◆ Rebuild

Part 6 · Building

Dams and Reservoirs

How to hold back a stream so the wet season's water lasts through the dry — small earth dams with a clay core and a spillway, masonry weirs, millponds and town reservoirs — and how dams fail, so that yours never sends a wall of water down the valley.

Difficulty
●●●●●
Time
A dry season with a team for a small earth dam; years for a town reservoir
Steps from zero
13 prerequisites →

You need first

Surveying and LevellingStone Masonry

This unlocks

—
The full path from nothing — 13 steps before this one
  1. Stone Tools
  2. Fire
  3. Finding and Preparing Clay
  4. Simple Machines
  5. Measurement from Scratch
  6. Writing and Numbers
  7. Quarrying and Cutting Stone
  8. The Kiln
  9. Arithmetic and Fractions
  10. Lime
  11. Surveying and Levelling
  12. Mortar and Concrete
  13. Stone Masonry
  14. Dams and Reservoirs

Do them roughly in this order. See it on the tech tree →

Why it matters

In most of the world rain comes in a wet season and then stops for months; a stream that floods in spring is dry stones by late summer. A dam is a bank or wall across a valley that makes the water pile up into a reservoir (a man-made lake; a tank in India and Sri Lanka). It turns a few wet months into a year of water:

A dam is also the most dangerous structure in this part of the book. A bank of earth 4 m high holding back a small lake can, if it breaks, release tens of thousands of tonnes of water in minutes. For a pond behind a dike under 2 m high, the simpler method in Fish Ponds is enough; for a low weir that only lifts a stream into a channel, see Water Turbines and Hydroelectric Power and Irrigation. This chapter is for anything bigger.

How it works

Water pushes harder the deeper it is. At 1 m depth it presses on each square metre of dam with the weight of 1 tonne; at 4 m, 4 tonnes. The total push on a 1 m wide strip of dam is about ½ × H × H tonnes for a depth of H metres: 2 tonnes at 2 m, 8 at 4 m, 18 at 6 m. Double the height, four times the push. Small dams are easy; big ones are not.

A dam resists that push in one of two ways. An earth dam (embankment) is so wide and heavy that the water cannot shove it aside; it is cheap, but water must never flow over it and seepage must never carry soil out of it. A masonry gravity dam is a stone wall too heavy to slide or tip; it can be overflowed, so it is the choice for a weir on a river that floods.

Water always seeps. No soil is watertight. Seepage is harmless if it comes out clear. The danger is piping: seepage fast enough to wash out fine grains. Each grain lost makes the path easier, the flow grows, and a tunnel eats back through the dam until it collapses — sometimes within hours. The clay core, the trench beneath it, careful ramming and the filter at the downstream foot all exist to keep seepage slow and clean.

The flood must have its own way out. Every reservoir eventually overflows. The spillway — a wide, low channel cut round the end of the dam in natural ground — carries the overflow past. More earth dams have been destroyed by water pouring over their top (overtopping) than by anything else.

Reservoirfull water level = spillway sill Upstream face 1 in 3riprap stones 20–40 cm Freeboardat least 1 m Crest at least 3 m widebuilt 5–10% high for settling Clay corein 15 cm layers Downstream face1 in 2, turfed Seepage linekept low by the core Toe drainsand, then gravel Sand and gravelwater would pipe through:the trench cuts right through it Cutoff trenchat least 1 m deep,0.5 m into watertight ground Watertight clay or rockheight drawn at twicetrue scale for clarity
Fig. 1 An earth dam in cross-section. The clay core sits in a trench dug down into watertight ground; the outer shells give weight; stones on the upstream face stop wave damage; the gravel toe drain lets seepage out without carrying soil.

What you need

Item Notes
A survey Water level or A-frame, staff, ropes, stakes: Surveying and Levelling. Map the valley before you dig.
Clayey soil For the core and the trench under it: up to 10 m³ per metre of dam length at the deepest part of a 4 m dam. See Finding and Preparing Clay.
Mixed earth Sandy-clayey soil with some gravel for the shells. A dam 4 m high and 50 m long needs roughly 1,500–2,500 m³ (3,000–4,000 tonnes), depending on the valley's shape.
Sand and gravel For the toe drain and filters.
Stones Fist- to head-sized and larger (fieldstone), for riprap and lining the spillway.
Turf To grass the downstream face and spillway.
Rammers Wooden tampers (a log 15–20 cm thick, 1.2 m long, with handles), or a herd of animals to tread the fill.
Moving earth Spades, baskets, barrows, ox-drawn scoops (Draft Animals and Harness).
Outlet Fired clay, bored log or iron pipe (Tiles and Clay Pipes, Pipes, Plumbing and Aqueducts); a valve or wooden gate.
For weirs Big stones and hydraulic mortar — lime with volcanic ash, or Portland Cement (Mortar and Concrete).

Labour is the real cost. One strong person digs and carries 2–4 m³ of earth a day over a short distance. The 4 m dam above takes roughly 800–1,500 person-days with ramming: twenty-five people for two months of the dry season.

Choosing the site

Walk the whole valley before you choose.

  1. A narrow neck below a wide basin. Where the valley pinches between two firm hillsides (the abutments) with a broad, gentle basin above, a short dam holds a big lake.
  2. Sound ground underneath. Dig test pits along the line, 2–3 m deep or to rock. You want clay or solid, uncracked rock within reach. Avoid sand or gravel beds running under the site (water pipes through them), limestone with holes, peat, springs on the site, and landslips (curved cracks, leaning trees, hummocky slopes).
  3. A place for the spillway: firm natural ground, ideally rock, round one end.
  4. Clayey soil close by, best from inside the future lake (digging it out adds storage).
  5. A modest catchment. The catchment is all the land that drains to the site; trace the ridges round it (Maps and Mapmaking). For a first dam, a few tens of hectares to a few square kilometres. A huge catchment brings floods you cannot pass.
  6. Nobody directly below. Ask: if this broke on a stormy night, whose house would the water reach? If the answer is a village, build smaller or elsewhere.

Planning: water and floods

Need. Daily use (20–50 litres per person, Pipes, Plumbing and Aqueducts, plus animals and crops) times the longest dry spell anyone remembers. Then add evaporation: an open lake loses 1.5–2.5 m of depth a year in hot dry climates (5–8 mm a day in summer), 0.5–1 m in cool damp ones. Shallow lakes lose a far larger share, so build deep rather than wide. Add dead storage — the bottom 0.5–1 m, which fills with silt — and a third more for safety.

Example. 400 people at 30 litres use 12 m³ a day: 1,800 m³ over 150 dry days. A 1-hectare lake losing 6 mm a day evaporates 60 m³ a day — 9,000 m³ in the season, five times the drinking water. In the tropics that is normal.

Storage. Survey the shoreline at the planned full level. For an ordinary valley, volume (m³) ≈ 0.4 × surface area (m²) × greatest depth (m). A 1 ha lake 4 m deep at the dam holds about 16,000 m³.

Yield. Each millimetre of rain on each hectare is 10 m³, but only part runs off: about 5–15% of the year's rain from forest, 15–30% from grass and fields, 50–80% from bare rock. A 50 ha catchment with 700 mm of rain at 15% yields about 52,000 m³ a year.

The worst flood. For small catchments: peak flood (m³/s) ≈ C × rain intensity (mm/hour) × catchment (ha) ÷ 360, with C = 0.3 for forest, 0.5 for fields and grass, 0.8 for rock. Use 75–100 mm/hour for tropical storms and 40–50 mm/hour for temperate ones unless local memory says worse. For 50 ha of fields in a temperate land: 0.5 × 50 × 50 ÷ 360 ≈ 3.5 m³/s. Compare with flood marks (debris lines in trees, scoured banks) and old people's memories; when in doubt, double it.

Spillway width. A wide, flat sill passes about 1.7 × width × (depth over the sill)^1.5 m³/s, in metres. At 0.5 m depth each metre of width carries 0.6 m³/s, so 3.5 m³/s needs about 6 m of width. Keep the flood depth over the sill to 0.5 m or less — widening the spillway is cheaper than raising the dam.

Method 1: The small earth dam

Keep a first dam under 5 m high. Build several small ones before anything bigger.

Part Size (dams up to 5 m)
Crest width At least 3 m
Upstream slope 1 in 3 (1 m up for 3 m across)
Downstream slope 1 in 2 to 1 in 2.5
Freeboard Crest at least 1 m above the highest flood level in the spillway
Settling allowance Build the crest 5–10% higher than designed, most in mid-valley
Core At least 1 m wide at the top, widening about 1 m for every 2 m down
Cutoff trench Under the core, at least 1 m deep and 0.5 m into watertight ground, 2–3 m wide at the bottom

Each metre of height adds about 5 m to the base: a 4 m dam with a 3 m crest is about 23 m wide at the bottom.

  1. Set out. Peg the crest centre line and survey ground heights along and across it (Surveying and Levelling). Peg the upstream and downstream toes (outer edges of the base) from the slopes above. Mark the spillway sill at full-water level.
  2. Divert the stream round the site in a ditch, or through the outlet once laid. Work in the dry season.
  3. Strip the footprint of all topsoil, roots, stumps and turf, usually 20–40 cm deep. Roots rot into tunnels; topsoil will not compact. Keep the turf.
  4. Dig the cutoff trench from abutment to abutment, down through any sand, gravel or cracked rock into clay or sound rock, sides sloping 1 in 1. It stops water sneaking under the dam.
  5. Lay the outlet (below) in firm natural ground before any fill.
  6. Core soil. Use your most clayey soil: it is sticky and rolls into a pencil-thin thread, but has some sand so it does not crack badly when dry. Pure greasy clay shrinks and cracks; sandy soil leaks.
  7. Moisture. Squeeze a handful hard. Right: a firm ball showing fingerprints, palm not wet, breaking into a few lumps when dropped from waist height. Crumbles: too dry — sprinkle and mix. Oozes or smears: too wet — spread it to dry.
  8. Thin layers. Spread fill 15 cm thick (loose) across the whole width, core and shells together, so the dam rises evenly. Ram each layer until the rammer rings and bounces instead of thudding, and footprints no longer show — six to eight passes, or a herd of sheep or cattle walked over it many times. Scratch each layer before the next goes on. Never tip fill in high heaps: loose fill settles, cracks and pipes.
  9. Coarse outside, clayey inside. If you have only one fairly clayey soil, a dam of it alone will do, with flatter slopes (1 in 3.5 and 1 in 2.5) and a bigger toe drain.
  10. The toe drain, built as the dam rises: a trench along the downstream foot filled with sand against the earth, then fine gravel, then coarse gravel, draining to the stream bed. Each layer is too fine for the grains of the one before to wash through, so seepage comes out clear. This filter is what stops piping.
  11. Finish. Trim to the pegged slopes. Lay riprap on the upstream face from 1 m below the lowest water level to the crest: 15 cm of gravel, then tightly packed stones 20–40 cm across, or waves will cut a notch. Turf the downstream face and crest; round the crest so rain runs off.
  12. Cut the spillway round one abutment in natural ground: a level sill of stone or timber at full-water level, then a channel that falls gently and rejoins the stream at least 20–30 m below the downstream toe. Turf where water runs slow and shallow, stone where it falls steeply. Spill water must never run against the dam.
  13. Fence it. Animals tread paths that become gullies. Never let trees or bushes grow on a dam: roots make seepage paths, and a fallen tree tears out a hole.
Reservoir stake out its shorelineat the full-water level intake stream in Damacross the narrow neck;dashed line = clay core Outletsiphon over the crest, orcollared pipe; to town or fields Sillat full-water level Spillwaycut in naturalground, neverover the earth Rejoins the stream20–30 m below the toe no houses on the valley floor below hillsidehillside
Fig. 2 Plan of a small reservoir. The dam closes the neck of the valley; the spillway is cut round one end in natural ground, so that floods never flow over the earth; the outlet draws water to the town or the fields.

The outlet

Water creeps along the outside of a pipe through a dam, so outlets cause many leaks.

  • Simplest: a siphon laid in a shallow trench over the crest and primed by filling it. Nothing crosses the dam's body. In practice it lifts no more than about 7 m above the water surface, and it must be airtight.
  • A pipe through the base must lie in natural ground, bedded in 15 cm of rammed core clay, with collars (flat plates of fired clay, wood or concrete) every 3 m standing out 50–60 cm, to lengthen the creeping path. Wrap the downstream third in sand and gravel joined to the toe drain. Put the valve at the upstream end so the buried pipe is not under pressure when shut.
  • For a town, draw from near the surface, where water is cleanest, through a small tower with plugged inlets at several heights — not from the silty bottom. Then to Water Treatment for a Town.

First filling. Let the lake fill slowly the first time, over weeks if you can. Walk the downstream face, toe and abutments every day. Damp patches are normal while the dam wets through; muddy, running or growing ones are not. The crest will settle a few centimetres in the first year.

Method 2: Masonry weirs and millponds

A weir is a dam meant to be overflowed — for a river too strong for any earth spillway, or a millpond on a stream that rises fast.

  1. Found it on rock, or on a deep, wide footing of big stones in hydraulic mortar (Foundations and Floors). Cut a key trench 0.5 m or more into the rock across the whole width, and carry the wall 1–2 m into each bank, so water cannot creep round or under.
  2. Make it heavy. For a weir up to 3 m high, make the base at least as wide as the weir is high and the top at least 0.6 m wide, sloping the downstream face. Lay the biggest stones you can handle (Cranes and Lifting) in broken-jointed courses (Stone Masonry), every joint full of hydraulic mortar. Ordinary lime mortar washes out under water.
  3. Protect the foot. Falling water digs a hole that can undermine a weir in one flood. Build an apron downstream — big stones or stone-filled timber cribs, 2–3 times as long as the fall is high — or step the downstream face.
  4. Round the crest, and raise and stone-face the banks beside it above any flood.
  5. Fit a sluice: an oak or elm gate sliding in grooves, to empty the pond for repairs and flush silt.

A millpond stores the night's flow. 1,000 m³ falling 4 m through an overshot wheel gives roughly 7 kWh at the shaft — two or three extra hours of milling. Headrace, sluices and wheel are in The Waterwheel.

Reservoirs for towns

The same dams, built bigger and guarded better:

  • Protect the catchment. No latrines, graves, tanneries or cattle yards draining to it (Sanitation and Germs); a belt of grass or woodland 30–50 m wide round the shore.
  • Clear the basin of trees, brush and root-rich topsoil before flooding, or rotting plants spoil the water for years.
  • Stop silt at its source with small check dams of stone and brush in gullies upstream and good farming on the catchment (Field Drains, Terraces and Erosion Control, Understanding Soil).
  • Keep edges steep and clean, with no warm, weedy shallows for mosquitoes and the snails that carry bilharzia (Infectious Diseases).
  • Appoint a keeper to walk the dam weekly and after every storm, clear the spillway, record the level on a marked post, and raise the alarm.

How to tell it worked

1. OvertoppingSpillway too small or blocked: water overthe crest cuts the earth away in minutes. muddy 2. PipingSeepage carries soil out and a tunnel eatsback to the lake. Muddy spring = emergency. 3. SlippingFaces too steep, badly rammed or soaked;a curved crack on the crest comes first. 4. Leak along the outlet pipeWater creeps along the outside of the pipe.Fit collars and a sand-and-gravel filter.
Fig. 3 The four common ways small earth dams fail. Almost every rule in this chapter exists to prevent one of them.
  • The level holds: after the first year, the dry-season drop matches evaporation and use.
  • Seepage is clear and steady: a little clear water at the toe drain, the same amount at the same water level, year after year.
  • The crest is straight and level when you sight along it; a dip or bulge means settling or slipping.
  • The first big flood leaves the dam untouched and the spillway not eroding back toward its sill.

Note Troubleshooting. The lake never fills → leaks through the floor (sand, gravel, cracked rock) or too small a catchment. Line leaking patches with 30 cm of rammed clay, or pen cattle on the dry bed for a season so their hooves seal it. Wet patch on the downstream face, clear water → watch and record it. If steady, add a gravel drain; if growing, lower the water. Muddy seepage, a whirlpool in the lake, or a sinkhole on the dam → piping: an emergency. Open the outlet fully, warn everyone downstream, and pile sand then gravel (not clay) over the muddy spring so it filters instead of eroding. Cracks along the crest → vertical cracks that close when wet are drying shrinkage. A curved crack with one side lower is a slip: rebuild that face flatter. Notch in the upstream face → waves. Add riprap. Holes → burrowing animals. Dig out, refill with rammed clay, keep the grass short so you can see them.

Dangers

Danger A breaking dam can kill everyone below it. The water arrives as a wall carrying earth, trees and boulders, faster than people can run. Keep first dams under 5 m, never build without a sized spillway, never let anyone live in the valley floor directly below, and agree an alarm (bell, drum or horn) and a route to high ground. If you see muddy seepage, a growing leak or water near the crest: warn first, repair second.

Danger Never raise the crest or block the spillway to store more water — not with boards, screens or a "temporary" heap of earth. That is how some of the worst dam disasters in history happened. If you need more water, build a second dam.

  • Drowning. Banks are steep and slippery and the water deep and cold. Fence near houses. Never swim near an outlet or sluice: suction can pin a person against the inlet.
  • Trench collapse. Trenches deeper than about 1.2 m in soft ground can bury a worker. Slope or shore the sides, and keep spoil back from the edge.
  • Disease. Still water breeds mosquitoes (malaria) and snails (bilharzia). Do not wade.
  • Upstream flooding. Make sure the full lake will not drown anyone's fields or wells.

What this unlocks

Stored water runs the The Waterwheel, The Watermill and Water Turbines and Hydroelectric Power all day, carries towns through the dry season via Pipes, Plumbing and Aqueducts and Water Treatment for a Town, waters fields, raises fish, and keeps the summit level of Canals and Locks full. Big dams of Portland Cement and Reinforced Concrete power whole grids. Where you place dams, wells and houses together is in Planning a Settlement.

How it was first done

The oldest known dams are at Jawa in the Jordanian desert, about 3000 BC: low stone walls with earth packed behind, storing winter runoff for a town. In Egypt the Sadd el-Kafara, south of Cairo, a stone-faced earth dam about 14 m high and over 100 m long, was built around 2600 BC; with no spillway, it was probably washed away by a flood before it was finished. The great dam of Marib in Yemen watered the fields of the kingdom of Saba for well over a thousand years, from at least the 8th century BC until its final breach around AD 570.

The Romans built dams across Spain, North Africa and the Near East; the Proserpina dam near Mérida, an earth bank faced with masonry, is about 1,900 years old and still holds water. Kings of Sri Lanka built thousands of earth-dammed tanks for rice, culminating in Parakramabahu's Parakrama Samudra in the 12th century; Japan's Sayamaike reservoir dates from the 7th century.

The hardest lesson came in 1889, when the earth South Fork Dam above Johnstown, Pennsylvania, failed in heavy rain. Its crest had been lowered and its spillway partly blocked with fish screens; water poured over the top, the dam washed out, and more than 2,200 people died downstream.

Source: content/entries/building/dams-and-reservoirs.md