◆ Rebuild

Part 10 · Machines

Lubricants and Greases

Oil and grease are what let a machine run for years instead of days. How to make and judge animal, plant and mineral oils, cook tallow and lime into axle and cup grease, use graphite and soapstone where oil fails, and build the oil cans, wick and drip oilers, grease cups and grease guns that deliver them to the bearing.

Difficulty
●●●●●
Time
An afternoon to cook a batch of grease; a day to make a wick oiler or oil can; two to three days to make a drip oiler or grease gun
Steps from zero
25 prerequisites →

You need first

Oils and PressingBearings and LubricationPetroleum and Refining

This unlocks

—
The full path from nothing — 25 steps before this one
  1. Stone Tools
  2. Cordage and Rope
  3. Fire
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Simple Machines
  7. Basic Woodworking
  8. Hunting and Trapping
  9. Charcoal
  10. Pottery
  11. Farming from Seed
  12. Hides and Leather
  13. Oils and Pressing
  14. Fermentation
  15. The Wheel and Axle
  16. Bellows
  17. Distillation
  18. The Lathe
  19. Copper Smelting
  20. Iron (the Bloomery)
  21. Bronze
  22. Blacksmithing
  23. Steel
  24. Bearings and Lubrication
  25. Petroleum and Refining
  26. Lubricants and Greases

Do them roughly in this order. See it on the tech tree →

Why it matters

Every machine wears itself out where its parts rub: Bearings and Lubrication, Gears, the slides of a The Lathe, the piston of a The Steam Engine, chain links (Belts, Chains and Power Transmission), press screws, hinges. A film of the right lubricant cuts friction five to fifty times, keeps the parts cool, and nearly stops wear. Without it a cart axle smokes within a few kilometres and a dry steam-engine bearing seizes in minutes.

The bearings chapter lists the four basic lubricants. This chapter covers which oil or grease to choose, how to make it well, how to test it without instruments, and the small devices that feed it steadily to a running machine: the oil can, the wick oiler, the drip oiler, the grease cup and the grease gun.

How it works

A lubricant does three jobs:

  1. It separates the surfaces. At speed, a shaft drags oil into the narrowing gap under it and floats on a wedge of liquid thinner than a hair (Bearings and Lubrication). At slow speed and heavy load there is no wedge. The lubricant then works only as a thin layer stuck to each surface. This boundary film lowers friction but cannot stop all wear.
  2. It carries heat away. Oil does this best, because it flows through the bearing and out.
  3. It keeps out dirt and water and stops rust. Grease is better at this than oil.

Viscosity means how thick a liquid is, how slowly it flows. The rule: fast and light → thin oil; slow and heavy → thick oil or grease; hot → thicker than you think, because every oil thins as it warms.

Grease is oil held in a sponge. Cook fat with lime or soda and you make soap (Soap), which forms a tangle of tiny fibres. Stirred into oil, the fibres hold it the way a sponge holds water. A turning shaft squeezes a little oil out to lubricate; at rest the sponge soaks it back. Grease stays put, seals out dirt, and needs topping up only every few days or weeks.

Solid lubricants work where oil cannot: very slow heavy sliding, great heat, or dusty places. Graphite and soapstone are built of flat sheets of atoms that slide over one another like a pack of cards.

Grease, magnified Flow-cup thickness test Soap fibres tangled like a sponge Oil held in the gaps Pressure squeezes oil out; at rest the fibres soak it back Fill to mark exactly 50 mL 3 mm hole finger over it until you start Time it seconds to empty Spindle oil 20–40 s · machine oil 40–100 sgear and cylinder oil over 250 s
Fig. 1 Two simple ideas behind lubricants. Left: grease is a tangle of soap fibres holding oil; pressure squeezes oil out where it is needed. Right: a flow cup gives a repeatable measure of thickness, the number of seconds a fixed amount of oil takes to run out through a small hole.

What you need

Item Use From
Hard fat (beef or mutton suet tallow) Grease base Oils and Pressing, Butchery and Meat
Cattle feet Neatsfoot oil, a fine light oil Butchery and Meat
Castor, rapeseed or olive oil Plant lubricating oils Oils and Pressing
Heavy fractions of crude oil Mineral lubricating oils Petroleum and Refining
Slaked lime, lye of soda Soaps for grease Lime, Lye and Potash
Pine tar and rosin Sticky axle greases Tar, Pitch and Glue
Graphite, soapstone Solid lubricants See below
Iron kettle, 10–40 litres, and a long paddle Cooking grease Pots, Pans and Kettles
Tinplate, brass sheet and tube, glass tube Oil cans and oilers Sheet Metal and Rolling, Tins, Cans, Drums and Tanks, Glass

Where to find it

  • Hard fat: the white, crumbly suet round the kidneys of cattle and sheep. Pig fat (lard) is too soft for grease on its own.
  • Castor beans: big mottled seeds of the castor plant, a tall shrub with large star-shaped leaves, common in warm dry places. Castor oil is the thickest plant oil and clings to hot metal: the best plant oil for engines and heavy gears. The seeds are deadly poisonous (Oils and Pressing).
  • Rapeseed (colza): the yellow-flowered crop whose oil was Europe's lamp and machine oil before petroleum.
  • Crude oil: seeps, springs and wells (Petroleum and Refining).
  • Graphite: soft, black-grey, greasy mineral that marks paper, in flakes and veins in marble, schist and other old metamorphic rocks (Pencils and Chalk).
  • Soapstone: soft grey-green rock that a fingernail scratches and that feels soapy (Rocks and Minerals). Powdered, it is talc.

Oils

Animal and plant oils

Neatsfoot oil is the classic oil for clocks, sewing machines and instruments: it stays liquid in the cold and hardly gums.

  1. Saw cattle feet and shins into 5–10 cm pieces and crack the bones.
  2. Cover with water and simmer, not boil, for 8–12 hours. Skim the oil off the top.
  3. Boil the oil briefly with clean water and let it stand a day so water and dirt settle.
  4. Cold-strain: stand it at 0–5 °C (an unheated shed in winter, or an ice house, Ice and Refrigeration) for a week. The harder fats freeze into white grains. Strain the oil through felt in the cold. What passes stays liquid down to about 0 °C (Watches and Small Clocks, The Sewing Machine).

Refining plant oils. Fresh oil carries gums that turn to varnish in a bearing. Stir in 1–2% of concentrated sulfuric acid (Sulfuric Acid) for an hour in a glazed or lead-lined tub; black flakes form. Stir in an equal volume of hot water, settle for two days, draw off the oil, and wash it with hot water until the washings no longer turn red-cabbage juice red (Acids, Bases and Testing). Filter through cotton wool.

Use only non-drying oils: castor, rapeseed, olive, groundnut and animal oils. Drying oils such as linseed, hemp and walnut set hard in a bearing like paint. All animal and plant oils slowly go rancid: sour and acid, attacking bronze. Keep them cool and covered, and change them often.

Mineral oils

Lubricating oils from Petroleum and Refining do not go rancid and come in every thickness. Dewax the heavy steam-distilled fraction by chilling (Waxes: Beeswax, Plant Waxes and Paraffin) and cut it into grades:

Grade Flow-cup time (test below) Use
Spindle oil 20–40 s Textile spindles, sewing machines, small tools
Machine oil 40–100 s Lathes, line shafting, general bearings
Engine oil 100–250 s Engine crankcases (The Internal Combustion Engine)
Gear and cylinder oil over 250 s Heavy gears; steam cylinders

Cleaning. Stir raw distillate with 2–5% concentrated sulfuric acid, let the black sludge settle for a day, and wash the oil with weak soda water, then plain water. Stir in 5–10% fine bleaching clay (fuller's earth, or any pale clay dried and ground, Finding and Preparing Clay) at about 80 °C for an hour and filter. It comes out clear amber.

Compounded oil is mineral oil with 5–10% tallow or rapeseed oil. It clings to wet metal. That makes it the old steam-cylinder oil, because steam washes plain mineral oil away.

Testing oil:

  • Flow cup. Make a tinplate cup holding exactly 50 mL with a 3 mm hole in the bottom. Time how many seconds 20 °C oil takes to run out. Always use the same cup. Repeat at 50 °C to see how much it thins.
  • Flash point. Heat 50 mL slowly in an open iron cup with a thermometer in it, passing a tiny flame over the surface every few degrees. The first blue flicker is the flash point. Machine oil should flash above 180 °C, cylinder oil above 250 °C. Work outdoors, with a lid ready.
  • Gumming. Leave a smear on warm glass for a week. Good oil is still slippery.

Greases

Axle grease

For cart axles, waterwheel shafts and windmill posts, which are slow, heavy, wet and dirty:

  • Tallow and tar: melt equal weights of tallow and pine tar together and stir until smooth (Bearings and Lubrication).
  • Set grease, the black "cart grease" of a century of tins, is very sticky and does not melt in summer. Warm 100 parts heavy oil (mineral, rapeseed or fish) with 10–15 parts rosin until dissolved, and cool to about 40 °C. Stir 5 parts slaked lime into 5 parts oil to a smooth cream. Pour this into the rosin oil, stir hard for five minutes, and pour into tins at once. It sets in a few hours. Too hard: use less lime next time. Too soft: more rosin and lime.

Lime grease (cup grease)

Lime grease, also called calcium grease or cup grease, is the general grease for slow and medium-speed metal bearings, gears, pump glands and grease cups. It is smooth, yellow-brown and buttery, and water does not wash it out. It is made in two stages.

1. Make the soap 2. Thin with oil 3. Pour into tins tallow + lime milk + water simmer and stir 2–3 h until a stiff curd; keep a trace of water Oil Off the heat soap base in kettle one bucket of oil at a time, work each in before the next: ⅓ of the oil = block grease ⅔ = cup grease · all = gun grease pour at 70–80 °C lid at once against dust
Fig. 2 Cooking lime grease. First boil tallow, slaked lime and water into a stiff soap. Then thin it with oil a little at a time, stirring, until it is as stiff as you want. Pour it into tins while still warm.
  1. Weigh. Every 100 g of tallow needs about 13 g of slaked lime. For 10 kg of grease: 2 kg tallow, 260 g slaked lime, 8 kg oil (mineral, or castor or rapeseed).
  2. Make the soap. Melt the tallow in the kettle with 2 litres of water. Stir the lime into a little water to make a milk and add it slowly. Simmer and stir for 2–3 hours, adding a splash of water if it starts to catch. It thickens into a stiff curd of lime soap.
  3. Dry it, but not completely. Heat gently until steam no longer rises in clouds and the soap looks smooth and glossy. A trace of water, about 1%, must stay, or the grease later falls apart into oil and grit. Keep below 110–120 °C: a drop of water flicked on the surface should sizzle quietly, not spit.
  4. Thin with oil. Off the heat, stir in the oil one bucket at a time, working each in completely. About a third of the oil gives hard block grease; two thirds gives cup grease; all of it, a soft grease for a grease gun.
  5. Stir as it cools to 70–80 °C and pour into lidded tins.

Its limit is heat. Lime grease softens and loses its water at 80–100 °C. Use it only where you can hold your hand on the bearing.

Soda grease is made the same way with lye of soda in place of lime (Soap), with all the water boiled off. It is stringy and survives about 150 °C, so it suits wheel hubs and dynamos. But it dissolves in water: keep it out of wet places.

Lithium and other modern greases, in outline

Lithium grease is the "multipurpose grease" of modern machines. Lithium hydroxide, from spodumene or salt-lake brine (Lithium Batteries), is cooked with hydrogenated castor oil, which is castor oil hardened with hydrogen over a nickel catalyst (Hydrogen, Oxygen and Gases, Nickel and Cobalt). About 8–10% of the resulting soap is milled into mineral oil. It works from below freezing to about 130 °C and does not wash out. Add molybdenum disulfide (Molybdenum) or graphite for shock loads. Silicone grease (Silicones and Synthetic Rubbers) is for rubber seals and vacuum.

Graphite and soapstone

Graphite lubricant

  1. Crush graphite ore to pea size and pick out the black, shiny pieces.
  2. Grind wet in a mortar or ball mill (Ball Mills, Crushers and Grinders).
  3. Float and settle. Stir the slurry, wait one minute, and pour the cloudy water off the grit into a second tub. The flakes stay up longest. Settle a day, pour off the water, and dry the black mud (Ore Dressing: Jigs, Tables and Flotation).
  4. Use it dry in locks (Locks and Keys), dusty pivots and drawer runners. Mix 1 part to 4 parts tallow or lime grease for heavy, slow, hot bearings and for threads that must come apart years later. Brush it on in water or oil on hot dies (Presses, Punches and Dies), on wire being drawn (Iron and Brass Wire) and on steam-fitting threads.

Graphite burns away in air above about 450–500 °C.

Soapstone and talc

Powdered soapstone is white and silky and never burns. Rub it on wooden slides, sledge runners (Snowshoes, Skis and Sledges) and cast-iron surfaces that must slide without oil. Dust rubber with it to stop sticking (Rubber), and use it as a parting powder in moulds. Mixed 1 to 3 with tallow, it greases slow wooden bearings.

Other simple lubricants: soap on wood screws; beeswax or paraffin on drawer runners and saws (Waxes: Beeswax, Plant Waxes and Paraffin); water for lignum vitae bearings (Bearings and Lubrication); soap-and-oil emulsions as cutting coolant (Detergents and Wetting Agents, Machine Tools).

Oilers and grease fittings

A bearing needs a little oil often, not a lot now and then. A flood runs straight out; a dry hour scores the shaft. These devices make the feed steady.

Oil can Wick oiler (section) Drip oiler Spout 12–20 cm long 1–1.5 mm tip Domed spring bottom thumb press = one squirt 7–8 cm hinged lid Oil Tube to bearing Wool wick Shaft oil climbs the wick, runs down the tube and drips onto the shaft Knob sets rate Lever Glass oil needle Sight count drops thread set 2–10 drops a minute; lever down stops the feed without losing the setting
Fig. 3 Three ways to feed oil. The thumb oil can squirts a few drops wherever it is pointed. The wick oiler siphons oil from its cup down a strand of wool, drop by drop, for as long as the wick is in. The drip oiler lets drops fall past a glass window at a rate set by a needle valve, and a lever stops the flow when the machine stops.

Oil can

  1. Body: a tinplate cylinder 7–8 cm across, 5–6 cm high, with a soldered cone top and a collar for the spout (Tins, Cans, Drums and Tanks, Soldering and Brazing).
  2. Pump bottom: a disc of springy brass or hard tinplate 0.3–0.4 mm thick, domed slightly over a hollow so that it clicks in when pressed and springs back (Metal Spinning and Raising). Solder it in, dome outward. A thumb press squirts oil; the spring-back draws air in.
  3. Spout: a soldered tube 12–20 cm long, tapering from 8 mm to a 1–1.5 mm tip.
  4. Test: one clean drop per short press, and no seep from any seam overnight.

Oil cup and wick oiler

An oil cup is a lidded reservoir screwed into a bearing's oil hole. The wick oiler makes its feed slow and steady.

  1. Make a brass cup 3–5 cm across and 4–6 cm deep with a hinged lid. Solder a tube of 4–5 mm bore up through the middle of its floor, standing to about 1 cm below the rim and running down into the bearing.
  2. Fold 4–12 strands of worsted wool over a wire loop and pull the fold down into the tube, with the loose ends hanging in the oil.
  3. Oil climbs the wool by capillary action, over the top of the tube and down into the bearing. Twelve thick strands of thin oil give about a drop every 10–20 seconds; fewer strands, less. Lift the wick out when the machine stands, or it empties the cup.

Pad oilers in railway axle boxes work the same way from below: a spring presses a wool or felt pad against the underside of the shaft, with its tail in an oil well (Railways).

Drip oiler (sight-feed oiler)

For a steam engine, lathe headstock or main shaft, the sight-feed drip oiler gives a set number of drops a minute, shows each drop falling, and stops at a flick.

  1. Reservoir: a glass tube 4–6 cm across and 6–10 cm long (Scientific Glassblowing and Glass-to-Metal Seals) clamped between turned brass ends by three or four thin rods, with leather or cork gaskets (Packing, Gaskets and Seals).
  2. Needle valve: a brass stem down the middle, threaded at the top to a knob, closes a fine conical seat about 1.5 mm across in the base.
  3. Shut-off: a small cam lever on top lifts the stem a few millimetres (on) or drops it to its seat (off) without changing the knob's setting.
  4. Sight glass: below the valve the drops fall past a little window before entering the stem that screws into the bearing.
  5. Set it to 2–10 drops a minute for an ordinary shaft bearing.

A good one keeps the same rate from full to nearly empty, within a drop or two a minute, and does not leak when shut.

Grease cup

The screw-down grease cup is a brass cup screwed to the bearing with a cap that screws over it like a jar lid. Turn both 3–4 cm across with a thread of about 1.5 mm pitch (Screws, Nuts and Bolts). Fill the cap with lime grease and screw it on until grease reaches the bearing. Every day or shift, give the cap a quarter to half turn to push in fresh grease. Spring cups push grease in with a spring-loaded piston.

Grease gun

A grease gun forces grease through a small nipple with a one-way ball valve into closed-in bearings: those of a The Tractor, an The Motor Vehicle, a reaper. New grease pushes the old, dirty grease out ahead of it.

Lever grease gun (section) Grease nipple (section) Lever 15–20 cm Plunger 6–8 mm Spring Follower piston leather cup Grease barrel 4–5 cm bore Check ball Coupler screw cap grease in Ball 3–4 mm Spring Hex thread Head 6–7 mm into the bearing
Fig. 4 The grease gun and nipple. Pumping the lever drives a small plunger that forces grease from the barrel out through the hose at high pressure. The nipple's spring-loaded ball lets grease in and keeps dirt out; the cup-shaped coupler grips its round head.
  1. Barrel: steel or brass tube 4–5 cm bore, 20–30 cm long (Metal Pipes and Tubes), screw cap at the back. A follower piston with a leather cup, pushed by a spring (Springs), keeps the grease pressed forward.
  2. Pump head: a plunger 6–8 mm across in a closely reamed bore, driven by a lever 15–20 cm long. The small plunger gives hundreds of atmospheres. A ball check valve at the outlet stops grease coming back.
  3. Outlet: a steel tube or armoured hose ending in a coupler of three or four spring jaws that snap over the nipple.
  4. Nipple: a hexagon steel fitting threaded at one end, with a rounded head 6–7 mm across at the other. Drill it through and fit a 3–4 mm steel ball (Making Ball and Roller Bearings) held against the inside of the head by a light spring.
  5. Use: wipe the nipple, snap on the coupler, and pump until old grease just shows at the bearing's edges.

A simpler screw-piston gun, its piston driven by a screwed rod, needs no pump or valve. It gives less pressure but is enough for open oil holes.

Choosing and changing lubricants

Job Use How often
Wooden axle, waterwheel shaft, mill gudgeon Tallow and tar, set grease, graphite grease Daily; repack weekly
Plain metal bearing, slow to medium Lime grease in a grease cup, or machine oil in a wick oiler Daily
Fast shaft, lathe spindle, dynamo Spindle or machine oil, drip or ring oiler Every few hours
Ball and roller bearings Lime grease (cool) or soda or lithium grease (warm), one third full Every few months (Making Ball and Roller Bearings)
Enclosed gears Gear oil, lowest teeth dipping one or two tooth-depths Change yearly
Steam cylinder Compounded cylinder oil Continuous
Engine crankcase Engine oil Change every 100–250 hours
Clocks, sewing machines, instruments Cold-strained neatsfoot or spindle oil, one tiny drop Yearly
Locks, dusty pivots Dry graphite or soapstone When stiff

Change oil warm, when it runs freely and carries its dirt out. Flush with a little thin oil, clean strainers and wicks, and refill. Change it sooner if it is black and gritty, milky (water has got in), smells burnt or sour, or flows faster or slower in the flow cup than new oil. When you open a greased bearing, wash out all the old grease with paraffin first. Do not mix lime and soda greases: the mixture often turns soft and runs out.

How to tell it worked

  • Bearings run cool: after an hour's work you can keep a hand on the housing, so it is below about 50–60 °C.
  • No squeal, smell or smoke.
  • Grease stays put: it does not drip from a vertical surface on a hot day, and feels smooth, not gritty, between finger and thumb.
  • Wear is slow: an opened bearing shows smooth polish, not scoring or blue heat tint.
  • Water test: shake a walnut-sized lump of lime grease in a jar of water for a minute. It stays whole and the water stays nearly clear. Soda grease clouds the water.

Note Troubleshooting Lime grease separates into oil and crumbs → cooked too dry or too hot; stop heating sooner next time. Grease lumpy or sandy → lime added dry or not fully reacted; make a smooth milk first and cook longer. Grease runs out of bearing → too much oil in it; work in more soap base. Wick oiler does not feed → wick dirty or too few strands, or oil below the tube top. Drip oiler floods → needle seat worn or dirty; lap it with fine abrasive (Abrasives and Grinding Stones). Oil turns sticky in the bearing → a drying oil, or rancid plant oil; clean out, use mineral or refined non-drying oil. Bearing hot although well oiled → misaligned, too tight, or oil too thick for the speed (Bearings and Lubrication).

Dangers

Danger Grease-gun injection. A grease gun's jet can pierce skin. Grease forced into a finger looks like a pinprick but spreads along the tendons and kills the tissue. Without urgent surgery the finger is often lost. Never cover the nozzle with a finger or clear a blocked gun by hand. Treat any injection as an emergency (Emergencies, Basic Surgery).

Danger Oily rags catch fire by themselves. Rags and sawdust soaked in linseed and other drying oils, and some fish and animal oils, heat up as the oil reacts with air. A heap can burst into flame hours later. Spread used rags flat outdoors to dry, or keep them in a closed metal tin of water.

  • Hot grease kettles: fat that smokes heavily is close to catching fire: from about 270–300 °C its vapour catches from any flame, and hotter still it can burst into flame by itself. Never let a grease kettle smoke. Keep a lid ready to smother it, and never pour water on burning fat (Firefighting). Water dropped into hot grease flashes to steam and throws it out.
  • Lye and acid burn skin and blind eyes. Wear eye protection and gloves (Lye and Potash, Sulfuric Acid).
  • Castor beans contain ricin. Never eat them, and keep the press cake from people and animals.
  • Skin cancer: years of skin soaked daily in crude or used mineral oil causes skin disease and cancer. Cotton spinners sprayed with shale oil suffered it. Use refined oil, wear an apron, and wash oil off after every shift.
  • Slips: wipe oil off floors and ladders at once.
  • Moving machines: place oilers where you can fill them without reaching near belts or gears (Belts, Chains and Power Transmission).

What this unlocks

Well-lubricated bearings turn The Watermill and The Windmill stones, workshop line shafting and the axles of Wagons and Carriages. Fine oils keep sewing machines, clocks and instruments running. Sight-feed oilers and cylinder oil make the The Steam Engine and Railways practical. Grease guns and lithium grease serve the The Tractor, the The Motor Vehicle and every sealed ball bearing. Cutting oils serve Machine Tools.

How it was first done

An Egyptian tomb painting of about 1880 BC shows a man pouring a liquid in front of a sledge that carries a colossal statue, probably to make it slide. Residue on a chariot axle from an Egyptian tomb of about 1400 BC has been analysed as animal fat. Around 160 BC the Roman writer Cato advised greasing axles with amurca, the watery dregs of olive pressing. Tallow, lard, whale and rapeseed oil greased the world's mills and machines until the mid-1800s.

After Edwin Drake's oil well in Pennsylvania in 1859, mineral oils took over. In 1883 Beauchamp Tower found that a well-oiled shaft floats on a film of oil under pressure, and Osborne Reynolds soon explained how that pressure arises. Sight-feed oilers and screw-down Stauffer grease cups were standard by the late 1800s. Oscar Zerk patented the ball-check grease nipple in the United States in 1929, and Clarence Earle patented lithium grease in 1942. It was used on wartime aircraft before it became the everyday grease of cars and machines.

Source: content/entries/mechanics/lubricants.md