◆ Rebuild

Part 9 · Health and Medicine

The First Aid Kit

How to make the things that go in a first aid kit — roller and triangular bandages, gauze, absorbent cotton, slings, padded splints, tweezers, sterile water and antiseptics — what to keep in a household box, a travelling pouch and a village clinic store, and how to keep it all clean, dry and ready.

Difficulty
●●●●●
Time
A few days of cutting, boiling and rolling to stock a household kit; ongoing checks every three months
Steps from zero
9 prerequisites →

You need first

Wound Care and AntisepticsSterilising Instruments and Dressings

This unlocks

Emergency Cards
The full path from nothing — 9 steps before this one
  1. Fire
  2. Finding and Preparing Clay
  3. Sanitation and Germs
  4. Finding and Purifying Water
  5. Pottery
  6. Fermentation
  7. Distillation
  8. Wound Care and Antiseptics
  9. Sterilising Instruments and Dressings
  10. The First Aid Kit

Do them roughly in this order. See it on the tech tree →

Why it matters

Bleeding must be stopped in minutes. A broken limb must be splinted before the person is moved. A burn must be covered before it is fouled. In each case, the person who helps has no time to weave cloth, boil it, find straight sticks or make an antiseptic. Everything must be ready, clean and in one known place before the accident happens.

This chapter is the companion to Wound Care and Antiseptics (what to do) and Sterilising Instruments and Dressings (how to make things germ-free). It explains how to make each item from raw materials, how much to keep, and how to keep it usable for months. A kit in every house, workshop, boat and wagon, and a well-stocked store at the clinic, will save more lives than any single medicine.

How it works

A first aid kit does four jobs:

  1. Stop bleeding and cover wounds — pads to press on and soak up blood, and bandages to hold them.
  2. Keep germs out — sterile dressings, clean water and antiseptics, so a small wound does not become a deadly infection.
  3. Hold injured parts still — splints and slings, which ease pain and stop broken bone ends doing more damage.
  4. Help a person through the first hours — rehydration salts, pain relief, warmth, and a way to record what was done.

Everything in it must be clean (sterile if it touches a wound), dry, labelled, and easy to grab in the dark.

What you need

To make From Chapter
Plain-woven linen or cotton cloth, close and open weave Flax, cotton Flax, Hemp and Linen, Cotton, Spinning and Weaving Cloth
Raw cotton fibre, or old linen — Cotton
Soda ash or wood-ash lye Ashes Soda Ash and Baking Soda, Lye and Potash
Light wood strips for splints Lime (basswood), willow, poplar Basic Woodworking
Wool for padding Sheep Wool
Steel or brass strip for tweezers and scissors Forge Steel, Zinc and Brass, Axes, Chisels, Knives and Planes
Strong spirit (70% alcohol) Wine, beer Distillation
Chlorine solution Salt, electricity Chlorine and Bleach
Honey, salt, sugar — Beekeeping, Salt, Sugar
Tins, glazed jars, wooden boxes — Tin and Pewter, Pottery, Furniture

Where to find it

  • Old linen and cotton — sheets, shirts — are the best starting material: soft, absorbent and already worn thin. Wash and boil them.
  • Raw cotton from cotton bolls (Cotton); if you have none, linen lint (below) or sphagnum moss from bogs, dried and sewn into cloth bags, makes absorbent padding (Wound Care and Antiseptics).
  • Light splint wood — lime (basswood), willow and poplar are light, easily shaped and do not splinter.

Making bandages

Roller bandages. The everyday bandage for holding pads in place and supporting sprains.

  1. Take boiled, washed, plain-woven cloth. Tear it into long strips along the threads (tearing follows the weave and gives a straight edge; cutting wanders). Widths: 5 cm for fingers and hands, 7.5 cm for arms and children's legs, 10 cm for adult legs and the trunk. Length: 4–5 metres.
  2. Pull off the loose threads along the edges. Sew strips end to end with flat seams to get the length.
  3. Roll tightly, like a scroll, so the bandage is firm and can be unrolled one-handed onto a limb.
  4. For a stretchy bandage (better for sprains and holding dressings on joints), cut the cloth on the diagonal (on the bias, at 45° to the threads) — bias-cut cloth stretches — or knit a long strip in plain stocking stitch from wool or cotton yarn (Knitting, Crochet and Netting).

Triangular bandages. The most useful single item in any kit.

  1. Cut a square of strong cloth 1 metre on each side and cut it corner to corner into two triangles. Each has a long side of about 140 cm.
  2. Hem the edges if you have time.
  3. Fold it neatly: open, it makes slings and covers a head, a hand or a foot; folded into a broad bandage (point folded to the long edge, then once more) or a narrow bandage (once more again), it ties splints, holds pads on, or makes an emergency tourniquet strap.
1. Cut a square 1 metrecut corner to corner:two bandages, longside about 140 cm 2. Open or folded long edge point broad bandageholds pads, splints narrow bandageties, ring pads 3. Arm sling Knotin the hollowabove thecollarbone,padded hand a littlehigher than elbow;fingers showing point pinnedat the elbow forearmcradled
Fig. 1 Making and using a triangular bandage. A one-metre square cut corner to corner gives two. Open, it makes an arm sling that supports the forearm with the hand a little higher than the elbow; folded, it becomes a broad or narrow bandage for tying splints and holding pads.

Arm sling (for a broken forearm, wrist or collarbone, or a hand wound):

  1. Support the injured arm across the chest, the hand a little higher than the elbow.
  2. Slide the open triangle between the chest and the arm, the long edge running down the body on the uninjured side, the point toward the injured elbow.
  3. Bring the upper end round the back of the neck on the uninjured side.
  4. Bring the lower end up over the forearm to meet it, and tie a reef knot in the hollow above the collarbone on the injured side, not on the bone. Pad the knot.
  5. Fold the point at the elbow forward and pin or twist it so the elbow cannot slip out.
  6. Check the fingertips are pink and warm.

Making dressings

Gauze. A loosely woven, open cloth that lets blood and pus pass through into the padding behind it. On the loom (The Loom), weave plain cloth with only about 8–12 threads per centimetre each way (ordinary shirt linen has 20–30), from fine, smooth cotton or linen yarn. Boil, rinse and dry it.

Pads. Fold gauze or soft cloth 8 layers thick into squares of 5 × 5 cm, 10 × 10 cm and 20 × 20 cm (large, for big wounds and burns), with all cut edges folded inside so no threads come loose in a wound (Sterilising Instruments and Dressings).

Absorbent cotton ("cotton wool"). Raw cotton is waxy and repels water; boiled with alkali, it soaks up blood like a sponge.

  1. Pull clean raw cotton apart into loose tufts, removing seeds and trash.
  2. Boil it for 1–2 hours in water with about 2 tablespoons of soda ash per litre (or clear wood-ash lye diluted until it feels only slightly slippery between the fingers — Lye and Potash).
  3. Rinse it in several changes of clean water until all slipperiness is gone. A final rinse with a little vinegar removes the last alkali.
  4. Squeeze, dry, and card it into soft, even sheets (Spinning and Weaving Cloth).
  5. Test: drop a pinch on water. Absorbent cotton sinks within seconds; raw cotton floats for minutes.

Wrap a layer of absorbent cotton in gauze to make a thick, soft pad dressing for heavily bleeding or weeping wounds. Never put loose cotton wool directly on a wound — the fibres stick in it.

Lint. Without cotton, scrape the surface of old, clean linen with a blunt knife to raise a soft, fluffy layer. Soldiers' wounds were dressed with this for centuries. Use it only behind gauze.

Honey dressings for burns and dirty wounds: a small, sealed glazed pot of honey in every kit (Wound Care and Antiseptics, Beekeeping).

All pads, gauze and cotton for wounds go into sterile packs — wrapped in two layers of cloth in the envelope fold, labelled, dated and sterilised by steam (Sterilising Instruments and Dressings).

Making splints

  • Board splints: strips of light wood 1 cm thick and 8–10 cm wide, in three lengths — 30 cm (forearm, wrist), 50 cm (lower leg, upper arm), 100 cm (whole leg). Round the corners and edges, sand them smooth, and pad them with a layer of wool or folded blanket about 1–2 cm thick, sewn into a cloth cover that can be washed.
  • Finger splints: thin strips of wood or bark 1.5 cm wide and 8 cm long, padded.
  • A bendable splint: a strip of thin, soft sheet metal (tin plate, copper, or later aluminium — Sheet Metal and Rolling, Aluminium) about 10 × 90 cm, its edges folded over and the whole sewn into a thick felt sleeve (Felt). Bent into a U along its length, it becomes stiff, and can be shaped to any limb and rolled up for carrying.
  • Improvised: a rolled blanket, a stick, a folded newspaper or bark, a padded board, or the uninjured leg itself (Wound Care and Antiseptics).

Keep splints in the kit with 4–6 triangular or narrow bandages for tying them.

Making small instruments

  • Tweezers (forceps). Forge or file two strips of spring steel 12 cm long, 8 mm wide, 1.5 mm thick (Springs). Overlap them at one end, rivet or forge-weld them together, then bend them apart so the free ends open 1–2 cm. Grind the tips so they meet exactly — test by picking up a single hair. Temper to a blue colour so they spring back (Steel). A single strip of brass folded in half and hammered hard also works. Splinter tweezers of split bamboo or hardwood, tips carved fine, will do in a pinch.
  • Scissors with blunt-ended blades for cutting bandage near skin (Axes, Chisels, Knives and Planes).
  • Needles and safety pins — fine steel needles for splinters (passed through a flame first), and pins for slings and bandages (Iron and Brass Wire, Sewing, Needles and Thread).
  • A tourniquet: a strap of webbing or leather 4–5 cm wide and 1 m long with a buckle or ring, and a smooth hardwood stick 15–20 cm long to twist it tight. Used only as Wound Care and Antiseptics directs.
  • Thermometer (The Thermometer), a small mirror for looking into eyes and throats, a notebook and pencil (Pencils and Chalk).

Liquids and medicines

Item How to make it Keeps
Sterile water for washing wounds and eyes Fill clean bottles three-quarters full of water, stand them in a pot of water, boil for 20 minutes, and close them while hot with boiled stoppers Months, unopened
Salt water (saline) 9 g of salt per litre — about 1½ level teaspoons — boiled and bottled as above. Gentler than plain water in wounds and eyes Months, unopened
Alcohol, 70% Distil twice and dilute (Distillation, Wound Care and Antiseptics); flame test Years, tightly stoppered
Chlorine solution 0.5% for surfaces and soaking instruments, made fresh; or keep concentrated stock in a dark bottle (Chlorine and Bleach) Concentrate weeks to months; dilute one day
Iodine, 2% in alcohol If you can make iodine from seaweed (Iodine) A year, in dark glass
Honey Sealed pot Years
Oral rehydration salts Pre-measured twists of paper or cloth, each holding 6 level teaspoons sugar + ½ level teaspoon salt for one litre of boiled water (Oral Rehydration) Years, dry
Pain relief Dried willow bark or a measured salicylate (Medicinal Plants, Making Medicines) A year, dry, labelled with dose
Soap A small bar (Soap) Years
Skin ointment Beeswax melted into equal parts animal fat or plant oil A year, cool

What to stock

A household kit, seen from abovebox about 30 × 20 × 12 cm, lid labelled with contents rollers 5, 7.5, 10 cm (2 each) 4 triangles sterile water, saline alcohol honey ORS tourniquet strap and stick sterile pad packs tweezers scissors soapointment pain-relief bark card In the lid orbeside the box 30 cm50 cm padded board splints
Fig. 2 A household first aid kit laid out in a wooden box: bandages and sterile packs in the top tray, liquids and the tourniquet in the middle, instruments and small items at the bottom, padded splints in the lid. A card of first steps for bleeding, burns, choking and CPR sits on top.

A household kit (a wooden box or tin about 30 × 20 × 12 cm):

Item Number
Roller bandages, 5 / 7.5 / 10 cm 2 / 2 / 2
Triangular bandages 4
Sterile packs of 10 × 10 cm pads (5 pads each) 4
Large 20 × 20 cm sterile pads 2
Absorbent cotton pad dressings 2
Board splints, 30 and 50 cm 1 each
Tweezers, scissors, needles, safety pins 1, 1, 2, 6
Sterile water or saline, 0.5 l bottles 2
70% alcohol, small stoppered bottle 1
Honey, small sealed pot 1
ORS packets 6
Soap, ointment, pain-relief bark 1 each
Tourniquet with stick 1
Card listing contents, and the first steps for bleeding, burns, choking and CPR (Emergencies, Emergency Cards) 1

A travelling or work kit (a leather pouch on the belt — for the field, the forest, the quarry, the boat): 2 rollers, 2 triangles, 2 sterile pad packs, tweezers, a tourniquet, a small bottle of alcohol, 2 ORS packets.

A village clinic store — for a community of about 200–500 people, reorder when any item falls to half:

Item Stock
Roller bandages, all widths 60
Triangular bandages 30
Sterile pad packs 100
Large burn pads 20
Absorbent cotton 2 kg
Board splints, all lengths, and 2 bendable splints 20
A long leg splint for a broken thigh 2
Sterile water and saline 20 litres
70% alcohol 5 litres
Chlorine stock to make 50 litres of 0.5%
Honey 5 kg
ORS packets 200 (more in the diarrhoea season)
Crutches, in 3 sizes 3 pairs (Crutches, Prosthetics and Rehabilitation)
Stretcher (two poles and canvas) 2
Instruments for suturing, in sterile packs 4 sets (Basic Surgery)
Blankets 6
Register book of every patient and every item used 1

Keeping it clean and ready

  1. Store dry. Damp ruins sterile packs and grows mould. Keep the box off the floor, in a dry place, closed. A pouch of dry wood ash or quicklime in a cloth bag in a large store absorbs moisture (Lime).
  2. Seal sterile packs in tins when you can. Tins of clean, dry instruments can be sterilised by dry heat (160 °C for 2 hours — Sterilising Instruments and Dressings) with the lid on, then sealed with a strip of waxed cloth round the joint.
  3. Label and date everything. Re-sterilise cloth packs older than one month unless sealed in tins.
  4. Check every three months: replace what was used, re-boil what is doubtful, top up liquids, test that scissors cut and tweezers grip. Use the oldest items first.
  5. One place, known to all. Every adult and older child in the house should know where the kit is and what is in it. Mark the box with a clear sign your community agrees on — a white cross on green is the usual first-aid sign. (The red cross on white is a protected emblem reserved for medical services in war.)
  6. Wash and re-boil reusable bandages and slings after use; burn anything soaked in blood or pus.

How to tell it worked

  • In an emergency, the kit is found in seconds and has what is needed.
  • Sterile packs are dry, sealed and in date; the absorbent cotton sinks in water; tweezers pick up a hair.
  • Wounds dressed from the kit heal without spreading infection (Wound Care and Antiseptics).

Note Troubleshooting. Bandages fray and shed threads → tear along the weave and pull off loose threads; hem them; never use frayed ends next to a wound. Absorbent cotton floats → not boiled long enough with alkali; boil again. Sterile packs mouldy or spotted → stored damp or packed while still wet; dry everything fully before packing and sterilising. Splints too hard on the skin → more padding over bony points; padding must be thicker than you think. Tweezers' tips don't meet → regrind together; temper softer if they spring apart too hard.

Dangers

Danger A dirty "sterile" dressing infects the wound it was meant to protect. If a pack is wet, torn, opened, dropped or of unknown age, treat it as unsterile: boil the contents, or use it only on unbroken skin. Never blow on, cough on or touch the side of a pad that goes on a wound.

  • Tourniquets misused kill limbs; read Wound Care and Antiseptics before you ever use one.
  • Old or mixed-up medicines. Label every bottle with name, strength, dose and date; keep medicines and alcohol out of children's reach. Throw out anything unlabelled.
  • Chlorine solutions burn eyes and skin and must never be mixed with acids or urine (chlorine gas — see Chlorine and Bleach).
  • Over-tight bandages and slings cut off circulation; check fingers and toes stay pink and warm.

What this unlocks

A stocked kit makes every other first-aid skill — Emergencies, Wound Care and Antiseptics, Safe Childbirth — possible on the spot. The clinic store, with its register, becomes the first step toward a hospital, and its records show what supplies the community must produce: cloth, alcohol, chlorine, splints and crutches (Nursing the Sick, Organising a Community).

How it was first done

Linen bandages are as old as written medicine: the Egyptian Edwin Smith Papyrus (about 1600 BC) describes binding wounds and splinting fractures with linen and wood. Armies carried scraped-linen lint for centuries. The Scottish surgeon Joseph Sampson Gamgee introduced absorbent cotton wool wrapped in gauze ("Gamgee tissue") in 1880. Friedrich von Esmarch, a German army surgeon, promoted the triangular bandage and first-aid training for soldiers and civilians in the 1870s and printed instructions for its uses on the bandage itself. After Joseph Lister showed in the 1860s that germs cause wound infection, the American company Johnson & Johnson began selling sterile, ready-wrapped dressings in 1887 and the first commercial first-aid kits — originally for railway workers — in 1888.

Source: content/entries/health/first-aid-kit.md