◆ Rebuild

Part 3 · Metals

Bellows

A bag of leather that pumps air into a fire. Forced air is what turns a campfire into a furnace hot enough to melt copper and smelt iron — no metal in this book can be made without it.

Difficulty
●●●●●
Time
An afternoon for bag bellows; two to four days for hinged bellows
Steps from zero
5 prerequisites →

You need first

Hides and LeatherBasic Woodworking

This unlocks

Copper SmeltingIron (the Bloomery)LeadTin and Pewter
The full path from nothing — 5 steps before this one
  1. Cordage and Rope
  2. Stone Tools
  3. Hunting and Trapping
  4. Basic Woodworking
  5. Hides and Leather
  6. Bellows

Do them roughly in this order. See it on the tech tree →

Why it matters

A good open fire of Charcoal reaches about 800–900 °C — a bright cherry to orange glow. That is enough to fire Pottery and to soften metal, but not enough to melt Copper Smelting (1,085 °C) or to smelt Iron (the Bloomery) (the furnace must reach about 1,200–1,300 °C). The difference is not the fuel. It is air.

Blow air into a bed of glowing charcoal and it burns many times faster, in a small space, so the heat piles up faster than it can escape. With a steady blast, charcoal reaches 1,300 °C and more — a yellow-white glare you cannot look into comfortably. Every smelting furnace, every forge, every crucible in this book depends on a device that pushes air steadily into the fire: the bellows.

Bellows are also the first real machine in the metals part — a bag that breathes. Later the same ideas give you pumps and Bellows to Air Compressors, and when the bellows are driven by a The Waterwheel, the blast furnace.

How it works

Every bellows is a chamber that gets bigger to suck air in, and smaller to push it out through a nozzle. The tricky part is stopping it from sucking hot gas back out of the fire when it refills. There are two solutions:

  • A valve — a flap of leather over a hole. When the chamber expands, the flap swings open and lets fresh air in. When the chamber is squeezed, air pressure slams the flap shut and air can only escape through the nozzle.
  • A gap — the simplest bellows have no valve at all. Their nozzle points into the end of a clay pipe (the tuyere, pronounced twee-AIR) but is not sealed to it; it stops 2–5 cm short. On the push stroke, the jet of air shoots into the tuyere and drags extra air along with it. On the refill stroke, the bellows sucks in cool air through the gap instead of hot gas from the furnace.

One bellows gives puffs. Two bellows worked in turn — one filling while the other empties — give a nearly steady blast. Steady air matters: if the blast stops for even a minute in a smelting furnace, the temperature falls and the metal and slag freeze.

How much air?

Job Air needed (roughly) What does it
Melting a few grams of copper in a tiny crucible 30–80 litres a minute 2–4 people with blowpipes
Small forge, crucible melting 100–300 L/min One pair of bag or pot bellows
Copper bowl furnace 200–400 L/min One or two pairs of bag or pot bellows
Iron bloomery, 25–30 cm wide 500–1,000 L/min Two pairs of pot bellows, or a large hinged bellows, with a team taking turns

A person sitting still breathes about 6–8 litres a minute; even hard blowing through a pipe gives only about 20–40. A pair of goatskin bellows moves 10–20 litres each stroke, at 40–60 strokes a minute.

What you need

Item For Notes
Leather The flexible walls Supple, airtight, without holes. Goat, sheep, deer or calf. See Hides and Leather. Rawhide works but goes stiff when dry; keep it greased.
Animal fat Keeping the leather supple and airtight Rub it into the leather every day the bellows are used.
Hardwood boards and sticks Frames, handles, nozzles See Basic Woodworking.
Cord or thin leather thongs Tying, sewing, hinges Cordage and Rope or strips cut from hide.
Clay with sand and chopped grass Tuyeres and nozzle tips See Finding and Preparing Clay.
Beeswax or pitch Sealing seams See Tar, Pitch and Glue.

Method 1: The blowpipe (stopgap)

Before bellows, people blew through pipes. It works for melting small amounts of metal in a crucible and for testing ores.

  1. Cut a straight hollow reed or cane about 1 m long with a bore of about 1 cm. Alternatively bore out a straight elder stem.
  2. Mould a clay tip around one end: a cone of clay 6–8 cm long with a 4–5 mm hole. Let it dry and fire it in your hearth. Without the tip, the reed burns.
  3. Sit 1 m from the fire so your face is out of the heat. Breathe in through your nose, blow steadily out through puffed cheeks, and keep the tip 3–5 cm from the coals.
  4. Use three or four blowers around one crucible, each taking a short rest in turn.

Warning Never breathe in through a blowpipe — you would draw in hot fumes. Over-breathing makes you dizzy: stop and sit if your hands or lips tingle.

Method 2: Bag bellows from a hide

This is the fastest real bellows to make, used across Africa and India for thousands of years.

nozzle mouth: two sticks loose leather stick air out flap valve: opens to let air in air in nozzle BAG BELLOWSa whole goatskin, used in pairs POT BELLOWSleather over a bowl HINGED BELLOWStwo boards, leather sides
Fig. 1 Three valveless and simple bellows. Bag bellows are a whole skin; pot bellows a skin over a bowl; hinged bellows two boards with leather sides and a flap valve.
  1. Take the skin off in one piece. When you skin a goat or sheep, cut around the neck and around each leg just above the hoof, then cut down the inside of the back legs to the tail and peel the skin forwards off the body like a sock (this is called case skinning). Do not slit the belly. Tan it or at least scrape and grease it (see Hides and Leather).
  2. Close the legs. Tie each leg hole tightly shut with cord, or fold the leg skin over and bind it.
  3. Fit the nozzle. Push a wooden tube, a hollow horn, or a fired clay pipe (about 25 cm long, bore 2 cm) into the neck opening and bind the skin round it very tightly with several turns of cord, then smear the joint with fat or pitch.
  4. Make the mouth. The wide opening at the back is the air inlet. Sew a flat stick about 40 cm long along each lip of the opening, so the two sticks lie side by side like the lips of a mouth. Fix a leather loop on each stick for your thumb and fingers.
  5. Pump. Kneel beside the bag. Lift and open: raise the sticks while spreading them apart, so the bag fills with air. Close and press: squeeze the sticks together tightly and push the bag down towards the ground. The air has nowhere to go but out of the nozzle.
  6. Work a pair. Use one bag in each hand, alternating: one opens while the other presses. A steady rhythm of 40–60 strokes a minute is sustainable for 15–30 minutes. Then swap with a rested operator.

Method 3: Pot bellows

Pot bellows (also called bowl or drum bellows) last longer than bag bellows and can be worked standing, even with the feet. Egyptian tomb paintings from about 1450 BC show smiths standing on a pair of them.

  1. Make the bowl. Form a thick clay bowl 30–40 cm across and 15–20 cm deep, with a clay outlet pipe (2–3 cm bore) coming out from the side at the very bottom. Fire it (see Pottery). A bowl carved from a hardwood log is better still — it does not crack.
  2. Cover it. Tie a loose, baggy piece of soft leather over the top, bound round the rim with cord in a groove. Leave enough slack that the centre can rise 15–20 cm.
  3. Make the inlet. Either tie a stick upright to the centre of the leather (for hand pumping, with the bellows nozzle left un-sealed from the tuyere as described above), or for foot pumping, cut a hole 3–4 cm across in the middle of the leather and tie a cord to its edge.
  4. Pump by hand: pull the stick up quickly, push it down firmly. Pump by foot: stand with one foot on each bellows. Lift one leather with its cord while your heel is off the hole (air rushes in), then put your heel over the hole and shift your weight onto it (air is forced out). Then the other foot.
  5. Peg the pots firmly into the ground so they do not walk away as you work.

Method 4: Hinged (accordion) bellows

This is the familiar forge bellows. It has a proper valve, so it can be sealed to the tuyere, and its big volume suits a forge or a small furnace.

  1. Cut two boards of hardwood, each about 60 cm long, 35 cm wide at the broad end and tapering to 12 cm at the narrow end (a pear or teardrop shape), and 2 cm thick. Split and smooth them as described in Basic Woodworking, or peg narrower planks together.
  2. Make the valve. Cut a hole about 6 cm square in the middle of the bottom board. On the inside, peg a flap of stiff leather 9 cm square over it, fixed along one edge only, so it swings freely upward (inward) and closes flat against the hole.
  3. Make the nozzle block. Carve a hardwood block 12 cm wide and 8 cm thick that fits between the narrow ends of the boards. Bore a 2.5 cm hole through it lengthways (burn it through with a red-hot rod if you have one, or carve two half-channels and bind the halves). Fix a nozzle — a fired clay tube, or later an iron one — into the outer end.
  4. Hinge. Peg both boards firmly to the top and bottom of the nozzle block. The top board must be able to swing up and down; a leather strap across the joint makes a good hinge.
  5. Fit the sides. Cut a strip of leather long enough to go round the edge from one side of the nozzle block, round the broad end, to the other side — about 1.7 m — and 30 cm wide in the middle. Nail it with wooden pegs every 3 cm to the edges of both boards, folding it inward like a paper fan. Inside, fix one or two hoops of bent green willow halfway between the boards so the leather folds neatly instead of collapsing.
  6. Seal all seams with melted beeswax and fat, or pitch.
  7. Mount and work. Fix the bottom board to a frame at knee height. Put a handle or a lever on the top board. Lift to fill, let it fall (or push) to blow. Hang a stone of 5–10 kg on top so its weight does the blowing and you only lift.

Method 5: Double-action bellows

A single hinged bellows stops blowing every time you lift it. The double-action (or great) bellows adds a second chamber on top that acts as a reservoir, so the blast is continuous. Blacksmiths used this design for centuries.

to the tuyere Weightstones, 10–20 kg Upper chamberstores air, blows steadily Middle boardfixed; valve opens upward Lower chamberthe pump Inlet valveopens as the board falls Handlepull down to pump
Fig. 2 The double-action bellows in cross-section. The lower chamber pumps; the upper chamber, weighted, stores the air and pushes it out steadily.
  1. Make three boards of the same pear shape. The middle board is fixed rigidly to the frame and to the nozzle block. It has a valve hole with a flap that opens upward.
  2. The bottom board hangs below on its own hinge and leather sides, with a valve that also opens upward. A lever or chain from the bottom board runs to a long handle (a pole pivoted on a post, 1.5–2 m long).
  3. The top board sits above the middle board with its own leather sides. It has no valve. The nozzle connects only to the upper chamber.
  4. Pull the handle down: the bottom board rises and pushes air through the middle valve into the upper chamber. Let the handle up: the bottom board drops under its own weight and refills through its valve.
  5. Load the top board with stones (10–20 kg for a forge). The weight pushes air out of the nozzle steadily even while the lower chamber refills. Pump just fast enough to keep the top board floating near the middle of its travel.

Chinese smiths went further with a box bellows: a long wooden box with a tight-fitting piston, packed round its edge with feathers or leather, and flap valves at both ends, so it blows on both the push and the pull. If you can build a straight, smooth box, it gives the steadiest air of all.

The tuyere

The tuyere is the clay pipe that carries the blast through the furnace wall to the heart of the fire. The bellows nozzle itself — wood or leather — would burn.

Bellows nozzlesnot sealed in: leave a 2–5 cm gap fresh air drawn in Tuyerefired clay, 25–40 cm longbore 2.5–3 cm, walls 1.5–2 cm Tipglazes and melts back— keep spares Furnace wall Charcoalyellow-white at the tip
Fig. 3 A tuyere of fired clay. Valveless bellows leave a gap at the back so they draw in fresh air, not hot gas.
  1. Mix Finding and Preparing Clay with about one-third its volume of coarse sand and a double handful of finely chopped dry grass or dung per bucket. This temper stops cracking and makes the pipe resist heat.
  2. Roll a slab 1.5–2 cm thick around a smooth greased stick 2.5–3 cm thick. Make it 25–40 cm long, flaring the outer end to 6–8 cm across to receive the nozzles.
  3. Slide the stick out when the clay is leather-hard. Dry slowly in shade for several days, then fire it in a The Kiln, or set it in your furnace during the preheating fire.
  4. Make three or four spares. The inner tip sits in the hottest part of the furnace, glazes, melts back and slowly clogs with slag. You will replace it often.

How to tell it worked

  • Hold your hand 15 cm in front of the empty nozzle: you should feel a strong, steady push of air, not weak puffs.
  • Listen. A fire under good blast roars steadily. Puffing and fading sounds mean the operators are out of rhythm.
  • Look into the tuyere (through the gap, briefly, squinting): the charcoal in front of it should glow yellow to white. Only dull red means too little air.
  • Sparks shooting high out of the top of a furnace mean the blast is stronger than the fire needs; slow down a little.

Note Troubleshooting. Bellows wheeze and the blast is weak → leaks. Rub fat into the leather, re-tie the nozzle, and smear seams with wax or pitch. Find leaks by pumping and feeling for jets of air with a wet hand. Hot gas or smoke comes back into the bellows → a valveless bellows sealed to the tuyere. Pull the nozzle back to leave a gap. Valve flap sticks open → it is too soft or curled; replace with stiffer leather and add a small wooden weight. Leather cracks → it dried out. Grease it every day of use and store the bellows in shade.

Dangers

Danger Carbon monoxide. Every forge and furnace makes this invisible, odourless gas, and bellows make the fire burn harder. Work only in the open or under a roof with open sides. Headache, nausea or confusion means get into fresh air now. Change operators often, and keep them on the upwind side.

  • Burns. Bellows operators sit close to the fire. Put a screen of wet clay or stone between the furnace and the bellows, and keep the leather from touching hot clay.
  • Fire in the bellows. A bellows that sucks back sparks can catch fire inside. Keep a gap or a working valve, and check the valve flap at every break.
  • Exhaustion and heat stroke. Long smelts are hard work. Rotate every 15–30 minutes, drink plenty of water, and rest in shade (Emergency Cards).

What this unlocks

With steady forced air you can melt and smelt Copper Smelting, make Bronze, build a bloomery for Iron (the Bloomery), and run a Blacksmithing forge. Joined to a The Waterwheel, bellows can run day and night without tiring — the step that made the blast furnace possible.

How it was first done

The earliest metalworkers, in the Near East and Egypt from before 3000 BC, melted copper using blowpipes with clay tips; Egyptian tomb reliefs show teams of men blowing through pipes round a crucible. Pot bellows worked by the feet appear in the tomb painting of the official Rekhmire at Thebes, about 1450 BC. Bag bellows of goat skin have been used in Africa and India for at least two thousand years and are still used by village smiths today. In China, the official Du Shi drove furnace bellows with a waterwheel in AD 31. The hinged, valved bellows familiar from European smithies was in use by Roman times, and the double-action great bellows came into use in Europe around the 1500s.

Source: content/entries/metals/bellows.md