◆ Rebuild

Part 7 · Home and Daily Life

Sacks, Boxes, Crates and Packaging

How to make the containers that move and store a community's goods — sewn sacks and cloth, paper, net and string bags; nailed boxes, crates, trunks and pallets; cardboard, corrugated board and folded boxes and cartons; labels, tags, wrapping and wax paper; water skins and gourd canteens — and how to pack things so they arrive whole.

Difficulty
●●●●●
Time
An hour for a sack or bag; a day for a crate or a batch of boxes; a few days to build a corrugator
Steps from zero
10 prerequisites →

You need first

PaperBasic WoodworkingSewing, Needles and Thread

This unlocks

—
The full path from nothing — 10 steps before this one
  1. Fire
  2. Stone Tools
  3. Cordage and Rope
  4. Finding and Preparing Clay
  5. Basic Woodworking
  6. Pottery
  7. Spinning and Weaving Cloth
  8. Sewing, Needles and Thread
  9. Lye and Potash
  10. Paper
  11. Sacks, Boxes, Crates and Packaging

Do them roughly in this order. See it on the tech tree →

Why it matters

A harvest that cannot be moved or stored is half lost: grain spills from torn bags, pottery breaks on the cart, tools rust, and nobody knows what is in the barrel. Good containers let a village trade with the next valley (Money, Trade and Record-keeping), feed itself through winter (Granaries and Food Storage) and send medicines, glass and instruments safely by cart, boat and rail (Wagons and Carriages, Railways).

Baskets, bark boxes and gourds are in Baskets and Containers; barrels in Barrels and Cooperage; tins and metal drums in Tins, Cans, Drums and Tanks; leather bags and suitcases in Bags, Backpacks, Wallets and Luggage. This chapter covers the rest.

How it works

Goods in transit are damaged in five ways. Every packing method fights one or more of them:

Danger What it does Answer
Shock A drop or a jolt breaks brittle things Cushioning all round; nothing touching the walls
Crushing Boxes stacked on boxes collapse Stiff corners and edges; load carried down the corners
Vibration and rubbing Loose things grind and wear each other Fill every gap so nothing can move
Water Rots paper and grain, rusts iron Waxed or oiled liners, tarred covers, off the ground
Pests and theft Rats, weevils, pilfering Tight lids, nailed or sealed closures, labels and counts

A box carries its load in its corners and edges: a sheet of card is floppy, but folded into a tube it stands a surprising weight. Corrugated board works on the same idea, making a wavy core between two flat sheets so the whole board is stiff, light and springy.

Where to find it

  • Jute grows in hot, wet river deltas (Bengal is the classic place): a tall annual with straight stems 2–4 m high. Its long golden fibre is retted and stripped like flax (Flax, Hemp and Linen) and makes the coarse cloth called hessian, burlap or gunny. In cooler lands, use hemp or the short waste fibre (tow) of flax.
  • Wood for boxes: pine, spruce, fir and poplar — light, cheap, easy to nail. Oak or other hardwood for battens, skids and anything that must take hard knocks.
  • Cushioning: straw and hay from the harvest; fine wood shavings ("wood wool") from a plane; dry moss; chaff; crumpled waste paper.
  • Gourds: bottle gourds (Lagenaria), grown like squash (Baskets and Containers).

Bags and sacks

Sacks

A sack is a large bag of coarse, strong woven cloth. For grain and flour the cloth must be tight; for potatoes and onions, open.

  1. Cloth: plain-woven jute, hemp or flax tow, about 300–400 g per square metre, roughly 5–7 threads per centimetre each way (The Loom).
  2. Size: for 50 kg of grain, a piece 200 × 70 cm, folded in half to make a sack 100 × 70 cm. A smaller 25 kg sack, 80 × 50 cm, is far kinder to backs; use it where people carry by hand.
  3. Sew: fold the cloth in half with the fold at the bottom. Sew up the side and across any open bottom with doubled twine 2 mm thick, in a double-folded seam: turn the raw edges in together 1.5 cm, then turn again, and stitch through all layers with stitches 5–8 mm apart. Use a sacking needle — a flat steel needle 12–15 cm long with a curved point (Needles and Pins).
  4. Hem the mouth by folding twice and stitching, so it does not fray.
  5. Close: gather the mouth and tie it with a miller's knot (a close relative of the constrictor knot): two turns of cord round the neck, the end tucked under both turns. It pulls very tight and releases with one tug if the end is left as a loop. For shipping, sew the mouth shut across with twine.
  6. Mark it with stencil and ink (Duplicating: Carbon Paper, Hectograph and Stencil, Ink): owner, contents, weight.

Flour sacks need tight cotton or linen cloth (12 or more threads per cm) or a paper inner bag. Store sacks on pallets, clear of walls, with gaps to check for rats (Granaries and Food Storage); patch holes at once from inside.

Cloth bags

A drawstring bag is a tube of cloth sewn shut at one end, with a channel stitched round the mouth for a cord (Sewing, Needles and Thread). Use French seams (sew with raw edges outside, trim, turn, sew again) so nothing frays inside. Sizes: 20 × 30 cm for seed, 40 × 50 cm for bread and shopping. A tote has two strap handles 60 cm long, each sewn on with a square and an X of stitching.

Paper bags

Flat bag (seeds, sugar, nails): paste a sheet into a tube round a wooden block and fold the bottom up twice and paste it. Square-bottomed bag, which stands up:

  1. Cut strong paper (thick, long-fibred — hemp or flax paper of 80–120 g/m², or wood-pulp "brown paper", Paper) to a rectangle width = 2 × (bag width + bag depth) + 2 cm, length = bag height + ¾ of bag depth.
  2. Wrap it round a wooden former block the size of the bag, paste the 2 cm overlap with starch paste, and press.
  3. Fold the bottom end over the end of the block like the end of a parcel: sides in, then the two long flaps over each other, pasted.
  4. Slide it off to dry. A bag 15 × 9 × 30 cm holds about 2 kg.

Net bags and string bags

Net bag (for onions, potatoes, fodder, fruit): knot a net exactly as for a fishing net (Fishing) — sheet bends round a mesh gauge with a netting needle — with meshes 3–5 cm across, in 2–3 mm cord. Make a strip 50–60 cm wide and 80 cm long, fold it, lace the sides together, and run a draw-cord through the top row of meshes. Air passes freely, so produce does not sweat and rot.

String bag (a shopping bag that folds into a pocket) is made by looping, with no knots, like the bilum bags of New Guinea. Tie a ring of cord 30 cm round. With fine cord (1–1.5 mm) on a blunt needle, make a row of loops round the ring, each passed through the ring and then through itself; each new row passes through the loops of the row above. Twenty rows of 3 cm loops make a bag that stretches round a large load. Bind the top row to two handles.

Boxes, crates, trunks and pallets

The wooden box

  1. Boards: pine 1.5–2 cm thick, planed on the outside if you will write on it.
  2. Corners: nail the two sides onto the edges of the two end pieces. Nails hold poorly in end grain, so where they would go into it, glue a corner post of 2 × 2 cm wood inside each corner and nail into that instead. Use nails 2.5–3 times as long as the board is thick, 6–8 cm apart, and drive alternate nails at a slight slant, in a dovetail pattern, so they resist pulling out.
  3. Bottom: nail it on through into the edges of sides and ends.
  4. Battens: nail a strip 2 × 4 cm across each end, 3 cm below the top, as a handhold and to stiffen the end.
  5. Lid: nailed down for shipping (a few nails only, so it can be prised off), or hinged with a hasp and padlock (Locks and Keys), or sliding in grooves cut near the top of the sides.
  6. Weight: a box one person must carry should weigh no more than 25 kg full; mark heavier ones "two people".

A tea chest is a light plywood box (Plywood, Veneer and Boards) on a frame of battens, about 48 × 48 × 60 cm, lined with foil or waxed paper.

The crate

A crate is an open box of slats: lighter than a box, cheaper in wood, and it lets produce breathe.

  • Fruit or vegetable crate: two solid end boards 2 cm thick, about 30 × 30 cm; sides and bottom of slats 1 cm thick and 7–8 cm wide, 50 cm long, with 1–2 cm gaps between them. Holds 15–20 kg. Make the corner of each end project 1 cm above the slats so crates stack on their ends, not on the fruit below.
  • Packing crate for heavy goods: a base of two or three hardwood skids (runners) 8 × 8 cm; a frame of 5 × 5 cm battens round each side with a diagonal brace (a frame with a diagonal cannot fold); boards or slats nailed outside. Bolt the load to the skids so it cannot shift. Lift it by slings passed under the skids, never by the lid.

The trunk

A travel trunk is a strong wooden box with a lid, covered and reinforced to survive years of being thrown on and off carts, ships and trains (Bags, Backpacks, Wallets and Luggage).

  1. Carcass: pine 1–1.5 cm thick, about 90 × 50 cm and 55 cm high, dovetailed or nailed and glued (Furniture). A domed lid sheds water; a flat lid stacks.
  2. Cover it with canvas glued on with hide glue and painted (Pigments, Paints and Varnish), or with leather.
  3. Strengthen it with hardwood slats outside, corner caps of sheet iron or brass (Sheet Metal and Rolling), and handles at both ends.
  4. Close it with hinges, a hasp, a lock and two straps; fit a lift-out tray inside on cleats 15 cm below the lid.

The pallet

A pallet is a low wooden platform that carries a load of sacks, boxes or crates as one unit, lifted by a fork truck, a pallet trolley, or a crane sling (Moving Goods: Pallet Trucks, Forklifts and Containers).

  • Standard sizes (worth keeping, so loads fit carts, wagons and ships): 120 × 80 cm and 120 × 100 cm.
  • Simple stringer pallet (120 × 100 cm): three runners (stringers) 7.5 × 10 cm and 120 cm long; seven top deck boards 2.2 × 10 cm and 100 cm long, spaced evenly; three to five bottom boards the same. Nail each board to each stringer with two ringed or twisted nails 7–9 cm long, clenched if they come through. It carries about 1,000 kg spread evenly.
  • A skid is the same without bottom boards: easier to make, and it can be dragged on rollers.

Stack sacks on pallets with each layer crossing the one below, no more than 1.5–2 m high. Without fork trucks, move pallets on wooden rollers with crowbars, or lift them with slings and a crane (Cranes and Lifting).

Cardboard

Cardboard and pasteboard

Cardboard is simply very thick paper. Two ways to make it from scratch (Paper); machine-made board from wood pulp is in Wood Pulp, Kraft Paper and Paperboard:

  1. Pasteboard: paste 3–6 sheets of paper together with starch paste (Glues and Adhesives), alternating the direction of the fibres if you can, and press between boards under weights for a day. Dry it slowly, or it curls.
  2. Couched board: form sheets with a mould and deckle as usual, but couch (turn out) several wet sheets on top of each other; the fibres knit together. Or use a deeper deckle to make one thick sheet. Press hard and dry flat between felts and boards. Board 1.5–3 mm thick.

Rough strawboard is made the same way from straw cooked in lime or lye; grey board from waste paper.

Corrugated cardboard

Hand corrugator, end view Kinds of board Damp paper in Grooved rollers 10–15 cm, warmed Fluted paper out 8 mm pitch, 4 mm deep Crank Single-faced bends one way: wraps bottles Single-wall two liners: most boxes Double-wall heavy goods Flat sheets: liners. Wavy sheet: fluting, pasted to the liners at every tip.
Fig. 1 Making corrugated board. Damp, warm paper passes between two meshing grooved rollers and comes out fluted. Paste on the flute tips holds a flat liner sheet: that is single-faced board. A second liner on the other side makes single-wall board, which is stiff and light.

Corrugated board is a wavy sheet (the fluting or medium) glued between two flat sheets (the liners). The arches make it stiff, light and a little springy, so it cushions too.

A hand corrugator:

  1. Rollers: two cylinders of hardwood or cast iron 10–15 cm across and 30–40 cm long, cut along their length with rounded teeth like long gears (Gears, Metal Casting), so they mesh. Pitch (tooth to tooth) about 8 mm, depth about 4 mm, for flutes 4 mm high.
  2. Frame: mount them one above the other in a stout frame, the top roller pressed down by screws or wedges, with a crank on the bottom roller (Cranks, Cams and Linkages).
  3. Heat: iron rollers work best heated — warm them over a charcoal pan until a drop of water hisses — so the paper takes and keeps its shape.
  4. Run: dampen the fluting paper (steam it over a kettle or sponge it lightly) and crank it through. It comes out pleated.
  5. Face it: at once brush starch paste on the flute tips on one side, lay a liner sheet on them, and press lightly with a flat board — not hard enough to crush the flutes. That is single-faced board, flexible one way: good for wrapping bottles and jars.
  6. Paste the other tips and add a second liner for single-wall board; two fluted layers and three liners make double-wall board for heavy goods.
  7. Dry it flat under light boards.
Flute size Height Use
Large ("A") about 4.5–5 mm Cushioning glass and pottery
Medium ("C") about 3.5–4 mm General shipping boxes
Small ("B") about 2.5–3 mm Boxes for heavy, compact goods; crush-resistant

The cardboard box

LflapflapWflapflapLflapflapWflapflap height H 2L + 2W + 3 cm H + W flutes run up and down Glue flap 3 cm Dashed: score and fold Gaps: slots cut 5–6 mm wide Each flap is W/2 tall, so the flaps of the long sides meet in the middle when folded.
Fig. 2 The most common box, cut from one sheet. Four wall panels in a row with a glue flap at one end; flaps above and below, each half the width of the box, meet in the middle when folded. Scored lines fold; cut slots separate the flaps.

The slotted box wastes almost nothing:

  1. For a box L long, W wide and H high, cut a sheet 2L + 2W + 3 cm long and H + W tall.
  2. Score (crease without cutting) the fold lines with a blunt bone or wooden tool against a straightedge: vertical lines at L, L+W, 2L+W and 2L+2W from one end; and two horizontal lines W/2 in from the top and bottom edges.
  3. Cut slots 5–6 mm wide along each vertical score line from the edges to the horizontal score lines, so the flaps are free.
  4. Fold into a tube and glue the 3 cm flap to the last panel with starch paste or hide glue.
  5. Fold the bottom flaps (short ones first) and seal them with gummed paper tape: strips of strong paper brushed with animal glue or starch and dried, wetted when used.

For corrugated board, run the flutes upright in the walls: the box will stand far more weight stacked on top.

Cartons

A carton is a light folding box of thin board 0.3–0.6 mm thick, for medicines, soap, matches and food. The tuck-end carton is laid out like the slotted box, but its lid flap ends in a tongue that tucks inside. Cut many at once round a metal pattern, or with a cutting die — knife-edged steel strip bent to the outline and set in a board — pressed through in a printing press. Waxed cartons hold milk; moulded pulp, pressed into a perforated mould and dried, makes egg trays.

Labels, tags and wrapping

Labels and shipping marks

Write labels with carbon ink or pencil, which do not fade or run (Ink, Pencils and Chalk). Stick them with starch paste; for "lick-and-stick" labels, brush the back with gum arabic and let it dry (Envelopes, Stamps, Clips and Office Supplies). On wooden boxes, stencil or brand the marks straight onto the wood.

Every shipped package should show:

  • From and to: names and places.
  • Contents and count ("12 jars honey").
  • Gross weight.
  • Handling marks: "THIS WAY UP" with an arrow, "FRAGILE", "KEEP DRY", "DO NOT DROP".
  • Number, e.g. "3 of 7", matching a written list (a bill of lading) carried separately.

Tags

A tag is a label tied on. Cut stiff card about 5 × 10 cm, round or clip the corners, and punch a hole near one end reinforced with a pasted paper ring or a metal eyelet (Buttons, Buckles, Hooks and Zips), or the string tears through. Tie it on with 25 cm of string. For outdoors and gardens, use tags of thin wood, or of zinc or lead sheet scratched with a point, which last for years.

Wrapping paper and parcels

Brown paper — strong, unbleached, long-fibred — is the standard wrapping (Paper); thin tissue wraps delicate things first.

  1. Put the item in the centre of a sheet big enough to go round it with 5 cm overlap.
  2. Fold the long edges over it, overlapping, and paste or tuck.
  3. At each end, fold the sides in to make triangles, and fold the triangles up over the end.
  4. Tie with string: once round the length, crossing round the width underneath and on top, knotted where the strings cross, so they cannot slide off.

Wax paper

Wax paper keeps out water and air and does not stick to food.

  1. Use thin, strong paper, 40–60 g/m².
  2. Dip method: melt beeswax (Beekeeping) in a pan standing in a larger pan of hot water, never over a bare flame, at about 70–80 °C. Draw each sheet through the wax and pull it between two warm rods or over the pan edge to scrape off the excess. Hang to cool.
  3. Iron method: lay paper on a board, sprinkle grated wax over it, cover with a second sheet, and press with a warm iron until the wax melts in (Laundry and Bleaching Cloth).
  4. Paraffin wax from Petroleum and Refining, and the other waxes in Waxes: Beeswax, Plant Waxes and Paraffin, work the same way.

Waxed cloth made the same way from linen or cotton can be washed in cool water and reused for months.

Water skins and gourd canteens

The water skin

The skin of a whole goat or sheep, taken off in one piece like a sock, makes a bag holding 15–25 litres of water; a smaller bag of hide or a stomach or bladder holds a litre or two.

  1. Skin the animal by "casing": cut round the legs and neck only and peel the skin off whole, inside out (Butchery and Meat).
  2. Clean off all fat and flesh, remove the hair or leave it outside, and tan it with bark or smoke so it does not rot (Hides and Leather).
  3. Close the three leg holes and the tail by tying them tightly with cord over a small wooden plug, or sewing and sealing them with pitch. The neck becomes the spout; tie it shut with a thong.
  4. Line the inside with melted pine pitch or tar (Tar, Pitch and Glue) for a watertight bag — the water will taste of it — or leave it unlined so a little seeps through and evaporation keeps the water cool, as in the deserts of Africa and Asia.

A bota is a small leather bottle of about 1 litre, two pear-shaped pieces sewn together and lined with pitch, with a horn or wooden spout.

The gourd canteen

Grow, cure, clean and seal a bottle gourd as in Baskets and Containers, choosing one holding 1–2 litres with a narrow neck. Then:

  1. Stopper: carve a tapered stopper of cork or soft wood, wrapped in cloth or leather so it seals.
  2. Carrying: knot a close net of cord round the body (or a sling of cord round the waist of the gourd) and a strap 1–1.2 m long to go over the shoulder. Tie the stopper to the neck with a thong so it is never lost.
  3. Care: rinse it out after every use and dry it upside down; a wax-sealed gourd must not be left in hot sun.

Metal canteens and flasks are in Tins, Cans, Drums and Tanks.

Packing goods to survive travel

Packing case, cut open Outside Lid, a few nails only Batten handhold Skid Straw packed firm 5 cm 5 cm 5 cm 5 cm Each jar wrapped, none touching THIS WAY UP FRAGILE KEEP DRY TO: name, place FROM: name, place 12 jars honey 24 kg · 3 of 7
Fig. 3 A packing case in section. Each fragile item is wrapped, kept at least 5 cm from its neighbours and from every wall, and the gaps are packed firm with straw so nothing can move; the case has battens and skids, and is marked on the outside.
Goods How to pack
Pottery, glass, bottles Wrap each in paper or straw; stand upright in a crate; 5 cm of firm cushioning between items and all round the walls; heavy things at the bottom
Eggs Pointed end down in chaff, bran or sawdust, or in egg trays (Poultry and Eggs)
Grain, flour, salt, sugar Sacks or lined barrels; keep dry and off the floor
Liquids Barrels, stoppered jars in straw, never more than full less a tenth (liquids expand when warm)
Iron tools and machine parts Grease all bright surfaces (Oils and Pressing); wrap in oiled or waxed paper; bolt down or wedge in
Books, papers, seed Wrapped in waxed or oiled paper inside a tight box (Bookbinding)
Instruments, lenses Double box: a padded inner box floating in cushioning inside an outer box
Plants Roots in damp moss wrapped in cloth or paper; tops open to the air; shade

Rules for every package:

  1. Nothing must move. Shake it: if you hear or feel movement, add packing.
  2. Nothing touches the outer wall. Shocks reach the wall first.
  3. Heaviest at the bottom, and the centre of weight low and in the middle.
  4. Fill every void — loose straw packed down firmly, wood wool, crumpled paper, sawdust (sawdust holds damp: not with iron).
  5. Weather: waxed paper inside; tarred or oiled canvas outside (Linoleum, Oilcloth and Floorcloths).
  6. Weight: no more than 25 kg for one porter; on pack animals, equal loads each side, about one-fifth of the animal's weight in all (Pack Animals).
  7. Test a new kind of package before trusting it: drop it, loaded, from 80 cm onto a corner, an edge and a face, then open it.

How to tell it worked

  • A full sack lifted by its ears does not split at the seams; no grain trickles out.
  • A crate stands with an adult standing on it.
  • A cardboard box takes the weight of two more full boxes on top without its walls bulging.
  • Wax paper beads water and does not crack when folded.
  • A water skin hung full overnight is still full in the morning (or, unlined, only damp on the outside).
  • Packages arrive with every item whole, and the list matches the count.

Note Troubleshooting. Sack seams split → stitches too far apart or thread too thin; double the seam and use heavier twine. Nails pull out of box corners → nails into end grain, or too short; nail into face grain, use longer nails, slant them. Corrugated board flat and floppy → rollers too cold or paper too wet; heat the rollers and dampen less. Press the liners on more gently. Cardboard warps as it dries → dried too fast or on one side only; dry it pressed between boards. Water skin smells → poorly cleaned or untanned. Clean, tan, and dry it between uses. Breakage in transit → items touching each other or the wall; more cushioning, tighter packing, a double box.

Dangers

Warning Hot wax catches fire if overheated and burns skin deeply. Melt it in a water bath only, never over a bare flame, and keep a lid nearby to smother a wax fire — never pour water on it.

  • Lifting: lift sacks and boxes with a straight back and bent knees, close to the body. Most injuries in stores and docks are backs.
  • Stacks of sacks and crates fall and crush. Interlock layers; keep stacks under 2 m; never climb them.
  • Nails sticking out of crates and pallets cause deep, dirty wounds; clench them or pull them (Wound Care and Antiseptics).
  • Water skins and old containers can grow germs; clean and dry them, and never store drinking water in a container that once held oil, lye or poison.
  • Children can suffocate shut in trunks: fit catches that open from inside.

What this unlocks

Standard sacks, crates and pallets make trade and storage measurable and efficient (Money, Trade and Record-keeping, Measurement from Scratch); they are what Railways, canals and harbours move. Cardboard leads to files and folders, book boards and Toys. Pallets and standard loads lead to the forklift and the shipping container (Moving Goods: Pallet Trucks, Forklifts and Containers).

How it was first done

Sacks and water skins are far older than writing, and water skins are still used by desert herders. Jute sacking from Bengal, woven by power looms in Dundee, Scotland, from the 1830s, became the world's sacks. Francis Wolle patented a paper-bag machine in the United States in 1852, and Margaret Knight invented a machine to make flat-bottomed paper bags, patented in 1871. Corrugated paper was patented in England in 1856 by Edward Healey and Edward Allen, to line tall hats; Albert Jones in New York patented corrugated paper for wrapping bottles in 1871, and Oliver Long added liners in 1874. Robert Gair, a Brooklyn printer, found in 1879 that cutting and creasing board in one stroke could make folding cartons by the thousand. The waxed paperboard milk carton was patented in 1915. The modern wooden pallet grew up with the forklift truck in the 1930s and 1940s, and the European pallet size of 120 × 80 cm was agreed in 1961.

Source: content/entries/home/containers-and-packaging.md