◆ Rebuild

Part 2 · Earth and Fire

Ball Mills, Crushers and Grinders

Machines that break rock, clinker, ore, coal and grain into gravel, sand and flour — the jaw crusher, roll crusher, hammer mill, stamp mill and edge runner, the ball mill and the small jar mill — and the sieves and air classifiers that sort what comes out. Grinding is the hidden half of cement, metal, glaze, paint and food.

Difficulty
●●●●●
Time
A day to make a jar mill on rollers; a few weeks to build a stamp mill or edge runner; one to three months to pattern, cast and machine a jaw crusher or ball mill
Steps from zero
19 prerequisites →

You need first

Portland CementBearings and Lubrication

This unlocks

Ore Dressing: Jigs, Tables and Flotation
The full path from nothing — 19 steps before this one
  1. Fire
  2. Stone Tools
  3. Cordage and Rope
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Basic Woodworking
  7. Hunting and Trapping
  8. The Kiln
  9. Charcoal
  10. Pottery
  11. Hides and Leather
  12. Lime
  13. The Wheel and Axle
  14. Portland Cement
  15. Bellows
  16. The Lathe
  17. Copper Smelting
  18. Bronze
  19. Bearings and Lubrication
  20. Ball Mills, Crushers and Grinders

Do them roughly in this order. See it on the tech tree →

Why it matters

Almost every mineral must be broken small before it is any use. Ore is crushed to free the metal grains from the rock (Finding and Identifying Ores); cement clinker is useless until it is flour (Portland Cement); glaze, enamel and paint must be finer than talc (Glazes, Enamel on Metal, Pigments, Paints and Varnish). By hand, with hammerstones and a quern, one person grinds a few kilograms a day. These machines grind tonnes — and since grinding eats most of the energy of a mine or cement works, the right machine for each step saves months of labour.

How it works

Break it in stages. No single machine takes a 30 cm rock to flour. Each machine handles a reduction ratio — the size going in divided by the size coming out — of about 4 to 20:

Stage Size in → out Machine
Primary crushing 300 mm → 50 mm Jaw crusher
Secondary crushing 50 mm → 5–10 mm Roll crusher, hammer mill, stamps
Grinding 10 mm → 0.1 mm (sand to flour) Ball mill, edge runner, millstones
Fine grinding 0.1 mm → 0.01 mm Ball or jar mill, long running

Squeezing (jaws, rolls) suits hard brittle rock; striking (hammers, stamps) suits coal, limestone, grain and bone; rubbing and rolling (balls, edge runners, millstones) makes fine powders.

Finer costs much more. Grinding sand to flour takes many times the energy of crushing rock to gravel. So never grind finer than the job needs, and take out what is already fine with a sieve or classifier and send only the oversize back: closed circuit.

Wet grinding (about equal weights of water and solids) is faster and dustless. Grind dry only when the product must stay dry, as with cement and flour.

What you need

The jaw crusher

rock in gape Fixed jawribbed wear plate Setbottom gap crushed rock falls out Swing jawnip under 25° Pivot shaft Eccentricshaft and flywheel Pitmanrises and falls Front toggle Rear toggleweak on purpose Springand tie rod
Fig. 1 The jaw crusher in section. An eccentric shaft lifts and drops the pitman; the two toggle plates straighten and fold, pushing the bottom of the swing jaw a few millimetres toward the fixed jaw on each turn. Rock is nipped in the V-shaped gap and works its way down until it falls out through the gap at the bottom, the set. A spring and tie rod pull the jaw back.

The jaw crusher breaks quarry rock to fist size between two heavy plates in a V, one fixed and one swinging a few millimetres with enormous force, hundreds of times a minute. A lump is nipped, cracked, drops lower, is cracked again, and falls out of the gap at the bottom.

Parts (the Blake type, still the standard):

  • Frame: a box of cast iron or cast steel, open top and bottom.
  • Fixed jaw: a wear plate bolted to the front of the frame.
  • Swing jaw: hung from a shaft at its top, with a wear plate on its face. Both plates are ribbed lengthwise, and reversible end for end so a worn plate gets a second life.
  • Pitman: a heavy rod hung on an eccentric shaft, rising and falling 10–25 mm each turn.
  • Toggle plates: one from pitman to frame, one from pitman to the foot of the swing jaw. As the pitman rises they straighten and push the jaw forward — a huge lever that turns a small push into many tonnes.
  • Tie rod and spring pull the jaw back; flywheels each side carry it through each blow.

Proportions for a small works crusher:

Size (gape × width) 250 × 400 mm 100 × 150 mm (laboratory)
Biggest lump 200 mm 80 mm
Set (bottom gap) 20–50 mm 3–15 mm
Throw at the set 8–12 mm 3–5 mm
Speed 250–300 rpm 300–350 rpm
Power 10–15 kW 1.5–3 kW
Output 5–15 tonnes an hour 100–300 kg an hour

The nip angle between the jaws must be no more than about 20–25°, or lumps squirt upward instead of being gripped. The gape should be about 1.2 times the biggest lump. Change the set by fitting longer or shorter toggles, or by packing shims behind the rear toggle seat.

The safety link. Make the rear toggle plate deliberately the weakest part, of cast iron. If a hammer head or a drill bit falls in, the toggle snaps instead of the frame. Keep spares.

The simplest version. Before you can cast a frame, a hand-worked lever crusher does the same job slowly: a hardwood beam 2–3 m long, hinged at one end, carrying a stone or iron jaw 30 cm from the hinge, drops onto a fixed jaw. Two people lifting the far end crack rocks to fist size faster than hammering.

Good versus bad. A good jaw crusher takes a steady feed without stalling, and the product is cubic, not slabby. Slabs mean the set is too wide or the plates are worn smooth; violent knocking means a loose toggle seat.

The stamp mill

Before engines, ore and quartz were crushed by stamps: heavy upright beams lifted by cams and dropped. They need no casting bigger than a shoe and run on a The Waterwheel (The Watermill, Cranks, Cams and Linkages).

  1. Stamps: square timbers 15–20 cm thick and 3–4 m long, each shod with an iron shoe of 15–30 kg, 50–150 kg in all, held upright in timber guides in rows of three to five. (Later iron stamps weighed 300–450 kg.)
  2. Cams on the wheel shaft catch a tappet collar on each stamp, lift it 15–25 cm and drop it, 50–100 times a minute, staggered so they fall one after another.
  3. Mortar box: a heavy box with an iron die under each shoe; water flows through and leaves by a screen of punched sheet that passes only what is fine enough.

A 50 kg wooden stamp crushes a few hundred kilograms of hard ore a day to coarse sand; a 400 kg iron stamp, 2–4 tonnes. Stamps are noisy, almost unbreakable, and ideal for gold ore before panning (Gold and Silver).

The roll crusher

Crushing rolls Fixed roll400–900 mm across Sprung rollsprings let trampiron pass spring gap sets the size Feedlumps under D ÷ 25 + gap Hammer mill Feed Breakerplate Hammersswing free Gratesets the size Rotor50–90 m/s at the tips
Fig. 2 Left: a pair of crushing rolls. The rolls turn toward each other; one runs in fixed bearings, the other is held by heavy springs so a lump of iron can pass. The largest lump that will be gripped is about one twenty-fifth of the roll diameter plus the gap. Right: a hammer mill. Swinging hammers on a fast rotor shatter the feed against the breaker plate; it leaves when it is small enough to fall through the grate.

Crushing rolls are two heavy cylinders turning toward each other, drawing material in and squeezing it. They give an even product with little dust: ore, coal and clinker, and cracked grain and malt (Grain, Flour and Bread, Beer, Wine and Cider).

  • Rolls: chilled cast iron, or steel tyres shrunk on cast-iron centres, 400–900 mm across; smooth for hard rock, fluted for coal and grain.
  • Bearings: one roll fixed, the other in sliding bearings held by heavy springs, so tramp iron pushes it back and passes.
  • Drive: a belt to each roll, surface speed 2–5 m a second for rock, slower for grain. Spread the feed across the full width, or the rolls wear grooves.

The size rule. Smooth rolls grip a lump only if it is small compared with the rolls: the largest lump is about one twenty-fifth of the roll diameter, plus the gap. Rolls of 600 mm take lumps of about 25 mm. Bigger lumps ride on top and chatter. The reduction ratio is only about 3 or 4 to 1, so use two pairs in series for a big reduction.

Good versus bad. Even product, quiet running, no lumps bouncing on top. Flats or grooves worn in the faces mean uneven feed: true them on a lathe (The Lathe).

The hammer mill

A hammer mill is a fast rotor carrying loose, swinging hammers inside a heavy casing. Material is smashed and thrown against a ribbed breaker plate again and again until it is small enough to escape through the grate round the bottom. The grate sets the size, from 10 mm gravel to coarse meal.

  • Rotor: discs 300–600 mm across on a shaft, with rods through their edges carrying the hammers, which swing back from anything too tough to break.
  • Hammers: hard steel bars about 10 × 50 × 150 mm, holed at both ends so they can be turned and used four times. Weigh them and hang equal sets opposite each other; an unbalanced rotor shakes itself apart.
  • Speed: tip speed 50–90 metres a second — a 500 mm rotor at 2,000–3,000 rpm. Faster makes finer.

Hammer mills are excellent for coal, limestone, gypsum, bone, dry clay, salt, grain and animal feed (Fodder Crops and Winter Feed, Compost and Manure). They are poor for hard, sharp rock like quartz or granite, which wears hammers away in hours.

Good versus bad. Steady hum and an even product. A rising rumble means a broken or worn hammer and lost balance: stop at once.

The edge runner

The edge runner (chaser mill) is a heavy wheel rolling round a circular pan; turning round a centre, it twists as it rolls, so it rubs as well as crushes. The animal-powered version is in Oils and Pressing and Animal Power and Treadwheels. For mineral work, use two wheels of granite or chilled cast iron, 1–1.8 m across, 30–40 cm wide and 1–4 tonnes each, set at different radii to cover the whole pan, at 15–30 turns a minute. Scrapers turn the material back under the wheels; for clay, part of the pan floor is a grating of 3–6 mm slots that lets finished material fall through. Edge runners grind clay and grog (Bricks, Firebrick and Refractories), mortar, pigments and clinker — slowly, but they tolerate anything.

The ball mill

Ball mill, end section Lineriron, or flint Shoulderballs leavethe wall Balls 40–50%material fillsthe gaps Toeballs land, grind Too slowballs slide Right65–75% of critical Too fastballs cling Jar mill, end view porcelain jar, lid clamped on Pebbles: half the jarslurry to three-quarters Rollersrubber-covered about ½ jar diameter Beltfrom motor
Fig. 3 Left: the inside of a ball mill turning at the right speed. Balls are carried up the rising side and cascade down, tumbling over each other and grinding the material between them. Too slow, and they only slide; too fast, and they cling to the wall and do no work. Right: a jar mill — porcelain jars lying on two long rollers, one roller driven by a belt.

The ball mill is a drum, about half full of hard balls, slowly turning on its side. The balls are carried up one side and tumble down, grinding the material between them by rolling and rubbing. It is the workhorse of fine grinding: cement, ore, glaze, paint, enamel frit, ferrites and powders for Powder Metallurgy.

Critical speed

Turn a drum too fast and the balls are pinned to the wall by their own swing and never fall. The speed at which this happens is the critical speed:

critical speed (turns a minute) = 42.3 ÷ √(inside diameter in metres)

Run the mill at 65–75% of critical. Examples:

Inside diameter Critical Run at
0.15 m (small jar) 109 rpm 70–80 rpm
0.3 m 77 rpm 50–58 rpm
1 m 42 rpm 28–32 rpm
2 m 30 rpm 20–22 rpm

Charging it

  • Balls: fill 40–50% of the inside volume with balls.
  • Material: enough to fill the gaps between the balls and just cover them. For wet grinding, about equal weights of solids and water, so the slurry runs like thin cream.
  • Ball size: the coarser the feed, the bigger the balls. For 5–10 mm feed, a mix from 25 to 60 mm; for sand-size feed or a glaze, 12–25 mm. Small balls grind fine; big balls break lumps.

Building one

  1. Drum: steel plate riveted or welded into a cylinder (Sheet Metal and Rolling) with cast heads. A first mill is 0.6–1 m across and as long as it is wide; a cement tube mill is up to four times as long as wide.
  2. Lining: white cast iron or manganese steel plates for ore and cement. For glaze and paint, where iron stains, line it with flint or porcelain blocks set in cement and use flint pebbles: a pebble mill.
  3. Trunnions: hollow axles on the heads, in big bearings (Bearings and Lubrication). Feed through one and overflow through the other, or load batches through a hatch.
  4. Drive: a girth gear and pinion (Gears), or a belt round a small drum. Allow about 10–15 kW per tonne of balls.

Batch grinding times are long: 4–12 hours for a glaze, 12–24 hours for a fine pigment or a ferrite powder (Permanent Magnets).

The jar mill

The jar mill is the small version, for a workshop, pottery or laboratory. A lidded jar lies on two parallel rollers, one driven; the jar turns by friction.

  1. Jars: thick stoneware or porcelain (Stoneware and Porcelain), 1–20 litres, with a wide mouth and a lid clamped on over a leather or rubber gasket (Rubber). Fire them well vitrified so they do not wear away.
  2. Rollers: two steel tubes or hardwood rollers covered with rubber or leather, as long as two or three jars, set apart about half the jar diameter, on ball or bronze bearings.
  3. Drive: a belt or a small motor to one roller, geared so the jar turns at 65–75% of its critical speed: work out the roller speed from the ratio of jar to roller diameters.
  4. Media: half the jar's volume of flint pebbles or porcelain balls 10–25 mm across. Make porcelain balls by rolling clay balls by hand and firing them with your ware.
  5. Charge: material and water up to about three-quarters of the jar, leaving a quarter empty for the balls to fall through.

The simplest version: any strong barrel or stoppered stoneware jar with a handful of flint pebbles, rolled to and fro on the floor by foot or turned on a spit by a water wheel. It works, slowly.

Good versus bad. Listen. A good mill roars and rattles evenly as the balls cascade. Silence means it is too full, too fast or too thick; a sharp clatter means too little charge, and the balls are just wearing each other.

Sieves and classifiers

Sieves

A sieve sorts by size. Woven wire cloth is described by its mesh — the number of openings per 25.4 mm (one inch). Approximate openings:

Mesh Opening Feels like
4 4.75 mm Pea gravel
10 2 mm Coarse sand
40 0.42 mm Fine sand
100 0.15 mm Gritty flour
200 0.075 mm Smooth flour; standard for cement and ore
325 0.045 mm Talc
  • Hand sieves: cloth in a wooden or iron hoop 30–45 cm across, shaken in a circle or washed through. A stack, coarsest on top, shaken for 10 minutes and each layer weighed, gives a sieve analysis.
  • Shaking screens: a sloping deck 1–2 m long rocked 200–300 times a minute by an eccentric, oversize running back to the crusher. A trommel is a slowly turning, tilted cylinder of screen doing the same.
  • Lawns for glaze and slip: silk or phosphor-bronze cloth of 80–200 mesh (Slip Casting, Jiggering and Ceramic Factories).

Air classifiers

Below about 0.1 mm, sieves clog and become slow. Instead, let air or water do the sorting: small grains fall more slowly than big ones. The settling speed goes with the square of the grain size, so a grain half the size falls four times slower. Water sorting by settling is in Abrasives and Grinding Stones.

The simplest air classifier is a long, low wooden box or tunnel with a centrifugal fan (Centrifugal Pumps and Fans) at one end. Dribble the powder into the air stream near the blower. Coarse grains drop at once; finer ones are carried farther along before they fall; the finest float out of the far end into a cloth bag or a cyclone (Pneumatic Conveying and Tube Post). Collect from bins along the floor, each a different grade.

The mechanical separator used in cement works: powder falls onto a spinning plate inside a tall drum, which flings it out; a fan on the same shaft draws air upward. Coarse grains fall back down a cone and return to the mill; fines are carried over and settle in an outer cone. Changing the fan blades changes the cut. Run with a ball mill in closed circuit, it can double the mill's output, because the mill no longer regrinds powder that is already fine.

Choosing for the job

Job Line of machines Target
Ore Jaw crusher → rolls or stamps → wet ball mill → concentrate (Ore Dressing: Jigs, Tables and Flotation, Finding and Identifying Ores) Fine enough to free the metal grains, often 65–200 mesh
Cement Hammer mill or rolls for raw stone; ball or tube mill for clinker with gypsum, plus separator (Portland Cement) 85–90% through 200 mesh
Glaze and enamel Jar or pebble mill, wet, 4–12 hours (Glazes, Enamel on Metal) All through 100–200 mesh lawn
Pigment Edge runner or ball mill, then muller (Pigments, Paints and Varnish) Smooth on the teeth
Food and feed Millstones or roller mills for flour (The Watermill, Grain, Flour and Bread); hammer mill for feed Never in a mill used for ore

Warning Keep food mills for food. A mill that has ground lead ore, glaze or pigment holds poisonous dust in every crack. Never use it for grain, salt, sugar or medicine.

How to tell it worked

  • Rub test: a pinch rubbed between finger and thumb. Gritty = coarser than about 100 mesh; smooth like flour = about 200; slippery like talc = finer. Between the teeth you can feel grit down to about 0.02 mm.
  • Sieve analysis: weigh 100 g, wash it through a 200-mesh sieve, dry and weigh what stays. Record it for every batch.
  • Output by the hour: weigh what comes out in an hour; a sudden fall means worn plates, a slipped belt, or a wrong ball charge.

Note Troubleshooting. Jaw crusher stalls or chokes → feed too fast, or wet clay packing the jaws; screen out fines before the crusher. Lumps bounce on top of rolls → feed too large for the roll diameter; crush smaller first. Hammer mill product too coarse → worn hammers or grate; turn the hammers or fit a finer grate. Ball mill grinds slowly → speed too far from 65–75% of critical, too few balls, or slurry too thick (add water) or too thin. Product stained grey → iron worn from balls and liner; use flint or porcelain, or take the iron out with a magnet.

Dangers

Danger Silica dust kills slowly. Grinding quartz, flint, sand, granite and clay makes fine dust that scars the lungs over years (silicosis) and leads to tuberculosis. Grind wet wherever you can, keep floors wet and swept with water, enclose dry mills and draw the dust away with a fan to a cloth bag filter outdoors, and wear a close-fitting mask of many layers of fine cloth — better, a proper respirator. Dust you can see in a sunbeam is already too much.

Danger Dust explodes. Fine flour, sugar, coal, starch, sulfur and many metal powders, stirred into air and lit by a spark or hot bearing, explode with force enough to flatten a building. Keep these mills and their dust clean, ground all metal parts, keep flames out, and put a magnet in the feed to catch iron that could strike a spark.

  • Crushing and nip points: jaws, rolls, belts and gears take a hand in a moment. Guard them; never reach into a running crusher, and lock out the power before clearing a jam.
  • Flying rock from jaw crushers and stamps: wear eye protection and keep people away from the feed opening.
  • Noise: hammer mills, stamps and ball mills deafen. Plug your ears with wax and wool.
  • Poisons: lead, arsenic, mercury and copper ores and pigments make poisonous dust (Lead, Arsenic). Grind them wet.

What this unlocks

Crushing and grinding make every later mineral industry possible: Portland Cement and Mortar and Concrete, ore dressing for Copper Smelting, zinc and tin, refractories and grog (Firebrick and Refractories), fine porcelain bodies (Stoneware and Porcelain), glazes, enamels, paints, magnetic ferrites (Permanent Magnets), metal powders (Powder Metallurgy), and phosphate fertilisers (Chemical Fertilisers). Fine, pure silica ground in a flint-lined mill is the start of Fused Quartz and Halogen Lamps.

How it was first done

Grindstones and pounding stones are as old as humanity. The Greeks and Romans crushed olives in the trapetum, a kind of edge runner, and Romans used water power to drive hammers and mills. Georgius Agricola's De re metallica (1556) shows water-driven stamp mills crushing ore across central Europe, with sieves and washing tables beside them. In 1858 Eli Whitney Blake in New Haven, Connecticut, patented his jaw crusher to make road stone, and it spread to mines worldwide within a decade. Hungarian millers developed steel roller mills for flour in the mid-1800s. Ball mills came into use in the later 1800s; in the 1890s the Danish firm F. L. Smidth made the long tube mill, filled with flint pebbles, that became the standard way to grind cement. Air separators for cement followed in the early 1900s.

Source: content/entries/earth/mills-and-crushers.md