Part 8 · Chemistry
Chromium and Its Compounds
Heavy black chromite, roasted in air with soda ash and lime, turns into a yellow salt that dissolves in water. From it come orange dichromate, the unfading green of chrome oxide, bright chrome yellow, the violet chrome alum that tans a hide into leather in a day instead of a year, and the chromic acid of chrome plating. The yellow and orange forms are among the most poisonous things in this book, so their making is given in outline only; the chapter is about turning them into the safe green forms and handling them safely.
- Difficulty
- ●●●●●
- Time
- An afternoon for green pigment; a day to make tanning liquor; one to two days to chrome-tan a hide
- Steps from zero
- 14 prerequisites →
This unlocks
—The full path from nothing — 14 steps before this one
- Fire
- Finding and Preparing Clay
- Finding and Identifying Ores
- Sulfur
- Pottery
- The Kiln
- Charcoal
- Lime
- Salt
- Lye and Potash
- Glass
- Saltpeter
- Sulfuric Acid
- Soda Ash and Baking Soda
- Chromium and Its Compounds
Do them roughly in this order. See it on the tech tree →
Why it matters
Chromium is named from the Greek chroma, "colour", because every one of its compounds is brightly coloured. Out of one black ore come:
- Chrome oxide green. A dull, opaque green that light, acid, lime, alkali and kiln fire cannot change. It colours paint, cement, glass and Glazes.
- Chrome yellow and orange. The brilliant yellows of road signs, carts and machinery (Pigments, Paints and Varnish).
- Dichromate. An orange salt that makes gelatin harden in light, which is the basis of photographic stencils and printing plates (Screen Printing, Photography). It also drives the old bichromate The Battery, and it is the starting point for everything below.
- Chrome tanning. Bark tanning takes six months to a year (Hides and Leather). Chrome tanning takes a day, and gives leather that is softer, stronger, lighter and stands boiling water. Nearly all shoe uppers, gloves and clothing leather are tanned this way (Footwear, Leatherwork and Harness-Making).
- Chrome plating. A hard, bright, non-tarnishing skin on taps, tools and shafts (Electroplating).
- Metal. A few percent of chromium makes tool steel, bearing steel and, above 12 %, stainless steel (Alloy and Stainless Steels). It also turns alumina into ruby (Synthetic Gems).
Danger Read the Dangers section before you start. The yellow and orange chromium compounds, called hexavalent chromium or "chrome six", cause lung cancer, eat holes in skin and in the wall between the nostrils, and a few grams swallowed can kill. The green compounds, trivalent chromium, are far safer. The whole craft is to spend as little time as possible in the yellow-orange stage, and to turn every scrap of it back to green before it leaves your workshop.
How it works
Chromium has two everyday forms, and you can see which you have by its colour:
| Form | Colour | Examples | Danger |
|---|---|---|---|
| Trivalent (chromium III) | Green, grey-green, violet | Chromite ore, chrome oxide green, chrome alum, tanning liquor, leather | Low: not absorbed through skin, not a known cancer cause in normal use |
| Hexavalent (chromium VI) | Yellow, orange, red | Chromate, dichromate, chromic acid, chrome yellow | High: burns, ulcers, allergy, cancer, poison |
Roasting. In chromite, chromium is locked with iron and oxygen in a hard, black, acid-proof mineral. Heated in plenty of air with soda ash, the chromium takes on more oxygen and becomes sodium chromate, yellow and soluble in water. The iron becomes rust and stays behind. Lime is added as a filler. It keeps the mass from melting into a sticky slag, so air can reach every grain.
Chromate to dichromate. Acid turns yellow chromate into orange dichromate. Both are hexavalent.
Back to green. Anything that burns, such as sugar, alcohol, sulfur, charcoal or sulfur dioxide, or green vitriol, pulls the extra oxygen off and returns chromium to the safe green trivalent form. This is how you make the green pigment, the tanning liquor and chrome alum. It is also how you make waste safe.
What you need
A chromate works, in outline:
| Item | Notes |
|---|---|
| Chromite, ground to flour | Hand-picked, washed ore; see below |
| Soda ash (Soda Ash and Baking Soda) or potash (Lye and Potash) | The alkali that carries the chromium into solution |
| Quicklime or crushed limestone (Lime) | Filler, so the roast stays crumbly |
| Reverberatory hearth or open kiln floor | Flames pass over the charge so air reaches it (The Kiln) |
| Wooden or stoneware leaching tubs; Sulfuric Acid | Not iron for acid work |
| Dust masks of many layers of wet cloth, rubber or oiled-leather gloves, eye protection, apron | Non-negotiable |
| Green vitriol (Sulfuric Acid) and lime | For treating every drop of waste |
Where to find it
Chromite (chrome iron ore) is the only practical ore (Finding and Identifying Ores, Alloy and Stainless Steels):
- Where. Only in dark green to black serpentine and related very dark, heavy rocks that came up from deep in the Earth. Serpentine country is easy to spot: greasy-looking green rock, often with white veins, and thin, poor soil where few plants grow. Chromite forms black pods, bands and scattered grains within it. Where serpentine weathers, chromite grains wash into stream and beach sands as heavy black grit with the magnetite.
- Identify. Black, with a dull metallic to pitchy shine. It is heavy, about 4.5 times water. Its streak is dark brown, while magnetite's is black. It is only weakly pulled by a lodestone, while magnetite jumps to it. It is too hard for a knife to scratch.
- Test. Fuse a pinch with soda ash and a crystal of saltpeter on a clay sherd for a few minutes, then drop it in water. A yellow solution means chromium. Manganese gives green. A borax bead (Identifying Substances) turns emerald green.
- Grade. Good ore is 40–50 % chromium oxide. Pan or wash crushed ore to throw off the lighter serpentine.
Crocoite, orange-red needles of natural lead chromate, is the mineral in which chromium was discovered. It is rare. Do not grind it.
Method 1: From chromite to dichromate (outline only)
Every useful chromium compound passes through the yellow and orange hexavalent stage, and that stage is a cancer hazard in dust, mist and waste water. This book therefore gives it in outline only: enough to understand what a chromate works does and to plan one with proper extraction, protective gear and waste treatment, not a batch recipe for a home workshop. Where you can, obtain dichromate or chrome alum by trade, and use the methods below that turn it into the safe green forms.
- Roast. Finely ground chromite is mixed with soda ash and a larger amount of lime and roasted at a bright orange heat in a thin, constantly raked bed, so air reaches every grain. The chromium takes up oxygen and becomes yellow, water-soluble sodium chromate; the iron stays behind as rust. The roast is done when a cooled sample turns water strongly yellow and the leftover grains are brown, not black.
- Leach. The cooled roast is soaked in hot water, which dissolves the chromate and leaves a brown residue that is itself contaminated waste.
- Acidify. Sulfuric acid turns the yellow chromate solution orange: dichromate.
- Crystallise. Sodium dichromate is very soluble, so works add a potassium salt (or roast with potash in the first place) and crystallise orange potassium dichromate from the cooled liquor.
- Store it in a stoppered glass or glazed jar, labelled POISON with a skull, locked away.
All of this happens wet or hot, with dust at the raking and shovelling stages; it is where the chrome workers of the 1800s got their nose ulcers and lung cancers.
Method 2: Chrome pigments
Chrome oxide green (the safe one)
This is the pigment to make first. It is permanent, cheap, non-toxic in use, and making it destroys hexavalent chromium.
- Mix 100 g of potassium dichromate with 12 g of powdered sulfur, dry, in a clay mortar. Or use 10 g of charcoal powder or 25 g of starch.
- Pack the mixture into a clay crucible, cover it, and heat it to red heat, 800–900 °C, for one hour (The Kiln). It glows and smokes as the sulfur reacts. Do this outdoors.
- Cool, then boil the green cake in water to dissolve the potassium sulfate. Pour off. Repeat until the wash water is colourless. Any yellow tint means unconverted dichromate: dry it, add a little sulfur, and fire it again.
- Dry and grind it fine in a mortar or pigment mill.
You get about 50 g of olive-green powder. It mixes into oil, egg, casein or lime for paint. 0.5–2 % in a glaze gives green, and with tin oxide in a lime glaze it gives a pink (Glazes). It also colours cement and glass green, and is a fine polishing compound for steel razors, rubbed onto a leather strop (Razors, Nail Clippers and Grooming Tools).
Viridian (Guignet's green). A brighter, transparent, bluish emerald green. Mix 1 part dichromate with 3 parts boric acid (Borax and Boric Acid), heat it in a clay dish at a dull red, about 500–550 °C, for 2–3 hours, then wash it thoroughly with hot water. The boric acid washes out and can be recovered. Viridian is the best green for artists' oil and watercolour.
Chrome yellow and orange (outline only)
Chrome yellow is lead chromate, a double poison: lead and hexavalent chromium together (Lead). It is made by mixing a lead salt solution with a chromate or dichromate solution, when a brilliant yellow powder falls out; small changes to the acidity give lemon yellow, deep yellow or, made basic, orange and red. Because it stays hexavalent in the finished paint, this book does not give a recipe.
Where old chrome yellow paint exists, use it only for outdoor signs, carts, machinery and road markings. Never use it on toys, cradles, food vessels, walls inside homes or anything children chew (Toys). Mixed with Prussian blue (Prussian Blue and the Prussiates), it was sold as "chrome green". That mixture is just as poisonous as chrome yellow and has nothing to do with chrome oxide green. For yellow, prefer ochre and other earth pigments (Pigments, Paints and Varnish).
Good or bad pigment: a good chrome oxide green is an even, opaque, mid-olive with no yellow streak when rubbed out with oil. A dull brown-green means iron in the ore. A yellowish wash means unconverted chromate, which must be refired.
Method 3: Chrome alum and chrome tanning
Chrome tanning liquor
This turns dichromate into a dark green-blue syrup of basic chromium sulfate, the tanning agent. Make it outdoors, in a 10-litre stoneware or wooden vessel, because it froths up violently.
For 10 kg of wet, limed and dehaired hide (pelt weight):
- Dissolve 500 g of potassium or sodium dichromate in 2 litres of hot water.
- Pour in 270 ml (500 g) of concentrated sulfuric acid, slowly, stirring. It gets hot.
- Dissolve 130–150 g of sugar or the equivalent in honey or molasses in 0.5 litre of water. Add it a spoonful at a time, waiting for each to stop frothing. The orange turns muddy brown and then a clear dark green-blue.
- Boil it gently for 30 minutes.
- Test it. Put a drop on a white plate. It must show no yellow or orange edge. Or add a drop of liquor to lead acetate solution: no yellow precipitate. If either test shows hexavalent chromium, add a little more sugar and boil again.
- Dilute it to 5 litres. This liquor contains about 2.5 % chromium oxide on the pelt weight, the normal dose.
Chrome alum crystals are the same thing in a purer, storable form. Use 100 g of potassium dichromate in 400 ml of water and 72 ml of concentrated sulfuric acid, cooled, then add 60 ml of strong alcohol (Distillation) in small portions, keeping the vessel in cold water below 40 °C. Leave it in a cool place. Dark violet, eight-sided crystals grow over a few days. Used in tanning and to harden gelatin in Photography.
Chrome tanning a hide
Prepare the hide by soaking, fleshing, liming and dehairing, then wash out the lime as for bark tanning (Hides and Leather). Remove the last of the lime by soaking it in water with a little vinegar or bran until a drop of red cabbage juice on a fresh cut no longer turns green (Acids, Bases and Testing). Then:
- Pickle. Put the pelt in a tub, or better a slowly turning wooden drum (Barrels and Cooperage) with 8 litres of water, 700 g of salt and 100–150 g of sulfuric acid stirred into the water first. Turn it or work it for 2–3 hours, then leave it overnight. The salt stops the acid swelling the hide. The pelt should be acid right through: a cut edge turns red cabbage juice red.
- Tan. Add the chrome liquor in three portions, an hour apart. Keep turning it gently. After 4–8 hours cut a corner: the blue-green colour must have gone right through with no white line in the middle.
- Fix (basify). Dissolve 100–150 g of baking soda (sodium bicarbonate, made by bubbling carbon dioxide into soda solution — Soda Ash and Baking Soda) in water. Add it in four portions over 2–3 hours. This makes the chromium bind permanently. Leave it overnight in the liquor.
- Horse up. Take the hide out, now pale blue-green ("wet blue"). Lay it over a wooden horse for a day to drain and finish fixing.
- Wash, neutralise and oil. Wash it, soak it for an hour in water with a little borax or baking soda, and rinse. Then work in a fat liquor: 1 part neatsfoot or fish oil shaken with 1 part soap solution and 4 parts warm water, about 5–8 % of the hide weight. Without oil, chrome leather dries hard.
- Dry and stake. Dry it slowly, stretched on a frame. While it is still slightly damp, work it soft over a blunt blade or the edge of a board (Leatherwork and Harness-Making). It can then be dyed any colour.
The boil test. Cut a strip 1 × 5 cm and drop it into boiling water for 3 minutes. Good chrome leather does not shrink or curl. Raw hide shrinks to half its length at about 65 °C, and bark-tanned leather at about 75–85 °C.
Good or bad: good chrome leather is soft, even in colour right through and stretchy, and passes the boil test. A white core means it was not tanned long enough. Hard, cracky leather was under-oiled or basified too fast. Green, blotchy surface stains came from adding the soda too quickly.
Chrome plating and chromium metal (outline)
Chrome plating (Electroplating) uses a warm, strong bath of chromic acid (hexavalent) with a small, exactly controlled amount of sulfuric acid, and lead anodes. It is unlike other plating. It needs a very high current density, several times that of nickel plating, and only about an eighth of the current deposits metal; the rest makes hydrogen, which throws up a fine mist of chromic acid. Decorative chrome is a film less than a micrometre thick over bright nickel. Hard chrome for shafts and gauges is much thicker.
The mist is the worst chromium hazard of all. Plating shops in the 1900s were full of workers with holes through the nose. Plate only with a lid of floating plastic balls or a layer of wetting agent on the bath, strong extraction drawing the mist away from the operator's face, and full skin and lung protection. Nickel plating does most of the same jobs with far less danger.
Chromium metal is made by heating chrome oxide green with powdered aluminium. The mixture burns fiercely and leaves a button of chromium under alumina slag. This is the aluminothermic or thermite process (Aluminium). Ferrochrome for steel is smelted from chromite and coke in an electric furnace (Alloy and Stainless Steels).
How to tell it worked
- Dichromate: orange-red prisms. A crystal dropped into sulfuric acid with a little alcohol turns green; the alcohol reduced it.
- Chrome oxide: green and colourless wash water, and the powder will not dissolve in acid or lye.
- Liquor: no yellow edge on a white plate.
- Leather: passes the boil test.
Note Troubleshooting. Green pigment dull and brownish → iron in the dichromate. Recrystallise it, or wash the green pigment longer. Liquor turns bright green and the leather is harsh → made too fast and hot, or too little acid. Make the next batch more slowly. Leather shrinks in the boil test → too little chrome, too short a time, or not basified. Return it to the liquor.
Dangers
Danger Hexavalent chromium (yellow and orange compounds) is a poison and causes cancer.
- Dust and mist breathed over months cause lung cancer, and can rot a hole through the wall between the nostrils within weeks. Never handle the roast, chromate or dichromate powder without a wet-cloth mask, and never grind it dry.
- On skin it causes painless, deep ulcers ("chrome holes") wherever there is a scratch, and a lifelong allergy, so that even cement or chrome leather then brings out an itching rash. Wear gloves; wash at once; cover all cuts.
- Swallowed, a few grams of dichromate destroy the kidneys and can kill. There is no home antidote. Give water to rinse, do not cause vomiting, and get help (Emergencies).
- Fire. Dichromate and chromic acid are strong oxidisers. Mixed with sugar, oil, glycerine, alcohol or sawdust they can heat and flare up. Store them alone.
Warning Treat every drop of yellow waste before it leaves the workshop. Acidify the waste water with a little sulfuric acid, then stir in green vitriol (iron sulfate) until the colour changes from yellow-orange to green or blue-grey, with no yellow left on a white plate. Then add lime until it no longer turns blue litmus red. The green-brown sludge that settles holds the chromium in its safe form. Dry it and bury it in a clay-lined pit away from wells (Sanitation and Germs). Treat the roast residue the same way. Never pour chromate onto the ground or into a stream: it travels in groundwater for decades.
- Chrome yellow carries lead poisoning as well (Lead).
- Trivalent chromium (green) is low-risk, but chrome-tanned leather scraps should not be burned. Burning can turn them back to the hexavalent form. Bury them.
What this unlocks
Chrome-tanned leather in a day (Footwear, Leatherwork and Harness-Making, Bags, Backpacks, Wallets and Luggage); permanent green paint and glazes (Pigments, Paints and Varnish, Glazes); dichromated gelatin for photo-stencils and printing plates (Screen Printing, Printing); the bichromate The Battery; hard chrome plating; chromium for Alloy and Stainless Steels and stainless steel; chromium oxide for Synthetic Gems; and chrome-magnesite bricks for steel furnaces (Firebrick and Refractories).
How it was first done
In 1797 the French chemist Louis-Nicolas Vauquelin studied the orange-red Siberian mineral now called crocoite and found a new metal in it. He called it chromium for its colours, and isolated it in 1798. He also suggested lead chromate as a pigment, and chrome yellow was on sale within twenty years. Isaac Tyson Jr. found chromite in the serpentine barrens of Maryland and built the Baltimore Chrome Works in 1845, the world's chief source of chromate for decades. Charles-Ernest Guignet patented his viridian green in 1859. Friedrich Knapp showed in 1858 that chromium salts tan hide, Augustus Schultz of New York patented a practical two-bath chrome tannage in 1884, and Martin Dennis introduced the one-bath method in 1893. Bright chrome plating became commercial in the mid-1920s, after work at Columbia University by Colin Fink.
Source: content/entries/chemistry/chromium.md