◆ Rebuild

Part 5 · Cloth and Clothing

The Spinning Wheel

A big wheel driving a small spindle by a cord turns one slow turn of your hand into forty fast turns of the spindle. Build a great wheel first, then a treadle flyer wheel that spins and winds at the same time while both hands draft — two to three times the yarn of a hand spindle.

Difficulty
●●●●●
Time
1–2 weeks to build a great wheel; 3–6 weeks for a treadle flyer wheel; a few days to learn each
Steps from zero
5 prerequisites →

You need first

Spinning and Weaving ClothThe Wheel and Axle

This unlocks

Textile Machinery
The full path from nothing — 5 steps before this one
  1. Cordage and Rope
  2. Stone Tools
  3. Basic Woodworking
  4. Spinning and Weaving Cloth
  5. The Wheel and Axle
  6. The Spinning Wheel

Do them roughly in this order. See it on the tech tree →

Why it matters

With a hand spindle (Spinning and Weaving Cloth), spinning is the slowest step in all of cloth-making: it takes several hours of spinning to supply one hour of weaving. A household that needed clothes, sheets, sacks and sails had someone spinning in every spare moment of every day.

The spinning wheel attacks that bottleneck. It does two things a spindle cannot:

  1. It turns the spindle much faster than fingers can, and keeps it turning.
  2. The flyer wheel adds continuous winding — the yarn is spun and wound on at the same time, with both hands free to draft.

A good spinner on a great wheel makes roughly two to three times as much yarn in a day as on a hand spindle, and the flyer wheel makes fine, even yarn — especially linen — with less effort still. The spinning wheel also taught the principles — drive bands, speed ratios, flyers, bobbins — that the first spinning machines were built on (Textile Machinery).

How it works

The drive ratio

A large wheel and a small pulley on the spindle (its whorl) are linked by an endless cord (the drive band). The band moves at the same speed along both rims, so the small pulley must turn as many times faster as it is smaller:

spindle turns per wheel turn = wheel diameter ÷ whorl diameter

A great wheel 100 cm across driving a whorl 2.5 cm across has a ratio of 40 : 1. Turn the wheel once a second, and the spindle spins 40 times a second — 2,400 turns a minute. This is the same principle as a belt drive on any machine (Belts, Chains and Power Transmission, The Wheel and Axle).

Twist from the tip

On a great wheel the yarn comes off the very tip of the spindle at an angle. Each turn of the spindle, the yarn slips off the tip and gains one turn of twist. To wind on, you swing the yarn round to stand at right angles to the spindle; now it cannot slip off, and it winds on. The work goes in two phases: spin (walk back drafting, with the yarn angled off the tip), then wind on (walk forward, yarn square to the spindle).

The flyer

The flyer solves the stop-and-wind problem. The spindle shaft carries a U-shaped wooden flyer with hooks along its arms, and a loose bobbin that can turn on the shaft independently. The yarn enters through a hole in the end of the shaft (the orifice), comes out of a side hole, runs along a flyer arm via a hook, and onto the bobbin.

  • If the flyer and bobbin turned at the same speed, the yarn would only be twisted.
  • Make the bobbin turn a little slower or faster than the flyer, and the yarn is twisted and wound onto the bobbin, steadily, as fast as you let it in.

The difference is made in one of two ways:

  • Scotch tension (flyer lead): the drive band turns only the flyer. A light cord brake rubs on a groove of the bobbin, slowing it down. Tighten the brake and the yarn pulls in harder. This is the easiest to build and adjust.
  • Double drive: one long band goes round the wheel twice, once over the flyer whorl and once over the bobbin whorl. The bobbin whorl is a little smaller (by about one-sixth), so the bobbin turns faster than the flyer and winds the yarn on.

Move the yarn from hook to hook along the arm every so often to fill the bobbin evenly.

What you need

Part Great wheel Flyer wheel
Wheel 90–120 cm diameter, light rim 45–60 cm diameter, heavier rim for momentum
Axle Hardwood or iron, 2.5–3 cm, on a wooden post Same, with a crank of iron or hardwood, throw 4–6 cm
Bench (table) Plank 120–150 cm × 25–30 cm × 5 cm, on three splayed legs Plank 50–70 cm long, three or four legs, tilted
Spindle / flyer Iron spindle 25–30 cm long, tapering to a fine point, with a wooden whorl 2.5–4 cm across Flyer of hardwood, arms 10–12 cm; shaft with an 8–10 mm orifice; bobbin
Bearings Loops of braided corn husk, leather or twisted fibre in two uprights Leather pads in two uprights (maidens)
Tensioner Head slides or tilts; wooden screw or wedge Mother-of-all slides on a wooden screw
Drive band Linen or cotton cord 3–4 mm thick, spliced into a loop Same
Treadle — Board 40 × 15 cm, hinged at the front, with a footman (rod) up to the crank

Tools: axe, saw, chisels, knives, drill or auger (Basic Woodworking, Drills and Boring). A The Lathe makes round axles, whorls, bobbins and hubs far easier. A smith can make the spindle and crank (Blacksmithing).

Where to find it

Everything here is wood, cord and leather:

  • Rims and spokes: straight-grained ash, oak, hickory, maple or birch, split along the grain and dried (Basic Woodworking). Ash bends well when steamed.
  • Hub, axle, bench and posts: any strong, dry hardwood.
  • Bearings: leather (Hides and Leather) or braided corn husk, greased with tallow (hard animal fat) or beeswax.
  • Drive band: a tight two-ply linen or cotton cord (Flax, Hemp and Linen, Cotton, Cordage and Rope).

Method 1: The great wheel (walking wheel)

This is the easiest wheel to build: just a wheel, a post, a bench and a spindle. It suits short wool and cotton, spun by the "long draw".

Wheel90–120 cm Whorl2.5–4 cm Spindle Headears with greased bearings Drive band Bench3 legs yarn tothe hand THE RATIO 100 cm wheel ÷ 2.5 cm whorl = 40 1 turn a second of the wheel → 40 turns a second of the spindle Spin:yarn at 45°, slips off the tip Wind on:yarn at 90°, winds on
Fig. 1 The great wheel. One turn of the big wheel spins the small whorl forty times. The yarn comes off the tip of the spindle at an angle while spinning, and is swung square to the spindle to wind on.

Build it

  1. The bench. Make a plank 120–150 cm long. Bore three holes underneath at a slant and drive in three legs, so the top stands at about 60–70 cm. Three legs never rock on an uneven floor.
  2. The wheel post. Mortise an upright post 60–80 cm tall into one end of the bench, sloping slightly away from the spindle end. Cut a slot or fork in the top to carry the axle. The wheel's centre should end up at about chest height of the spinner.
  3. The wheel. Choose one of two ways:
    • Bent rim: split and shave an ash strip 5–6 cm wide, 8–10 mm thick, and long enough to go round (π × diameter: for a 100 cm wheel, 314 cm plus 20 cm overlap). Steam it for about an hour per 2.5 cm of thickness (Steam-Bending Wood), bend it round a circular form of pegs, and let it set for a week. Glue or peg the overlap (a long tapered scarf). Turn a hub 10–12 cm across and 12–15 cm long, bore 12–16 holes round it, and fit spokes from hub to rim, each pegged into a hole in the rim. Cut a shallow groove round the outside of the rim for the band.
    • Laced rim (charkha style, easier): fit two sets of spokes, side by side, into the hub, about 10 cm apart at their tips. Zigzag a strong cord from the tip of one spoke to the next on the opposite set, all the way round. The cord forms the rim, and the band runs in the V between them. This is how the Indian charkha is built, and it needs no steam bending.
  4. Mount the wheel on its axle in the post. Spin it: the rim must not wobble sideways by more than about 5 mm, or the band will jump off. Adjust spokes until it runs true. If it always stops in the same place, it is heavy there — add a little weight to the opposite side.
  5. The head. At the other end of the bench, fit a sliding block or a post that tilts, carrying two short uprights (ears) 8–10 cm apart. Bore a hole in each ear and fit a bearing: a loop of braided corn husk, or a ring of leather, greased.
  6. The spindle. Forge or file an iron rod 25–30 cm long and 6–8 mm thick, tapering to a fine but not sharp point at the front. (A smooth, hard, straight wooden spindle works for a start.) Fit a wooden whorl 2.5–4 cm across with a groove round it, tight on the spindle between the ears. Line the whorl up exactly with the wheel rim.
  7. The band. Run a cord round the wheel rim and the whorl and splice the ends into a smooth loop. Slide or wedge the head away from the wheel until the band is just firm. Too tight and the wheel drags; too slack and it slips.

Spin on it

  1. Tie a leader to the spindle near the whorl, wind it on, and take it out to the tip.
  2. Stand beside the wheel, left hand holding the fibre (a rolag — Wool) joined to the leader, right hand on a spoke or using a short stick (a wheel finger).
  3. Turn the wheel clockwise with one push. Hold the yarn at about 45° to the line of the spindle, so it slips off the tip each turn. Walk backwards 1–2 m, drafting the rolag out as the twist enters.
  4. When the yarn is twisted enough, give the wheel a slight backwards turn to unwind the few turns that wrap the spindle tip (backing off), then swing the yarn round to 90° and turn the wheel forward again while walking in. The yarn winds onto the spindle in a cone.
  5. Repeat. A spinner might walk many kilometres in a day at a great wheel — hence its other name, the walking wheel.

Method 2: The treadle flyer wheel

This takes more skill to build, but once working, the spinner sits, treadles with one foot, and drafts with both hands, never stopping to wind on. It is the best wheel for flax (Flax, Hemp and Linen) and long wool.

TREADLE FLYER WHEEL Mother-of-allslides totighten band Maidensleather bearings Footmancrank totreadle Treadlepress as the crank tops Wheel45–60 cm FLYER AND BOBBIN, FROM ABOVE yarn in Orifice8–10 mm, side exit Flyer armshooks guide the yarn; move it along Bobbinloose on shaft Brakemakes bobbin lag Whorlband drives it flyer turns faster than the bobbin, so the yarn istwisted and wound on at the same time
Fig. 2 The flyer wheel with Scotch tension. The treadle and footman turn the wheel by a crank; the drive band turns the flyer; a light brake on the bobbin makes it lag, so the yarn winds on as it is spun.

Build it

  1. The bench is a plank about 60 cm long, slanting, on three or four legs.
  2. The wheel is 45–60 cm across, built as above but heavier at the rim (thicker felloes — rim segments — or a wider bent rim), so its momentum carries it smoothly round. Mount it between two uprights on the bench, on an axle with a crank at one end.
  3. The treadle: a board hinged at its front edge to a cross-bar between the front legs. A footman — a light rod 50–60 cm long — joins the back end of the treadle to the crank, with a loose leather loop or hook at each end. Pressing the treadle pulls the crank down; the wheel's momentum carries it over the top. This is the crank-and-connecting-rod linkage of Cranks, Cams and Linkages.
  4. The mother-of-all: a horizontal bar on a post at the other end of the bench, with two uprights (maidens) 15–20 cm apart, each with a leather bearing. Make it slide towards or away from the wheel by a wooden tension screw (Screws, Nuts and Bolts) or a wedge, to adjust the band.
  5. The flyer. Turn a shaft 25–30 cm long and about 15 mm thick. Bore an orifice 8–10 mm wide down its front 4–5 cm, and a side hole where it exits. Carve the U-shaped flyer arms from one piece of hardwood (each arm 10–12 cm long) and fix it tight on the shaft just behind the side hole. Set 6–10 small bent-wire hooks along each arm, alternating sides. Fix a whorl (grooved pulley) 5–8 cm across to the back end of the shaft.
  6. The bobbin: a wooden spool 10–12 cm long with a hollow core, so it turns loosely on the shaft between the flyer arms, with a grooved end for the brake band. Make three or four bobbins.
  7. The brake (Scotch tension): a thin cord fixed to the maiden frame, passing over the bobbin groove, and held by a small spring (a strip of springy wood or a loop of gut) on the other side, with a wooden peg to tighten it.
  8. The band runs from the wheel to the flyer whorl. Ratio: a 50 cm wheel with a 6 cm whorl gives about 8 : 1; a 4 cm whorl about 12 : 1. Cut two or three whorls of different sizes to change speed.
  9. Smooth everything. Oil or wax the bearings. A rough hook or orifice catches the yarn.

Spin on it

  1. Tie a leader to the bobbin, lead it along the hooks and out through the orifice.
  2. Treadle slowly and evenly, about once a second. Practise treadling alone until the wheel always turns the same way, and starts again with your hand on a spoke when it stops.
  3. Join fibre to the leader. Hold back the fibre with one hand, draft forward with the other, and let the twist run into the drafted fibre — the yarn feeds in through the orifice.
  4. Adjust the brake until the yarn pulls in gently but steadily when you relax your hold. Move the yarn to the next hook every minute or two to fill the bobbin evenly.
  5. For flax, tie the line onto a distaff standing beside the wheel and keep your fingers wet (Flax, Hemp and Linen).

How to tell it worked

  • The great wheel keeps spinning for several seconds after one push, the band stays on, and the spindle tip runs without visible wobble.
  • The flyer wheel turns steadily in one direction with gentle treadling, never reverses, and the yarn draws in smoothly at a steady rate you can control with the brake.
  • The yarn is as even as or better than your spindle yarn, and you make several times more of it per hour.

Note Troubleshooting. Band jumps off → wheel wobbles, or wheel and whorl are out of line. True the wheel; move the head to line them up. Spindle slows or stops while the wheel turns → band too slack, or band slipping on a greasy whorl. Tighten the head; roughen the whorl groove. Wheel heavy and hard to turn → band too tight, or dry bearings. Loosen; grease. Yarn won't pull in (flyer) → brake too loose. Tighten slightly. Yarn snatched from your fingers → brake too tight, or whorl too small. Loosen it. Treadle wheel goes backwards → you pressed the treadle when the crank was rising. Press only as the crank passes the top; start the wheel by hand. Yarn catches → rough orifice, hook or flyer arm. Smooth it with sand, horsetail, or polish with wax.

Dangers

  • Hair and clothing can catch in a spinning flyer or wrap round a great-wheel spindle. Tie back long hair, keep scarves clear, and keep small children away from the wheel and treadle.
  • Fire. Spinners sit by the hearth for light and warmth, surrounded by dry fibre. Keep fibre and the wheel well back from open flame and sparks.
  • Strain. Hours of treadling and standing at a great wheel strain backs and legs. Alternate tasks; set the wheel and seat at the right height.

What this unlocks

Far more yarn per person: cloth for Making Clothes, sails, sacks, thread for Sewing, Needles and Thread and Knitting, Crochet and Netting, warp and weft for the The Loom. The great wheel's principle — one wheel driving several spindles — became the spinning jenny, and the flyer became the water frame and later the throstle and ring spinning frames of Textile Machinery. The same drive band and flyer ideas are used for winding wire (Copper Wire) and for making rope and twine (Ropewalks and Sailcloth).

How it was first done

The spinning wheel probably began in India, perhaps by the middle of the first millennium AD, as the charkha with a laced rim. The earliest clear pictures come from China (around AD 1035) and from the Islamic world (an illustration in Baghdad, 1237). The wheel reached Europe in the 13th century: a guild rule in Speyer, Germany, around 1280 forbade using wheel-spun yarn for warp — evidence of both its arrival and early doubts about its quality. The flyer appears in a German manuscript (the Wolfegg Housebook) around 1480 and in Leonardo da Vinci's notebooks around 1490; the treadle was added in the early 1500s. Hand spinning wheels were in nearly every rural European and American household until the mid-1800s. In the 20th century, Mahatma Gandhi made the charkha the symbol of India's independence movement, urging every Indian to spin their own cloth.

Source: content/entries/textiles/spinning-wheel.md