Part 7 · Home and Daily Life
Musical Instruments
How to make rattles, log drums and skin drums, willow whistles, bamboo flutes and panpipes, gut strings, a musical bow, a monochord and a lyre — and how to tune them by ear and by simple ratios of length. Music sets the pace of shared work, carries memory and news, and holds a community together through hard times.
- Difficulty
- ●●●●●
- Time
- An hour for a willow whistle; a day for a bamboo flute; a few days for a skin drum or a lyre
- Steps from zero
- 3 prerequisites →
This unlocks
Horns, Pianos, Organs and AccordionsViolins, Guitars and HarpsSound, Pitch and AcousticsThe full path from nothing — 3 steps before this one
- Stone Tools
- Cordage and Rope
- Basic Woodworking
- Musical Instruments
Do them roughly in this order. See it on the tech tree →
Why it matters
Music is not a luxury that comes after survival. In every human society ever found, people sing and drum, and they do it for practical reasons as well as joy.
- Shared work goes better to a beat. Hauling ropes, rowing, hoeing, threshing, grinding grain and pounding cassava are all done to songs whose rhythm tells everyone when to pull together. Sailors' shanties, African work songs and the grinding songs of village women all do this job.
- Songs carry memory. Before writing (Writing and Numbers), and long after, genealogies, laws, calendars, farming lore and the way to distant places were kept in songs, because tune and rhyme make words hard to forget.
- Signals carry farther than voices. Drums, horns and whistles call people in from the fields, warn of fire or attack, and pass messages across a valley; West African "talking drums" imitate the rise and fall of tonal speech.
- It holds people together. Singing and dancing together calm fear and grief, mark births, marriages and deaths, and turn a group of survivors into a community with a shared identity. That matters as much as food in the long first years of rebuilding.
Instruments also teach physics: the link between length and pitch led to the first mathematical laws of nature, and later to the telephone, Recording Sound and Radio.
How it works
Sound is vibration. A drum skin, a string or a column of air in a tube moves back and forth hundreds of times a second and pushes the air in waves to your ear. The number of vibrations per second is the frequency; we hear it as pitch. More vibrations per second = higher note.
Strings vibrate faster (higher) when they are:
- shorter — halve the length and the pitch doubles;
- tighter — four times the tension doubles the pitch;
- lighter (thinner) — a string a quarter the weight per metre sounds twice as high.
Tubes sound when the air inside them vibrates. The note depends on the tube's length: a tube open at both ends (a flute) sounds a note whose wavelength is about twice its length; a tube closed at one end (a panpipe) sounds about an octave lower, with a wavelength four times its length. Sound travels about 343 metres per second in air, so:
Open tube: frequency ≈ 343 ÷ (2 × length in metres). Closed tube: frequency ≈ 343 ÷ (4 × length in metres).
A 30 cm open flute tube sounds about 570 vibrations per second; a 30 cm closed panpipe about 285. (Real tubes sound a little lower because the air vibrates a little beyond the ends; trim to tune.)
Simple ratios sound sweet. When two notes' frequencies are in a ratio of small whole numbers, they blend:
| Interval | Ratio | String length for the higher note |
|---|---|---|
| Unison | 1 : 1 | the whole string |
| Octave | 2 : 1 | 1/2 |
| Fifth | 3 : 2 | 2/3 |
| Fourth | 4 : 3 | 3/4 |
| Major third | 5 : 4 | 4/5 |
| Minor third | 6 : 5 | 5/6 |
| Whole tone | 9 : 8 | 8/9 |
Notes an octave apart sound like "the same note, higher" in every culture. Almost all the world's scales are built from these ratios.
Resonators make sound loud. A string alone is nearly silent; stretched over a hollow box, gourd or skin, it makes the whole body and the air inside it vibrate, and the sound becomes loud.
What you need
| Item | For | Chapter |
|---|---|---|
| Knife, saw, drill or hot iron rod, rasp | Cutting tubes, drilling finger holes | Axes, Chisels, Knives and Planes, Drills and Boring |
| Rawhide — goat, deer, calf, sheep | Drum heads | Hides and Leather |
| Cord: rawhide thong, sinew or strong plant cord | Lacing drums, tying | Cordage and Rope |
| Sheep or goat intestines | Gut strings | Below |
| Horsehair, silk | Strings, fiddle bows | Silk |
| Hollow stems: bamboo, cane, elder, reed | Flutes, whistles, panpipes | Below |
| Gourds, hollow logs, thin boards | Resonators, drum bodies, sound boxes | Basic Woodworking, Barrels and Cooperage |
| Pine resin, beeswax, hide glue | Sealing, gluing, rosin for bows | Tar, Pitch and Glue, Glues and Adhesives |
Where to find it
- Bamboo and cane — look along warm rivers and hillsides for hollow, jointed stems. Choose dry, straw-coloured stems with thick walls and a bore of 1.2–2 cm for flutes; 0.8–1.5 cm for panpipes. Giant cane (Arundo) and common reed work too.
- Elder — a shrub or small tree of hedges, woodland edges and waste ground, with clusters of tiny white flowers in early summer and black-purple berries in autumn. Its young stems are filled with soft white pith that pushes out to leave a ready-made tube. (The leaves, bark, roots and raw berries are poisonous; don't chew it.)
- Willow — in spring, when the sap is rising, the bark of young shoots slips off whole: the basis of the willow whistle. Found along streams and in wet ground.
- Gourds (bottle gourds, calabash) — a climbing vine crop grown in warm summers; dried, the fruit becomes a light, hard, hollow shell for rattles, resonators and containers. Grow from seed (Farming from Seed).
- Hides and gut — from every animal you slaughter or hunt (Keeping Animals, Hunting and Trapping).
- Soundboard wood — light, straight-grained, knot-free softwoods ring best: spruce, fir, cedar, willow, poplar. Split it thin along the grain.
Method 1: Rhythm instruments
- Clapping sticks: two pieces of dry, dense hardwood 25–30 cm long, struck together. Different woods and thicknesses give different tones.
- Rattle: a dried gourd with a handful of small, hard seeds, pebbles or shell bits inside; plug the stem hole with wood and resin. Or a bundle of dry seed pods, deer hooves or shells tied to a stick.
- Log (slit) drum: take a log 60–150 cm long and 25–40 cm across. Cut a long slot 3–5 cm wide along one side, and hollow the log out through it by burning and scraping (Basic Woodworking), leaving walls about 2–4 cm thick. The two lips of the slot are the "tongues". Leave one lip thicker than the other: it will sound a different pitch. Strike with a padded stick. A big slit drum can be heard several kilometres away.
Method 2: Skin drums
The rawhide
- Take a fresh or soaked hide of goat, deer, calf or sheep. Remove hair and flesh as for rawhide (see Hides and Leather) — soaking in wood-ash water for a few days loosens hair.
- Scrape it thin and even: about 0.5–1 mm for a hand drum, 1–2 mm for a big drum played with sticks. Thin spots tear; thick spots dull the sound.
- Keep it wet until you use it. Do not tan it — tanned leather stretches and stays soft; rawhide shrinks hard as it dries, which is what makes the drum tight.
A frame drum
- The frame: a strip of ash, oak or willow 6–8 cm wide, 6–8 mm thick and long enough to make a hoop 40–50 cm across, plus 15 cm overlap. Steam it (Steam-Bending Wood) and bend it round a form, overlap the ends, and nail, peg or glue them. Round the top edge so it doesn't cut the skin.
- Cut the skin in a circle 10–12 cm larger all round than the hoop.
- Punch holes round the edge of the skin every 4–5 cm, 2 cm in from the edge.
- Stretch: lay the wet skin over the frame and lace it across the back, from hole to hole on opposite sides, with rawhide thong or strong cord, pulling evenly all round until the skin is smooth and taut. The lacing crossing at the back makes a handle.
- Dry slowly for 1–3 days, in the shade, away from fire. The skin shrinks drum-tight.
A rope-tensioned drum
- The body: a hollowed log, or a stave-built shell (Barrels and Cooperage), 30–60 cm long and 25–40 cm across, open at both ends.
- Two heads: lap each wet skin over a thin hoop of bent wood a little bigger than the shell, and sew or fold it round the hoop.
- Lace the two heads together with a long cord zigzagging from one hoop to the other all round the drum.
- Tension: thread a short leather loop around each pair of cords; sliding the loops toward the middle of the drum pulls the cords together, which pulls both heads tighter. This lets you tune the drum and retighten it in damp weather.
Tuning a skin drum: tighter = higher. Rawhide slackens in damp air and tightens in dry; warm a slack drum gently near (not over) a fire for a few minutes before playing.
Method 3: Whistles and flutes
The willow whistle (spring only)
- In spring, cut a smooth, knot-free willow shoot 1–1.5 cm thick and 15–20 cm long.
- 3 cm from the thicker end, cut a notch: a straight cut 5 mm deep into the wood, then a sloping cut back towards the mouth end to meet it.
- Cut a ring through the bark all round, 8–10 cm from the mouth end.
- Tap the bark all over with a knife handle for a minute to loosen it, then twist and slide the bark tube off whole. Keep it wet.
- On the bare wood, shave a flat strip 1–2 mm deep from the mouth end to the notch — the windway. Deepen the notch backward by a few centimetres to make the air chamber.
- Slide the bark back on. Blow. Sliding the wood further in or out of a longer bark tube changes the note.
It works for a day or two before the bark dries and splits.
A lasting whistle (fipple flute)
Make the same thing from a permanent tube — bamboo, cane, elder with the pith pushed out, or a bored stick.
- Cut a tube 20–35 cm long, open at both ends (for bamboo, cut just past a node and burn the node out with a hot iron rod).
- Cut the window: 2–3 cm from the mouth end, a rectangular hole about 6 mm wide and 5 mm long, with its far edge cut down at a slope to make a sharp edge (the labium).
- Make the block (fipple): a plug of wood that fills the mouth end exactly up to the window, with one flat side shaved to leave a thin slit — the windway — about 1 mm deep and as wide as the window. The windway must aim the breath exactly at the sharp edge.
- Blow gently. If it only hisses, adjust the block a fraction in or out, or make the edge sharper.
Finger holes and the scale
Every uncovered hole effectively shortens the tube and raises the pitch. For a major scale (do-re-mi) on a tube whose sounding length — from the sharp edge (or, on a side-blown flute, from the centre of the blowing hole) to the open end — is L:
| Note | Ratio to the lowest note | Hole centre, measured from the edge |
|---|---|---|
| Lowest note (all closed) | 1 | L (the open end) |
| 2nd (re) | 9/8 | 0.89 L |
| 3rd (mi) | 5/4 | 0.80 L |
| 4th (fa) | 4/3 | 0.75 L |
| 5th (so) | 3/2 | 0.67 L |
| 6th (la) | 5/3 | 0.60 L |
| 7th (ti) | 15/8 | 0.53 L |
| Octave | 2 | blow harder with all holes closed |
These are the positions for holes as wide as the bore. Smaller holes sound flat (too low). So: drill each hole small (3–4 mm) at the position in the table, starting from the bottom hole, play it, compare it by ear to the note you want, and enlarge it a little at a time to raise the pitch. Enlarging or moving a hole toward the mouth raises it; you can only go up, so start low. A five-hole pentatonic flute (leave out the 4th and 7th) is easier and sounds good in any order.
A side-blown flute
The same bamboo tube, closed just above the blowing hole by a node or a cork. Burn a round blowing hole 8–10 mm across, 2–4 cm from the closed end. Blow across it as across the neck of a bottle, with your lips almost closed. Finger holes as above, measured from the centre of the blowing hole.
Panpipes
A row of tubes, each closed at the bottom (by a node in bamboo, or a plug of wax). Each tube makes one note. Cut them to length using the closed-tube rule and the ratios: if the longest is 20 cm, the octave above is 10 cm, the fifth 13.3 cm, the fourth 15 cm. Bind them in a row with cord or glue them to a curved splint, and tune each by pushing a little wax down into it (raises the pitch) or trimming the top (also raises it).
Method 4: Strings
Gut strings
- Clean the small intestine of a sheep or goat immediately after slaughter: squeeze out the contents, turn it inside out, and wash it repeatedly in cold water.
- Scrape it on a board with the back of a knife to remove the soft inner lining and the outer fatty layer, leaving the thin, tough middle layer.
- Soak for one to several days in water with a little wood ash or Lye and Potash added (a weak alkaline bath), changing it daily, until the gut is white and clean.
- Split it lengthwise into ribbons if needed. Twist 2–3 ribbons together for a thin string, 6–10 for a thick bass string, while wet, by fixing one end to a peg and twisting the other with a spinning hook (see Cordage and Rope).
- Stretch it tight between two pegs and let it dry for a day or two. Polish smooth with a rag and a little oil.
Horsehair strings (several dozen hairs twisted together) and silk strings work too. Twisted plant fibre gives a dull, short-lived string. Later, brass and iron wire (Copper Wire) make bright, long-lasting strings.
The musical bow
The simplest stringed instrument: a bow (like a hunting bow, 1–1.5 m long) with a single string, held against an open gourd, or with one end held in the mouth, which acts as a resonator. Tap the string with a thin stick; change notes by touching the string, and by changing the shape of your mouth or moving the gourd against your chest.
The monochord: a tuning instrument
- Make a long, narrow hollow box 80–100 cm long and 10 cm wide from thin boards, with a soundboard top 3–4 mm thick and a small round sound hole.
- Fix a hitch pin at one end and a tuning peg at the other. Stretch one gut or wire string over two fixed bridges set exactly 60 cm apart (or any length you like; call it L).
- Mark the board under the string at 1/2, 2/3, 3/4, 4/5, 5/6 and 8/9 of L measured from one bridge.
- Put a small movable bridge under the string at any mark and pluck the long side: it sounds the interval in the table above, against the open string.
The monochord makes the ratios visible and teachable. It is a scientific instrument as well as a musical one: with it, you can show children that harmony follows numbers (Arithmetic and Fractions).
A lyre
- The body: a hollow sound box of thin boards, a dried gourd, or a tortoise shell, roughly 30 × 25 × 8 cm, covered with a thin wooden soundboard or a stretched rawhide.
- The arms and yoke: two arms of bent wood or horn rising from the body, joined at the top by a crossbar (the yoke) 30–40 cm above the body.
- Strings: 5–7 gut strings from a tailpiece on the body, over a small bridge on the soundboard, up to the yoke. Wind each round the yoke over a strip of leather, or fit each with a tapered peg in a tapered hole, which holds by friction and turns to tune.
- Tune the strings to a pentatonic scale (below) and pluck or strum.
Tuning pegs: carve hardwood pegs tapered about 1 in 30, and ream the holes with a tapered knife to match. Rub the peg with chalk if it slips, with soap if it sticks.
Fiddle bows: a stick 60–70 cm long with a hank of 100–150 horsehairs stretched along it. Rub the hair with rosin — the hard, clear, amber residue left when pine resin is heated to drive off the turpentine (Tar, Pitch and Glue, Distillation) — so it grips the string and makes it sing.
Tuning by ear and by ratio
Listening for beats
When two notes are almost but not quite the same, you hear a slow, regular wavering ("wah-wah-wah") called beats. The nearer the notes, the slower the beats. Tune by tightening or loosening one string until the beating slows and stops — then the two are exactly in tune. Octaves and fifths have beats too, though fainter; tune them until they sound smooth and still.
Building a scale from fifths
The oldest tuning method, used in China, Greece and many other places:
- Tune string 1 to any comfortable note. Call it do.
- Tune string 2 a fifth above it (3:2) — that is so.
- Tune a fifth above so; if it goes too high, tune it an octave lower instead. That is re.
- A fifth above re is la.
- A fifth above la (brought down an octave) is mi.
You now have do, re, mi, so, la — the pentatonic scale, found in folk music on every continent. Five strings tuned like this sound pleasant together in almost any order, which makes them easy for beginners. Two more fifths give ti and fa (fa a fifth below do) and the full seven-note scale.
Keeping a standard pitch
So that instruments in different houses agree, keep a reference: a carefully made pipe or whistle stored in a dry place, or — once you have steel — a tuning fork, a two-pronged steel bar that rings at one pitch for centuries. Modern music uses 440 vibrations per second for the note A. You do not need that exact pitch; you need everyone to use the same one.
How to tell it worked
- A drum gives a clear, ringing tone, not a dull thud, and the same tone all round the head.
- A whistle sounds cleanly with gentle breath and jumps to the octave when you blow harder.
- The notes of a flute or lyre match the notes of the monochord, with no beating.
- People pick it up and play it.
Note Troubleshooting. Drum sounds dead → head too thick, too slack, or damp; scrape thinner, tighten, or warm it. A buzz means something is loose: a lace, a crack in the shell. Drum head splits as it dries → stretched too tight while wet, dried too fast, or had a thin spot. Dry in the shade. Whistle hisses but won't sound → windway not aimed at the edge, or edge not sharp; adjust the block, sharpen the edge. Whistle squeals high → blowing too hard, or windway too wide. A finger hole is too high (sharp) → you can't undo it; make that hole smaller with a ring of wax, or start another flute. Gut string frays or breaks → twisted unevenly or dried with too little tension; polish and oil strings, and replace when frayed. Strings slip out of tune → pegs not fitting their holes; re-shape the taper, and chalk the peg.
Dangers
Danger Anthrax and other infections from raw hide and gut. Rawhide and gut from an animal that died of disease, or from unknown dead animals, can carry anthrax spores. Use hides and intestines only from healthy animals you have slaughtered; wash your hands well after handling them, and never put raw gut or hide in your mouth.
- Loud sound damages hearing permanently. Do not play loud drums, horns or whistles right beside anyone's ear, and give drummers rest.
- Splitting bamboo and cane have razor edges and splinters; burn out nodes with a hot rod, not by stabbing with a knife towards your hand.
- Elder is poisonous to chew; children should not suck on green elder whistles. Make them from dry, cleaned stems.
- Small parts — rattles' pebbles, whistle blocks — can choke babies.
What this unlocks
The monochord's ratios are among the first laws of nature written in numbers, and they lead into Arithmetic and Fractions and Forces, Energy and Heat. Tuning forks and pipes lead to Sound, Pitch and Acoustics, the The Telephone and Recording Sound. Fiddles, guitars and harps are in Violins, Guitars and Harps. Organ pipes need Bellows, and keyboards need levers and fine joinery; both, with brass horns, are in Horns, Pianos, Organs and Accordions. Instrument-making trains the precise woodworking that clocks and scientific instruments need. And songs remain the oldest library there is — a way to keep knowledge alive alongside books (Libraries and Preserving Knowledge, Teaching and Schools).
How it was first done
Flutes made from the wing bones of a griffon vulture and from mammoth ivory, found in the caves of the Swabian Jura in Germany, are about 40,000 years old; they have carefully spaced finger holes. Bone flutes from Jiahu in China, about 9,000 years old, can still be played. Drums are almost certainly as old, but skin and wood rarely survive; clay drum bodies appear in Neolithic Europe and China. The magnificent lyres buried in the Royal Tombs of Ur in Mesopotamia date from about 2500 BC. Greek tradition credits Pythagoras (6th century BC) with discovering that octaves, fifths and fourths come from string lengths in the ratios 2:1, 3:2 and 4:3; Chinese scholars independently built their twelve pitches by the same chain of fifths. The equal temperament used on modern keyboards was worked out mathematically by Zhu Zaiyu in China in 1584 and by Simon Stevin in the Netherlands at about the same time.