Part 14 · Electronics and Computing
Flat Screens: LCD and LED Displays
Screens a few millimetres thick that need only a few volts. How liquid crystals between polarisers make light and dark, how a grid of transistors on glass controls millions of dots, how backlights and colour filters work, and how LED, OLED and glowing-powder screens make their own light. A workshop can make conductive glass, polarising film, simple segment displays and glowing panels; full colour screens need a chip industry.
- Difficulty
- ●●●●●
- Time
- A week to make conductive glass and polarising film; a month for a first segment LCD once you have a liquid crystal; a whole industry for colour screens
- Steps from zero
- 77 prerequisites →
This unlocks
SmartphonesThe full path from nothing — 77 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Sulfur
- Writing and Numbers
- Hunting and Trapping
- Basic Woodworking
- The Kiln
- Pottery
- Charcoal
- Arithmetic and Fractions
- Hides and Leather
- Lime
- Bricks
- Salt
- Mercury
- Lye and Potash
- Fermentation
- The Wheel and Axle
- Logic and Binary
- Glass
- Firebrick and Refractories
- Bellows
- Saltpeter
- The Lathe
- Gears
- Glass Fibre and Glass Wool
- Copper Smelting
- Iron (the Bloomery)
- Lead
- Laboratory Glassware
- Sulfuric Acid
- Pumps
- The Waterwheel
- Lenses
- Blacksmithing
- Gold and Silver
- The Blast Furnace and Cast Iron
- Bronze
- Hydrochloric Acid
- The Battery
- The Vacuum Pump
- Magnets
- Optical Glass and Achromatic Lenses
- Steel
- Chimneys, Stoves and Heating
- Bearings and Lubrication
- The Steam Engine
- The Light Bulb
- Copper Wire
- Electrolysis
- Photography
- Polarised Light
- Hydrogen, Oxygen and Gases
- Centrifugal Pumps and Fans
- Machine Tools
- The Generator
- The Electromagnet
- The Vacuum Tube
- The Electric Arc Furnace
- Ammonia
- The Induction Coil
- The Telegraph
- Ice and Refrigeration
- The Telephone
- Pure Silicon
- Ventilation and Air Conditioning
- Semiconductors and the Transistor
- Radio
- Clean Rooms
- Integrated Circuits
- Cathode Rays and Television
- The Computer
- Making Microchips
- Displays, Printers and Data Storage
- Flat Screens: LCD and LED Displays
Do them roughly in this order. See it on the tech tree →
Why it matters
The cathode-ray tube of Cathode Rays and Television is heavy, deep, fragile, and needs thousands of volts. A flat screen is a few millimetres thick, runs on a few volts, and can be the size of a watch face or a wall. Flat screens made pocket calculators and digital watches possible in the 1970s, laptops in the 1980s, and Smartphones in the 2000s.
There are two families. A liquid crystal display (LCD) makes no light; it is a grid of tiny electric shutters in front of a lamp or a mirror. An emissive screen makes its own light at every dot: light-emitting diodes (LEDs), organic LEDs (OLED), or glowing powders. Both are explained here, with the parts a workshop can make: conductive glass, polarising film, a segment LCD, an electroluminescent panel, an LED matrix and touch panels.
How it works
Liquid crystals
Some substances made of long, rod-shaped molecules melt in two stages. Above their melting point they become a cloudy liquid in which the rods flow but stay roughly parallel to each other, like logs floating down a river. Hotter still, they become an ordinary clear liquid. In between they are liquid crystals. The common kind for displays is called nematic (from the Greek for "thread").
Two facts make displays possible:
- The rods line up with a surface. Rub a thin film of plastic on glass in one direction with a cloth, and the rods touching it lie along the rubbing.
- An electric field turns them. The rods carry a slight electric imbalance along their length, so a voltage of a few volts across a thin layer swings them to point along the field.
Liquid crystals are birefringent, like the Iceland spar of Polarised Light: they change the polarisation of light passing through them.
The twisted-nematic cell
Take two glass plates, each coated on the inside with a transparent conductor and a rubbed film. Set them 5–10 micrometres (μm) apart with the rubbing directions at right angles, and fill the gap with nematic liquid crystal. The rods lie along the rubbing at each plate and twist smoothly through a quarter turn between them, like a spiral staircase. Put a polariser outside each plate, crossed.
- No voltage: light passing the first polariser is turned through a quarter turn by the twist, so it passes the second polariser. The cell looks clear.
- 3–5 volts: the rods stand up along the field, the twist is gone, the light is not turned, and the crossed polariser blocks it. The cell looks black.
Shape the conductor on one plate into seven bars and you have a seven-segment digit that draws a few millionths of an ampere. Put a mirror behind it and it works by room light alone, which is why calculators and watches could run for years on one small cell.
Always drive with alternating voltage. Steady (direct) voltage slowly splits the liquid crystal by Electrolysis and ruins it within days. Feed the common plate a square wave of 30–100 cycles a second; feed each segment either the same wave (no voltage across it: clear) or the inverted wave (full voltage, alternating: dark). An exclusive-OR gate per segment does it.
Many dots: passive and active matrix
A screen of many dots cannot have a wire for each. In a passive matrix, one plate carries row stripes and the other column stripes; rows are selected one at a time, as in the keyboard matrix. It works for a few dozen rows, but each dot gets its voltage only a small fraction of the time, so contrast falls as rows increase.
In an active matrix each dot has its own thin-film transistor (TFT), made directly on the glass, and a tiny capacitor. The row line turns on all transistors in a row for a moment; each column line charges its dot's capacitor to the right voltage; the transistor turns off and the capacitor holds the charge until the next frame. On a screen of 1,080 rows refreshed 60 times a second, each row gets about 15 millionths of a second. The transistors are made of silicon laid down from gas onto glass at about 300 °C, by the same loop of layers, masks and etching as Making Microchips, but over glass sheets the size of a door.
Colour and light
Each dot is split into three: red, green and blue, under a colour filter of dyed resin printed on the front glass. Behind the panel a backlight shines evenly: LEDs along one edge shine into a clear acrylic plate printed with white dots that scatter the light forward, through diffusing and prism sheets. Only about 5% of the backlight reaches your eye; the rest is lost in polarisers and filters.
Emissive screens
- LED screens: each dot is a light-emitting diode (Light-Emitting Diodes). Large outdoor screens are boards of separate red, green and blue LEDs, 2–20 mm apart.
- OLED: layers of organic compounds about a tenth of a micrometre thick, between two electrodes, glow when current passes. Every dot makes its own light, so blacks are truly black; but the materials are destroyed by traces of water and must be sealed perfectly.
- Electroluminescent panels: a powder of zinc sulfide containing a trace of copper glows green-blue when an alternating voltage is put across it. Dim, but simple enough for a workshop.
What you need
| Item | For | Notes |
|---|---|---|
| Flat glass, 1–2 mm thick | All panels | Window Glass; soda-free glass is best but not essential for segment displays |
| Tin(IV) chloride | Conductive glass | From tin and chlorine (Tin and Pewter, Chlorine and Bleach) |
| Hotplate or small furnace to 500 °C | Conductive glass | With a thick iron plate to keep the glass evenly hot |
| Sprayer | Conductive glass | A glass atomiser blown by a hand bellows or air pump |
| Polyvinyl alcohol, iodine, potassium iodide | Polarising film | From acetylene (Calcium Carbide and Acetylene) and Iodine |
| Nematic liquid crystal | LCD | See Where to find it |
| Glass fibre or beads 5–10 μm | Spacers | Glass Fibre and Glass Wool |
| Epoxy or other strong two-part glue | Seals | Glues and Adhesives |
| Zinc sulfide, copper sulfate, salt | Electroluminescent powder | From zinc ore and Copper Smelting |
| A transformer giving 100–200 V at 400–1,000 cycles a second | Electroluminescent panel | From an oscillator and The Transformer |
Where to find it
- Tin for tin oxide: cassiterite, heavy brown-black pebbles in stream gravels (Tin and Pewter).
- Indium, for the better conductor indium tin oxide, is recovered in small amounts from the residues of zinc smelting of sphalerite (Zinc and Brass). Tin oxide alone works well enough to start.
- Iodine from seaweed ashes (Iodine).
- Quinine, for the older crystal polariser, from cinchona bark (Making Medicines).
- Liquid crystal: the simplest useful one, MBBA, is made by warming two compounds together and driving off water: anisaldehyde, made by oxidising the oil of anise or fennel seed, and butylaniline, made from benzene (Coal Tar Chemicals). It is a liquid crystal from about 21 °C to 47 °C. It suits the "dynamic scattering" display below but not the twisted-nematic cell, which needs liquid crystals of the cyanobiphenyl family. Those take several steps of skilled organic synthesis. A real LCD therefore depends on a working organic chemistry laboratory; this is the hardest part of the chapter.
Conductive glass
Conductive glass carries a film thin enough to see through that conducts electricity. It is the front electrode of every flat screen, touch panel and many Solar Cells.
- Dissolve tin(IV) chloride in alcohol or water, about 1 part in 5 by weight. A few percent of ammonium fluoride (made from fluorite) or antimony chloride makes the film conduct several times better.
- Clean the glass in hot soapy water, then alcohol. Lay it on a thick iron plate heated to 450–550 °C — a scrap of zinc laid beside it should melt (419 °C) and a scrap of aluminium should not (660 °C).
- Spray a fine mist over it in short passes, a second or two each, letting the glass recover its heat between passes. The tin chloride turns to tin oxide on the hot surface. As the film thickens it shows interference colours, as oxide on silicon does; stop at the first or second full cycle of colours.
- Let the plate cool slowly on the iron, or it will crack.
Patterning: before spraying, paint the areas that must stay bare with a thick paste of chalk and water-glass (Water Glass (Sodium Silicate)) and wash it off afterwards. Or coat the whole plate, protect the pattern with a resist (wax, varnish or photoresist, Integrated Circuits), and etch the rest by dusting with zinc powder and wetting with dilute Hydrochloric Acid: the oxide dissolves in a minute.
Good or bad: measure the resistance between two straight copper bars laid 1 cm apart on a 1 cm wide strip: this is the resistance per square. Good tin oxide reads 10–50 ohms; industrial indium tin oxide, about 10. The glass should look clear, perhaps faintly tinted, with no milkiness.
Polarising film
Every LCD needs two polarisers, larger and more even than the pile-of-plates or Nicol prism of Polarised Light.
Stretched-film polariser (the modern kind):
- Cast a film of polyvinyl alcohol (PVA) 0.05–0.1 mm thick by pouring a warm 10% solution in water onto clean glass and drying it.
- Soften the dry film in warm air (about 100 °C) and stretch it slowly to 4–5 times its length between two clamps. The long molecules line up.
- Dip it for a minute in a solution of iodine and potassium iodide in water (roughly 1 g iodine and 2 g iodide in 100 ml), then in a few percent boric acid to fix it. The iodine forms long chains along the stretched molecules, which absorb light polarised along them.
- Glue it between two sheets of clear film or glass to protect it from damp.
Crystal polariser (the older kind): dissolve quinine sulfate in acetic acid and alcohol and add iodine solution; olive-green needle crystals of herapathite form. Ground very fine and stirred into a lacquer, they are lined up by drawing the wet film out through a narrow slot, and the film dries as a polariser.
Good or bad: two films held together and turned look clear when their stretching directions are parallel and nearly black when crossed. Good film passes about 40% of ordinary light (the best possible is 50%) and stays evenly dark when crossed, with no blue or brown tint.
The liquid crystal display
Method 1: dynamic scattering (no polarisers)
MBBA with a pinch of a salt dissolved in it conducts slightly. Put 10–30 V across a thin layer and the flowing ions stir it into turbulence that scatters light: the clear cell turns milky white where the electrodes are. Viewed against a black background, the lit segments show white. It needs no polarisers and no rubbed alignment, so it is the easiest liquid crystal display to make; but it draws more current, and its life is shorter.
Method 2: twisted nematic
- Pattern two plates of conductive glass: the front with the segments, each with a thin track running to a contact pad along one edge; the back with one large common electrode. A first display: one digit, segments 3 mm wide and 12 mm long, on plates 40 × 60 mm.
- Alignment layer: spin or wipe on a very thin film of PVA or a similar clear plastic, dry, and rub it in one direction 10–20 times with velvet or cotton cloth wrapped on a block. Rub the second plate at right angles to the first.
- Spacers: sprinkle a few glass-fibre pieces or beads, 6–10 μm thick, over one plate, and mix more into the glue for the seal.
- Seal: draw a thin line of glue around the edge of the display area, leaving a 2–3 mm gap as a fill hole. Press the plates together, rubbed faces inside, offset so the contact pads stick out, and let the glue set.
- Fill: stand the cell in a jar, pump out the air (The Vacuum Pump), dip the fill hole into a drop of liquid crystal, and let the air back in: it pushes the liquid crystal in. Close the hole with glue.
- Polarisers: glue one on each face, crossed, each lined up with the rubbing of the plate under it. For a reflective display, put a sheet of crinkled aluminium foil or brushed metal behind the back polariser.
- Drive with a 3–5 V square wave as explained above. The average steady voltage across any segment must stay below about 0.05 V.
Good or bad: the background is evenly light, with no swirls (uneven rubbing) or coloured patches (uneven gap); segments turn fully dark at 3 V and clear again in a fraction of a second; no bubbles; no segment shows a faint "ghost" when off.
The electroluminescent panel
A glowing panel needs no liquid crystal and no polarisers.
- Make the powder: precipitate zinc sulfide from a zinc salt solution with a sulfide (Zinc and Brass, Sulfur); wash and dry it. Mix in copper sulfate to give about 0.1% copper and 2–5% salt as a flux. Fire in a covered crucible at about 1,000 °C for an hour, cool, wash out the salt, and grind gently.
- Build the panel: on conductive glass, brush or screen-print (Screen Printing) a layer of the powder mixed in a clear varnish, about 0.05 mm thick. Over it, a layer of the whitest, finest insulating powder you have (barium titanate is best; titanium oxide from rutile will do) in the same varnish. Over that, a back electrode of silver or aluminium paint, shaped as the segments or letters you want.
- Seal the back with wax or glue against damp.
- Drive with 100–200 V AC at 400–1,000 cycles a second. Higher frequency gives more light and a bluer colour, but shorter life.
It glows green-blue in a dim room, enough for a clock face or an instrument dial. Expect it to fade to half brightness in some thousands of hours.
LED screens
The workshop version is a board of separate LEDs in a grid — the dot-matrix display made large. Modules of 8 × 8 LEDs, 5 mm across on a 10 mm pitch, are driven one row at a time by a transistor, with one current-limiting resistor per column, fed by a microprocessor that scans all rows at least 100 times a second. Because each LED is lit only one eighth of the time, it is pulsed at up to eight times its steady current (for example 80–100 mA for a lamp rated at 20 mA), within the maker's pulse rating. Tile modules together for a sign or a scoreboard. For colour, use three LEDs per dot and vary each one's brightness by switching it on for a varying fraction of each scan.
Making the LEDs themselves needs crystals of gallium compounds grown in very thin layers (Germanium, Gallium and Compound Semiconductors, Light-Emitting Diodes), using toxic gases and the machinery of Making Microchips. Until then a society makes the board and imports, salvages or substitutes the lamps (neon or filament lamps work, larger and hungrier).
Industrially, phone and television OLED screens evaporate the organic layers through thin metal masks with openings a few hundredths of a millimetre wide onto transistor glass, and seal them against all but a millionth of a gram of water a day per square metre.
How factories make colour LCDs
- Glass: sodium-free glass 0.5–0.7 mm thick, drawn from molten glass so neither face touches anything, in sheets up to about 2.9 × 3.4 m.
- Transistor glass: four or five rounds of deposit–print–etch make row lines, insulator, amorphous silicon, column lines and dot electrodes — a TFT for every coloured dot; about 25 million in a 4K television.
- Colour filter glass: a black grid, then red, green and blue resins, then a common electrode.
- Assembly: alignment layers are rubbed, seal glue drawn, liquid crystal dropped on in measured drops, the sheets joined in vacuum and cut into panels.
- Finishing: polarisers laminated on, driver chips bonded to the glass edge, backlight and frame added.
Touch screens
- Infrared grid (workshop): around the edges of any screen, a row of infrared LEDs along the top and left, facing phototransistors along the bottom and right (Photocells and Sensors). A finger breaks one beam in each direction. With beams every 5–10 mm and a scan by the computer, it finds the finger to within a few millimetres. No coating on the screen at all.
- Resistive (workshop): conductive glass at the back, and a thin clear plastic sheet with a conductive coating in front, separated by tiny insulating dots about 0.1 mm high and a few millimetres apart. Put 5 V across the glass from left to right; when a finger presses the sheet onto the glass, the sheet picks up a voltage that tells the left–right position. Then swap roles to read up–down. A pen or gloved finger works. The sheet wears and scratches in time.
- Projected capacitive (industrial): two layers of fine transparent conductor patterned as rows and columns behind the cover glass. A controller chip measures the tiny capacitance at every crossing (around a picofarad) about a hundred times a second; a finger nearby reduces it. Many fingers at once are found, nothing moves, and the glass on top can be tough and thick. This needs fine patterning and a dedicated chip.
Good or bad: a touch screen should report the same point to within a few millimetres every time, nowhere on the screen should be dead, and it should not report touches when none occur (wet or dirty edges are the usual cause).
How to tell it worked
- Conductive glass: clear, 10–50 ohms per square, even across the plate.
- Polariser: crossed films go nearly black.
- LCD: every segment switches fully and evenly, the background stays clear, and the display still works after a week of running.
- Electroluminescent panel: even glow, no bright sparking spots.
- LED matrix: no flicker when you move your eyes quickly across it; all dots equally bright.
Note Troubleshooting. Tin oxide film milky → glass too cool or spray too wet; hotter plate, finer mist, shorter passes. Film does not conduct → glass too hot or film too thin; add more passes. LCD dark all over, even with no voltage → polarisers parallel instead of crossed, or rubbing directions not at right angles. Swirling patterns → rubbing too light or uneven; dirt under the alignment layer. Display slowly fades or turns brown → steady voltage on the cell, or moisture in the liquid crystal (MBBA is ruined by damp air). Segments show when they should not → tracks to the pad also switch; make tracks narrow and hide them under a printed mask. Electroluminescent panel sparks and burns through → dust or a pinhole in the insulating layer; thicker insulating layer.
Dangers
Danger Electroluminescent drivers give 100–200 V AC, enough to kill. Enclose the transformer and connections; never touch the panel terminals while running.
Warning Tin(IV) chloride fumes in moist air, giving off hydrochloric acid; spray only outdoors or under a strong draught, with eyes and lungs protected. The hot spray plate burns badly.
- Liquid crystal chemicals: aniline compounds poison through the skin and as vapour; gloves, and work under a draught (Coal Tar Chemicals).
- Iodine stains and burns skin; its vapour irritates lungs.
- Old backlights (thin fluorescent tubes in screens before about 2010) contain mercury: break them only outdoors and do not burn them.
- Bright LEDs, especially blue ones, can damage eyes if stared at closely.
What this unlocks
- Displays for computers, instruments, clocks and calculators that run for years on small batteries.
- Smartphones: a touch screen is half of a phone.
- Solar Cells use the same conductive glass.
- Advertising signs, scoreboards and timetables with LED boards.
How it was first done
In 1888 the Austrian botanist Friedrich Reinitzer noticed that cholesteryl benzoate had two melting points, cloudy at 145 °C and clear at 179 °C; Otto Lehmann named such materials liquid crystals. Charles Mauguin described twisted layers guiding polarised light in 1911. Edwin Land made the first sheet polariser from herapathite crystals in 1929 and the stretched iodine–PVA film in 1938. Georges Destriau saw electroluminescence in zinc sulfide in 1936.
George Heilmeier's team at RCA showed dynamic-scattering displays in 1968. The twisted-nematic display was invented in 1970–71 by Martin Schadt and Wolfgang Helfrich at Hoffmann-La Roche and, independently, by James Fergason in the United States; George Gray's group at Hull found stable cyanobiphenyl liquid crystals in 1972. Sharp sold an LCD calculator in 1973, and LCD watches followed. Peter Brody at Westinghouse made the first active-matrix LCD in 1973; Walter Spear and Peter LeComber at Dundee showed amorphous-silicon transistors in 1979, which made large panels possible. Nick Holonyak made the first visible LED in 1962; Ching Tang and Steven Van Slyke at Kodak the first efficient OLED in 1987; Isamu Akasaki, Hiroshi Amano and Shuji Nakamura bright blue LEDs around 1993, which gave white backlights. E. A. Johnson described the capacitive touch screen in Britain in 1965, Samuel Hurst the resistive one in the early 1970s, and the PLATO teaching computer of 1972 used an infrared grid.