◆ Rebuild

Part 15 · Knowledge and Science

Polarised Light

Light can be sorted so that all its waves shake in one direction. With a slanted black glass, a pile of thin plates or a crystal of Iceland spar you can make such light, and with it see hidden strain in glass, tell one mineral from another in a slice thinner than paper, and measure how much sugar is dissolved in a juice.

Difficulty
●●●●●
Time
An afternoon for a black-glass polariscope; a week to cut a Nicol prism and build a sugar polarimeter
Steps from zero
18 prerequisites →

You need first

Optical Glass and Achromatic Lenses

This unlocks

Flat Screens: LCD and LED Displays
The full path from nothing — 18 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Hunting and Trapping
  7. Basic Woodworking
  8. The Kiln
  9. Pottery
  10. Charcoal
  11. Hides and Leather
  12. Lime
  13. Lye and Potash
  14. Glass
  15. Bellows
  16. Lead
  17. Lenses
  18. Optical Glass and Achromatic Lenses
  19. Polarised Light

Do them roughly in this order. See it on the tech tree →

Why it matters

Ordinary light can be sorted so that every wave in a beam shakes in the same direction, like a rope shaken only up and down. The eye cannot tell such polarised light from ordinary light, yet it reveals things that are otherwise hidden:

How it works

Light is a wave that shakes across its direction of travel. In sunlight or flame light the shaking direction changes at random, so all directions are mixed. A polariser lets through only the part shaking in one direction.

Put a second polariser (the analyser) behind the first and turn it. The light dims, and at a right angle the field goes dark: the polarisers are crossed. In between, the brightness follows the square of the cosine of the angle (Malus's law): at 45° half the light gets through. Anything put between crossed polarisers that changes the light makes the dark field light up again. That is the whole trick of the chapter.

There are three ways to make a polariser from natural things:

  1. Reflection. Light reflected from glass or water at a slant is partly polarised. At one angle, Brewster's angle, the reflected light is completely polarised, shaking parallel to the surface. For ordinary glass (refractive index 1.52) it is 56.7° from straight on, so the ray meets the glass at about 33° to its surface. Glare off water and wet roads is polarised the same way.
  2. A pile of plates. At the same angle, each glass surface reflects away about 15% of the light shaking the "wrong" way and almost none of the other. Ten to fifteen thin plates in a stack, tilted so the light meets them at 33° to their surface, remove most of the wrong light; what comes through is well polarised.
  3. Crystals. In most crystals light travels at two speeds, depending on its shaking direction, so a ray splits into two rays polarised at right angles. This is double refraction (or birefringence). Clear calcite, called Iceland spar, does it so strongly that you see a double image through it. Some crystals, like brown or green tourmaline, also absorb one of the two rays, so a thin slice is a polariser by itself.

Why things light up. A birefringent slice between crossed polarisers splits the light into two parts, one lagging behind the other; when they recombine at the analyser some light gets through. Because each colour has its own wavelength, a large lag shows as interference colours: grey, white, yellow, red, blue, green, then paler repeats. Glass and water stay dark unless stress squeezes the glass, which makes it slightly birefringent.

Turning the light. Quartz cut across its axis and solutions of sugar rotate the direction of polarisation as the light passes, in proportion to how much they contain. Cane and beet sugar turn it to the right (clockwise, looking towards the light); fruit sugar turns it left.

1. Reflection 2. Pile of plates 3. Double refraction 33° Black glass light meets it at 33° to the surface reflected light: polarised 12–15 thin plates each surface reflects away some of the wrong half light through: mostly polarised ordinary extraordinary One dot is seen as two Iceland spar ordinary light: all directions mixed shaking in the page shaking across the page
Fig. 1 Three ways to polarise light. Left: light reflected from black glass at 33 degrees to its surface is fully polarised. Middle: light passing a slanted pile of thin glass plates loses most of the wrong half at each surface. Right: a calcite rhomb splits a ray into two rays polarised at right angles, so a dot seen through it appears double.

What you need

Item For Notes
Plate glass, two pieces about 10 × 15 cm Black-glass polariser and analyser Any flat glass. Paint the back black, or use dark bottle glass ground flat (Glass).
Thin glass plates, 12–15, about 4 × 5 cm Pile-of-plates analyser Microscope slide glass or thin blown and flattened sheet; clean and unscratched.
Iceland spar, a clear rhomb at least 2 × 2 × 5 cm Nicol prism See below. Smaller pieces work for a double-image analyser.
Canada balsam Cementing prisms and thin sections Clear resin from balsam fir; it sets to a glass with nearly the same refractive index as glass (1.54).
Corundum or emery powder, coarse to fine Grinding prisms and rock slices See Abrasives and Grinding Stones.
Lampblack in varnish Blackening glass backs and tube insides Soot from a smoky flame stirred into oil varnish (Pigments, Paints and Varnish).
Glass tube, 15–25 mm bore, 20 cm long Sugar polarimeter Ends ground square and flat (Laboratory Glassware).
Salt Yellow sodium light for the polarimeter A pinch on a wick or in a spirit flame.

Where to find it

Iceland spar is clear, colourless calcite (calcium carbonate). It grows in veins and cavities in limestone and in gas holes in old basalt lava (the famous mine in eastern Iceland is in basalt). Tests: it fizzes with acid; a knife scratches it easily (hardness 3); it always breaks into rhombs, slanted boxes with faces meeting at about 75° and 105°; and laid on a printed line it shows two lines, one of which walks around the other as you turn the crystal. Only clear pieces without cracks or milky clouds are useful; most calcite is cloudy.

Tourmaline forms long grooved crystals with a rounded triangular section, in coarse granite veins (pegmatites) with quartz, feldspar and mica. It scratches glass. Brown and green crystals make the best polarisers; black ones are too dark.

Selenite, clear gypsum, splits into thin sheets like mica but a fingernail scratches it (Gypsum and Plaster of Paris).

Canada balsam is drained from blisters on the bark of the balsam fir. Elsewhere, clear pine or fir resin thinned with a little turpentine, then cooked until a drop sets hard when cool, is a fair substitute (Ether, Acetone and Solvents).

Method 1: The black-glass polariscope

  1. Make the polariser. Paint the back of a 10 × 15 cm glass plate with lampblack varnish, two coats. The black stops the back surface from reflecting, so only the clean front surface works.
  2. Build the base. Lay the black glass flat in a shallow wooden tray about 20 × 30 cm. Stand the tray on a table facing a bright window or an open sky, or a white wall lit by the sun.
  3. The viewing arm. At the near end of the tray, fix a wooden arm that holds a tube of blackened card, 4–5 cm across and about 20 cm long, pointing down at the middle of the black glass at 33° to its surface. Cut a wooden wedge to set the angle. Looking down the tube you should see the bright sky reflected in the glass.
  4. The stage. Across the lower end of the tube, square to it, fix a small shelf of clear glass. Specimens lie or stand on it, in the polarised beam.
  5. The analyser. At the eye end, fit a pile of plates: 12–15 thin, clean glass plates stacked together in a short square card tube, blackened inside, and tilted inside it so that the light meets them, too, at 33° to their surface. Mount the pile in a ring so it turns about the line of sight.
  6. Find the crossed position. With nothing on the stage, turn the analyser until the field is darkest. Mark that position. Turn it 90° and the field is brightest.

Using it. Lay a glass object on the stage with the analyser crossed. Well-annealed glass stays as dark as the empty field. Strained glass shows grey or white patches, or coloured bands if bad; a disc cooled too fast shows a dark cross with light between its arms. Put the glass back in the annealing oven and cool it more slowly (Glass, Optical Glass and Achromatic Lenses).

The sensitive tint plate. Split a flake of selenite with a knife point until, laid on the stage at 45° to the polarisers, it shows an even deep magenta-purple — that is the first-order red, and the flake is about 0.06 mm thick. Fix it between two thin glass plates with balsam. Laid under a specimen, it shows even strain too faint to show grey, as blue on one side and yellow on the other.

Bright sky or a white wall in sun 33° 33° Black glass, lying flat painted black on the back Specimen Stage clear glass, square to the tube Analyser 12–15 thin plates, light meets them at 33°; turns Card tube black inside Wooden strut sets the 33° slope Eye
Fig. 2 The black-glass polariscope. Light from the sky meets the black glass at 33 degrees to its surface and leaves it polarised, rising through the specimen on the stage. The eye looks down the tube through a pile of thin plates, also met at 33 degrees, which can be turned to the crossed (dark) position.

Photoelastic models

Make a stiff jelly of 15% gelatine in water (Glues and Adhesives) and cast it in a tray as a slab 1.5–2 cm thick. When set, cut a model of a beam, a hook or a plate with a hole. Stand it on edge in the polariscope (or hold it between two polarisers in front of a bright window) and press on it. Bright and dark bands appear. Where the bands crowd together, the stress is greatest; that is where the real part will crack first. Rounding a sharp corner, or adding material there, spreads the bands.

Method 2: The Nicol prism

For a straight-through polariser that gives a truly black field, needed for the polarimeter and the microscope, cut a Nicol prism from Iceland spar.

  1. Choose the rhomb. A clear cleavage rhomb roughly three times as long as it is wide, for example 1.5 × 1.5 × 4.5 cm. Split it to shape by setting a knife blade along the cleavage and tapping.
  2. Grind the ends. The natural end faces make an angle of about 71° with the long edges. Grind each end on a glass plate with medium then fine emery and water until the angle is 68°. Calcite is soft; grind gently, flat, and with little pressure.
  3. Saw it in two. Cut the rhomb along the long diagonal, through the obtuse corners, so that the cut is at right angles to the new end faces. Use a thin copper or iron strip charged with emery, or a fine saw, and go slowly; calcite splits easily along cleavage planes and will spoil. Grind both cut faces flat and polish them (Gem Cutting and Lapidary).
  4. Cement. Warm the halves, spread a thin layer of Canada balsam on one cut face, press the halves together in their original position, squeeze out bubbles, and let it harden for a few days.
  5. Blacken the long sides and mount the prism in a cork-lined tube.

One ray meets the balsam so slantwise that it is totally reflected into the blackened wall; the other passes straight through, completely polarised.

Quick substitutes. A clear calcite piece over 1 cm thick behind a pinhole card gives two images of the pinhole; block one, and the other is perfectly polarised over a small field. Or saw a slice about 1 mm thick from a brown or green tourmaline crystal, parallel to its length, and polish both faces: it polarises on its own, though its colour tints the view.

Ordinary light all directions mixed 68° Blackened side absorbs the reflected ray Ordinary ray totally reflected at the balsam Canada balsam layer along the sawn diagonal Iceland spar, two halves about 3 times as long as wide Extraordinary ray passes, fully polarised
Fig. 3 The Nicol prism. A long rhomb of Iceland spar is sawn along its diagonal and cemented back with Canada balsam. One ray is reflected aside at the balsam and absorbed by the blackened wall; the other passes straight through, completely polarised.

Method 3: Identifying minerals in thin section

Making a thin section

  1. Saw or chip a flat piece about 2 × 3 cm and 3–5 mm thick from the rock.
  2. Grind one face flat on an iron or glass plate with coarse, then medium, then fine emery and water. Wash between grades so no coarse grain is carried on.
  3. Cement the flat face to a glass slide with hot Canada balsam, cooked on the slide until a drop taken out on a pin snaps when cold. Press out every bubble.
  4. Grind the exposed side down, coarse at first and fine for the last part, until the slice is 0.03 mm thick — about a third of a hair. You judge it by the quartz in it: check often in the polariscope or a microscope with polarisers; when the quartz grains show grey to white and no brighter colours, you are there. Yellow quartz means it is still too thick.
  5. Cover it with a thin glass cover slip in balsam.

Reading it

Use the The Microscope with one polariser below the stage and one in or above the eyepiece, crossed. Turn the slide on the stage and watch each grain:

What you see between crossed polarisers Likely mineral
Stays black however you turn it Glass (volcanic or slag), garnet, fluorite, rock salt, other cubic minerals
Grey to white, goes black four times in a turn Quartz or feldspar (feldspar often shows stripes of light and dark)
Bright blues, reds, greens Mica, olivine, many dark minerals
Pale pinky-cream colours of very high order, and lines of cleavage in two directions Calcite or dolomite
Black and opaque even with one polariser Ore minerals: pyrite, magnetite, galena — examine these by reflected light

The same test sorts gems from glass: a stone that stays dark through a full turn is glass, garnet, spinel or diamond; one that blinks bright and dark four times is a crystal such as quartz, ruby or topaz.

Method 4: The sugar polarimeter

Building it

Fix everything to one straight board about 50 cm long, in this order along the line of sight:

  1. Sodium lamp. A spirit flame with a pinch of Salt on a loop of iron wire held in it, or a wick soaked in brine. It gives a strong pure yellow light. Use this, not daylight: the rotation is different for each colour, and white light gives a coloured field you cannot set accurately (The Spectroscope).
  2. Polariser. A Nicol prism in a holder, fixed. A small lens in front of it, about 5 cm from the flame, makes the beam roughly parallel.
  3. Tube holder. Two wooden V-blocks to cradle the sample tube.
  4. Analyser. A second Nicol prism in a tube that turns in a collar. On the turning part fix a pointer; on the fixed collar a divided circle marked in degrees, with a vernier reading to 0.1° if you can make one (Measuring Angles: Theodolite and Sextant, Scientific Instrument Making).
  5. Eyepiece. A low-power lens behind the analyser, focused on the far end of the sample tube.

The sample tube. A glass tube exactly 20 cm long inside (2 decimetres — the standard), 1.5–2.5 cm bore, ends ground square and flat. Close each end with a round of thin, flat, unstrained glass pressed on by a screw cap or a wooden collar with a cork washer. Check the end glasses in the polariscope first: strained glass upsets the reading.

Using it

  1. Zero. Fill the tube with clean water, close it with no air bubble, lay it in the holder. Turn the analyser until the field is darkest. Read the circle. Do it five times and take the average: that is your zero.
  2. Prepare the sample. Weigh the sugar or juice, dissolve and make up to an exact volume, for example 100 mL in a measuring flask (Laboratory Glassware). It must be perfectly clear. Cloudy juice is cleared by stirring in a little white clay or lead acetate solution and filtering; Sugar gives the lime method.
  3. Read. Fill the tube with the solution, set the analyser to darkness again, and read. Subtract the zero. The difference α is the rotation.
  4. Calculate. For cane or beet sugar (sucrose), in yellow sodium light at about 20 °C:

sugar (grams per 100 mL) = α ÷ (0.665 × tube length in decimetres)

With the standard 2 dm tube: grams per 100 mL = α ÷ 1.33.

Example: A juice sample, cleared and filled into the 2 dm tube, reads 17.3° after subtracting the zero. Sugar = 17.3 ÷ 1.33 = 13.0 g per 100 mL.

The check standard. Dissolve exactly 26.0 g of your purest white sugar, dried, in water and make up to 100 mL at room temperature. In a 2 dm tube it must read 34.6°. If it reads less, either your sugar is not pure or the instrument is out; the sugar trade's whole scale was built on this test.

Other sugars have other strengths. On the same scale on which cane sugar is +66.5, glucose (grape sugar, the sugar in diabetic urine) is +52.7, about four-fifths as strong; fructose (fruit sugar) is −92, to the left. For glucose, divide α by 1.05 instead of 1.33. Cane sugar boiled with a little acid splits into glucose and fructose ("inversion") and the reading swings left; honey reads left for the same reason.

Setting by eye. The darkest point is hard to judge within a degree; average several settings approached from both sides. Later instruments added a half-shade, a thin crystal plate over half the field, so that the eye matches two equally dim halves instead of judging darkness.

Salt flame yellow Lens Polariser Nicol, fixed Sample tube solution, glass end caps Analyser Nicol, turns against a divided circle Eyepiece 20 cm = 2 decimetres inside Light enters shaking one way and leaves turned by the sugar wooden board Eye
Fig. 4 The sugar polarimeter. Yellow light from a salt flame passes the fixed Nicol prism, a 20 cm tube of the solution, and a second Nicol prism that turns against a divided circle. The sugar turns the light, and the angle the analyser must be turned back to darkness measures the sugar.

How to tell it worked

  • Crossed polarisers go dark. Through any of your polarisers, look at glare off a table top, a pond or a window at a slant and turn it: the glare should nearly vanish at one position. The blue sky about 90° away from the sun should also darken strongly at one position.
  • The empty field is black, not grey, when crossed. A grey field means the pile has too few plates, the black glass is at the wrong angle, or there is stray light; blacken more, add plates, adjust the 33°.
  • A strip of plain glass bent in your fingers between crossed polarisers should glow white at its edges and stay dark along its middle (the neutral line).
  • The sugar check standard reads 34.6° within half a degree.
  • Without any instrument, many people can glimpse polarisation directly: look at blue sky 90° from the sun and you may see a faint yellowish bow-tie, Haidinger's brush, that fades in seconds and returns when you tilt your head.

Note Troubleshooting. Field never gets fully dark: the polariser or analyser is not polarising well; check each against glare off water. The Nicol prism shows two images: the cut angle is wrong, so both rays pass; regrind the ends to 68° and recement. Prism split during sawing: normal; saw slower, with lighter pressure, and support it in a bed of plaster. Polarimeter readings jump by degrees: bubble in the tube, cloudy sample, or the flame flickering; let the flame settle, refill. Thin section shows bright colours everywhere: still too thick; keep grinding.

Dangers

Warning Lead acetate, used to clear dark juices, is a poison that builds up in the body, and it tastes sweet, so children and animals will eat it. Never taste a sample cleared with it, never pour it where food is made, discard every such sample, and wash hands and glassware (Lead).

  • Hot balsam and turpentine catch fire easily. Heat them on a warm plate or water bath, never over an open flame.
  • Rock dust from grinding. Grind wet. Dry dust of quartz-bearing rock causes lasting lung disease.
  • Do not look at the sun through any polariser. A polariser cuts glare but not enough to protect the eye (Eye Health and Preventing Blindness).
  • Urine sugar readings are approximate, because other substances in urine also turn light a little. Use them with symptoms and other tests, never alone (Chronic Diseases).

Going further

  • The polarising microscope: a Nicol below the stage, one in the tube, a rotating stage with a degree scale, and a slot for the sensitive tint plate. It is the main tool of the geologist (The Microscope).
  • The saccharimeter with a quartz wedge. Instead of turning the analyser, a sliding wedge of quartz turned the light back; it can be read with white light and was the standard in sugar factories.
  • Finding the hidden sun. Mark the direction on your polariser that stands upright when glare off water is darkest. Aimed at clear sky overhead and turned to its darkest, that mark points towards the sun, even when it is behind cloud or just below the horizon: a fair sky compass at high latitudes (Finding Direction).
  • Polarising sheet for sunglasses and camera filters is made of stretched plastic film stained with iodine (Iodine, Early Plastics).

How it was first done

In 1669 the Danish physician Rasmus Bartholin described the double image seen through Iceland spar. In 1690 Christiaan Huygens explained it with two wave speeds. In 1808 the French engineer Étienne-Louis Malus, looking through a calcite crystal at sunset light reflected from the windows of the Luxembourg Palace in Paris, saw one of the two images vanish as he turned it: reflection polarises light. In 1811 François Arago saw colours in thin crystal plates between polarisers, and Jean-Baptiste Biot found that quartz and, in 1815, sugar solutions and turpentine rotate the polarisation. David Brewster in Scotland found the polarising angle (1815) and showed that stressed glass becomes doubly refracting (1816). William Nicol of Edinburgh made his prism in 1828; Henry Clifton Sorby in Sheffield ground rocks to thin sections and founded the microscopic study of rocks in the 1850s. Louis Pasteur, in 1848, used polarised light to show that tartaric acid crystals come in left- and right-handed forms. Sugar polarimeters, refined by Jean-Baptiste Soleil and others in the 1840s, became standard in the sugar trade, and the polarised-light study of stress models was developed by engineers in the early 1900s.

Source: content/entries/knowledge/polarised-light.md