◆ Rebuild

Part 4 · Food and Farming

Troughs, Separators and Livestock Gear

The equipment that lets a few people look after many animals — water troughs, rat-proof feed bins and hay racks that stop waste, sheep hurdles, handling pens and races, sheep dips, cattle grids, barbed wire, branding irons and ear tags, ways to weigh livestock without a weighbridge, and the cream separator that spins every drop of cream out of milk.

Difficulty
●●●●●
Time
An afternoon for a hay rack or hurdle; a week for a handling yard and dip; a cream separator is a workshop project of several weeks
Steps from zero
19 prerequisites →

You need first

Keeping AnimalsBlacksmithingIron and Brass Wire

This unlocks

—
The full path from nothing — 19 steps before this one
  1. Stone Tools
  2. Fire
  3. Cordage and Rope
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Hunting and Trapping
  7. Basic Woodworking
  8. Charcoal
  9. Pottery
  10. Farming from Seed
  11. Hides and Leather
  12. Keeping Animals
  13. Bellows
  14. Iron (the Bloomery)
  15. Copper Smelting
  16. Blacksmithing
  17. Steel
  18. Copper Wire
  19. Iron and Brass Wire
  20. Troughs, Separators and Livestock Gear

Do them roughly in this order. See it on the tech tree →

Why it matters

Keeping animals is mostly carrying water, handing out feed, and catching animals one at a time. Good equipment cuts that work to a fraction. A self-filling trough waters a herd with no one there; a hay rack saves a third of the winter's hay from being trampled; a pen with a narrow race lets two people sort and treat three hundred sheep in a morning; marks and tags tell you whose animal is whose, and which ewe had twins.

Housing, feeding and breeding are in Keeping Animals; disease and treatments in Animal Health; fences, hedges and woven hurdles in Fences and Hedges; butter and cheese in Dairy and Cheese.

How it works: moving animals

Handling gear works with an animal's instincts, not against them.

  • Flight zone. Step into an animal's personal space and it moves away; step out and it stops. A tame cow's zone may be 1 m, a wild steer's 10 m.
  • Point of balance. Standing behind the shoulder moves an animal forward; standing in front of it turns it back.
  • Follow the leader. Sheep and cattle follow the animal in front. Keep the line moving and the rest follow.
  • They move towards light and open space, away from people and dead ends, and balk at shadows, puddles, bright reflections, dangling things and sharp corners.

So races have solid sides (the animal sees only the way ahead), curve gently, run towards light and an apparent way out, and are just wide enough for one animal so it cannot turn round.

What you need

Item For
Logs 40–60 cm thick, sawn timber, split ash or chestnut (Basic Woodworking, Doors, Windows and Joinery) Troughs, racks, hurdles, races
Stone, lime mortar, concrete (Stone Masonry, Mortar and Concrete) Troughs, dip bath, grid pit
Iron rod, sheet and wire (Blacksmithing, Sheet Metal and Rolling, Iron and Brass Wire); zinc for galvanising (Zinc and Brass) Bins, brands, tags, grid rails, barbed wire
Quicklime and sulfur (Lime, Sulfur) Dip
A lathe, gears and good steel (The Lathe, Gears, Making Ball and Roller Bearings) Cream separator

Water troughs

Animals need clean water always. Daily needs: cattle 40–80 L (a milking cow in summer, over 100 L), horses 30–50 L, pigs 10–20 L, sheep and goats 4–8 L. Give enough trough length that about a tenth of the herd can drink at once: about 60 cm per cow or 30 cm per sheep.

Rim height: cattle and horses 50–60 cm, sheep and goats 30–40 cm, pigs 20–25 cm, with a lower trough for calves and lambs.

Ways to make one:

  • Log trough. Split a log 40–60 cm thick in half and hollow the flat face with an adze, helped by laying coals on it and scraping out the char. Leave the ends solid and walls 6–8 cm thick. Oak, elm and chestnut last 10–20 years.
  • Stone trough. Cut from a block of sandstone with point and chisel (Stone Carving), walls 8–10 cm thick. It lasts centuries.
  • Concrete trough. Cast in a wooden mould with walls 8 cm thick and a wire mesh inside them, in a 1 : 2 : 3 cement–sand–gravel mix (Reinforced Concrete). Keep it wet for a week as it hardens.
  • Sheet-iron trough. Rivet galvanised iron sheet over an iron frame (Sheet Metal and Rolling). Light and movable.

Good practice. Stand the trough on a pad of stones or gravel so the ground round it does not churn to mud (which spreads foot rot). Fill it from a pipe with a float valve (Pipes, Plumbing and Aqueducts) or from a spring led in and out by a channel. Put a sloping stick or stone inside as a ramp so birds and small animals that fall in can climb out. Pig troughs must be heavy, round-bottomed and divided by iron bars every 30 cm, or pigs lie in them and tip them over. Scrub out green slime weekly. In frost, break the ice morning and evening; a log floating in the trough keeps a hole open longer.

Feed bins and hay racks

Feed bin. Grain for animals must be dry and rat-proof (Granaries and Food Storage). Build a wooden box on short legs, line it inside with tinned iron sheet nailed over every corner and edge, and give it a lid with a sloping top (so nothing is stacked on it) and a latch an animal cannot work. Divide it inside for oats, barley and bran. A box 120 × 60 × 70 cm holds about 500 litres: some 225 kg of oats or 375 kg of wheat or maize (oats weigh about 0.45 kg per litre, barley 0.6, wheat and maize 0.75).

Hay rack. Hay thrown on the ground is trampled, dunged on and refused; a third or more is wasted. A rack lets animals pull out a mouthful at a time.

  • Cattle and horses: a V-shaped rack 2–3 m long, two sloping sides of round bars 3 cm thick (or 12 mm iron rod) set 8–10 cm apart, the top about 1.5 m high. Allow 60–70 cm of rack per cow.
  • Sheep and goats: a lower rack with bars 5–7 cm apart, its bottom at shoulder height, set over a trough that catches the fallen leaves and seeds so they are eaten too. Allow 30–40 cm per sheep. Never feed sheep from a high rack: seeds fall into the wool and spoil it.

Pens, races and sheep hurdles

PLAN (from above) Gathering pen 0.5 m² per sheep Forcing pen solid funnel Race 40–45 cm wide, solid sides 6–10 m long single file Pen A Pen B Drafting gate swings to sort Draining pen drips run back Dip DIP BATH, cut along its length steep slide in: each sheep goes under 1.2–1.5 m 3–4 m at the surface Dip, 35–40 °C Cleated ramp out cleats every 20 cm draining pen floor slopes back end view: 60 cm top, 25–30 bottom
Fig. 1 A sheep handling yard and plunge dip, seen from above, with the dip in cross-section below. Sheep pass from the gathering pen through a funnel-shaped forcing pen into a narrow race with solid sides; a swinging gate at the end sorts them into pens, or sends them into the dip and out through the draining pen.

A handling yard is a set of pens laid out so animals flow through them in one direction:

  1. Gathering pen, big enough for the flock at about 0.5 m² per sheep (2 m² per cow).
  2. Forcing (crowding) pen — a funnel that narrows into the race. Make its sides solid.
  3. Race (chute) — a single-file passage, 6–10 m long, with solid sides. For sheep 40–45 cm wide inside and 90 cm high; for cattle 70–75 cm wide and 1.6–1.7 m high, built of heavy posts set 1 m deep and thick boards.
  4. Drafting gate — a gate at the end of the race that swings to send each animal into one of two or three pens: ewes from lambs, fat from thin, sick from well.
  5. Holding pens, and the dip or a crush.

Cattle crush. The end of a cattle race closed by a head bail: two upright bars hinged at the bottom that a person pulls together on the animal's neck as it pushes forward, with a bar behind its rump. Add a side gate that opens. The crush holds a cow safely for checking feet, giving medicine, marking or helping a birth (Animal Health).

Sheep hurdle (gate hurdle). Woven wattle hurdles are in Fences and Hedges. The gate hurdle is stronger and lasts longer, and is what yards and races are built of:

  1. Heads (the two uprights): cleft ash or chestnut 5 × 7 cm, 1.2 m long, the bottom 20 cm pointed to push into the ground.
  2. Rails: five or six cleft rails 1.8 m long, 7 × 2 cm, tenoned into mortises chopped through the heads. Space them closer at the bottom (gaps of about 10, 12, 15, 18 and 20 cm from the ground up) so lambs cannot squeeze through.
  3. Brace: an upright in the middle and two diagonals from its foot to the top corners, nailed to every rail with nails clenched over.
  4. The hurdle is about 1.8 m long and 1 m high and weighs 8–10 kg. Set hurdles end to end, each joint tied to a stake with a rope or withy loop.

Sheep dips

Sheep scab (a mite), lice and keds ruin fleeces and flocks (Animal Health). Ointment takes days for 200 sheep; dipping takes an hour.

The plunge dip is a narrow concrete or mortared-stone bath:

  • 3–4 m long, 1.2–1.5 m deep, about 60 cm wide at the top and 25–30 cm at the bottom, so a sheep can swim forward but not turn round. It holds roughly 1,500–2,500 litres.
  • Entry: the race ends in a short steep slide, so each sheep goes in over its head.
  • Exit: a ramp at the far end with wooden cleats every 20 cm for the feet.
  • Draining pen: a pen with a concrete floor sloping back into the bath, so the dip dripping from the fleeces runs back in. Put a small settling pit at the inlet to catch dung and wool.

The dip. Old arsenic and tobacco dips killed sheep and shepherds; never use them. The traditional wash against scab and lice is lime-sulfur, made as in Pests and Plant Diseases but weaker. For each 100 litres of dip: boil 1 kg of quicklime and 3 kg of flowers of sulfur in about 20 litres of water for 2 hours, outdoors, stirring and topping up, until it is a clear dark orange-brown. Let it settle, pour off the clear liquid into the bath, and make up to 100 litres with water. Use it warm, at 35–40 °C (hot bath water).

Dipping:

  1. Dip on a dry, mild morning, 2–6 weeks after shearing, so the wool is short enough to soak through.
  2. Let thirsty sheep drink water first, so they do not drink dip.
  3. Hold each sheep in the bath for 1–2 minutes, pushing its head under twice with a crook ending in a cross-piece — briefly, never holding it down.
  4. Leave them in the draining pen 10–15 minutes, then turn them out to shade.
  5. For scab, dip again after 10–14 days to kill the mites that hatch from eggs.

Lime-sulfur stains wool yellow and roughens it a little. Never let used dip reach a stream — it kills fish; empty it into a deep soakaway far from wells.

Cattle grids

CATTLE GRID, cut along the track a hoof slips through Rails across gaps 10–13 cm cross-beam at least 2.4–3 m 30–40 cm deep drain GATE HURDLE, about 1.8 × 1 m heads pointed to push into the ground; rails closer at the bottom so lambs cannot pass BARBED WIRE, close up barbs every 10–15 cm Barb 2 mm, two turns, slanting points Two 2.5 mm strands twisted about once every 10–15 cm, which locks the barbs in place
Fig. 2 Cattle grid, gate hurdle and barbed wire. Rails over a pit leave gaps a hoof would drop into, so cattle and sheep will not cross, but wheels roll over. The gate hurdle has rails closer at the bottom for lambs. Barbed wire is two twisted strands with short barbs locked between them.

A cattle grid is a gap in a fence, across a road or track, covered with spaced rails over a shallow pit. Cattle and sheep will not step onto it because their hooves would slip between the rails; carts, wagons and people cross without opening a gate.

  • Pit: at least 2.4–3 m long in the direction of travel (too short and animals jump it), as wide as the track plus 30 cm each side, and 30–40 cm deep under the rails. Line it with stone or concrete walls, give it a drain, and leave a way to shovel out the silt.
  • Rails: iron rails, iron pipe 7–10 cm thick, or hardwood beams 10 × 10 cm set on edge, laid across the road, with gaps of 10–13 cm between them. They must carry the heaviest wagon: rest them on strong cross-beams every metre.
  • Wings: fences meeting the grid ends tightly, so no animal can squeeze round.
  • A small ramp of stone or a board in one corner of the pit lets hedgehogs and other small animals that fall in climb out.

Horses can trap and break a leg in a grid: where horses are kept, put a gate beside it.

Barbed wire

Cattle push through plain wire. Barbed wire — two twisted wires carrying sharp barbs — stops them with a few strands on light posts. It injures animals that run into it: never use it for horses.

Making it by hand.

  1. Line wire: two strands of soft iron or mild steel wire 2.5 mm thick (Iron and Brass Wire), galvanised by dipping in molten zinc (Zinc and Brass).
  2. Barbs: cut 2 mm wire into pieces 5 cm long, each cut on a sharp slant at both ends.
  3. Stretch one line wire between two posts. Wrap each barb two tight turns round its middle about the line wire, with a slotted iron bar as a lever, so the two points stick out on opposite sides. Space barbs every 10–15 cm.
  4. Lay the second strand beside the first. Fix one end, hook the other to a crank, and turn it so the two strands twist together about one full turn every 10–15 cm. The twist locks the barbs so they cannot slide.
  5. Roll it onto a wooden drum.

Fencing with it. Three to five strands on posts 3–5 m apart. At each end and corner set a strainer post 15–20 cm thick, 1 m deep, propped by a diagonal stay. Pull the wire tight with a lever or windlass until it hums when plucked, and fix it to the posts with iron staples (Nails, Rivets and Wire Fasteners).

Branding irons, marks and ear tags

Branding iron. Bend 12 mm iron rod into a simple letter or symbol 8–12 cm tall, with its face rounded and 5–8 mm wide. Avoid closed loops (an O or a B), which blotch; leave gaps. Forge-weld the shape to a stem 60–75 cm long and fit a wooden handle.

  1. Hold the animal still in a crush.
  2. Clip the hair at the spot (hip or shoulder, not the middle of the back, where the best leather is) and make sure the hide is dry.
  3. Heat the iron to the colour of grey ash seen in daylight — hot, but not red. A red-hot iron burns too deep.
  4. Press firmly, rocking slightly, for 3–5 seconds (less on calves), until the burned mark is the colour of saddle leather. Too light and the hair grows back; too deep and it leaves an open wound.
  5. Treat the burn as in Wound Care and Antiseptics.

Branding hurts: use it only where a permanent mark is truly needed, and be quick. For sheep, never hot-branded on the body, mark the fleece each season with raddle — ochre or charcoal ground into fat or oil (Pigments, Paints and Varnish) — and brand the horns or use ear tags.

Ear tag. Cut a strip of brass, copper or tinned iron 5 × 0.8 cm, about 0.7 mm thick. Sharpen one end to a point and punch a slot near the other. Stamp the number with steel figure punches. To fit it, pierce the ear in its middle third, between the two ridges of cartilage and away from the large veins you can see against the light; pass the point through and bend it through the slot to lock. A plier-shaped tool with a hollow jaw makes it one squeeze. Dip the tag in boiled water first.

Ear notches (small V-shaped cuts in the ear rim, read by a code of positions) and tattoos (needles pricked through carbon ink, Ink, inside the ear) need no metal at all. Record every number in a herd book (Writing and Numbers).

Weighing livestock

Weight tells you if young stock are growing, how much medicine to give and what an animal is worth. Hang a crate from a steelyard or big balance and you can weigh sheep, calves and pigs exactly (Balances, Steelyards and Weighing Machines, Measurement from Scratch). For cattle, there is a good estimate that needs only a cord:

  • Measure the heart girth (round the chest just behind the front legs) and the body length (from the point of the shoulder to the bone beside the tail), both in centimetres, with the animal standing square.
  • Cattle: weight in kg ≈ girth × girth × length ÷ 10,800. A cow with girth 190 cm and length 160 cm weighs about 190 × 190 × 160 ÷ 10,800 ≈ 535 kg.
  • Pigs (length from between the ears to the root of the tail): weight in kg ≈ girth × girth × length ÷ 14,400.

The estimate is within about 5–10%. Better: weigh a dozen animals on a steelyard, measure their girths, and mark your own weigh tape — a strip of cloth or leather marked with weights instead of centimetres.

The cream separator

Supply tank warm milk, 32–37 °C Central feed tube Skim spout Holes line up into channels Disc stack 20–40 cones, 0.5 mm apart Skim milk heavier: flung out to the wall, up and out Cream spout Cream lighter: squeezed in to the middle Bowl 10–15 cm across, 6,000–10,000 turns/min Ball bearing Spindle and worm Worm wheel geared from a crank turned 45–60 times a minute
Fig. 3 Inside a cream separator bowl. Milk runs down the central tube and up through holes in a stack of cone-shaped discs. Spinning at thousands of turns a minute, the heavier skim milk is flung outward to the wall and up to the skim spout; the light cream is squeezed inward and out through the cream spout near the middle.

Left in a shallow pan, cream rises in a day, but a tenth or more of the butterfat stays in the skim (Dairy and Cheese). A cream separator spins milk so fast that cream and skim part within a second, leaving only a trace of fat behind.

How it works. Cream is fat droplets that are a little lighter than the watery milk around them. Gravity makes them rise slowly. A bowl 12 cm across turning 7,000 times a minute pushes outward on everything inside it several thousand times harder than gravity pulls. The heavier skim milk crowds to the outside; the cream is pushed to the middle. A stack of thin cones (discs) inside the bowl, about 0.5 mm apart, gives the fat droplets only half a millimetre to travel before they reach a surface and slide inward, so separation is almost instant.

The parts.

  1. Supply tank on top, with a tap.
  2. Bowl: a strong steel shell 10–15 cm across, threaded shut, with a central feed tube.
  3. Discs: 20–40 cones of thin tinned steel sheet, sloping at about 45–60°, each with small raised bumps that space it from the next, and a ring of holes about two thirds of the way out. The holes line up and make channels up through the stack.
  4. Outlets: a cream spout near the centre and a skim spout at the rim, each catching into its own tray. A small screw in the cream outlet sets how thick the cream is.
  5. Drive: a hand crank turning 45–60 times a minute, through a gear train and a worm gear (Gears), spins the bowl spindle about 150 times faster. The spindle runs in ball bearings (Making Ball and Roller Bearings) with a slightly springy top bearing so the bowl finds its own centre.

Building one is a serious workshop project: the bowl must be turned true on a The Lathe and balanced — rested on two level knife-edges and filed on its heavy side until it stays put in any position. A bowl that is out of balance shakes, wears its bearings, and can burst.

Using it.

  1. Separate milk straight from milking, at 32–37 °C (blood-warm). Cold milk separates badly.
  2. Turn the crank up to speed slowly, over about a minute, before opening the milk tap. Keep the speed steady; too slow lets fat go out with the skim.
  3. Close the tap, run a jug of warm water or skim milk through to flush it, then let the bowl coast to a stop by itself.
  4. After every use, take the bowl apart, rinse the discs, wash them in hot water with soda (Soda Ash and Baking Soda), scald them and dry them. A dirty separator sours every batch.

Without a separator: deep setting. Stand milk in tall tin cans about 20 cm across and 50 cm deep, set in cold spring water or ice water below 10 °C, for 12–24 hours, and skim or draw the skim from a tap at the bottom. Cold, deep setting recovers far more cream than warm shallow pans.

How to tell it worked

  • Troughs stay full and clean, with firm ground round them.
  • Hay racks leave little hay on the floor; the animals clean up what falls into the trough below.
  • Sheep run through the race without stopping, balking or turning; two people can handle a flock in a morning.
  • After dipping, scratching stops within a week and no new bald, crusty patches appear.
  • No cattle cross the grid, and none try after the first day.
  • Brands read clearly a year later; tags stay in.
  • Skim milk from the separator looks thin and bluish; a jar of it left 24 hours shows almost no cream line.

Note Troubleshooting. Sheep balk at the race entrance → they can see out through gaps, a shadow lies across the floor, or it faces into the sun; board the sides and turn or roof it. Animals turn round in the race → too wide; add a board to narrow it. Scab returns after dipping → too short a soak, the dip too weak or cold, a second dipping missed, or untreated sheep joined the flock. Brand faded or bald and spreading → too cool, or too hot and held too long; practise on a board. Separator skim still creamy → crank too slow, milk too cold, or the tap opened too wide. Separator shudders → bowl out of balance or discs assembled wrong; stop it and check.

Dangers

Danger Cream separator bowls can burst. A bowl spinning at thousands of turns a minute holds enormous energy; a cracked, corroded or unbalanced bowl can fly apart like a bomb. Never exceed the designed speed, never run it if it shudders, and never stop it with your hand. Cattle in pens and crushes can crush a person against a rail or kick with killing force: never stand in a race or pen with a frightened bull or a cow with a calf, and work from outside the rails.

Warning Dip and barbed wire. Lime-sulfur burns eyes and skin, and boiling it gives off poisonous hydrogen sulfide — make it outdoors, upwind, and wear eye protection when dipping. Barbed wire under tension whips back when it breaks or is cut: stand to the side, wear leather gloves, and keep children away.

  • Water troughs drown toddlers. Fence them off from children or keep them shallow where children play.
  • Branding works with hot iron next to a restless animal; hold the animal firmly and keep others back.
  • Zoonoses. Wash hands after handling animals, dung and fleeces (Keeping Animals).

What this unlocks

With troughs, racks and a handling yard, a family can keep a flock or herd big enough to sell wool, hides and meat. Records of tagged animals make careful breeding possible (Heredity and Genetics). The cream separator turned butter-making into a dairy industry and gave skim milk for pigs, cheese and casein (Early Plastics); its spinning bowl is the same machine as the laboratory centrifuge used to separate blood and chemicals. Working dogs (Working Dogs) make all of this handling far easier.

How it was first done

Troughs, hurdles and folds are as old as herding; Roman farm writers describe hay racks and sheepfolds much like these. Sheep washing and dipping against scab is very old, but the first commercial dip powder was sold by the English vet William Cooper in 1852 — an arsenic and sulfur mixture that worked but poisoned many. Branding is shown on Egyptian tomb walls from about 2000 BC. Barbed wire was patented in many forms in the 1860s and 1870s; Joseph Glidden's two-strand twisted wire of 1874 won, and closed the open range of the American West within twenty years. The continuous cream separator was built by the Swedish engineer Gustaf de Laval in 1878, and the stack of conical discs was patented by the German Clemens von Bechtolsheim in 1888. Hand-cranked separators spread to small farms across the world by 1900.

Source: content/entries/food/livestock-equipment.md