◆ Rebuild

Part 11 · Power and Energy

Coal and Coke

Coal is ancient forest turned to stone — twice the heat of wood for its weight, lying in seams under the ground. This chapter covers finding and judging it, digging it safely, baking it into coke for iron, and capturing the gas and tar that come off.

Difficulty
●●●●●
Time
Days to find and open a seam; 2–3 days per coke burn; weeks to build a beehive oven or gas retort
Steps from zero
4 prerequisites →

You need first

Mining and Tunnelling

This unlocks

Coal Tar ChemicalsLanterns, Gas Lamps and Lighters
The full path from nothing — 4 steps before this one
  1. Stone Tools
  2. Simple Machines
  3. Quarrying and Cutting Stone
  4. Mining and Tunnelling
  5. Coal and Coke

Do them roughly in this order. See it on the tech tree →

Why it matters

A coppice grows only a few tonnes of wood per hectare per year. When a country needs millions of tonnes of fuel — to smelt iron, fire Bricks and Lime, boil Salt and drive The Steam Engines — the woods run out. Coal is the way past that wall. A tonne of good coal gives the heat of about two tonnes of seasoned wood, and a seam a metre thick under a hectare of land holds roughly 13,000 tonnes — the wood that hectare could grow in four or five thousand years.

Coal on its own is a dirty fuel for metal: its sulfur and smoke spoil iron. Baked into coke, it becomes a strong, clean, hot fuel that can carry the weight of a tall blast furnace — the step that made The Blast Furnace and Cast Iron cheap and started the Industrial Revolution. The same baking gives off coal gas, which lit cities (Lanterns, Gas Lamps and Lighters) and ran the first engines (Gas Engines and Producer Gas), and coal tar, the starting point for antiseptics, wood preservatives, dyes and later plastics.

How it works

Coal formed from plants that grew in vast swamps, fell into waterlogged mud where they could not rot, and were buried under kilometres of later rock. Heat and pressure over millions of years drove out water and gases and left more and more carbon. The steps of that change are the grades (ranks) of coal:

Grade Looks like Carbon Heat per kg Notes
Peat Brown, fibrous, spongy; you can see plant bits ~55% 14–16 MJ dry Not yet coal. Dug from bogs, dried as turves. See below.
Lignite (brown coal) Brown to black, dull, crumbly, often woody 60–70% 10–20 MJ Much water; crumbles as it dries; smoky
Bituminous (ordinary black coal) Black, in bands of shiny and dull layers, breaks into blocks 75–90% 25–33 MJ The common coal. Some kinds make coke.
Anthracite (hard coal) Jet black, very shiny, hard, breaks with curved glassy faces 90–95% 30–33 MJ Hard to light, burns slowly with almost no smoke

What happens when coal is heated without air. Bituminous coal heated to about 350–500 °C softens, bubbles and gives off tarry vapours and burnable gas, like toffee boiling. Keep heating to 900–1,100 °C and the bubbly mass sets hard. What is left is coke: grey, porous, almost pure carbon and ash, strong enough to bear a heavy load, burning with a short blue flame and no smoke. It is to coal what Charcoal is to wood — but much stronger, which is why it can be piled 20 m deep in a blast furnace where charcoal would crush.

Only coking coals (a middle range of bituminous coal) melt and fuse like this. Others give a weak powder ("char") or no coke at all. Test before you build anything.

What you need

Item Purpose
Picks, iron wedges, hammers, shovels, baskets Digging coal. See Mining and Tunnelling
Timber props and planks Holding up the roof
A clay or iron crucible or old pot with a lid Testing coal for coke
For heap coking: turf, clay, coke dust or earth, poles Covering a coke heap
For a beehive oven: about 8,000–10,000 bricks (half of them firebrick), fireclay mortar (Firebrick and Refractories) One oven
Water and a long-handled hoe or rake Quenching and drawing coke
For coal gas: an iron or fireclay retort, iron pipe, a water tank and a floating bell See below

Where to find it

Coal lies in seams — flat or gently tilted layers, from a few centimetres to several metres thick — sandwiched between beds of sandstone, shale and fireclay. These "coal measures" are found on every continent.

Where a coal seam comes to the surface Bell pitshaft to a shallow seam, coal dugout in a bell, then abandoned Shale rooffossil leaves and bark Fireclay"seat earth" withfossil roots Coal seam0.3–3 m thick Driftfollows the seam in, rising 1 in 100,so water drains out by itself; propshold up the roof Outcropblack streaks in the bank "Float"coal pebbles in thestream point upstreamto the seam Sandstone
Fig. 1 A coal seam where it comes out on a hillside. Coal crops out where a stream has cut down through the layers; a drift follows the seam into the hill and drains itself; a bell pit reaches a shallow seam from above.

Clues:

  • Black float. Black, light, shiny or dull pebbles in a stream bed. Walk upstream until they stop: the seam is near where they first appear.
  • Black streaks in the soil, in fresh landslips, river banks, sea cliffs and gullies, or dark staining on the downhill side of an outcrop.
  • Fossil plants. Grey or black shale with clear fossils of fern leaves, bark with diamond or scale patterns, and long ribbed stems is the typical roof of a coal seam.
  • Fireclay ("seat earth"). A pale grey, soft clay full of black root fossils lies just under many seams — the soil in which the coal forest grew. Fireclay is itself valuable: see Firebrick and Refractories.
  • Burnt ground. Red or purple baked rock and clinker on a hillside can mean a seam once caught fire.
  • Iron and sulfur. Orange water seeping from a hillside and yellow crusts may point to coal with pyrite in it.

Peat is easier still: in wet, cold uplands and lowland bogs, the ground itself is a fuel. Cut it in spring with a narrow spade into bricks the size of a large loaf (turves), spread and stack them to dry through the summer (they shrink by more than half), and burn them in winter. Peat burns slowly with a smoky, sweet-smelling flame. It makes a weak, crumbly char, not coke.

Tests for coal:

  1. Weight. Coal feels light for a rock — about 1.3 kg per litre, half the weight of sandstone.
  2. Streak. Rubbed hard on unglazed pottery, black coal leaves a black or dark brown streak; lignite leaves brown. Black shale leaves a grey streak and is heavy.
  3. Burn it. Put a lump in a hot fire. Coal catches, flames with a smoky yellow flame and a tarry smell, and leaves glowing embers. Black shale only glows and turns grey or red without really burning.
  4. Pyrite. Look for brassy gold specks or films. Lots of pyrite means a sulfurous coal — poor for iron.

Getting it out

Mining is covered in Mining and Tunnelling; coal adds a few rules of its own.

  1. Start at the outcrop. Dig the seam out along the hillside in a trench, as far as the overburden lets you.
  2. Follow it in with a drift. Drive a tunnel (drift or adit) into the hillside along the seam, sloping slightly upwards into the hill (about 1 in 100) so water runs out by itself. Most early coal was won like this.
  3. Bell pits for flat, shallow seams under fields: sink a round shaft 1–1.5 m wide down to the seam (up to about 10–12 m), then dig the coal out around the bottom in a widening bell until the roof starts to crack — then stop and sink another pit a few metres away. Wasteful but simple.
  4. Room and pillar. Underground, cut the seam in "rooms" (stalls) about 4–5 m wide, leaving solid pillars of coal 5–10 m square between them to hold up the roof. Leave at least a third to a half of the coal in place. Robbing pillars to get "a bit more" brings the roof down.
  5. Ventilation. Coal mines need two openings — a shaft or drift for fresh air in and another for stale air out — from early on. Never use a fire at the shaft bottom to drive air in a coal mine (it can ignite gas; see Mining and Tunnelling).
  6. Store coal under cover, in heaps no higher than about 2 m, and watch them (see Dangers).

Making coke

First, test your coal

Fill a small clay pot or crucible two-thirds with crushed coal (pea-sized), put a lid on loosely, and set it in the hottest part of a charcoal fire for an hour, until no more flames come from under the lid. Let it cool covered.

  • A single hard, silvery-grey lump that has swelled to fill the pot, is full of small bubbles, rings when tapped and does not crumble in your fingers: good coking coal.
  • A loose black powder or the original grains barely stuck together: a non-coking coal. Use it for boilers, kilns and smithing, not for coke.
  • A puffy, very light, fragile foam: swelling coal. Blend it with some non-coking coal or coke dust (about one part to three) and test again.

Method 1: The coke heap

This is how coke was first made, exactly like a Charcoal mound.

  1. Clear and level a circle 3–4 m across. Stand a central chimney of loose bricks or three stakes, 1.2 m high.
  2. Pile lumps of coking coal (fist-sized and larger; save small coal for later) around it in a dome 1–1.5 m high, with the biggest lumps at the bottom. A heap this size holds about 5–10 tonnes.
  3. Leave several air channels through the base from the edge to the chimney, made with poles that you pull out afterwards.
  4. Cover the outside with coke dust, damp earth or turf 10–15 cm thick, leaving the bottom 30 cm uncovered at first.
  5. Drop burning coals down the chimney. The fire spreads outward and upward. As each part of the heap stops giving off yellow smoke and flames and glows with a clear blue flame, cover it more thickly. Close the air holes progressively.
  6. After 4–6 days, when no more flames show anywhere, seal the whole heap with damp earth and let it cool for a day or two, or open it and quench it with water.

Yield: about half the weight of coal as coke. Much of the coal near the surface burns away.

Method 2: The beehive oven

A domed brick oven gives better, more even coke and needs less labour per tonne. It was the standard method for more than a hundred years.

Earth bankholds heat; coal is tippedin from above Charging hole40 cm; waste gases flame out here Gases burn in the domeand their heat bakes the coalfrom the top downward Firebrick lining Ordinary brick outside Airthrough a slit over the door;close it as the flames shorten Doorloose bricks and clay; opened toquench and rake out the coke 3.5–4 m inside; dome 2–2.5 m high Cokegrey, glowing on top Coal still cookingcharge 60–90 cm deep, 5–7 t
Fig. 2 A beehive coke oven in cross-section. Coal is charged through the top; the gases burn in the dome and their heat cooks the coal from above. After two or three days the coke is quenched with water and drawn out through the door.
Part Size
Floor Round, 3.5–4 m across inside, firebrick on a solid clay and stone base
Dome 2–2.5 m high inside, firebrick inner skin, ordinary brick outside, packed round with earth
Charging hole (trunnel head) 40 cm across, at the top of the dome
Door 60–70 cm wide and high, at floor level, closed with a stack of loose bricks plastered with clay
Charge 5–7 tonnes of coal spread 60–90 cm deep
  1. Build the oven from firebrick set in fireclay mortar, and dry it slowly over a week with wood fires (see The Kiln). Ovens are usually built in a row against a bank, so the earth insulates them and coal can be tipped in from above.
  2. Heat it with a wood fire for a day until the inside glows red. Once in use, each charge starts from the heat left by the last.
  3. Charge coal through the top hole and level it through the door with a rake. Brick up the door to a few centimetres from the top, leaving a slit for air, and plaster the joints with clay.
  4. Coking. The hot dome lights the gases rising from the coal. They burn in the space above the charge with long yellow flames, and their heat bakes the coal downward from the top. Gradually close the slit as the flames shorten so that only enough air enters to burn the gas, not the coke.
  5. After 48 hours (for coke for furnaces) or 72 hours (harder coke for foundries), the flames die to almost nothing and the top of the charge is bright yellow-red. Quench: break open the door and spray water through it until steam stops pouring out.
  6. Draw the coke with a long iron rake into barrows. Recharge at once while the oven is still hot.

Yield: about 55–65% of the coal's weight. The beehive wastes all its gas and tar; to save them you need closed ovens or a gas retort (below).

Using coke

Coke needs a strong blast — it will not burn in an open grate the way coal does. It is the fuel for the The Blast Furnace and Cast Iron blast furnace and cupola, crucible Steel, Metal Casting, and for blacksmiths who want a clean, sulfur-free fire. An 18th-century coke furnace burned several tonnes of coke per tonne of iron, a 1900 furnace about one tonne — against 8–15 tonnes of wood for charcoal iron.

Coal gas and coal tar

Heat coal in a closed retort (a sealed iron or fireclay tube with fire around it) instead of letting the gas burn, and you can collect everything that comes off.

Coal gas: bake, cool, wash, purify, store 1. Retortcoal sealed in, heatedto ~1,000 °C, 4–6 hours;leaves coke behind 2. Condenserlong cooling pipes Tar welltar sinks, ammonialiquor floats on top 3. Washergas bubblesthrough water 4. Purifiertrays of slaked limeremove sulfur gas 5. Gasholderbell floats in water,rises as it fills; itsweight sets the pressure to lamps, stovesand engines
Fig. 3 A simple gasworks. Coal is baked in a closed retort; tar and water drop out in the cooling pipes; lime takes out the foul-smelling sulfur gas; and the clean gas lifts a floating bell over a tank of water, which stores it under steady pressure.
  1. Retort. A horizontal tube 30–40 cm across and 2–3 m long, sealed by a clamped lid, set in a brick furnace and heated to bright orange (about 1,000 °C). Charge with coal, seal, and bake for 4–6 hours. A small trial can use an old iron pot with a clay-sealed lid and a pipe.
  2. Cooling. The gas leaves through a pipe and runs through a long iron or clay pipe (the condenser), air- or water-cooled. Thick black tar and a stinking watery ammonia liquor condense and drain into a sealed pit.
  3. Washing. Bubble the gas through water to take out more ammonia.
  4. Purifying. Pass the gas through boxes of slaked lime (Lime) or rusty iron ore spread on trays. These take out hydrogen sulfide, the rotten-egg gas that makes smelly, sulfurous flames.
  5. Storing. The gas goes into a gasholder: a large inverted bell of sheet iron (or, for a small plant, tarred wood) floating in a tank of water. The weight of the bell keeps the gas at a small steady pressure; the bell rises as it fills.

What you get from a tonne of coal: roughly 300 m³ of gas, 650–700 kg of coke, 40–50 kg of tar and 100–150 litres of ammonia liquor. Coal gas is about half hydrogen and a third methane, with some carbon monoxide. It gives a bright light with a suitable burner, cooks, heats, and runs gas engines (Gas Engines and Producer Gas).

Coal tar is distilled (see Distillation, with an iron still, and Coal Tar Chemicals for the details) into fractions by temperature: light oils below about 170 °C (benzene and similar solvents — Ether, Acetone and Solvents); carbolic oil at 170–230 °C (phenol, the first surgical antiseptic); creosote at 230–270 °C (the classic wood preservative for posts, sleepers and piers); heavier oils; and pitch, left behind, for roofing, waterproofing and roads (Tar, Pitch and Glue). The ammonia liquor, boiled with lime and caught in Sulfuric Acid, gives ammonium sulfate fertiliser (Chemical Fertilisers).

How to tell it worked

  • Good coal lights from a wood fire, burns for hours with a steady red glow, and leaves less than about a tenth of its weight as ash.
  • Good coke is silvery to dark grey (never black), full of small pores, hard and rings like pottery when two pieces are knocked together. It does not soil your fingers. Under the blast it glows white and burns with a short pale blue flame and no smoke. A 5 cm lump dropped from head height onto stone should not shatter into powder.
  • Clean coal gas burns with a steady flame, does not smell strongly of rotten eggs when burning, and does not blacken a cold white plate held in the flame for a second.

Note Troubleshooting. Coke black, soft, crumbly at the bottom → not coked long enough or the oven was too cold; give it 12–24 hours more. Coke burned to ash at the top of the heap → too much air; cover and close the vents sooner. Coke weak and fingery → poor coking coal, or the coal was charged too fine or too wet; blend with a better coal, use larger lumps. Iron made with the coke is brittle when hot → too much sulfur; wash out pyrite (it is heavy and sinks when crushed coal is stirred in water) or find a different seam. Gas burns with yellow smoky flames and stinks → lime boxes exhausted; renew them. Too much tar → cool the gas longer.

Dangers

Danger Firedamp explodes. Coal releases methane (firedamp) into mine workings, especially in deep, fresh-cut seams. At 5–15% in air it explodes with a flame that races through the workings, followed by afterdamp — carbon monoxide that kills the survivors. Fine coal dust stirred up by the blast can explode too, turning one small explosion into a disaster that spreads through the whole mine.

  • Keep air moving through every working, all the time, with two separate openings.
  • Test the air with a small flame held low, then slowly raised (see Mining and Tunnelling): a pale blue cap on the flame means gas. Leave at once. Better, use a safety lamp — a flame wholly enclosed in a cylinder of fine iron-wire gauze (Davy's had about 11 wires to the centimetre, some 120 holes to the square centimetre), which lets air in but cools any flame trying to escape. Its flame still shows the blue cap.
  • Never strike sparks, carry open flames or smoke in a gassy mine. Wet down dust, or spread crushed limestone on floors so the dust cannot burn.

Danger Carbon monoxide comes from every coal fire, coke oven and gas plant, and coal gas itself is poisonous. It has no smell and no warning. Never burn coal or coke in a room without a chimney, never sleep near a coke heap or oven, and test gas pipes for leaks only with soapy water, never a flame. Warning signs are headache, dizziness and confusion — get into fresh air at once.

  • Roof falls kill more coal miners than explosions. Prop the roof, leave pillars, and listen to the timber (Mining and Tunnelling).
  • Blackdamp (air with too little oxygen) gathers in old workings and low places. Small birds such as canaries, carried down in cages, collapse long before people do.
  • Spontaneous fire. Big heaps of coal, especially small, fresh and pyrite-rich coal, can heat up by themselves and burst into flame weeks later. Keep heaps low, compact and dry; push a long iron rod into them and feel it: if it comes out hot, spread the heap out.
  • Lung disease. Breathing coal dust for years causes "black lung", a crippling and incurable scarring. Wet the coal when cutting and loading; ventilate; rotate workers.
  • Smoke. Burning raw coal in towns fills the air with soot and sulfur fumes; London's smog of December 1952 killed thousands of people in a week. Burn coke or smokeless coal in towns, and build tall chimneys.
  • Tar and creosote irritate and burn the skin and cause cancer with long contact. Wear gloves and wash well. Benzene from the light oil is also poisonous and causes cancer.

What this unlocks

Coke smelts iron in quantity in the blast furnace (The Blast Furnace and Cast Iron), which gives Steel in Quantity, rails (Railways) and machines. Coal fires the boilers of the The Steam Engine, Steamships and the The Steam Turbine power station. Gas from coal lights streets (Lanterns, Gas Lamps and Lighters) and runs the first internal-combustion engines (Gas Engines and Producer Gas); a gas producer turning coal into fuel gas is described in Biogas and Wood Gas and Gas Engines and Producer Gas. Coal tar gives Ether, Acetone and Solvents, antiseptics, synthetic dyes (Dyes and Mordants) and the first plastics (Early Plastics), and coke with lime makes Calcium Carbide and Acetylene.

How it was first done

Coal was burned in China more than two thousand years ago, and by the 11th century the iron industry of northern China ran largely on coal and probably coke; Marco Polo was astonished at the "black stones" that burned like logs. The Romans in Britain burned coal in forts along Hadrian's Wall. In medieval England "sea coal", washed up on the Northumberland shore and then dug from outcrops, was shipped to London, where by 1306 its smoke was so bad that the king tried to ban it.

By 1700 English wood was scarce and coal was everywhere — but its sulfur ruined iron. In 1709 Abraham Darby at Coalbrookdale in Shropshire smelted iron with coke made in open heaps from a low-sulfur local coal, and within a century coke iron had replaced charcoal iron in Britain. Beehive ovens spread from the 1700s and were still in use in the 20th century. William Murdoch lit his house in Redruth, Cornwall, with coal gas in 1792; London's streets were gaslit from the 1810s. In 1815 Humphry Davy invented the gauze safety lamp, and in 1856 William Perkin, an 18-year-old chemist in London, made the first synthetic dye, mauve, from a coal-tar chemical — the start of the modern chemical industry.

Source: content/entries/energy/coal.md