or explode.
  2. The stack. A thick, square, tapering stone tower bound with iron bars or timbers, with a work arch at the front for tapping and a tuyere arch at the side for the blast pipe.
  3. The lining. Inside, build the shaft of fireclay brick or firestone: the hearth at the bottom; above it the bosh, widening upward at about 60–70°; then the long stack, narrowing gently to the throat, so the charge can settle without sticking.
  4. Leave a gap of 10–15 cm between lining and stack, filled with dry sand or broken stone, so the lining can expand without bursting the stack.
  5. The hearth front. Close the bottom of the front of the hearth with a heavy dam stone whose top is a little below the tuyere, leaving a notch for slag to run over. The tap hole is at the very bottom, beside the dam, plugged with clay. A tymp stone above the front of the hearth holds back the charge.
  6. The tuyere goes through the side wall, sloping slightly down, its tip just inside the hearth wall, about 60–80 cm above the hearth floor.
  7. The bellows. Two great bellows side by side feed the tuyere. Cams on the waterwheel shaft press each down in turn, as in a trip hammer (see Sheet Metal and Rolling), and counterweights lift them, so the blast never stops. Later, blowing cylinders (pistons in tubs) give a stronger blast (see Bellows to Air Compressors).
  8. Dry it for weeks, then keep small wood fires going in the hearth for several days.

Step by step: running the furnace

  1. Blow in. Fill the furnace with charcoal and start the blast gently. Over several days, add charges with only a little ore and limestone, increasing the ore slowly as the hearth gets hotter. Rushing this freezes the hearth.
  2. Charge. Keep the furnace full to the top. Each time the charge sinks, tip in a basket of charcoal, then the measured ore and limestone — in a full-size furnace, about every half hour. Write down every charge and every tap.
  3. Watch the blast. Through a sight hole at the back of the tuyere, the fire must be dazzling white.
  4. Watch the slag. Slag runs over the dam continuously, or is drawn off every hour or two, into a channel of sand. Good slag is runny, and cools to a glassy light grey, green or blue. Black, heavy slag means iron is being lost into it: the furnace is too cold or carrying too much ore. Put less ore on each charge until it clears. Stiff, stony slag that won't flow means too much limestone, or too little.
  5. Prepare the pig bed. On the dry sand floor in front of the work arch, mould a main channel (the sow) leading away from the tap hole, and short side channels (the pigs) branching off it like the teeth of a comb, each about 1 m long and 10–15 cm wide and deep. Warm and dry the sand thoroughly.
  6. Tap. Every 8–12 hours, when the hearth is full, clear the slag, then drive a long iron bar into the clay plug of the tap hole. White-hot iron gushes out, spitting stars of sparks, and runs down the sow into the pigs. When the hearth is empty and the blast starts to blow out of the tap hole, push in a ball of wet clay on the end of a stick to plug it again.
  7. Break and sort. When cool, break the pigs from the sow with a sledgehammer. Break a pig and look at the fracture: grey for casting, white for fining.
  8. Keep going. A good furnace runs for months. When the hearth lining has worn through, blow out: stop charging, let it burn down, cool it, and reline it.

Casting

Large castings can be poured straight from the furnace into moulds in the casting floor. For smaller work, remelt pig iron:

  • In a crucible, in a powerful charcoal forge, for castings of a few kilograms (see Metal Casting).
  • In a cupola: a small shaft furnace about 50–60 cm across inside and 2–3 m tall, lined with fireclay, with a tuyere near the bottom and a tap hole below. Charge it with layers of charcoal (or coke) and broken pig iron, with a little limestone, and blow hard. It melts iron at a steady rate for as long as you charge it. Every later foundry used one.

Mould in dry sand or loam (see Metal Casting). Cast iron rules:

  • Keep walls at least 5–6 mm thick, and as even as possible. Thin sections cool fast and turn white and brittle; sudden changes of thickness crack.
  • Round every inside corner.
  • Allow 1% for shrinkage.
  • Pour hot and fast, at a white-yellow heat that runs like water, and let the casting cool slowly in the mould, overnight for anything large.

Refining cast iron into wrought iron

Finery hearth Puddling furnace Pig of white iron pushed in above the blast Blast burns out the carbon Loop pasty lump of soft iron, 30–50 kg firebox (coal) fire bridge molten pig iron, stirred: it "boils" Low roof throws flame down rabble to chimney
Fig. 2 Two ways to burn the carbon out of pig iron. In the finery, pig iron melts drop by drop through an air blast. In the puddling furnace, the flame passes over molten iron that is stirred by hand, so the fuel never touches the metal.

The finery forge

  1. Build an open hearth like a large forge (see Blacksmithing), 60–80 cm across, with a strong water-powered blast angled down into it.
  2. Fill it with charcoal and push the end of a pig of white iron into the fire above the tuyere.
  3. The pig melts drop by drop, and each drop falls through the blast, which burns out most of its carbon. The refined iron no longer melts at this heat; it collects in the bottom as a pasty, spongy lump.
  4. The finer lifts the lump back into the blast two or three times until it is all soft iron.
  5. Lift out the loop (30–50 kg) and hammer it under the water-powered hammer (see Anvils, Trip Hammers and Power Hammers), like a bloom. Reheat and draw it into bars.

It takes roughly 1⅓–1½ tonnes of pig iron, and a great deal of charcoal, for each tonne of bar.

Puddling

In 1784 Henry Cort found a way to refine iron with coal, which ruins iron if they touch.

  1. Build a reverberatory furnace: a firebox at one end, a low wall (the fire bridge), and a shallow hearth lined with iron oxide (roasted ore or hammer scale), all under a low arched roof that reflects the flame down onto the hearth.
  2. Melt 200–250 kg of pig iron on the hearth.
  3. The puddler stirs it through a small door with a long hooked bar. The carbon burns: the bath boils, with little blue flames of carbon monoxide.
  4. As the carbon goes, the iron "comes to nature" — thickens into pasty grains.
  5. The puddler gathers it into balls of 30–40 kg, which are hammered and rolled into bar.

Each two-hour heat is brutal work. Puddled iron built the railways, bridges and ships of the 1800s.

How to tell it worked

  • It runs. Liquid iron flows from the tap hole like water, white-hot, throwing sparks.
  • The fracture and the file. Grey, grainy iron that a file bites; or silvery, glittering white iron that a file skates on. Neither bends.
  • Castings come out sharp, without holes or cracks, and ring when tapped. A dull sound means a hidden crack.
  • Refined iron from the finery or puddling furnace forges and welds, bends cold, and breaks with a fibrous grey fracture, like good bloom iron.

Note Troubleshooting. Black slag; little iron → furnace too cold or overloaded with ore. Lighten the ore on each charge; check the blast. Hearth "freezes" — iron and slag set solid → blast failed, or too much ore, wet charge or too fast a blow-in. Keep the blast going at all costs; carry spare bellows leather and cams. A frozen hearth often means tearing the furnace down. Charge "hangs" and then drops suddenly → too many fines. Screen them out; keep charge sizes even. Iron all white and hard → furnace running cold or overloaded with ore. Lighten the ore. Iron brittle when red-hot after fining → sulfur. Use charcoal, not raw coal, in the blast furnace and finery. Castings full of holes → damp moulds, or no vents for the gas. Dry moulds thoroughly; vent them. Castings cracked → uneven wall thickness or sharp corners; cooled too fast. Redesign and cool slowly.

Dangers

Danger Molten iron and water. A cupful of water trapped under molten iron turns in an instant to steam well over a thousand times its volume, and throws white-hot iron in every direction. Every mould, ladle, tool, pig bed and floor must be bone dry and warmed before it meets the iron. Never tap or pour in the rain without a roof. Never stand where a splash can reach you; wear leather and wool, never anything that melts, and wear high boots.

Danger Furnace gas. The gas leaving the top of a blast furnace is mostly carbon monoxide and nitrogen. It kills quickly and without warning, especially on the charging platform and at the top of the shaft. Never lean over the throat; work upwind; keep the charging area open to the wind; and treat headache, dizziness or confusion as an emergency — get the person out into fresh air immediately.

Danger Hangs, slips and breakouts. A hung charge that suddenly drops can blow a jet of flame and burning charge out of the top. A worn hearth can burst and pour iron across the floor. Keep the area round the furnace clear of people who don't need to be there, and inspect the lining between campaigns.

What this unlocks

Cast iron gives you Gears, cylinders and frames for the The Steam Engine, The Lathe beds and Machine Tools, rolls for Sheet Metal and Rolling, cooking pots and stoves, water pipes, and the rails and chairs of early Railways. Refined, it gives wrought iron in quantity for Nails, Rivets and Wire Fasteners, chain, boiler plate and bridges. Blown with air in a converter, or melted with scrap in an open hearth, pig iron becomes Steel in Quantity. Burning coke instead of charcoal (see Coal and Coke) frees the furnace from the forest.

How it was first done

Chinese ironworkers were casting iron by the 5th century BC, more than 1,500 years before anyone in Europe; they cast tools, pots and moulds in quantity, and refined cast iron into wrought iron by stirring it in an open hearth. Around AD 31 the official Du Shi is recorded as building water-powered bellows for iron furnaces in China. In Europe, the oldest known blast furnaces, such as Lapphyttan in Sweden, date from roughly the 12th–14th centuries, and the technique spread slowly; the first English blast furnace was built at Newbridge in Sussex in 1496. In 1709 Abraham Darby at Coalbrookdale in England smelted iron with coke instead of charcoal, and his works cast thin-walled iron pots in sand. Henry Cort's puddling furnace (1784) and James Neilson's hot blast (1828) made iron cheap and plentiful, and the Iron Bridge at Coalbrookdale, cast in 1779, showed the world what the new material could do.

Source: content/entries/metals/cast-iron.md