Part 15 · Knowledge and Science
Colour Photography
Every colour the eye sees can be built from three, so three black-and-white pictures taken through red, green and blue filters hold a whole colour scene. How to make the filters and the three-colour camera, rebuild the colours by projection or as a three-layer pigment print, make the autochrome screen plate of dyed potato starch, understand modern dye-coupler film in outline, and keep colour pictures from fading.
- Difficulty
- ●●●●●
- Time
- A week to make filters and take a first set of separations; a month to master the three-colour pigment print; autochrome plates and colour film are the work of a factory
- Steps from zero
- 22 prerequisites →
This unlocks
—The full path from nothing — 22 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- The Kiln
- Pottery
- Charcoal
- Hides and Leather
- Lime
- Lye and Potash
- Dyes and Mordants
- Glass
- Bellows
- Copper Smelting
- Lead
- Laboratory Glassware
- Lenses
- Gold and Silver
- Photography
- Colour Photography
Do them roughly in this order. See it on the tech tree →
Why it matters
A black-and-white photograph records shape and brightness but throws away colour. For many jobs colour is the whole point: the rash of a disease, the stain on a microscope slide (Biological Stains), the ripeness of a crop, the hue of a mineral, the colours of a flag, a painting or a map.
It rests on one discovery: the eye has only three kinds of colour sensor, so every colour it sees can be matched by mixing three lights. Once you have Photography, a darkroom and dyes (Dyes and Mordants), colour is "only" three black-and-white pictures and a way to put them back together.
How it works
The eye. The retina has three kinds of cone cell, most sensitive to long (red), middle (green) and short (blue-violet) light. Yellow light excites the red and green cones together; so does a mixture of red and green light, and the eye cannot tell the two apart. That is why three are enough.
Separation. Photograph a scene three times on black-and-white plates, once through a red filter, once through green, once through blue. Each separation negative records how much of that third of the spectrum came from each point. A red apple is dense (dark) on the red negative and nearly clear on the other two.
Putting it back: two ways.
- Additive. Print each negative as a positive transparency and project it with light of the same colour as its filter. Red + green + blue light on one screen rebuild the scene. Red and green light make yellow; all three make white.
- Subtractive. For a print on paper you cannot add light; you can only take it away. So each layer uses the complementary colour, the one that absorbs that third: cyan (blue-green) absorbs red, magenta (purple-pink) absorbs green, yellow absorbs blue. The red negative controls the cyan layer, the green negative the magenta, the blue negative the yellow. All three layers together make black.
The sensitive plate is the problem. Plain silver bromide sees only violet and blue light (Photography). Red and green look black to it. Some dyes, soaked into the emulsion, pass the energy of the light they absorb to the silver: orthochromatic plates (with erythrosine or eosin) see green too; panchromatic plates (with cyanine dyes) see red as well. Without a panchromatic plate you cannot make a red separation, and nothing else in this chapter works.
What you need
| Item | Notes | See |
|---|---|---|
| Camera with a steady stand and a lens corrected for colour | An achromatic lens; a single simple lens focuses red and blue at different distances | Lenses, Optical Glass and Achromatic Lenses |
| Panchromatic plates | Bathed with sensitising dye, below | Making Photographic Papers and Plates |
| Three filters: red, green, blue | Dyed gelatin between glass, or liquid cells | Below |
| Grey scale | A card painted with 6 steps from white to black | Pigments, Paints and Varnish |
| Darkroom with total darkness possible | Panchromatic plates fog under red light | The Darkroom and the Enlarger |
| Developer, fixer, glass plates | As for black and white | Photography |
| For prints: gum arabic, potassium dichromate (by trade or from a chromate works), Prussian blue, madder lake or carmine, a yellow pigment, sized rag paper | Tri-colour gum print | Chromium and Its Compounds, Prussian Blue and the Prussiates |
| For projection: three lanterns or one triple lantern, a white screen | Cinema: Film Cameras and Projectors | |
| Spectroscope or a glass prism | To test filters | The Spectroscope |
Where to find it
- Sensitising and filter dyes: eosin, erythrosine and cyanines are coal-tar dyes made from aniline and resorcinol (Coal Tar Chemicals, Organic Synthesis and Fine Chemicals). Chlorophyll from leaves (soaked out with alcohol) sensitises weakly to red and fades fast; use it only to prove the idea.
- Potato starch for screen plates: grate potatoes into water, let the white starch settle, pour off and wash it several times, dry it.
- Pigments: Prussian blue for cyan (Prussian Blue and the Prussiates), madder lake or carmine from cochineal for magenta (Dyes and Mordants), chrome yellow (Chromium and Its Compounds) or a weld lake for yellow.
- Canada balsam or clear lac varnish to cement filters (Pigments, Paints and Varnish).
Colour filters
A filter is a sheet that passes one band of colour and absorbs the rest. A tricolour set splits the spectrum into thirds: red passes everything longer than about 600 nanometres (orange-red to deep red); green about 500–580 nm; blue about 400–500 nm.
Dyed gelatin filters
- Soak 7 g gelatin in 100 ml water, melt at 50 °C, and stir in dye solution.
- Pour about 7 ml per 100 cm² onto a levelled, cleaned glass plate (as for plates in Making Photographic Papers and Plates), let it set on cold stone and dry for a day under a dust cover.
- Cut out the best area and cement it between two thin, flat cover glasses with a drop of Canada balsam, squeezed out to a film with no bubbles. Bind the edges with black paper.
Mixing a colour from what you have. Filters subtract, so combine two:
| Filter | Mix | Why |
|---|---|---|
| Red | Yellow-orange (potassium dichromate or a yellow dye) + magenta (eosin or carmine) | Yellow removes blue, magenta removes green |
| Green | Yellow + cyan (ammoniacal copper, or a blue dye) | Yellow removes blue, cyan removes red |
| Blue | Cyan + a little violet dye | Cyan removes red, violet removes green |
The liquid filter cell
The quickest set to make, and the kind Maxwell used. Cut a U-shaped spacer 5 mm thick from glass or brass, and cement two flat glass squares (5 × 5 cm) to it with balsam or wax. Fill with solution and stopper the top.
- Blue-cyan: dissolve copper sulfate (Copper Smelting) in water and add ammonia until the pale blue cloud that first forms dissolves to a deep royal blue (Ammonia).
- Yellow: potassium dichromate, about 2 % (Chromium and Its Compounds).
- Combine cells, or mix in one, by the table above. Adjust the strength until the test below is passed.
Test every filter. Look at a spectrum from a prism or The Spectroscope through it: it should pass its own third brightly and cut off the other two sharply, with little overlap. With no spectroscope, look at a green leaf through the red filter (it should look nearly black) and at a red flower through the green and blue ones (also nearly black). Place filters in front of the lens; a poor filter there blurs the picture, so check sharpness on the ground glass.
Filter factors. Each filter cuts the light, so exposures lengthen, often 5 to 10 times with a panchromatic plate, and differently for each colour. Find them with the grey scale (below), not by guesswork.
Making plates see red
Bathe ordinary gelatin bromide plates in a sensitising dye just before use. This is how panchromatic plates were made by hand in the early 1900s.
- Make a stock of 1 g dye in 1 litre of alcohol (Distillation). For green sensitivity use erythrosine; for red, a cyanine such as pinacyanol, often mixed with a little erythrosine.
- In total darkness, mix about 2–4 ml of stock with 100 ml water and 1 ml of ammonia water. That is a dye strength of about 1 part in 25,000–50,000.
- Bathe each plate 2–3 minutes, rocking. Rinse for a few seconds in clean water.
- Dry fast in a dark, dust-free box with a gentle current of air; slow drying gives fog. Use within a few days.
Load, develop and fix in total darkness, or by a very dim dark green light glanced at for a few seconds only. Develop by time and temperature (The Darkroom and the Enlarger), not by eye.
Note Is it panchromatic? Photograph a spectrum, or a strip of red, green and blue paper beside a grey card. A plain plate shows the red as black. A good panchromatic plate shows the red patch with some density on the negative.
Method 1: Three separation negatives
The repeating back
For a still subject you can simply change filter and plate three times. To catch anything that moves (leaves, faces, clouds), make the three exposures as quickly as possible on one long plate with a repeating back.
- Make a plate holder three frames long, for example 9 × 30 cm for three 9 × 9 cm pictures, sliding sideways in grooves across the back of the camera.
- Fix the three filters side by side in a strip in front of the plate, inside the holder, so each frame always gets the same filter.
- Cut notches in the edge of the holder and fit a spring catch so it clicks into the exact position for each frame.
- Expose: frame one (blue, which needs the longest), slide, frame two (green), slide, frame three (red). Practised hands can do all three in a few seconds.
Prokudin-Gorsky photographed the Russian Empire this way about 1905–1915; a century later his glass separations were combined into colour pictures that look as if taken yesterday.
Balancing the three
Put a grey scale (white, four greys, black) and patches of red, green and blue paper in the corner of every scene.
- Expose a test set. Develop all three plates together for the same time.
- Compare the grey scale on the three negatives. They should match step for step. If the red negative is thinner, its exposure was too short: lengthen it in proportion.
- Write down the three exposures as ratios, for example blue 1 : green 1.6 : red 2.5. They hold as long as the filters, plates and light stay the same.
Develop separations to moderate contrast. Too-dense negatives lose the bright colours; too-thin ones make everything grey.
Method 2: Additive projection
The tricolour projector is Maxwell's experiment made into a machine.
- Contact-print each separation negative onto a glass plate to make three positive transparencies.
- Mount three lanterns (Cinema: Film Cameras and Projectors) side by side, each with the filter that matches its slide: the red-filter positive behind the red filter, and so on.
- Aim all three at one white screen and move them until the grey scale lines up exactly. A triple lantern with three lenses on one board, each adjustable by screws, holds registration better.
- Balance the colours by dimming or brightening each lamp until the grey scale looks grey.
It needs strong light: each filter passes only a third, so the picture is dim.
Method 3: The three-colour pigment print
The most practical lasting colour print for a workshop is the tri-colour gum print: three thin layers of pigment in gum, each hardened by light through one separation negative, printed one on top of the other in register. It uses only Pigments, Paints and Varnish, gum arabic and dichromate.
How it works. Gum arabic mixed with potassium dichromate becomes insoluble where light hits it. Coat paper with gum, dichromate and pigment, expose it under a negative, and soak it in water: the gum washes away where the negative was dense, and stays where light passed. Since the light passed where the negative was thin, the print is a positive.
- Prepare the paper. Choose strong, smooth rag Paper. Soak it 30 minutes in hot water and dry it, so it will not shrink between layers. Size it with 3 % gelatin hardened with a pinch of alum. Punch two registration holes in the margin, or mark corners with pin holes.
- Mix the gum. Dissolve 40 g gum arabic in 100 ml water (a day's soaking). The sensitiser is a saturated solution of potassium dichromate, about 12 g in 100 ml water.
- Coat in dim light: mix 1 part gum, 1 part dichromate and a little pigment (start with about 0.5 g per 10 ml of gum; a strong layer looks clearly coloured but you can still see the paper through it). Brush it on evenly and smooth with a broad soft brush until no streaks show. Dry in the dark.
- Yellow first. Lay the paper in a printing frame under the blue-filter negative, lined up on the pins, and expose in sunlight, typically 3–10 minutes (find it by test strip).
- Develop by floating the print face down on water at about 20 °C for 30 minutes to a few hours, until the clear parts are clean. Dry.
- Magenta (madder lake or carmine) under the green-filter negative; cyan (Prussian blue) under the red-filter negative. Same steps, same registration.
- A fourth thin layer of lampblack under the best of the three negatives gives deeper shadows.
Tip Which negative goes with which colour? Each pigment absorbs the light its negative recorded: yellow absorbs blue, so it goes with the blue negative. Mix them up and a blue sky prints yellow.
The carbon print (pigment in gelatin) and the dye transfer print (dye soaked into gelatin relief images and pressed onto paper, as Technicolor films were printed) do the same job more finely. Learn gum first.
Method 4: The autochrome screen plate
The autochrome (1907) put the three filters inside the plate as millions of tiny coloured grains, so one exposure in an ordinary camera gave a colour picture. It is beautiful and hard. Make a few as a demonstration; a works makes them in bulk.
- Sieve the starch. Shake dry potato starch through fine silk bolting cloth and wash out the finest dust by settling in water. You want grains of 10–15 micrometres, the size of a fine flour.
- Dye three batches: red-orange, green and blue-violet, with water-soluble dyes. Dry and break up the lumps.
- Mix them in proportion (find it by looking at the mixed powder: it must look neutral grey, neither pink nor green).
- Coat a glass plate with a thin sticky varnish, dust the mixed grains on with a soft brush, and brush off all that do not stick, leaving a single layer.
- Fill the gaps by dusting on fine carbon black (Lampblack and Carbon Black), which stops white light leaking between grains.
- Press flat under a hard roller so the grains spread into a mosaic. The Lumière plates held about 6,000 grains per square millimetre.
- Varnish with a thin waterproof varnish, then coat with panchromatic emulsion.
Exposing. Load the plate with the glass towards the lens, so the light passes through the grains first. Use a pale yellow-orange filter to hold back the excess blue. Exposure is long: about a second in sunshine at f/8, a minute or more indoors.
Reversal processing. Develop the first image (the negative) fully. Bleach it away in an acid permanganate bath (Potassium Permanganate, with a little Sulfuric Acid), which dissolves the developed silver but leaves the unused silver bromide. Expose the plate to daylight, then develop again: the remaining bromide turns black. Silver now blocks the grains whose colour was not in the scene, and the grains whose colour was there show through clear. Wash, dry, varnish.
An autochrome is dark: hold it to a bright window or project it. Later screen plates used ruled lines of the three colours instead of grains, which suit machines better.
Dye-coupler colour film (in outline)
All modern colour film works on a different principle: the developer makes the dye.
- Three layers of emulsion on one base. Top: blue-sensitive. Then a yellow filter layer to stop blue light going deeper. Then green-sensitive, then red-sensitive.
- When a colour developer (a derivative of p-phenylenediamine, from Organic Synthesis and Fine Chemicals) turns exposed silver bromide into silver, the used-up developer joins with a colourless chemical called a coupler to form a dye on the spot: yellow in the top layer, magenta in the middle, cyan at the bottom.
- A bleach then turns all the silver back into a salt, the fixer removes it, and only the three dye images remain.
- Colour negative film gives a negative in complementary colours, with an orange mask that corrects the dyes' faults; it is printed on colour paper made the same way. Reversal (slide) film gets a first black-and-white development, then fogging, then colour development, giving a positive.
Processing is chemistry with no slack. The standard colour-negative process develops for 3 minutes 15 seconds at 37.8 °C, held within about ±0.2 °C, followed by bleach, fix, wash and stabiliser. A tenth of a degree off, or a minute's error, shifts the colours. Use a big water bath with a thermostat, and agitate exactly the same way every time.
Making the film is a factory job: many layers a few micrometres thick, coated at once in total darkness, with synthetic couplers and dyes. Master separations and pigment prints first; they last longer anyway.
Keeping colour pictures
- Dyes fade. Light fades them fastest; heat and damp fade them even in the dark. Many colour prints and films of the 1950s–1970s have turned pink or yellow as one dye failed before the others.
- Store cold, dry and dark. Each 5 °C cooler roughly doubles the life of a dye image. Keep master films and prints in closed boxes at below 10 °C and 30–40 % relative humidity; a refrigerator, or better a freezer in a sealed bag with the air pressed out, keeps them for centuries.
- Display copies, keep originals. Never hang the only copy in the sun.
- The best archive is silver. Three black-and-white separation negatives, well fixed and washed, last as long as any photograph. From them you can make new colour prints in any century. Pigment prints (gum or carbon) with lightfast pigments are the most lasting colour prints.
How to tell it worked
- The grey scale is grey in the final print or projection, with no tint in the whites, greys or blacks. This one test catches most faults.
- Known colours look right: green leaves, blue sky, skin, a red patch on the card.
- Registration: edges are crisp, with no coloured fringes.
Note Troubleshooting. Reds come out dark and dirty → the plate is not red-sensitive; check the dye bath. Or the red exposure was too short. Everything has one tint → that colour's exposure, development or pigment layer is too strong; balance with the grey scale. Coloured fringes on edges → layers out of register (paper shrank, or pins moved), or the subject moved between exposures, or the lens focuses colours at different distances (use a smaller stop, or refocus through each filter). Gum layer washes off completely → under-exposed, or too much pigment. Will not clear → over-exposed, or coated too thick, or the coating was old. Panchromatic plates fogged → any safelight at all, slow drying, or plates kept too long after bathing. Autochrome too dark → over-exposed in the first stage or under-developed in the second; grains too large or carbon too heavy.
Dangers
Danger Dichromate is a cancer-causing poison that also burns the skin and causes lasting allergy. Weigh it in still air, wear gloves, never let dust fly, and never pour it on the ground. Spent dichromate and the washings from gum prints must be made harmless as Chromium and Its Compounds describes, by turning the chromium to its green, less dangerous form.
- Coal-tar dyes and colour developers soak through skin and cause allergies; p-phenylenediamine developers are well known for severe dermatitis. Use gloves and tongs.
- Ammonia and acid permanganate baths irritate eyes and lungs; work with ventilation.
- Working in total darkness: lay out trays and tools in the same order every time, keep the floor clear, and never pour concentrated acid in the dark.
- Lantern heat cracks gelatin filters and can set fire to nitrate film (Photographic Film Base).
What this unlocks
Colour separations are the basis of all colour printing: separate an original through the three filters, make a halftone plate from each, and print yellow, magenta, cyan and black inks one over another (Printing, Lithography and Offset Printing, Screen Printing). The same three-colour idea is how Cathode Rays and Television cameras and screens, and every digital camera, work: three sensors or three coloured dots per point. Colour photographs serve medicine (Ultrasound, CT and MRI), microscopy, Maps and Mapmaking from the air, and the Cinema: Film Cameras and Projectors.
How it was first done
Thomas Young suggested in 1802 that the eye has three colour sensors. James Clerk Maxwell showed a colour photograph of a tartan ribbon in London on 17 May 1861, from three separations taken by Thomas Sutton through liquid filters and projected through the same filters. In 1868–69 Louis Ducos du Hauron and Charles Cros, working separately in France, described the additive and subtractive methods. Hermann Vogel in Berlin found in 1873 that dyes make silver plates sensitive to green; panchromatic plates followed with the cyanine dyes, sold in England from 1906. John Joly patented a ruled screen plate in 1894. Auguste and Louis Lumière patented the autochrome in 1903 and sold it from 1907; it ruled colour photography for thirty years. Leopold Mannes and Leopold Godowsky Jr., two musicians working with Kodak, produced Kodachrome in 1935; Agfa's film with couplers built into the layers followed in 1936, and colour negative film for prints in 1942.
Source: content/entries/knowledge/colour-photography.md