◆ Rebuild

Part 9 · Health and Medicine

Tissue Slides and the Microtome

To see disease in a lump, an ulcer or an organ, you must slice tissue thinner than a single cell. How to fix a biopsy, carry it through alcohol and wax in a tissue cassette, cast it into a paraffin block, build a hand microtome and a rocking microtome with a lever feed, sharpen the knife, cut and float ribbons of sections onto glass slides, make frozen sections in minutes during an operation, and begin to read tissue for inflammation, tuberculosis and cancer.

Difficulty
●●●●●
Time
A week to build a rocking microtome; one to two days from biopsy to stained slide; 15 minutes for a frozen section
Steps from zero
18 prerequisites →

You need first

Biological StainsThe Microscope

This unlocks

—
The full path from nothing — 18 steps before this one
  1. Stone Tools
  2. Fire
  3. Finding and Preparing Clay
  4. Simple Machines
  5. Quarrying and Cutting Stone
  6. Pottery
  7. The Kiln
  8. Mining and Tunnelling
  9. Lime
  10. Fermentation
  11. Lye and Potash
  12. Glass
  13. Distillation
  14. Coal and Coke
  15. Coal Tar Chemicals
  16. Lenses
  17. The Microscope
  18. Biological Stains
  19. Tissue Slides and the Microtome

Do them roughly in this order. See it on the tech tree →

Why it matters

A lump in a breast, an ulcer that will not heal, a swollen gland. Eyes and hands often cannot tell whether it is harmless, an infection, tuberculosis or cancer. Under the microscope, a thin slice of it usually can.

  • Cancer or not, and whether the surgeon has cut it all out.
  • Which infection: tuberculosis, leprosy, fungus, parasites, each treated differently (Infectious Diseases).
  • What killed someone, so the living can be protected.
  • Teaching: a set of slides of normal tissue teaches How the Body Works and Cells, Life and Evolution better than any picture.

Light cannot pass through a lump of tissue. It must be cut into slices about 5 µm thick (5 thousandths of a millimetre, thinner than one cell) and stained (Biological Stains). Cutting that thin and evenly is a mechanical problem, and this chapter is mostly about the machines that solve it.

How it works

  • Fixing kills the tissue instantly and links its proteins together so it does not rot or change shape (Methanol and Formaldehyde).
  • Soft tissue cannot be sliced thin. It squashes like jelly. So the water in it is replaced, step by step, with paraffin wax, which fills every cell. Wax and tissue then cut together like one firm, uniform block.
  • Water and wax do not mix. Alcohol pulls out the water (dehydration). A clearing agent, a liquid that mixes with both alcohol and wax (xylene, toluene, cedarwood oil), replaces the alcohol. Molten wax replaces the clearing agent.
  • A microtome moves the block past a very sharp knife and, between strokes, advances it by an exact, tiny step. Each stroke shaves off one section. Warm wax sections stick edge to edge and come off as a ribbon.
  • Frozen sections skip the wax: ice does the stiffening. Faster, but thicker and cruder.

What you need

Item Notes
Fixative 10% formalin, 10–20 times the tissue's volume (Biological Stains)
Alcohol 70%, 90% and absolute (Distillation); about 1 litre of each to start
Clearing agent Xylene or toluene (Coal Tar Chemicals), or cedarwood oil
Paraffin wax Melting at 56–58 °C, 2–3 kg (Petroleum and Refining)
Wax oven or bath Held at 58–62 °C (Thermostats and Automatic Control, The Thermometer)
Tissue cassettes Below
Embedding moulds Brass L-pieces on a metal plate
Microtome and knife Below
Water bath A dish of water held at 40–45 °C
Slides and cover slips Below
Egg white, glycerol Section adhesive
Stains and Canada balsam Biological Stains

Where to find it

  • Paraffin wax — pressed from chilled heavy oil from Petroleum and Refining or oil shale. Beeswax alone is too sticky, but up to 5% in the paraffin helps the ribbon hold together (Beekeeping).
  • Cedarwood oil — steam-distilled from the heartwood of eastern red cedar or other junipers (Distillation); slower but less harmful than xylene.
  • Canada balsam — the clear resin from blisters in the bark of the balsam fir.

Taking and fixing tissue

The slide can only be as good as the specimen.

  1. Fix at once. Put the tissue into formalin within half an hour of removal. Delay lets the cells digest themselves, and nuclei, the main thing you look at, go blurred.
  2. Label the jar with name, site, date and time. Mixed-up specimens are the worst mistake a laboratory can make.
  3. Measure and describe the specimen before cutting: size in cm, weight, colour, firmness, any lump and its distance from the cut edges (Writing and Numbers).
  4. Ink the margins. Paint the cut surgical edges with carbon ink (Ink) and let it dry a minute. Ink survives processing. If cancer later touches the ink on the slide, it reaches the edge: some was left behind.
  5. Slice it with a sharp blade into slices no more than 3–4 mm thick and small enough to fit a cassette (about 2 × 2.5 cm). Fixative creeps in only about 1 mm an hour, so thick pieces rot in the middle.
  6. Fix at least 24 hours, longer for fatty tissue.

The tissue cassette

A tissue cassette is a small perforated box that holds each piece of tissue, with its label, through all the baths, so that pieces never mix and are never lost.

  • Simplest: a square of fine cotton gauze or lens paper folded around the tissue and its label, tied with thread.
  • Better: a box about 30 × 25 × 6 mm of thin tinned brass or copper sheet (Sheet Metal and Rolling), punched all over with 1 mm holes 3 mm apart, with a lid hinged on a wire pin and a spring catch. Holes must be small enough that tiny biopsies cannot fall out; for very small pieces, wrap them in lens paper inside the cassette.
  • Label with a slip of card written in soft pencil. Graphite survives alcohol, xylene and hot wax; most inks dissolve.

A good cassette drains completely when lifted, shuts firmly, and does not rust.

Processing schedule for 3 mm slices, with the cassettes moved by hand from jar to jar (each jar at least 20 times the volume of tissue):

Bath Time
70% alcohol 1 hour
90% alcohol 1 hour
Absolute alcohol, 3 changes 1 hour each
Xylene or toluene, 2 changes (or cedarwood oil overnight) 1 hour each, until the tissue looks translucent
Molten paraffin, 3 changes at 58–62 °C 1 hour each

Absolute alcohol takes up water from the air; keep it stoppered and dry it with a spoonful of white, roasted copper sulfate in the bottle (it turns blue when spent). Never heat wax above 65 °C: overheated tissue turns brittle and crumbles in the microtome.

Embedding: the paraffin block

1. Cassette 2. Embed in L-pieces 3. Trim the block 4. Cut a ribbon 5. Float at 40–45 °C 6. Pick up on a slide B7 30 × 25 × 6 mm, 1 mm holes; pencil label inside two brass L-pieces on a plate; tissue cut face down on the bottom 2–3 mm wax margin; top and bottom parallel sections 4–5 µm, stuck edge to edge in a ribbon wrinkles flatten in 20–30 s slide smeared with egg white and glycerol; dry overnight at 37–60 °C, then stain
Fig. 1 From tissue to slide. Fixed tissue travels through alcohols, clearing agent and wax in a labelled perforated cassette. It is set face down in molten wax inside a mould of two brass L-pieces. The cooled paraffin block is trimmed to a neat shape with parallel top and bottom edges, cut on the microtome into a ribbon, floated flat on warm water, and picked up on a glass slide.

Embedding moulds. The classic mould is a pair of Leuckart's L-pieces: two L-shaped bars of brass about 1–1.5 cm high and 5 cm along each arm, laid on a flat brass or glass plate so their arms overlap to make a rectangle of any size. Paper boats folded from stiff paper smeared with glycerol, or small tin trays, also work. Warm the mould and smear it with a trace of glycerol so the wax lets go.

  1. Fill the mould with clean molten wax, a few degrees above its melting point.
  2. With warmed forceps, lay the tissue in it cut face down, flat on the bottom. That face becomes the face you section.
  3. Slide the mould onto a cold metal plate. As a skin of white wax forms on the bottom, the tissue is held in place. Lay the pencil label in the wax at one end.
  4. When a skin forms on top, float the mould in cold water to set the block quickly. Slow cooling grows coarse crystals that crumble.
  5. Lift off the L-pieces. You have a paraffin block.

Trimming. Cut away surplus wax with a sharp blade, leaving 2–3 mm of wax around the tissue. Make the top and bottom edges exactly parallel: they will meet the knife edge-on, and parallel edges give a straight ribbon. Melt the back of the block onto a hardwood holder or metal chuck with a hot spatula.

A good block is milky white throughout, with no cracks, crystals or soft spots, and the tissue sits flat at one face. Chalky white patches inside the tissue mean water or alcohol was left behind: melt it out, and redo the clearing and wax.

The microtome

Every microtome has three parts: a rigid knife clamp, a block holder that moves past the knife, and a feed that advances the block by a fixed step between strokes.

The hand microtome (simplest)

A brass or hardwood cylinder about 4 cm across and 10 cm tall with a flat, polished glass or brass table on top and a 12 mm hole in its middle. Below the hole, a well holds the specimen; a fine screw underneath pushes it up. With a screw of 1 mm pitch and a head divided into 50 marks, each mark raises the specimen 20 µm. Clamp the specimen in the well between two halves of carrot or elder pith, or set it in wax. Slide a razor flat across the table in one drawing stroke, raise one or two marks, and cut again.

It cuts 15–30 µm: good for plants and frozen tissue, too thick for fine detail. Build it first; it teaches you about knives.

The rocking microtome (to build)

Fixed knife edge horizontal Paraffin block on its holder Rocking arm, 25 cm swings the block down past the edge handle Knife-edge pivot Sliding carriage moves 2 µm per tooth Lever 10 : 1 Screw 1 mm pitch Ratchet 50 teeth Return spring lifts the block back up pawl, worked by the handle
Fig. 2 A rocking microtome. The block is held at the front of a rocking arm that swings up and down past a fixed knife. The arm's pivot sits on a carriage that a lever moves towards the knife. A fine screw, turned one or more teeth of its ratchet wheel at each stroke, pushes the long end of the lever; the short end moves the carriage ten times less, a few micrometres per stroke.

The rocking microtome, invented in Cambridge in 1885, is simple enough to build in a good workshop (Scientific Instrument Making) and cuts paraffin ribbons as well as far costlier machines.

  1. Base. A heavy, rigid base of cast iron, or thick, well-seasoned hardwood bolted to a stone or heavy table. Any flex shows as uneven sections.
  2. Knife clamp. Two strong pillars at the front holding the knife with its edge horizontal, facing back towards the block, gripped by screws.
  3. Rocking arm. A stiff steel bar about 25 cm long. Its front end carries the block holder; its rear rests on a pivot, ideally a pair of hardened steel knife-edges sitting in V-grooves (no slack, no wear). A spring or weight on a cord pulls the rear down, so the front rises. Pulling a handle (or a cord) rocks the front down, sweeping the block past the knife in a gentle arc; releasing it lets the block rise behind the knife.
  4. Carriage. The pivot sits on a carriage that slides towards the knife in tight, oiled guides, held back against the feed by a light spring so all slack is always taken up in one direction.
  5. Feed. A screw of 1 mm pitch (Screws, Nuts and Bolts) carries a ratchet wheel of 50 teeth. At each stroke, a pawl on the handle linkage turns the wheel by an adjustable number of teeth. One tooth turns the screw a fiftieth of a turn: the screw tip advances 20 µm. The screw pushes the long arm of a 10 : 1 lever; the short arm pushes the carriage 2 µm. Set the pawl to take 2–5 teeth and you cut 4–10 µm sections. The lever also divides any error in the screw thread by ten.

Feed per stroke = screw pitch ÷ teeth on wheel × teeth taken ÷ lever ratio.

Rocking microtomes cut slightly curved sections, which does not matter for blocks up to 2–3 cm across.

The rotary microtome (industrial)

A handwheel drives the block straight up and down on precision slides past a fixed knife, advancing it by a micrometer screw at each turn. It cuts large blocks perfectly flat, but needs precision-ground slides and screws (Machine Tools, Precision Grinding).

The microtome knife

  • Shape. A steel blade 12–25 cm long, wedge-shaped, ground plane on both faces, 1–2 cm deep. A long knife lets you move along to a fresh part of the edge many times before resharpening.
  • Steel. High-carbon steel, hardened and tempered to a light straw colour (Axes, Chisels, Knives and Planes).
  • Edge. The final facet is ground at about 25–35° with the help of a back, a split sleeve slipped over the blade's back that holds it at a fixed angle on the hone.
  • Sharpening. On a flat glass plate with fine abrasive and oil, or a fine natural hone, edge leading, with light, even strokes on alternate faces; finish on a leather strop, edge trailing (Sharpening and Honing, Abrasives and Grinding Stones).
  • Clearance angle. Set the knife so its lower face clears the cut surface of the block by 3–5°. Too little and the block rubs and sections are compressed; too much and the knife scrapes and chatters.
  • Testing. Look along the edge at 50–100× under the microscope with light from the side. It should be a thin, unbroken line with no nicks or bright spots.
  • Razor blades. A safety-razor blade clamped firmly in a holder (Razors, Nail Clippers and Grooming Tools) cuts excellent paraffin sections. Use a fresh part of the blade for each block.

Cutting sections

  1. Chill the block face on ice for a few minutes. Cold wax cuts thinner and cleaner.
  2. Align the block so its top and bottom edges are parallel to the knife edge.
  3. Face the block at 15–20 µm until the whole cut face of the tissue is exposed. Re-chill.
  4. Set 4–5 µm and cut with a steady, unhurried rhythm. A ribbon forms on the knife. Lift its end with a fine wet brush and lay it on dark paper.
  5. Float short lengths of ribbon on the water bath at 40–45 °C, about 10 °C below the wax's melting point. In 20–30 seconds the wrinkles flatten.
  6. Pick up each section on a slide smeared with a very thin film of egg-white adhesive (equal parts egg white and glycerol, filtered through cloth, with a crystal of thymol to keep it). Dip the slide under the section and lift it out at an angle.
  7. Drain upright 30 minutes, then dry overnight at 37–60 °C. Undried sections float off in the stains.
  8. Stain and mount: haematoxylin and eosin, or special stains, then Canada balsam under a cover slip (Biological Stains).

Slides and cover slips

Slides are 76 × 26 mm (the old 3 × 1 inch), 1.0–1.2 mm thick.

  1. Choose the flattest, clearest window or plate glass, free of bubbles and ripples.
  2. Score it on a ruled jig with a diamond or a hardened steel wheel, and snap (Glass).
  3. Grind the edges and corners smooth on a flat stone with emery and water (Abrasives and Grinding Stones), so they do not cut fingers.
  4. Grind one end matt with emery: a frosted label patch to write on in pencil.
  5. Clean in hot soapy water, rinse, then in alcohol with a drop of hydrochloric acid. Store in alcohol or dust-free boxes.

Cover slips are thin glass, 0.13–0.17 mm, about 22 × 22 mm or longer. High-power objectives are designed for 0.17 mm of glass; much thicker and the image goes soft (The Microscope). Make them by blowing thin glass bubbles or drawing very thin sheet; measure each batch with a micrometer and sort by thickness.

Good or bad: a clean slide sheets water evenly without beading; a flat one does not rock on a glass plate; a good cover slip is free of scratches and flat enough not to show rainbow rings when pressed on a slide.

Frozen sections

When a surgeon has the patient open and needs to know now whether a lump is cancer, or whether the edges are clear, wax takes too long. Freezing takes minutes.

  1. The freezing stage is a block of copper or brass, about 3 cm across, fitted to the microtome in place of the block holder, with a hollow under it. Cool it by any of:
    • packing the hollow with crushed ice and salt (2 : 1), reaching about −15 to −20 °C (Ice and Refrigeration);
    • spraying ether through a fine jet against its underside, where evaporation chills it;
    • letting carbon dioxide gas from a cylinder expand through a nozzle under it, the classic freezing microtome.
  2. Freeze. Put a drop of water or thin gum on the stage, press a fresh or briefly fixed slice of tissue 3 mm thick onto it, and freeze until it is white and hard right through.
  3. Cut at 10–20 µm with a cold knife. Sections curl onto the knife; take them off with a cold wet brush into water.
  4. Fix and stain fast. Pick a section up on a slide, fix 30 seconds in alcohol or formalin, and stain with a quick haematoxylin and eosin, or 30 seconds in 1% methylene blue (Biological Stains). Rinse, cover, look.

From specimen to answer takes 10–20 minutes. Frozen sections are thicker and blurrier than paraffin sections; report only what you are sure of, and always confirm with a paraffin section the next day. Frozen sections are also needed to stain fat, which wax processing dissolves away.

Reading tissue for disease

Reading slides is a skill of years. Start by learning normal: cut and keep a reference set of every normal tissue you can get from operations, post-mortems and butchered animals (How the Body Works, Butchery and Meat). Always look at low power first to see the pattern, then high power for the cells.

Normal lining Cancer one row, small even nuclei intact basement membrane big dark nuclei, varied shapes odd mitosis cells invade the tissue below membrane broken Haematoxylin stains nuclei dark blue-purple (shown dark here); eosin stains cytoplasm and supporting tissue pink. Invasion through the membrane is the surest sign of cancer; odd-looking cells alone may be only irritated.
Fig. 3 Normal and cancerous lining, as seen in a section. Left: a normal lining with one orderly row of similar cells, small even nuclei, all sitting on an unbroken basement membrane. Right: cancer, with crowded, disorderly cells; large, dark nuclei of different sizes and shapes; abnormal dividing cells; and groups of cells breaking through the membrane into the tissue below.
What you see What it suggests
Tissue swollen, crowded with cells with 2–5-lobed nuclei (neutrophils), threads of pink fibrin Acute inflammation; a dense mass of them with dead tissue is an abscess
Many small round dark nuclei (lymphocytes), cells with off-centre "clock-face" nuclei (plasma cells), pink bands of collagen Chronic inflammation and scarring
Tight clusters of pale, elongated cells, giant cells with many nuclei in a horseshoe, a ring of lymphocytes Granuloma. With cheesy, structureless pink centres: probably tuberculosis; confirm with an acid-fast stain (Biological Stains)
Cells pale pink, nuclei shrunken, broken or gone, outlines still visible Dead tissue (necrosis): infarct, infection or tumour
Orderly cells much like the tissue they came from, even nuclei, smooth border, often a capsule Benign tumour
Large, dark nuclei varying in size and shape, big nucleoli, many and odd dividing cells, loss of normal layers, cells breaking through the basement membrane, into vessels or nerves Cancer
Spiny eggs in bladder or liver; worm segments; fungal threads; brown-black malaria pigment Parasites and fungi

Warning A wrong reading can kill. Calling a harmless lump cancer can lead to a mutilating operation; missing cancer lets it spread. Report what you see, in plain words, with how sure you are. When unsure, say so, cut more levels, ask another reader, and decide with the patient's whole story (Examining a Patient). Photograph difficult slides (Photography) and keep every block and slide: they can be re-cut and re-read for decades.

How to tell it worked

  • Sections are thin and even: at high power you see one layer of cells, not overlapping ghosts, with crisp nuclei.
  • The whole tissue face is in the section, with no holes, tears or folds.
  • The ribbon is straight and continuous.
  • A good stain shows blue nuclei with visible inner detail and pink background (Biological Stains).

Note Troubleshooting. Block crumbles, tissue falls out of the wax → poor fixation, dehydration or clearing; or wax too hot. Reprocess from absolute alcohol. Lines or scratches along the section → a nick in the knife. Move to another part of the edge. Thick and thin bands across the section (chatter) → something loose: tighten knife, block and holder; reduce the clearance angle; cut more slowly. Sections squashed and wrinkled → blunt knife, warm block or room. Sharpen, chill. Ribbon will not form → room too cold or wax too hard; breathe on the block, or dip its top and bottom edges in softer wax. Ribbon curves → top and bottom edges of the block not parallel. Re-trim. Alternate thick and thin sections → slack in the feed or a worn pivot; check the spring takes up all play. Sections float off the slide → no adhesive, or not dried long enough.

Dangers

Danger Microtome knives are sharper than surgical scalpels. Always fit a guard over the edge when not cutting, lock the arm or wheel before changing blocks, keep fingers out of the line of the edge, and never try to catch a falling knife.

  • Formalin fumes irritate eyes and lungs, cause lasting allergies, and cause cancer with long exposure. Work in a strong draught, keep jars closed.
  • Xylene, toluene, alcohol and ether are highly flammable; ether vapour can explode. No flames near them; heat wax ovens electrically or with a closed, distant flame.
  • Hot wax causes burns and fires. Never heat it directly on a flame. Smother a wax fire with a lid; never use water.
  • Fresh tissue can be infectious: tuberculosis, hepatitis, HIV. Wear gloves; fix tissue before handling it when you can. Never freeze-section tissue suspected of tuberculosis: cutting it frozen throws infectious particles into the air.
  • Avoid mercury fixatives and dry picric acid (which can explode).

What this unlocks

Tissue diagnosis makes Basic Surgery rational: what to remove, how much, and whether it worked. It decides which cancers need Radiotherapy (Overview), and it belongs on the same bench as the The Medical Laboratory. It recognises tuberculosis, leprosy and parasites (Infectious Diseases), explains Animal Health post-mortems, and serves Cells, Life and Evolution, Saving Seed and Breeding Plants and the study of Rot, Woodworm and Termites.

How it was first done

Robert Hooke sliced cork with a penknife for his Micrographia in 1665 and saw the first "cells". The Microscopical Society of London fixed the 3 × 1 inch slide in 1840. Rudolf Virchow argued in 1858 that every disease is a disease of cells, which made the tissue section the foundation of pathology. Wilhelm His built a microtome with a mechanical feed in 1866; Edwin Klebs introduced paraffin embedding in 1869. Horace Darwin, Charles Darwin's son, designed the Cambridge rocking microtome in 1885, and Charles Minot in Boston developed the rotary microtome in the 1880s. Ferdinand Blum found that formaldehyde fixes tissue in 1893. William Welch at Johns Hopkins made one of the first frozen-section diagnoses during an operation in 1891, and Louis B. Wilson at the Mayo Clinic made rapid frozen sections a routine service from 1905.

Source: content/entries/health/histology.md