◆ Rebuild

Part 12 · Transport

Rafts and Canoes

How to cross and travel on water with nothing but logs, reeds, bark, hides and fire — log and reed rafts, dugout canoes, birch-bark canoes, coracles and skin boats, the paddle, the outrigger, and how to stay alive while doing it.

Difficulty
●●●●●
Time
A raft in a day; a coracle in two or three days; a dugout canoe in two to four weeks
Steps from zero
3 prerequisites →

You need first

Basic WoodworkingCordage and Rope

This unlocks

—
The full path from nothing — 3 steps before this one
  1. Stone Tools
  2. Cordage and Rope
  3. Basic Woodworking
  4. Rafts and Canoes

Do them roughly in this order. See it on the tech tree →

Why it matters

A river is a road that is already built and that carries your load for free. A person on foot carries 20–30 kg for a day's march; the same person in a small dugout canoe moves 200–300 kg, and downstream the current does most of the work. Before roads, almost all heavy goods — stone, timber, grain, salt, ore — travelled by water whenever water went the right way (Quarrying and Cutting Stone). Boats also reach the fish in the middle of a lake (Fishing) and cross rivers that would otherwise end your journey.

This chapter covers craft you can build with stone tools, fire and Cordage and Rope. They lead directly to plank-built Boats and Sails, and later to Steamships.

How it works

Floating

Anything put in water pushes aside some water. The water pushes back upward with a force equal to the weight of the water pushed aside. One litre of fresh water weighs 1 kg. So an object floats if it weighs less than the same volume of water, and it sinks until it has pushed aside its own weight plus its load.

That gives two ways to make something float:

  1. Use a light material. Dry wood is lighter than water. How much lighter decides how much it carries:
Material (dry) Weight of 1 litre Spare lift per litre
Balsa 0.15 kg 0.85 kg
Cedar, dry poplar, willow 0.35–0.45 kg 0.55–0.65 kg
Dry pine, spruce, fir 0.45–0.55 kg about 0.5 kg
Dry oak, ash 0.65–0.75 kg about 0.3 kg
Green (freshly cut) wood of almost any tree 0.8–1.1 kg almost none — some sinks
Bundled dry reeds about 0.2 kg (with air between stems) about 0.8 kg, until they soak up water
  1. Make a hollow shell. A boat's hull pushes aside a large volume of water while weighing little itself — most of the volume is air. This is why a canoe carries far more than a raft of the same wood.

A worked example. A dry pine log 30 cm across and 3 m long holds π × 0.15 × 0.15 × 3 ≈ 0.21 m³, or 210 litres. It weighs about 105 kg and could hold up another 105 kg before it went completely under. In practice you want logs only half sunk, so count on about 50 kg of load per log of that size. A raft of six such logs carries two or three people and their gear.

Staying upright

A boat that floats can still roll over. Two things keep it upright:

  • Width. When a wide hull tips, the side going down pushes aside much more water than before and is pushed back up hard. A narrow one has little to resist with. Doubling the width makes a hull roughly eight times harder to tip.
  • Low weight. Weight high up pulls the boat over once it starts to lean. Kneel or sit on the bottom, never stand, and stow heavy loads flat on the floor in the middle.

Freeboard is the height of the side above the water. Keep at least 15 cm in calm water and 25 cm or more on open lakes, where waves come over a low side and swamp the boat.

What you need

Craft Main materials Tools Carries
Log raft 6–8 dry, dead logs 25–35 cm thick and 3 m long; 3 crossbars; 40 m of strong rope Stone or iron axe, wooden pegs, mallet 2–3 people
Reed raft 30–50 big armfuls of dry reeds or bulrushes; 100 m of cord Knife 1–2 people, for a few weeks
Dugout canoe One straight log 50–80 cm thick, 4–6 m long Axe, adze, wedges, fire, clay, scrapers 2–4 people, or 300 kg
Birch-bark canoe One large sheet of birch bark; cedar or spruce for frame; 50–100 m of split spruce root; pine or spruce gum Knife, awl, axe, stakes 2–3 people
Coracle 20–30 hazel or willow rods; one large cowhide or 2–3 smaller hides Knife, awl, cord 1 person and a load
Paddle A split plank of ash, maple, spruce or cedar 1.5 m long Axe, knife, scraper —

Where to find it

  • Light, dry logs. Look for standing dead trees with the bark falling off, and driftwood piles along rivers and beaches — already dry and seasoned. Tap a log with a stone: dry wood gives a ringing knock, wet or rotten wood a dull thud. If a knife point sinks in and the wood crumbles, it is rotten and will soak up water.
  • Dugout logs. A big, sound, straight trunk with few low branches. Traditional woods are cedar (light and rot-resistant), white pine, cottonwood and poplar, tulip tree, basswood (lime), and many light tropical woods. Oak makes heavy but long-lived dugouts. A green log is easier to carve than a dry one.
  • Reeds (common reed, bulrush, cattail, papyrus) grow in still water at lake and river edges. Cut them in late summer or autumn when the stems are full-grown, and dry them for two or three weeks.
  • Birch bark comes from paper birch and other white birches. It peels most easily in late spring and early summer, when the sap is running; then a cut down the trunk lets the whole sheet spring free. See Baskets and Containers for testing and peeling.
  • Spruce roots run just under the moss around spruce and pine trees. Spruce and pine gum oozes from wounds on the trunk; collect the hard lumps.
  • Withies for a coracle — long, straight shoots of hazel or willow — grow wherever these shrubs have been cut back. Cut them 2–3 m long and 1.5–3 cm thick.
  • Hides come from Hunting and Trapping and from your animals (Keeping Animals). See Hides and Leather.

Method 1: The log raft

FROM ABOVE FROM THE END Lashingfigure-of-eight, ropeor green withies Pointed frontrides over waves Crossbar10–12 cm pole,sits in notches hardwood peg 3 m forward Logs6–8 dry, dead,25–35 cm thick Tie between every log Top crossbar Waterlinelogs about half under Bottom crossbarclamps the logs like a vice
Fig. 1 A log raft. Top: logs laid side by side with three crossbars on top, each lashed to every log and pinned into notches. Bottom: seen from the end, the logs float about half under water; a second crossbar under the logs, tied to the top one, clamps them together.
  1. Choose the logs. Six to eight dry logs, 25–35 cm thick and about 3 m long. Lighter woods (cedar, pine, poplar, willow) are better than heavy ones. Trim off branch stubs.
  2. Shape the ends. Cut the front ends to a blunt point, or angle the underside up like a sledge runner so the raft rides over waves and floating branches instead of ploughing into them.
  3. Lay them out at the water's edge, on rollers if they are heavy, side by side, thickest ends alternating so the raft is square.
  4. Cut notches. Across the top of the logs, 30 cm from each end and once in the middle, cut a shallow notch 5–8 cm deep in each log, so that a crossbar sits in all of them in a straight line.
  5. Lay in the crossbars. Three straight poles 10–12 cm thick, a little longer than the raft is wide. For a really strong raft put a matching crossbar under the logs too, and tie the top and bottom bars together tightly between every pair of logs, clamping the logs like a vice.
  6. Lash and pin. Bind each crossbar to each log with a figure-of-eight lashing of strong rope or green withies (Cordage and Rope, Knots, Lashings and Rigging). Better still, drill a hole down through each crossbar into each log with a fire-heated rod or an auger and drive in a hardwood peg; a pegged raft does not loosen as wet rope stretches.
  7. Add a deck of thin poles or split boards on top if you are carrying goods that must stay dry.
  8. Make poles and a sweep. In water less than 2 m deep, push the raft with a 3–4 m pole against the bottom ("poling"). In deeper water, steer with a long oar (a sweep) pivoting on a forked stick at the back.

A bamboo raft is built the same way and is even better: each closed section of bamboo is a sealed air chamber. Use poles 8–12 cm thick and keep the ends closed at a node so water cannot get inside.

Method 2: The reed raft

Dry reeds are mostly air. Bound into tight bundles they make surprisingly good boats — the people of Lake Titicaca in the Andes, the marsh people of southern Iraq and the ancient Egyptians all built them.

  1. Make the bundles. Lay dry reeds in a long heap, butts and tips alternating, and squeeze them tight. Wrap cord around the bundle every 20–30 cm, pulling each wrap as tight as you can (stand on the bundle and haul). A good bundle is 30–40 cm thick and 3–4 m long, tapering to a point at each end.
  2. Join the bundles. Lay two or three bundles side by side and bind them together with cords passed around all of them. Tie the pointed ends together and bend them up by pulling a cord from the tips back to the middle.
  3. Add a top layer. A smaller bundle along each side as a rail stops water washing over and keeps the load in.

Reed boats soak up water slowly and ride lower every day. Pull them out and dry them in the sun for a few days every week or two, and expect them to last a few months.

Method 3: The dugout canoe

The dugout is the most widely made boat in human history: a log, hollowed out. It is heavy and slow to make, but tough enough to last for years. The basic skills — controlled burning and adzing — are in Basic Woodworking.

SIDE VIEW CROSS-SECTIONS, STAGE BY STAGE FROM ABOVE, FINISHED Solid end block20–30 cm, stops splitting Hollowdashed line Rockerbottom curves up60–80 cm at each end waterline 1. Peel the log50–80 cm thick 2. Split off the top thirdwedges and adze 3. Hollowfire and adze, in turns Rimsmear with wet clay Walls 2.5–3 cmstop at the dark pegs Bottom 4–5 cmpegs driven 4–5 cm deep inside, hollowed 60–75 cm wide wider = steadier 4–6 m long
Fig. 2 Making a dugout. Top: side view, with the bottom curved up at bow and stern. Middle: the log in cross-section at each stage — whole, with the top third removed, and hollowed. Short dark pegs driven in from outside show when you have reached the right wall thickness. Bottom: the finished hull from above.

Step by step

  1. Fell and move the log. Fell the tree in winter if you can (less sap, less splitting). Cut a length 4–6 m long. Carve it close to where it fell; a green log 60 cm thick and 5 m long weighs more than a tonne. Peel off all the bark.
  2. Choose the top. Roll the log until its most curved or most knotty side faces up — that is the side you will remove. Cut away the top third of the log along its whole length: chop notches every 30 cm, split off the wood between them with wedges, and flatten the surface with the adze. You now have a flat deck 35–50 cm wide.
  3. Shape the outside first. Roll the log over. With axe and adze, round the bottom and taper the ends into a pointed bow and stern. Curve the bottom up for the last 60–80 cm at each end (this is called rocker) so the canoe turns easily. Look along it from each end, and from a distance, to check that it is even on both sides.
  4. Set the depth gauges. Drill holes 3 cm deep from the outside all over the hull, about every 30 cm, and drive in pegs of a dark or contrasting wood, cut off flush. On the bottom drill 4–5 cm deep. When your hollowing from inside reaches a peg end, you know the wall is the right thickness there.
  5. Hollow it. Roll the log deck-up again. Mark a line 4 cm in from the edges. Alternate fire and adze:
    • Lay hot coals along the middle, protect the rims with a thick smear of wet Finding and Preparing Clay, and blow or fan the coals so they char 1–2 cm into the wood.
    • Scrape and adze out the charcoal and soft wood beneath.
    • Repeat. Keep the fire away from the ends, which you finish by adze alone. Leave walls 2.5–3 cm thick and the bottom 4–5 cm thick. Leave a solid block 20–30 cm long at each end; these keep the ends from splitting and give somewhere to tie ropes.
  6. Keep it damp. A green log dries and cracks fast once its inside is opened. Cover it with wet leaves, grass or mats whenever you are not working, and keep it in shade.
  7. Spread it (optional, for a wider, more stable canoe). This is how the peoples of the American north-west coast turned a narrow log into a wide, stable boat. Fill the finished hull with water. Drop in red-hot stones from a fire until the water steams and simmers, and cover the hull with mats to hold the steam in. After several hours the softened sides can be pushed outward a little at a time; wedge them apart with crossbars (thwarts) cut a little longer each hour. Spreading by 15–25 cm is realistic. Leave the thwarts in and let it cool and dry slowly.
  8. Finish. Smooth inside and out. Rub the hull with hot animal fat or paint with pine tar (Tar, Pitch and Glue) to slow rot and cracking.

A good working size is 5 m long and 60–75 cm wide; it carries two people and their load comfortably.

Method 4: The birch-bark canoe

The bark canoe of the northern American forests is light enough for one person to carry around rapids — a 5 m canoe weighs 25–35 kg. It is a skilled craft; expect your first to be crude. The outline:

  1. Make the building bed. On level, packed ground, lay out the gunwale frame (the two long side rails, bent and joined at the ends) and drive pairs of stakes around it to form the canoe's outline.
  2. Lay the bark on the bed white side up: the white outer surface of the tree's bark becomes the inside of the canoe, and the tougher inner surface faces the water. Soften it with hot water if it is stiff, and set the gunwale frame on it with stones to weigh it down. Fold the bark up against the stakes. Where it bunches, cut slits (gores) and overlap the edges.
  3. Sew. Punch holes with a bone or iron awl and sew the bark to the gunwales and the gores closed with split spruce root, soaked to make it pliable. Join extra pieces of bark the same way where one sheet is not big enough.
  4. Line and rib it. Lay thin strips of split cedar lengthways inside (the sheathing). Then bend ribs of split cedar, 6–8 mm thick and 5–7 cm wide, softened in boiling water (Steam-Bending Wood), into a U and force them in under the gunwales every 5–8 cm. The ribs stretch the bark tight like a drum.
  5. Seal the seams. Melt spruce or pine gum with a little animal fat (about 5 parts gum to 1 part fat) and a pinch of powdered Charcoal. Test a drop on cold stone: it should be hard but not crack when bent. Smear it hot over every seam and gore, outside, and press it in with a wet thumb.

Method 5: The coracle and other skin boats

A coracle is a round basket covered with a hide. It looks absurd and works well: it is stable, it carries one person and a load across a river or along a lake shore, it weighs 13–18 kg, and its owner carries it on their back.

THE FRAME, FROM ABOVE CROSS-SECTION, AFLOAT THE STROKE, FROM ABOVE Woven rimwithies, 10–15 cm deep Seat planklashed at rim height Ribs14–16 each way,15–20 cm apart Tiesat every crossing 1.2–1.4 m long Rim Hidelaced on wet,greased Ribs Seat 10–15 cm draught Figure-of-eight the blade sweeps side to side ahead of the coracle, which follows it forward travel
Fig. 3 A coracle. Left: the frame of woven hazel or willow rods, with a seat across the middle. Right: in cross-section, the hide stretched over the frame. The paddler kneels or sits on the seat and paddles over the front in a figure-of-eight stroke.
  1. Lay out the frame. On flat ground, mark an oval 1.2–1.4 m long and 1–1.1 m wide. Drive 14–16 withies into the ground around it, 15–20 cm apart, upright. These are the ribs.
  2. Weave the rim. With more withies, weave a band 10–15 cm deep around the ribs right at ground level, as in a basket (Baskets and Containers). This becomes the gunwale.
  3. Bend the ribs over. About 35–40 cm above the ground, bend each rib across to the rib opposite and tie them where they cross, forming a shallow, flat-topped dome. Add a second set crossing at right angles. Tie every crossing. The dome becomes the bottom of the boat.
  4. Pull it up out of the ground, turn it over, trim the rib ends flush with the rim, and lash a seat plank across the middle at the height of the rim.
  5. Cover it. Soak a fresh or rehydrated cowhide until it is soft. Turn the frame upside down on the hide, hair side in, pull the hide up over the rim, and lace it to the rim through holes cut every 8–10 cm. As the hide dries it shrinks and tightens like a drum.
  6. Waterproof it. Rub melted animal fat, or a mix of fat and pine tar, into the outside of the hide and let it soak in. Repeat every few trips.

Paddling a coracle. Sit facing forward, holding a short paddle (1.2–1.5 m) over the front with both hands. Sweep the blade in a figure-of-eight in the water ahead of you — this pulls the coracle forward without spinning it. It takes an afternoon to learn.

Bigger skin boats — the Irish curragh of poles and ox hides, the Inuit umiak and kayak of driftwood, bone and seal or walrus skin — are built the same way: a light frame, lashed rather than nailed, with the skin sewn on wet so it shrinks tight.

Tip Hide rots if it stays wet. After every use, take a skin boat out of the water, turn it over and let it dry in the air — never leave it floating overnight.

The paddle

Split a plank from a straight log of ash, maple, spruce or cedar. Shape it with axe and knife:

  • Length. For a canoe, standing, the paddle should reach between your chin and your nose. Kneeling paddlers in a narrow canoe can use a shorter one.
  • Blade. 50–70 cm long and 15–18 cm wide, thinning to 6–8 mm at the edges and tip, with a ridge down the middle for strength.
  • Shaft. Round or oval, about 3 cm thick, with a T or knob grip at the top.

The basic strokes. Paddle with the blade upright, pulling straight back close to the side. In a two-person canoe the one in front supplies power and the one behind steers. A lone steerer stops the canoe turning by twisting the blade outward at the end of each stroke, so the blade pushes the stern back on course (the J-stroke — the blade traces a J).

Method 6: The outrigger

A long narrow hull is fast but tippy. The peoples of the Pacific and Indian Oceans solved this with the outrigger: a float lashed out to one side that the hull leans on.

  1. The float. A light log (or a bundle of bamboo) about half to two-thirds the length of the canoe and 15–25 cm thick, pointed at the front.
  2. The booms. Two straight poles, 7–10 cm thick, lashed across the canoe near bow and stern and reaching 1.5–2 m out to one side.
  3. Join them. Connect each boom to the float with forked sticks or short posts lashed with tight cord, so the float rests lightly on the water when the canoe is upright.

With an outrigger, even a narrow dugout can safely carry a sail (Boats and Sails) on open water. Two hulls joined side by side with a platform between (a double canoe) is even more stable and carries more, and Polynesian double canoes like this crossed thousands of kilometres of ocean (Navigation).

How to tell it worked

  • Float it empty in calm, waist-deep water near shore. It should sit level, without leaning to one side. Watch inside for 10 minutes for leaks.
  • Load it gradually, with stones first, then with people. Measure the freeboard: at least 15 cm in calm water.
  • The tip test. In shallow water, have one person get in and lean gently one way, then the other, while others stand beside it. You will learn exactly how far it can lean before it goes over.
  • A day's work. A good canoe paddled steadily covers 4–6 km an hour on still water. A raft with a pole makes 2–3 km an hour.

Note Troubleshooting. The raft rides lower each day → the logs are soaking up water. Pull it out to dry, or rebuild with drier logs. The dugout splits along the end → it dried too fast. Keep it wet while working, leave the solid end blocks thicker, and drive a wooden peg or bind a wet rawhide strap across the crack. The canoe always leans one way → one wall is thicker. Thin it, or put a stone on the high side. The canoe is very tippy → it is too narrow or too round-bottomed. Paddle kneeling, add stone ballast low in the middle, spread it, or fit an outrigger. The bark canoe leaks at seams → re-gum them on a warm day, after drying the canoe. Find leaks by putting water inside and watching the outside. The coracle hide sags → it was put on too dry or is soaking up water. Dry it fully, re-grease it, and tighten the lacing.

Dangers

Danger Drowning is the greatest danger in this chapter. Most people who drown never meant to go into the water. Learn to swim in calm, shallow water before you build a boat. Never go out alone on a new craft, never go in water you could not swim out of, and carry something that floats — a dry log, a sealed gourd, an inflated animal bladder — tied to the boat. Rescue and resuscitation are in Life Jackets, Lifebuoys and Lifeboats and Emergency Cards.

Danger Cold water kills fast. Falling into water colder than about 15 °C causes a sudden gasp that can fill your lungs, then fast breathing and panic for a minute or two. Within about 10 minutes your arms grow too weak to swim; after that, cold slowly kills. If you capsize in cold water, keep your head out, hold on to the boat (it floats even when full of water), and kick to shore with it. Do not try to swim away from it. See Surviving Cold and Heat.

  • Moving water. Fast rivers hide rocks. A fallen tree in a current (a strainer) lets water through but pins a person or boat against it. A low dam or weir creates a backwards-rolling wave at its foot that holds a swimmer under — never go over or near one. Scout rapids from the bank and carry around anything you are not sure of.
  • Wind. On a lake or the sea, a wind blowing from the land is dangerous: the water near shore looks calm, but you are being blown out and the waves grow with every minute. Stay close to shore and come in when the wind rises.
  • Overloading. Every capsize is more likely with low freeboard. Never load past the 15 cm line.
  • Working fire and adzes. Hollowing with fire can set the whole log alight; keep water at hand. An adze swung toward your feet takes off toes — stand with your feet wide and back from the cut.

What this unlocks

Water craft open Fishing beyond the shore and trade along every river and coast. Join planks to a keel instead of hollowing a log, and you can build boats bigger than any tree: see Boats and Sails. Out of sight of land you need Navigation. Inland, people learned to dig their own rivers: Canals and Locks. And the same steam that later drives Railways drives Steamships.

How it was first done

People reached Australia at least 50,000 years ago, crossing open sea of 70 km or more on rafts or canoes that do not survive. The oldest boat found so far is the Pesse canoe from the Netherlands, a dugout of Scots pine about 3 m long, made around 8000 BC with stone tools and fire. The Dufuna canoe from Nigeria, about 8,000 years old, is Africa's oldest.

Julius Caesar described hide-covered boats on light wooden frames in Britain in the 1st century BC; Welsh and Irish coracles of the same build were still used in the 20th century. Birch-bark canoes were perfected by the peoples of the North American forests, and in the 1700s European fur traders adopted them almost unchanged. In 1947 the Norwegian Thor Heyerdahl and five companions sailed a raft of balsa logs, the Kon-Tiki, about 7,000 km from Peru to the Tuamotu Islands in 101 days, to show that a raft built with ancient methods can cross an ocean.

Source: content/entries/transport/rafts-and-canoes.md