Duplicating: Carbon Paper, Hectograph and Stencil

Ways to make copies of letters, forms, lessons and notices without setting type — linked twin pens, carbon paper, the copying press, the gelatin hectograph and the stencil duplicator, or mimeograph, which turns out hundreds of copies from one hand-cut or typed stencil.

Difficulty
●●●●●
Time
An afternoon for a hectograph pad; a week to build a flatbed stencil duplicator and learn to cut stencils
Steps from zero
25 prerequisites →

You need first

The TypewriterPaper

This unlocks

Copying Documents and Xerography
The full path from nothing — 25 steps before this one
  1. Fire
  2. Stone Tools
  3. Cordage and Rope
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Basic Woodworking
  7. Hunting and Trapping
  8. Pottery
  9. Charcoal
  10. Hides and Leather
  11. Lye and Potash
  12. The Wheel and Axle
  13. Ink
  14. Bellows
  15. The Lathe
  16. Paper
  17. Iron (the Bloomery)
  18. Copper Smelting
  19. Printing
  20. Blacksmithing
  21. Steel
  22. The Steam Engine
  23. Springs
  24. Machine Tools
  25. The Typewriter
  26. Duplicating: Carbon Paper, Hectograph and Stencil

Do them roughly in this order. See it on the tech tree →

Why it matters

A community that is growing needs the same words in many hands: lesson sheets for a school (Teaching and Schools), the rules and minutes of a council (Organising a Community), forms and receipts (Money, Trade and Record-keeping), instructions for a vaccination round (Vaccination), copies of a drawing for three workshops (Technical Drawing), and a weekly news sheet. Copying by hand takes a good scribe 20–30 minutes a page and introduces mistakes in every copy.

A printing press (Printing) is the answer for books and long runs, but it needs cast type, a press, and hours of setting for each page. For 10 to 1,000 copies of something written today and needed tomorrow, simpler methods are faster:

Method Copies from one original Speed Needs
Polygraph (linked pens) 2 originals Writing speed Woodwork, two pens
Carbon paper 2–5 Writing or typing speed Wax, soot, thin paper
Copying press 1–3 2 minutes each Special ink, tissue, a press
Hectograph 20–50 15 seconds each Gelatin, glycerine, a strong dye
Stencil duplicator 200–1,000+ 5–10 a minute by hand Waxed tissue, oily ink, a frame

How it works

Each method moves ink from one master to many sheets, in a different way:

  • Pressure through carbon: a pen or type blow squeezes a waxy black layer onto the sheet below.
  • Soluble ink offset: ink that stays partly soluble is lifted off by damp paper pressed against it.
  • Dye reservoir: a strong dye soaks into a jelly pad, and each damp sheet pressed on it takes a little of the dye back out — fainter each time.
  • Stencil: ink is pushed through holes in a sheet that is otherwise ink-proof. The stencil is not used up, so the number of copies is limited only by its wear.

What you need

Item For Source
Thin, strong paper Carbon copies, copying tissue, stencil base Long-fibre paper from mulberry or hemp bark (Paper)
Absorbent, unsized paper Stencil copies Paper made without size, or lightly sized
Beeswax, tallow, castor oil Carbon paper and stencil coating Beekeeping, Soap (tallow), Oils and Pressing
Soot Carbon paper and stencil ink Lamp soot (Ink)
Iron-gall ink and sugar Copying ink Ink, Sugar
Gelatin and glycerine Hectograph pad Hide glue boiled clear (Glues and Adhesives); glycerine from soap-making (Soap)
Aniline violet dye Hectograph ink Coal Tar Chemicals
A screw or lever press Copying press Bookbinder's press (Bookbinding, Screws, Nuts and Bolts)
Fine silk or cotton gauze, a wooden frame, a roller Stencil duplicator Silk, Basic Woodworking
A file plate Cutting stencils by hand A fine, flat file, or a steel plate cut with fine grooves (Files and Saws)

Method 1: The polygraph — two pens at once

The simplest copier needs no chemistry at all. Two pens are joined by a frame of light rods so that whatever one pen does, the other copies exactly, 15–20 cm to the side.

  1. Make a parallelogram of four light hardwood rods, pinned at the corners with brass pins so they move freely but without play. Two opposite sides each carry a pen holder, at the same distance from the pins.
  2. Fix one corner to a pivot on the desk, so the frame can swing across the paper and lift slightly.
  3. Fit identical pens and lay two sheets side by side. Write with one; the other writes the same.

The copy is as good as the original, but only one extra copy is possible, and the joints must be precise. A pantograph — the same linkage with unequal arms — copies drawings larger or smaller (Technical Drawing).

Method 2: Carbon paper

  1. Make it: melt 1 part beeswax with 1 part tallow or castor oil, stir in about half as much fine soot, and brush it thin and hot onto one side of thin, strong paper. Wipe off the excess with a warm cloth. Let it cool (The Typewriter).
  2. Use it: lay the original sheet, a carbon (coated side down), and the copy sheet in a pile. Write firmly with a hard pencil, a stylus or a ball-pointed bone tool, or type with a firm stroke. With thin paper, 3–5 copies come through.
  3. Books of receipts: bind numbered pages in pairs with a loose carbon; the customer takes the top copy, the book keeps the second.

A carbon sheet gives 20–50 uses. Keep it flat and cool; in heat it smears.

Method 3: The copying press

For two hundred years, merchants and governments kept a copy of every letter they sent this way.

  1. Copying ink. Add sugar or honey to good iron-gall ink (Ink) — start with about 1 part sugar to 5 parts ink by volume — so it dries on the surface but stays slightly soluble underneath. Test and adjust: too little sugar and no copy comes off; too much and the original smudges.
  2. Write the letter normally. Copy it within a day.
  3. Prepare the tissue. A letter book is a bound book of very thin, unsized tissue paper. Put an oiled sheet behind the page you will use, to keep damp from the rest of the book. Brush the tissue page with clean water and blot it with cloth until it is evenly damp but not shiny.
  4. Press. Lay the letter face down on the damp tissue, close the book, and squeeze it in a screw press for 1–2 minutes.
  5. Read the copy from the other side of the tissue: the ink has come through the thin paper, so it reads the right way round.

Close the book only when the copied page has dried. A good letter gives one strong copy, sometimes two or three fainter ones.

Method 4: The hectograph (jelly pad)

NOTICE NOTICE NOTICE 1. Write the master strong violet dye ink, plenty of it 2. Face down on the pad smooth gently, leave 1–3 minutes 3. Peel off; print copies one clean sheet at a time smooth, hard-sized paper Gelatin pad gelatin, water, glycerine in a shallow tray 1st 20th 40th copy image on pad, reversed
Fig. 1 The hectograph. 1: write the master with strong violet dye ink. 2: lay it face down on the gelatin pad for two minutes; the dye soaks into the jelly. 3: peel it off and lay clean sheets on the pad one after another, smoothing each with the hand; each lifts a little dye. Copies fade gradually — 20 to 50 good ones.

The pad

  1. Soak 1 part (by weight) of clear gelatin — the purest hide glue (Glues and Adhesives) — in 2 parts of clean water for 12 hours.
  2. Warm it in a pot standing in hot water (a water bath, never over a direct flame) until it melts. Stir in 6 parts glycerine, warmed. Keep it hot, stirring gently, for 15–20 minutes to drive off a little water.
  3. Pour into a shallow tray of tin or wood lined with oiled paper, about 25 × 35 cm and 1.5–2 cm deep. Drag a strip of paper across the surface to pull off bubbles.
  4. Set for 12–24 hours on a level table, covered against dust.

The pad should feel like firm rubber, smooth and slightly tacky. If it is runny or sticks to the paper, it needs more gelatin; if it is hard and the dye will not soak in, more glycerine.

The ink

Hectograph ink must be an intensely strong dye that dissolves in water. The classic one is methyl violet (an aniline dye from coal tar — see Coal Tar Chemicals): about 1 part dye to 7 parts water, with 1 part alcohol and 1 part glycerine. Violet gives the most copies; aniline reds, greens and blacks give fewer.

Note Without aniline dyes this method is much weaker. Strong extracts of natural dyes may give a few faint copies; test what you have on a small pad before relying on it (Dyes and Mordants).

Printing

  1. Write or draw the master on smooth, hard-sized paper with a clean steel or quill pen, using plenty of ink. Let it dry until the lines have a coppery shine.
  2. Wipe the pad lightly with a damp sponge; let it stand a minute.
  3. Lay the master face down on the pad, smooth it gently with your palm, and leave it 1–3 minutes. Peel it off from one corner. The writing is now on the pad, reversed.
  4. Lay a sheet of plain paper on the pad, smooth it with the palm or a roller, and peel it off: a copy. Repeat, steadily, 3–4 sheets a minute.
  5. After use, the dye slowly sinks into the pad. Leave it a day or two before the next master, or wash the surface with lukewarm water, or melt the pad in a water bath and pour it again.

Method 5: The stencil duplicator (mimeograph)

This is the workhorse: from one stencil, hundreds of sharp black copies, by hand, at 5–10 a minute.

Hinged frame Silk screen fine, stretched tight Stencil waxed tissue; ink passes only where lines are cut Oily ink soot in castor oil Roller one firm pass Absorbent paper the copy Padded bed Hinge Flatbed stencil duplicator, cross-section thicknesses greatly exaggerated
Fig. 2 The flatbed stencil duplicator, in cross-section. The stencil hangs from a hinged frame under a fine silk screen. Oily ink spread on the screen is pushed by the roller through the screen and through the cut lines of the stencil onto the absorbent paper on the bed below.

Stencils

A stencil is a sheet of very thin, strong, long-fibred tissue — the kind of paper made from mulberry or hemp bark (Paper), about as thin as onion skin — soaked with a waxy coating that ink cannot pass. Wherever the coating is broken, the open web of fibres lets ink through.

  1. Coating. Melt beeswax with a little pine resin and a little tallow or castor oil — begin with 4 : 1 : 1 by weight. Brush it thinly over the tissue while warm, or dip the tissue and draw it between two warm smooth boards. Hang to cool. It should be translucent, flexible, and not tacky.
  2. Test. Fold a corner: the coating must bend without cracking. Write on it over the file plate (below): the stylus should cut clean, fine lines without tearing the tissue. Too brittle → more oil or tallow. Too soft and greasy, so it smears → more wax and resin.
  3. Backing. Fix each stencil by its top edge to a stiff paper backing sheet, and put a thin sheet of carbon paper or soft card between them so you can see your writing as you cut.

Cutting a stencil

  • By hand. Lay the stencil on a file plate — a flat steel plate covered with very fine grooves or teeth, about 30–40 to the centimetre, like a fine file. Write with a stylus: a smooth steel point with a tip about 0.5 mm wide, in a wooden handle. Firm, even pressure. The teeth beneath break the coating into tiny dots along each line. For lettering, rule faint guide lines; for drawings, use a ruler and a fine wheel-pointed stylus.
  • On the typewriter. Disengage the ribbon so the type slugs strike the stencil directly (The Typewriter). Type firmly and evenly. Each letter punches its shape through the coating. This is how most stencils were cut once typewriters spread.
  • Corrections. Brush a little melted coating mixture (or "correction fluid" of wax dissolved in turpentine — see Ether, Acetone and Solvents) over the mistake, let it set, and cut again.

The ink

Stencil ink must be soft and oily, so it flows through tiny holes and soaks into the paper rather than sitting on top. Grind fine soot into castor oil or raw (unboiled) linseed oil to a soft paste, like thick cream — much softer and slower-drying than letterpress ink (Ink). Grind it thoroughly on a stone slab with a muller; lumps clog the stencil.

The flatbed duplicator

  1. Bed. A flat board 40 × 30 cm, padded with a layer of felt under smooth card or a sheet of rubber.
  2. Frame. A wooden frame a little larger, hinged at the back edge of the bed so it lifts and lowers like a lid.
  3. Screen. Stretch fine silk gauze (or very fine cotton lawn) tightly across the frame and glue and tack it. Wet the silk first; it tightens as it dries.
  4. Mount the stencil on the underside of the screen, coated side down, by its top edge, smooth and without wrinkles. Peel off the backing.
  5. Ink. Spread a thin, even film of ink on top of the screen with the roller, working it in until the cut lines show black through the stencil.
  6. Roller. A wooden cylinder 5–6 cm thick and as wide as the frame, covered with felt or with a cast "composition" of hot glue and glycerine (the same stuff as printers' rollers), on handles.

Printing

  1. Lay a sheet of absorbent paper on the bed against two stops, so every sheet goes in the same place.
  2. Lower the frame. Roll once, firmly and evenly, from back to front.
  3. Lift the frame. The sheet often sticks to the stencil; peel it off and lay it aside to dry, spread out — do not stack wet copies.
  4. Repeat. Add ink to the screen every 10–20 copies, before the copies grow grey.
  5. At the end, lift the stencil off, blot it between sheets of newsprint, and store it flat if you may need more copies later. Clean the screen with a rag and a little oil or turpentine.

The rotary duplicator (later): the stencil wraps around a drum of perforated metal covered with a cloth pad, with ink inside; a crank turns the drum against a pressure roller that feeds paper through. It prints 30–60 copies a minute — the machine that ran school and office printing for most of the 20th century. It needs Sheet Metal and Rolling and Gears.

How to tell it worked

  • Hectograph: the 20th copy is still easily readable.
  • Stencil: the 200th copy is as sharp as the 20th; letters are solid, not speckled; no ink "halo" around them; nothing comes through where nothing was cut.
  • Copying press: the copy is readable everywhere, with no blurred patches.

Note Troubleshooting. Hectograph copies faint from the start → dye too weak, master not left long enough, or the pad too dry; use more dye, wait longer, sponge the pad. Hectograph copies blurred → the pad is too wet; wait a few minutes after sponging. Stencil copies grey and broken → lines not cut through: press harder, use a sharper file plate; or ink too stiff — add oil. Ink spreads and blots → ink too thin or paper too absorbent; add soot, use lightly sized paper. Copies show smudges where nothing was cut → coating cracked by folding or handling; make it more flexible; never fold stencils. Letter "o" and "e" fall out of a typed stencil → too hard a blow; type more lightly or use a thicker coating. Copying-press copies blurred → tissue too wet; blot more.

Dangers

Warning Aniline dyes are poisonous and stain skin for days. Do not lick pens or fingers; wash hands before eating; keep dye away from children and food. Some old hectograph and spirit-duplicator recipes used wood alcohol (methanol), which causes blindness and death if swallowed and is harmful to breathe — use grain alcohol (Distillation) and good ventilation.

Danger Oily rags can set themselves on fire. Rags soaked with linseed oil used to clean screens and rollers heat up as the oil dries, and can burst into flame hours later. Spread them flat outdoors to dry, or keep them under water in a closed tin.

  • Hot wax and glue for coatings and pads burn and stick to skin; heat them over water, never over open flame. Molten wax splashed on a fire flares violently.
  • Presses crush fingers; keep hands clear when screwing down.

What this unlocks

Cheap copies make possible schools with a lesson sheet for every pupil (Teaching and Schools), published accounts and rules that everyone can check (Organising a Community), forms that make record-keeping fast and consistent (Money, Trade and Record-keeping), and spreading this book itself, chapter by chapter, to every settlement (Libraries and Preserving Knowledge). Stencils on silk screens also print posters, labels, signs and patterns on cloth — Screen Printing.

How it was first done

Ralph Wedgwood in England patented carbon paper for his "stylographic writer" in 1806. James Watt, wanting copies of his business letters, patented the copying press in 1780; it was used in offices until the typewriter and carbon paper replaced it in the early 1900s. John Isaac Hawkins and Charles Willson Peale made a polygraph that Thomas Jefferson used from 1804 to keep copies of his letters. The gelatin hectograph came into use in the late 1870s, using the new aniline dyes. In 1876 Thomas Edison made an "electric pen" whose needle punched holes in paper stencils, and in 1880 he patented "autographic printing" with a stylus on a file plate; the Chicago firm of A. B. Dick sold it from 1887 as the Mimeograph. In London David Gestetner, from Hungary, patented his Cyclostyle wheel-pen in 1881 and later made stencils for typewriters and rotary duplicators. In 1923 the German Wilhelm Ritzerfeld made the spirit duplicator. Stencil duplicators printed most school worksheets, church bulletins, union leaflets and underground newspapers of the 20th century, wherever a printing press was too costly, too slow, or too dangerous to own.