Part 15 · Knowledge and Science
The Compass
How to turn a magnetised needle into a real instrument — a floating compass, then a pivoted needle under glass with a card marked in degrees — and how to correct it for magnetic declination and use it with a map to find your way and your position.
- Difficulty
- ●●●●●
- Time
- An afternoon for a floating compass; two or three days for a pivoted compass with a card and sights
- Steps from zero
- 12 prerequisites →
You need first
MagnetsThe full path from nothing — 12 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- Charcoal
- Hides and Leather
- Bellows
- Iron (the Bloomery)
- Magnets
- The Compass
Do them roughly in this order. See it on the tech tree →
Why it matters
The sun and stars give you true direction (see Finding Direction), but only when you can see them. Under cloud, in fog, in thick forest, underground or at sea at night, they are gone. A compass works in all of these. It lets you:
- Walk a straight line through forest or across featureless country, and come back the same way.
- Find where you are on a map from two landmarks you can see (Maps and Mapmaking).
- Steer a boat out of sight of land and keep a record of the course (Navigation, Boats and Sails).
- Survey fields, roads and mine tunnels: miners used compasses to follow a vein and to know which way a tunnel ran beneath the ground (Mining and Tunnelling, Surveying and Levelling).
- Lay out buildings and fields to the sun when the sky is grey.
This chapter assumes you already have a magnetised steel needle and know how to make one (see Magnets, which also covers the simplest floating needle). Here we turn that needle into an instrument you can read to a degree or two and trust.
How it works
The Earth is a weak magnet. A magnetised needle that is free to turn lines itself up with the Earth's magnetic field, so one end points to magnetic north. Three facts matter for making and using a compass:
- Magnetic north is not true north. The magnetic poles are hundreds of kilometres from the geographic poles, and the field is lumpy. The angle between the way the needle points and true north is called declination (sailors call it variation). Depending on where you are, it may be anything from 0° to 20° or more, east or west. It also drifts slowly, typically a few tenths of a degree per year, so a value measured once is good for some years but not for ever.
- The field dips into the ground. In the northern hemisphere the north end of a freely hung needle tips downward — about 60–70° below level in Europe, northern China or most of North America, and almost level near the equator. In the southern hemisphere the south end dips. A compass needle must be balanced against this dip with a small weight, or it drags on its pivot or the card.
- Iron pulls the needle aside. A knife, axe, iron pot, nail-studded box or iron-rich rock close by bends the needle off true. This is called deviation. The fix is simple: keep iron at least 1 m away, and never build iron into the compass itself.
Bearings. Directions are given as an angle measured clockwise from north, from 0° to 360°: east is 90°, south 180°, west 270°. A bearing is the direction from you to something, written this way. The older sailors' system divides the circle into 32 points (north, north by east, north-north-east, north-east by north, north-east…), each 11¼°; you will see it on old charts.
What you need
| Item | Details |
|---|---|
| Needle | Hardened Steel, 6–10 cm long, 2–4 mm wide in the middle, 0.5–1 mm thick. A thin strip of spring steel (Springs) cut to a long diamond shape is ideal |
| Lodestone or a strong magnet | To magnetise and re-magnetise the needle (Magnets) |
| Cap | A small cone-shaped hollow for the needle to sit on: a punched cup of thin Copper Smelting or brass, or a drilled bead of agate or Glass |
| Pivot | A hardened steel needle with a sharp, polished point, set upright in the base |
| Bowl | Turned wood (boxwood or any close-grained hardwood), Pottery, brass or copper — never iron — 8–15 cm across inside |
| Card | Stiff Paper or thin card, or a disc of split mica, marked with the points and degrees |
| Cover | A disc of clear Glass or Window Glass, or split mica, or thin scraped horn, bedded in the rim with putty or wax |
| For a sighting compass | Two thin upright vanes of brass or wood, one with a narrow slit, one with a hair or thread stretched vertically |
| Small tools | File, fine drill or awl, a centre punch, fine abrasive and rouge (Abrasives and Grinding Stones) |
Where to find it
- Lodestone and magnetite: see Magnets and Finding and Identifying Ores.
- Boxwood: a slow-growing evergreen shrub or small tree with small, shiny, leathery leaves in pairs and very hard, fine, yellow wood that hardly moves with damp. It turns beautifully on a The Lathe. Pear, apple, hornbeam and maple also do.
- Agate: a banded form of quartz, found as rounded nodules and pebbles in old lava flows and in river gravels downstream from them. It is waxy-smooth, translucent at thin edges, often banded in rings, scratches glass, and cannot be scratched by steel. A polished hollow in agate is an excellent, almost frictionless pivot cap. Rock crystal (clear quartz, see Rocks and Minerals) works as well.
- Mica: shiny flakes in granite and pegmatite that split into thin, clear, flexible sheets (see Rocks and Minerals). A sheet the thickness of paper makes a light, unbreakable card or cover.
- Horn: cattle or goat horn, boiled until soft, split, pressed flat and scraped thin, is translucent — the "glass" of old lanterns (Lamps and Candles).
Method 1: The improved floating compass
The floating needle in Magnets already points north. Three improvements make it a working instrument.
- Give it a fixed bowl and a mark. Use a round bowl 12–15 cm across, of wood or pottery. Cut or paint a short line on the rim — the lubber line — and a matching line on the opposite side. When you travel, point the lubber line where you are going.
- Mark the rim in degrees. Divide the rim into 36 equal parts of 10° each (see the card, below), numbered clockwise.
- Keep the needle off the sides. Float the needle on a disc of cork or light wood 3–4 cm across; push a straw or thin reed upright through its centre and slip a loose ring of the same reed over a thin stick fixed upright in the middle of the bowl. The float can turn freely but cannot drift to the edge.
To read it: hold the bowl level, let the needle settle, then turn the whole bowl (not the needle) until the north end of the needle points to 0° on the rim. Now the lubber line shows your heading in degrees.
This is the compass of Chinese sailors in the 1100s. It is crude but it works on a boat in light weather. For walking and for any accuracy, build the dry compass.
Method 2: The pivoted dry compass
1. Shape the needle
- Cut a strip of hardened steel 8 cm long and 3 mm wide. If it is not already hard, shape it first, then heat it to a bright cherry red (about 800 °C) and quench in water (see Steel).
- Grind it to a long diamond, pointed at both ends and widest in the middle, on a wet stone. Keep the two halves equal in shape and weight.
- Make the centre hole: soften just the middle by holding it against a red-hot iron bar until it turns blue, then drill or punch a hole 2–3 mm across through the exact centre. Find the centre by balancing the needle across a knife edge, both lengthwise and crosswise.
2. Make the cap
The cap is a tiny inverted cone that sits on the pivot point. It must be hard, smooth and sharply pointed inside, so the needle balances on a single point with almost no friction.
- Metal cap. Cut a disc of thin brass or copper sheet 6 mm across. Lay it over a conical hollow drilled in a block of hardwood, and drive a hardened steel punch, ground to a 60° point, into it with a light hammer blow. You get a small cone with a sharp inside apex. Polish the inside with rouge on a sharpened stick. Solder or rivet it into the needle's centre hole, cone pointing up (Soldering and Brazing).
- Stone cap. Better and longer lasting: grind a 5–6 mm pebble of agate or rock crystal flat on two sides, then drill a conical pit in one face with a copper wire point charged with emery and oil, twirled between the fingers or with a bow drill (Drills and Boring). Polish the pit with rouge. Fix it in a small brass collar through the needle. This is the "jewel" of later compasses; it hardly wears.
3. Make the pivot
Take a hardened steel sewing needle or a small steel rod 2 mm thick. Grind and then polish the end to a point with a cone angle a little sharper than the cap (so the point touches only at the very bottom of the cap). Hone it on a fine stone and finish on leather with rouge until it looks bright under a lens (Lenses). Drive it upright into a hole in the centre of the bowl's floor, standing tall enough that the needle swings 1 cm above the floor.
4. Balance against dip
Set the needle on the pivot, before magnetising it. It should hang level. If not, file a little off the heavy arm. Now magnetise it by stroking (Magnets). Put it back: the north end now dips (in the northern hemisphere). Wrap a few turns of fine copper or brass wire round the other arm, or press on a small bead of wax, and slide it along until the needle hangs level again. If you take the compass far north or south, re-adjust it.
5. Make the card
- On stiff paper, draw a circle the size of the needle, plus 1 cm. Draw two lines through the centre at right angles (see Geometry and Trigonometry): north–south and east–west.
- Divide each quarter into three by stepping out the radius around the circle — the radius steps off exactly 60° — and then each 30° by eye or by bisecting into 15° and halving again. Mark every 5° with a short line and every 10° with a longer one. Number every 30° or every 10°, clockwise from N.
- Draw a bold arrow or a fleur-de-lys at north, so it can be read in poor light.
- For a ship's or traveller's compass, glue the card to the top of the needle, N over the north end, so the whole card turns. You read your heading against the lubber line on the bowl.
- For a surveyor's compass, do the reverse: fix the card to the bowl and let a bare needle swing over it. You read where the needle points on the card. (Number this card anticlockwise, so that turning the box towards an object gives you its bearing directly. Many old surveyors' compasses have east and west swapped on the card for this reason.)
6. Close it
Set a glass or mica disc into a groove in the rim of the bowl, bedding it in putty, wax or pitch so that it is airtight and dust cannot get in. Leave 3–5 mm of clearance above the card. Make a small lever or a pin through the side that can lift the needle off its pivot when the compass is carried; this keeps the pivot sharp.
For use at sea, hang the bowl in gimbals — two rings, one inside the other, each pivoted at right angles to the last — so it stays level as the boat rolls. Filling the bowl with alcohol and water (which does not freeze easily) slows the card's swing, which helps in a rough sea.
7. Add sights (optional)
For accurate bearings, fit two upright vanes 8–10 cm tall on opposite sides of the box along the N–S line of the box: one with a vertical slit 1 mm wide, the other with a vertical hair. Look through the slit, line the hair up on the object, and read the needle. A sighting compass like this reads to about 1°.
Finding your declination
Do this once, carefully, wherever you settle, and again every few years.
- Lay out a true north–south line on flat ground using the equal-shadow method or the Pole Star (Finding Direction). Mark it with two stakes at least 10 m apart.
- Stand the compass on a post on the line, well away from iron. Sight along the line to the far stake.
- Read the angle between the line and where the needle points. If the needle points to the east of true north, declination is east; if to the west, west.
- Write it down, with the place and the year.
Correcting bearings. A compass reading is a magnetic bearing; a map drawn from the sun and stars uses true bearings.
- If declination is east: true bearing = magnetic bearing + declination.
- If declination is west: true bearing = magnetic bearing − declination.
Example: declination is 8° west. Your compass shows a hilltop at 50°. The true bearing is 42°.
A good habit: draw your map's north lines to magnetic north as well as true north. Then you can lay the compass straight on the map with no arithmetic.
Using a compass with a map
Orienting the map. Lay the map flat and set the compass on it. Turn the map until its magnetic-north line runs parallel to the needle. Now every road, river and hill on the map lies in the same direction as the real one.
Walking on a bearing.
- On the map, draw a line from where you are to where you want to go. Measure its angle from north with the compass card or a protractor. Correct it to a magnetic bearing.
- Hold the compass level in front of your chest, lubber line forward. Turn your whole body until the needle shows that bearing.
- Pick a landmark straight ahead on that line — a tree, a rock — and walk to it. Then take the bearing again and pick the next one. Never try to watch the needle while walking.
- Count paces to measure distance (Measurement from Scratch, Finding Direction).
- Getting round obstacles: walk at a right angle for a counted number of paces, then forward past the obstacle, then back at a right angle for the same number of paces.
The back bearing. To come home, add 180° to your outward bearing (or subtract 180° if it is over 180°). Out on 60°, home on 240°.
Finding where you are (resection).
- Find two landmarks you can see and can also find on the map, ideally 60–120° apart.
- Take a bearing to each. Correct each to true.
- On the map, from each landmark draw a line along the back bearing (bearing ± 180°).
- You are where the two lines cross. A third landmark makes a small triangle; you are inside it. A small triangle means good bearings.
Aiming off. If you are heading for a point on a long river or road and cannot see it, deliberately steer 5–10° to one side. When you reach the river, you know which way to turn.
How to tell it worked
- It always comes back. Deflect the needle with a knife held near it, then take the knife away. A good compass swings back to exactly the same reading, from either side, within a degree. If it stops at different places, the pivot is blunt, the cap is rough, or the card is rubbing.
- It swings freely. Disturbed, it should swing back and forth 4–8 times before settling. If it stops at once, there is too much friction.
- It agrees with the stars. After correcting for declination, a sight on the Pole Star (or the south celestial pole region) should give 0° (or 180°) within 1–2°.
- Two compasses agree when set side by side, far apart from each other and from iron.
Note Troubleshooting. Needle sticks or stops in different places → regrind and polish the pivot point; re-polish the cap. Make sure it lifts off the pivot when carried. One end drags on the card or floor → re-balance against dip with the wire rider. Readings jump when you move a few steps → there is iron near you, on you or in the ground. Look for buckles, knives, nails in the box, or dark iron-rich rocks; move away and try again. The needle has grown sluggish over months → it has lost magnetism, or the pivot has worn. Re-stroke it with the lodestone; resharpen the pivot. Card swings wildly at sea → fill the bowl with liquid (alcohol and water), and hang it in gimbals.
Dangers
A compass is safe to make. The danger lies in trusting it when you should not.
- Local attraction. Iron-rich rocks — dark, heavy basalt and magnetite-bearing ground — can swing a compass by tens of degrees over a few hundred metres. If readings change as you walk, use the sun and stars instead.
- Iron on a boat. Anchors, cannon-sized ironwork, a stove, or iron nails near the binnacle (the compass stand) make steady errors. Keep iron at least 1 m away, and check the compass on every heading against the sun or a known line.
- Lightning can reverse or wipe a compass needle's magnetism. After a storm, check that north is still north.
- Near the magnetic poles, in the far north of Canada or near Antarctica, the needle is weak and wanders. Rely on the sky.
- Getting lost. Tell someone your route, carry water, and turn back while you still know your back bearing.
Going further
- Dip needle. A needle pivoted on a horizontal axle, free to swing up and down, shows the angle of dip. It roughly tells your magnetic latitude, and finds buried iron ore: the dip changes sharply over a magnetite body (Finding and Identifying Ores, Mining and Tunnelling). Electronic instruments that do this far more sensitively are in Hall Sensors and Magnetometers.
- Prismatic compass. A small prism or mirror next to the sights lets you read the card while sighting the object — reading to half a degree.
- Surveying. A sighting compass and a chain make quick, rough surveys of fields and woods (Surveying and Levelling, Maps and Mapmaking). For better than a degree, use a theodolite with a The Telescope.
- The gyrocompass. A fast-spinning wheel that finds true north by itself, with no magnetism at all, and is not fooled by iron or by the magnetic poles (Gyroscopes and Inertial Guidance).
- Charting declination. If many people record declination at many places, the readings make a map of the Earth's field. It is also a way, though a rough one, of telling roughly where you are east–west.
How it was first done
Chinese writers of the 1st century AD describe a "south-pointer" spoon, probably of lodestone, spun on a smooth plate for divination, though how it was made is still argued over. By 1044 a Chinese military manual describes a heated iron fish floated on water to point south. In 1088 the scholar Shen Kuo described needles rubbed on lodestone and hung by a single silk thread, and noted they point slightly east of south — the first record of declination. By 1117 Chinese sailors were steering by compass in fog.
In Europe the English monk Alexander Neckam wrote of a needle that shows sailors the way, around 1190. In 1269 Petrus Peregrinus described a pivoted needle in a box with a marked scale and sights — the first dry compass. Mediterranean sailors put the card on the needle around 1300. Columbus noticed in 1492 that declination changed as he sailed west. The English compass-maker Robert Norman described dip in 1581, and in 1635 Henry Gellibrand showed that declination at a place slowly changes. Edmond Halley published the first chart of declination over the oceans in 1701. In the 1870s William Thomson (Lord Kelvin) built ship's compasses with many small light needles and with iron balls beside the binnacle to cancel the iron of steamships.
Source: content/entries/knowledge/compass.md