Part 13 · Electricity
Synchronous Motors and Converters
A motor that turns in exact step with the alternating current that feeds it — never faster, never slower. It runs electric clocks off the mains, holds machines at a fixed speed, and can even correct a grid's wasteful "power factor". Joined to a dynamo or given a commutator, it changes AC into DC for trams, batteries and electrolysis works. How they work, how to build a clock motor and use an alternator as a motor, and what power factor means in plain words.
- Difficulty
- ●●●●●
- Time
- An evening to run an alternator as a motor; a week for a mains clock; months for a rotary converter or a large motor with its exciter
- Steps from zero
- 24 prerequisites →
This unlocks
—The full path from nothing — 24 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- Charcoal
- Pottery
- Hides and Leather
- Fermentation
- The Wheel and Axle
- Bellows
- Gears
- Copper Smelting
- Iron (the Bloomery)
- The Waterwheel
- Blacksmithing
- The Battery
- Magnets
- Copper Wire
- The Electromagnet
- The Generator
- The Electric Motor
- Synchronous Motors and Converters
Do them roughly in this order. See it on the tech tree →
Why it matters
An ordinary induction motor always runs a little slower than its magnetic field, and slows a little more under load. A synchronous motor does not. Its rotor turns in exact step with the alternating current: on a 50 Hz supply, a four-pole synchronous motor turns exactly 1,500 times a minute, whether lightly or heavily loaded, as long as it is not overloaded altogether.
That exactness is useful in three ways:
- Timekeeping. A small synchronous motor geared to clock hands keeps time as well as the power station keeps its frequency. Power stations learned to keep that frequency so well that mains clocks became the most accurate clocks most people owned. Synchronous motors also time cooking ovens, dishwashers (Fans, Vacuum Cleaners and Washing Machines), record turntables (Recording Sound) and laboratory instruments.
- Changing one kind of electricity into another. A synchronous motor driving a The Generator — a motor-generator — turns AC into DC, one frequency into another, or one voltage into another. The rotary converter does the AC-to-DC job in a single machine. Before solid-state Rectifiers: Turning AC into DC, these machines fed tramways, Railways, Electrolysis works and battery charging rooms.
- Making the grid efficient. A synchronous motor can be adjusted to supply the "magnetising" current that other motors and The Transformers waste the grid's capacity on — improving what engineers call power factor.
How it works
Locked to the field
In an AC machine with three-phase windings, the stator makes a magnetic field that rotates round the inside of the machine, one pole-pair's worth per cycle (The Electric Motor, Method 3). Put a magnet on the rotor — a permanent magnet, or an electromagnet fed with DC through slip rings — and it is dragged round, locked to the rotating field like a dog on a lead. The speed is fixed by the frequency and the number of poles:
turns per minute = 120 × frequency (Hz) ÷ number of poles
| Poles | At 50 Hz | At 60 Hz |
|---|---|---|
| 2 | 3,000 | 3,600 |
| 4 | 1,500 | 1,800 |
| 6 | 1,000 | 1,200 |
| 8 | 750 | 900 |
| 12 | 500 | 600 |
| 24 | 250 | 300 |
This is exactly the The Generator rule run backwards: every alternator is a synchronous motor, and every synchronous motor will generate if driven.
The load angle
With no load, the rotor's poles sit right in line with the field's. Load it, and the rotor drops back by an angle — the load angle — but keeps the same speed, like a dog pulling back harder on its lead while still walking at its owner's pace. The more load, the bigger the angle. When the angle reaches about a quarter of a pole-pair (90° "electrical"), the motor is giving its greatest pull, usually 1.5–2.5 times its rated load. Beyond that it pulls out of step: the rotor slips back pole after pole, the current surges in heavy pulses, the machine shudders and roars, and it must be switched off at once.
Starting
A synchronous motor cannot start itself from rest. Its field spins at full speed from the instant you switch on; the rotor, heavy and still, is pulled forward for half a cycle and backward the next, and just shivers. It must be brought up to nearly the right speed first, then it pulls into step by itself. Ways to do it:
- By hand — small clocks: spin the knob.
- A pony motor — a small induction or DC motor on the same shaft, or a belt from another machine, brings it up to speed.
- A damper winding (amortisseur) — copper bars through the rotor's pole faces, joined at the ends like a squirrel cage. The machine starts as an induction motor; at about 95% of full speed, switch on the DC to the field and it snaps into step. The same bars also stop hunting — the rotor swinging back and forth around its true position after each change of load.
- Self-starting small motors — the hysteresis motor has a rotor ring of hardened magnet steel; the rotating field drags it round by magnetising and re-magnetising it, and it runs up smoothly and locks into step by itself. The reluctance motor has a soft iron rotor with notches cut in it to make "poles" that the field can grip.
Power factor in plain words
A heater or lamp takes current exactly in step with the voltage: the current peaks when the voltage peaks. Motors and transformers also take a second current, the magnetising current, that builds up their magnetism and gives it back each half-cycle. It peaks a quarter-cycle late, flows back and forth, and does no work — but it still flows in every wire, and still heats them.
Think of a horse pulling a barge from the towpath. The rope is at an angle: only the forward part of the pull moves the barge; the sideways part is wasted, yet the horse, harness and rope must bear the whole pull. Power factor is the fraction of the pull that is useful:
power factor = real power (watts) ÷ (volts × amps)
- Heaters, lamps: about 1.0.
- An induction motor at full load: 0.8–0.85; lightly loaded: 0.3–0.5.
- A whole village of motors and transformers: often 0.7.
At a power factor of 0.7, the generator, transformers and lines carry about 1.4 times the current they would need for the same useful power, and lose about twice the power in heat (loss grows with the square of the current). You pay for bigger machines and thicker wire, and get dimmer lamps at the ends of lines (Power Lines and Distribution).
Two cures, both of which supply the magnetising current near the motors so it no longer flows all the way from the power station:
- Capacitors across the supply at or near big motors. A capacitor on AC takes a current that peaks a quarter-cycle early — the exact opposite of magnetising current — so the two cancel.
- An over-excited synchronous motor. Turn up a synchronous motor's DC field current beyond the normal amount, and it starts to supply magnetising current to the rest of the grid instead of taking any. A large synchronous motor running a compressor or pump in a factory can correct the whole factory's power factor at the same time. A synchronous motor run with no load at all, purely for this, is called a synchronous condenser.
What you need
| Item | Notes |
|---|---|
| An AC supply | An alternator or grid of known, steady frequency (The Generator, Power Lines and Distribution) |
| For a clock: soft iron sheet, 0.4–0.6 mm wire, brass gear blanks | Iron (the Bloomery), Copper Wire, Gears, The Mechanical Clock |
| For a motor: a second alternator like your generator, a small DC source for its field | The Generator, The Battery |
| For conversions: a DC dynamo of matching size; a sturdy base and coupling | The Generator, Belts, Chains and Power Transmission |
| Lamps | Two lamps each for the full line voltage, for synchronising (The Light Bulb) |
| AC meters | Moving-iron ammeter and voltmeter, which read AC (Measuring Electricity) |
| Capacitors | Paper-and-oil or mica, rated for AC at well above the line voltage (Resistors, Capacitors and Coils) |
Method 1: Run an alternator as a motor
The quickest way to see synchronous running, and the start of every bigger use.
- Take two similar alternators — say two of the magneto-type machines of The Generator, Method 2, or two dynamo-excited alternators. One is driven by your The Waterwheel or engine and feeds the line. The other will be the motor.
- Excite the motor's field with DC (or use permanent magnets). Bring it up to speed with a belt from another machine or by hand, until it turns at very nearly the line machine's speed (if they have the same number of poles, the same speed).
- Synchronising lamps. Connect a lamp across each pole of the switch between the line and the motor. Each lamp sees the difference between line and motor voltage. When the two are out of step the lamps glow brightly; when they are in step, they go dark. As the speeds approach, the lamps flicker slowly bright and dark.
- Close the switch in the middle of a dark period, when the flicker is slowest. The motor locks in with a slight jolt. Remove the starting drive — it keeps turning, exactly in step.
- Load it gently. Watch the speed stay fixed. Now vary its DC field current and watch an AC ammeter in its line: the current is lowest at one field setting (power factor 1); more or less field both raise it. Plotted, this is the famous V-curve.
Warning Closing the switch when the lamps are bright connects two machines that are half a cycle apart: a dead short through both. It gives a violent jolt that can twist shafts, throw belts and burn windings. Always wait for dark, and practise first with small machines on low voltage.
Method 2: A synchronous clock
This is a reluctance motor, the simplest synchronous motor to make, after the "phonic wheel" of the 1870s.
- Frame: cut a C-shaped frame from soft iron sheet 0.5 mm thick, a dozen pieces stacked, varnished and riveted (laminations stop the iron heating). The gap between the two pole tips is 2.5 cm.
- Coil: on the back of the C, wind 800–1,200 turns of 0.3 mm covered wire, and feed it from 6–12 V AC taken from a small The Transformer on the mains. Never connect home-made clock coils straight to the mains.
- Toothed wheel: a disc of soft iron sheet 1 mm thick and about 2.4 cm across, with 20 teeth filed evenly round its edge, each tooth as wide as its gap. Mount it on a fine steel arbor in jewelled or brass pivots (Watches and Small Clocks), with the teeth passing between the pole tips with less than 0.3 mm of clearance.
- Speed: the magnet pulls hardest twice each cycle (on both the north and the south half), and each pull draws the next tooth into line. So the wheel moves 2 × 50 = 100 teeth a second — 5 turns a second, 300 a minute on 50 Hz (360 on 60 Hz). In general: turns a minute = 120 × frequency ÷ teeth.
- Gearing: a single-thread worm on the arbor driving a 30-tooth wheel (30 : 1), then an 8-leaf pinion driving an 80-tooth wheel (10 : 1), gives 1 turn a minute — the seconds hand. From there, use the ordinary minute and hour gearing of The Mechanical Clock: 60 : 1 to the minute hand, 12 : 1 to the hour hand.
- Start it with a flick of a starting knob on the wheel's arbor. Too slow or too fast a flick, and it may lock at the wrong speed or stop; a light flywheel on the arbor helps it settle. Mark the dial with a start dot and check it against a good clock the next day.
A good one runs for weeks with no change in its error other than the grid's, restarts at once after a power cut (it then shows the wrong time — a little red flag that drops when the power fails warns the owner), and is quiet: a loud buzz means loose laminations or too much voltage.
Note The clock is only as good as the power station. A 50 Hz grid must give exactly 4,320,000 cycles a day. The station keeps a master clock driven by a synchronous motor from its own output beside an accurate pendulum or quartz clock (Quartz Crystals and Frequency Control). If the mains clock has fallen behind, the operator runs the turbines a fraction faster for a while until it catches up. With that habit, every mains clock in the village keeps time to a few seconds a month (Standard Time and Timetables).
Method 3: Converting AC to DC
The motor-generator
A synchronous (or induction) motor coupled to a DC dynamo (Rectifiers: Turning AC into DC, Method 1). Robust and simple; it isolates the DC side completely, and the dynamo's field rheostat sets the DC voltage from zero up. Efficiency is only about 75–85%, because the power passes through two machines.
The same set, with a dynamo whose voltage is controlled through its field, gives the smoothest possible speed control of a big DC motor: the Ward Leonard system. The dynamo feeds the motor's armature alone; turning the dynamo's field knob from zero to full takes the motor from standstill to full speed, either way round, with no starting resistance at all. It ran lifts, mine winders, rolling mills and big Machine Tools for most of the 20th century.
A motor-generator can also be a frequency changer — for example a 50 Hz motor driving a 25 Hz alternator with half as many poles for an old railway, or a 400 Hz alternator for small, light transformers and tools.
The rotary converter
A rotary converter is a DC dynamo's armature with slip rings added at the end opposite the commutator, each ring connected to evenly spaced points round the armature winding. Fed with AC on the slip rings, it runs as a synchronous motor; the same winding, turning in the DC field, delivers DC at the commutator. One machine, one winding, so it is smaller and more efficient — about 92–95%.
- The voltages are fixed by the machine: for three-phase rings, the AC between lines is about 0.61 times the DC voltage; for single-phase, about 0.71 times. To get 600 V DC for trams from three-phase, feed it about 370 V AC through a The Transformer.
- Starting: from the DC side, as a shunt motor (if DC from batteries is already there), then synchronise with lamps and switch the AC on; or from the AC side at reduced voltage through taps on the transformer, starting on its damper bars like an induction motor. Started from AC, the DC may come up the wrong way round, and the field must be reversed.
- Hunting and flashing over at the commutator are its weaknesses; damper bars and careful brush setting tame them.
Be honest about the effort: a rotary converter is a precision machine, with tens of commutator segments and a three-phase supply. Build the motor-generator first. Build a rotary converter only when you have a three-phase grid, tramways or electrolysis works to feed.
How to tell it worked
- Speed: count turns against a good clock with a revolution counter or a chalk mark. It must be exactly 120 × frequency ÷ poles — not 2–5% low, like an induction motor.
- Under load, the speed stays exactly the same until the motor pulls out.
- Power factor: with a known resistor in series with the motor, measure three voltages with an AC voltmeter: across the resistor (V₁), across the motor (V₂) and across both (V). Then power factor of the motor = (V² − V₁² − V₂²) ÷ (2 × V₁ × V₂). Over-exciting a synchronous motor should raise the power factor of the whole installation, seen as a fall in the generator's current for the same load.
- Clocks gain or lose no more than the grid does.
Note Troubleshooting. Hums and shivers but will not run → not brought up to speed; bring it nearer to synchronous speed before closing the switch, or apply the DC field later. Runs, then falls out with a roar under load → overloaded, or field too weak. Increase field current; reduce load. Speed swings back and forth (hunting) → no damper bars, a pulsing load, or a governor fighting it. Add damper bars or a flywheel. Clock runs at a fraction of the right speed → locked at a wrong speed; stop and restart with a better flick, and check the tooth spacing is even. Clock loses time over days → the grid frequency is low. Tell the power station. Rotary converter flashes over at the commutator → sudden overload, rough commutator or brushes misplaced. Fit a fast breaker on the DC side.
Dangers
Danger Out-of-phase closing wrecks machines. Connecting a synchronous motor or a second generator to the line out of step causes a dead short and huge twisting forces. Always synchronise with lamps or a meter, and fit fuses or breakers on both sides.
Danger High voltage in the field. If the DC field winding of a large synchronous motor is left open while it starts as an induction motor, the rotating field can induce thousands of volts in it, enough to kill and to puncture its insulation. Short the field through a resistance of about ten times its own while starting.
- Capacitors for power-factor correction hold a charge after the power is cut. Fit each with a permanent discharge resistor, and short it with an insulated tool before touching.
- Rotating machinery: guard couplings and belts (The Electric Motor).
- Mains clocks: the small transformer must be fused and enclosed; a clock coil wired straight to 230 V is a shock and fire risk (Wiring and Electrical Safety).
What this unlocks
- Accurate mains clocks in every house, school and railway station, and a shared time across a whole grid (Standard Time and Timetables).
- DC for tramways and Railways, Electrolysis of brine and Aluminium, Electroplating and battery charging, until Rectifiers: Turning AC into DC replace the machines.
- Smooth, powerful speed control for lifts and hoists (Lifts, Hoists and Mine Winding), mine winders and rolling mills.
- A healthier Power Lines and Distribution, carrying more useful power over the same wires.
- Constant-speed drives for Recording Sound, Cathode Rays and Television scanning discs and the teleprinter's timing (The Teleprinter).
How it was first done
In 1883–84 John Hopkinson in Britain showed that alternators could be run in parallel and that an alternator connected to the line would run as a motor, locked in step. In 1878 the Danish physicist Paul la Cour built the phonic wheel, a toothed iron wheel driven step by step by an electromagnet pulsed from a vibrating tuning fork, to keep distant telegraph instruments in step — the ancestor of the synchronous clock. Charles Proteus Steinmetz at General Electric gave engineers, from 1893, a simple mathematics for alternating currents that peak at different times, and with it a clear way to reckon power factor. Rotary converters were developed in the early 1890s and fed most of the world's tramways and electrochemical works until mercury-arc rectifiers displaced them from the 1920s and 1930s. Harry Ward Leonard patented his speed-control system in 1891.
Henry Ellis Warren of Massachusetts built a small self-starting synchronous motor for clocks and, around 1916, persuaded the Boston Edison company to install his master clock so its operators could hold the frequency to time; his Telechron clocks followed. Laurens Hammond sold synchronous clocks from 1928 and later used synchronous motors to turn the tone wheels of his electric organ, launched in 1935. By the 1930s most power stations in Europe and North America kept their frequency to clock time, and the mains clock became an ordinary household object.
Source: content/entries/electricity/synchronous-motors.md