Part 7 · Home and Daily Life
Lamps and Candles
How to make light after dark from fat, oil and wax — rushlights, open and spouted oil lamps, dipped and moulded candles of tallow and beeswax, safe lanterns, and finally the bright kerosene lamp with its glass chimney.
- Difficulty
- ●●●●●
- Time
- An evening for rushlights and a clay lamp; a day to dip a winter's supply of candles
- Steps from zero
- 3 prerequisites →
The full path from nothing — 3 steps before this one
- Fire
- Finding and Preparing Clay
- Pottery
- Lamps and Candles
Do them roughly in this order. See it on the tech tree →
Why it matters
A campfire lights a circle a few metres wide, and only while you feed it. Away from the fire, the night is half of every day — in high latitudes in winter, two-thirds of it. Without portable light, all work stops at dusk: no sewing, no reading, no tending a sick child, no checking the animals.
A lamp is simply a small, controlled fire that burns a liquid or solid fuel through a wick. With it you get long evenings for the quiet work that fills a household — Spinning and Weaving Cloth, Sewing, Needles and Thread, mending, carving, keeping accounts in Writing and Numbers, teaching children to read. Light in a closed lantern lets you go safely into a hayloft or a mine. And the search for better light drove real progress: better fats and waxes, Glass chimneys, Distillation of Petroleum and Refining into kerosene, and finally the electric The Light Bulb.
How it works
A candle or lamp does not burn liquid fat. It burns fat vapour.
- The flame's heat melts the fuel near the wick (a candle) or the fuel is already liquid (a lamp).
- The liquid climbs the wick by capillary action — the same pull that lets a cloth corner soak up a spilled drink. The fibres must be fine and touch each other closely, with tiny gaps between them.
- Near the top of the wick the liquid boils into vapour. The vapour mixes with air and burns.
- The yellow light comes from tiny specks of soot glowing white-hot inside the flame. If the flame gets too little air, those specks escape as smoke; if it gets plenty, they burn away before leaving.
Three rules follow, and almost every problem with lamps comes back to them:
- Wick size must match the fuel supply. Too thick a wick for the fuel it can draw → a big, smoky flame that gutters. Too thin → a tiny flame that drowns in its own pool.
- The wick must stay short. A long charred wick makes a tall, smoky, dim flame. Old wicks had to be trimmed with snuffers every 15–30 minutes.
- More air through the flame = brighter, cleaner light. That is why a glass chimney, which pulls a draught past the flame, multiplies the light of a lamp several times.
What you need
| Fuel | Where from | Melts at | Light and smell |
|---|---|---|---|
| Tallow (beef, mutton, deer fat) | Rendered suet (Oils and Pressing) | 40–50 °C | Yellow, a little smoky; smells of fried meat. Mutton tallow is hardest |
| Lard, bear, goose fat | Rendered fat | 30–40 °C | Too soft for candles; good in open lamps |
| Beeswax | Old comb (Beekeeping) | 62–64 °C | Bright, clean, sweet-smelling. The best candle material you can make |
| Plant oil (olive, linseed, rapeseed, nut) | Pressed seeds (Oils and Pressing) | Liquid | Clean, steady flame in a lamp. Olive oil is the classic |
| Fish and seal oil, whale oil | Boiled-out blubber and livers | Liquid | Bright but smelly |
| Kerosene (paraffin oil) | Distilled from crude oil (Petroleum and Refining) | Liquid | Very bright with a chimney; needs a proper burner |
Wick materials: cotton yarn (best), linen (Flax, Hemp and Linen) thread, the white pith of soft rush, dried mullein leaves, cattail fluff, twisted moss, strips of old cloth. Loosely spun yarn wicks better than tightly spun.
Tools: a pot for melting fat (clay or metal), a deep narrow container for dipping, sticks or rods, scissors or a knife, and clay for lamps (see Pottery).
Where to find it
- Soft rush (Juncus effusus) — clumps of smooth, round, dark-green stems 50–100 cm tall in wet pastures, ditch edges and marshes. Squeeze a stem: it is solid, filled with white spongy pith, not hollow like a reed. Cut it in late summer when the stems are tallest and greenest.
- Mullein — a tall roadside plant with very soft, thick, woolly grey-green leaves (like flannel) in a big rosette, and a tall spike of yellow flowers. The dried leaf fuzz and the rolled leaves make wicks; the dried flower stalk dipped in fat made the medieval "hag taper", a torch.
- Cattail — the brown "sausage" of the cattail breaks into fluff that can be twisted into a wick.
- Fat comes from every animal you butcher. Save the hard, crumbly fat from around the kidneys of cattle and sheep (suet): it renders into the hardest tallow.
- Beeswax comes from wild or kept bees. A strong hive yields 0.5–1 kg of wax a year from old comb and cappings.
- Horn — the hollow, keratin sheath from cattle, sheep and goat horns, from every animal you slaughter. It is needed for lantern windows (below; see Horn and Bone Working).
Method 1: The rushlight
The rushlight lit most poor homes in northern Europe for centuries. It costs almost nothing.
- Cut soft rushes in late summer, as long as possible. Soak them in water for a few hours if they have dried.
- Peel. With a thumbnail, strip away the green skin, leaving one narrow strip of skin running the whole length as a backbone. Without it the soft pith falls apart. This takes practice; expect to ruin a few.
- Dry the peeled piths in the sun or by the fire for a day or two.
- Dip. Melt fat (any kind — kitchen drippings or tallow) in a long, shallow pan, so the rushes lie flat. Draw each rush slowly through the hot fat, then lay it on bark to set. Once is enough; twice makes it last longer.
- Burn it held at about 45° in a rushlight holder — a pair of iron or wooden jaws on a stand (a split stick works). Held level it goes out; held upright it burns too fast and drips.
A rush 60–70 cm long burns for about an hour, with a light somewhat dimmer than one candle. Move it up in the holder as it burns. A bundle of 50 is a fortnight of evenings.
Method 2: Open and spouted lamps
The open saucer lamp
The oldest lamp is a hollow in a stone, a shell or a clay saucer, filled with fat or oil, with a wick lying in it and its tip resting on the rim.
- Make the saucer. Pinch a clay saucer 8–12 cm across and 2–3 cm deep (see Pottery). Pinch one side of the rim into a spout — a little channel — to hold the wick. Fire it. A glaze (Glazes) stops oil soaking into the clay; without one, soak the new lamp in oil for a day before use, or the first fills will vanish into the walls.
- Make the wick. Twist a strand of cotton, linen or plant fibre 15 cm long and 3–5 mm thick, or roll a strip of mullein leaf or cloth.
- Fill with oil or soft fat to 1 cm below the rim. Lay the wick in, with 5–10 mm of its tip lying in the spout, sticking just over the edge.
- Light the tip. If the flame is big and smoky, pull the wick back; if it is tiny, draw it out a little with a pin.
A lamp of this kind burns roughly 5–10 ml of oil per hour — a 100 ml lamp lasts an evening. It gives about the light of a candle. Use several wicks at once for more light, but each needs its own spout.
The covered (Roman) lamp
A closed lamp — a round clay body with a filling hole on top and a spout nozzle at the front — spills less and keeps mice and dirt out. Make it by joining two pressed halves from a two-part clay or plaster mould (Gypsum and Plaster of Paris), so a workshop can make dozens a day. The filling hole should be about 1.5 cm across; the nozzle hole about 6–8 mm.
The Arctic stone lamp
Peoples of the far north burned seal blubber in a long, half-moon dish of soapstone, with a wick of moss or cotton-grass laid along the straight edge. Tended well, it gave a long, smokeless flame that heated and lit the whole snow-house and melted snow for water. The lesson: a long, low wick along a broad edge gives a wide, clean flame.
Method 3: Dipped candles
A candle is solid fuel wrapped round a wick: it does not spill and can be carried. Dipping builds it up layer by layer.
- Render the fat (see Oils and Pressing). Chop suet small, melt it slowly with a cup of water, strain through cloth, and let it set. To make it harder and cleaner, melt it again in water with a handful of salt, let it set, and scrape off the dirty underside. Do this twice for good candles.
- Make wicks. Twist or plait cotton or linen yarn. For a candle 2 cm thick, plait three strands of ordinary sewing-thickness yarn, each of 4–6 threads — the wick should be about 2–3 mm thick. A plait curls over as it burns, so its tip reaches the outer edge of the flame, burns away and trims itself. Twisted wicks stand straight and need trimming.
- Prime the wicks. Soak them in melted fat and pull them straight as they cool. Some chandlers first soaked wicks in a weak solution of borax or salt and dried them, which slows burning — optional.
- Hang them. Tie pairs of wicks over a stick 2–3 cm apart so the candles won't touch. A board can carry six sticks.
- Fill the dipping pot. Use a tall, narrow pot at least 5 cm deeper than the candles you want — 30 cm for 25 cm candles. Keep it warm in a water bath or beside, not over, the fire. Tallow dips best just above its melting point — when a scum of solid fat begins to form round the edge of the pot, it is right (about 55–60 °C). Beeswax at 70–75 °C.
- Dip. Lower the wicks in for 2–3 seconds, lift them out smoothly, let them hang and harden — about a minute, longer in a warm room. Dip again. Each dip adds a layer about 0.5 mm thick.
- Straighten after the first few dips by pulling the bottom gently. Cut off drips at the bottom with a knife.
- Keep going for 20–40 dips, until the candles are 2–2.5 cm thick at the base. Finish with one dip in hotter fat for a smooth surface.
- Cure tallow candles for a week or more in a cool, dark, mouse-proof box. They burn longer and drip less when old.
Tip The water trick. If you have little tallow, fill the dipping pot two-thirds with hot water and pour melted tallow on top. The tallow floats in a deep layer, so you need much less fat to fill the pot to dipping depth.
A candle 2 cm thick burns about 7–10 g of fuel an hour — roughly 2–3 cm of length. A 25 cm tallow candle lasts 8–10 hours. A household needs 200–400 candles for a northern winter, which is why candle-making was a whole day's work each autumn after the animals were slaughtered.
Method 4: Moulded candles
A mould makes straight, even candles quickly, and is best for tallow.
- Make the mould. Each mould is a smooth tube, slightly tapered, closed at the narrow end except for a small wick hole. Make it from rolled tin or pewter sheet soldered along the seam (Tin and Pewter, Soldering and Brazing), from glazed fired clay, or from a split hardwood block with matched half-round channels, bound shut. Typical size: 2–2.5 cm across, 20–25 cm long. Several tubes are fixed in one frame with a trough on top.
- Thread the wick. Pass a wick through the tip hole, knot it outside, and tie its other end round a stick laid across the open top, pulling it tight and centred.
- Warm the mould a little and grease the inside very lightly with fat.
- Pour melted tallow, just hot enough to be fully liquid, into the trough. It will shrink as it sets and leave a hollow at the top; top it up once.
- Cool slowly — a few hours, then an hour in cold water or cold air.
- Release. Untie the knot at the tip, and pull the candle out by the stick. If it sticks, dip the mould in warm water for a moment.
Beeswax sticks to most moulds. It is better dipped, poured (ladle hot wax down a hanging wick again and again, rolling the candle on a damp board between pours), or rolled: warm a thin sheet of wax until it is soft, lay a wick along one edge, and roll it up tightly.
Lanterns
An open flame carried into a barn full of hay, a workshop full of shavings, or a mine is how towns burn down. A lantern encloses the flame while letting light out.
- Horn lantern (the old "lanthorn"). Soak cattle or sheep horns in water for a few weeks until the core falls out. Boil the horn sheath for an hour until soft, slit it lengthwise, open it out and press it flat between warm boards. Split the flat sheets along their layers into leaves 1–2 mm thick, scrape and oil them, and press them again. They are amber and translucent — not clear, but they pass a soft light. Fix the panes into a wooden or tin frame with a vented top for heat and smoke, and a door for the candle.
- Pierced tin lantern. A tin cylinder punched with hundreds of small holes in patterns, with a cone top. Gives little light but is nearly fireproof and windproof.
- Glass lantern. Once you have Glass or Window Glass, panes in a metal frame give the best light.
Every lantern needs holes at the bottom to let air in and a chimney cap at the top to let hot gas out, or the candle smothers.
Better lamps: chimneys and kerosene
In 1780 the Swiss chemist Aimé Argand made two changes to the oil lamp: a hollow, tube-shaped wick, so air reached the flame from inside as well as outside, and a glass chimney over it, which pulled a strong upward draught. The flame became white and smokeless and gave about ten times the light of a candle. Every later oil lamp copied this idea.
The kerosene lamp (1850s) brought it to every home:
- A fuel tank of glass or metal, holding 0.3–0.5 litres.
- A burner screwed into the top, with a flat woven cotton wick 1.5–2.5 cm wide moved up and down by a small toothed wheel.
- A perforated gallery round the wick that lets air in from below and holds the chimney.
- A glass chimney 20–25 cm tall, narrowed just above the flame so the air is pushed into it.
Such a lamp gives the light of about 10 candles and burns roughly 20–40 ml of kerosene an hour. Kerosene is the middle-boiling fraction of crude oil, roughly 150–275 °C (see Distillation and Petroleum and Refining). It must be free of the light fraction (gasoline): good lamp oil does not catch fire from a match dipped into a spoonful of it at room temperature.
Trim the wick straight across, level with the top of the burner, and remove the charred crust before every lighting. Turn it up slowly over a few minutes after lighting — a cold chimney cracks if heated fast, and a high wick smokes the glass black.
How to tell it worked
- A good flame is steady, yellow-white, tapered, and about 3–4 cm tall for a candle. No black smoke rises from the tip.
- A good candle burns down with a shallow pool of liquid fuel at its top that does not overflow, and the wick stays short — 1 cm — on its own.
- A good lamp burns for hours without attention, and the wick does not dry out at its tip.
Note Troubleshooting. Candle drips and runs down one side → wick off-centre, or a draught; move it out of the wind and centre wicks better next time. Flame drowns in a deep pool → wick too thin for the candle; plait more threads. Big smoky flame, wide hollowing cup that breaks through → wick too thick, or the wick is too long; trim it to 1 cm. Candles crack or have holes → poured too hot or cooled too fast; pour cooler and cool slowly. Tallow candles soft and greasy → too much soft fat in the mix; use more mutton or beef suet, purify with salt water, or add 10–25 % beeswax. Oil lamp flame shrinks after half an hour → the wick is too tightly spun or too long between oil and flame, or the oil is thick; use looser wick and raise the oil level. Kerosene chimney blackens → wick turned up too high or cut unevenly.
Dangers
Danger Fires kill households. Never leave a flame burning unattended, near curtains, bedding or thatch, or where a child or animal can knock it over. Set candles in a heavy holder on a dish of sand or water. Use lanterns, not open flames, in barns, haylofts and workshops.
Danger Never put gasoline, naphtha or any light, quick-evaporating spirit into a lamp. Its vapour fills the tank and explodes. In the 1850s and 60s, lamps filled with cheap "burning fluid" (turpentine mixed with alcohol) and badly refined kerosene killed thousands of people. Never fill a lamp while it is lit or still hot.
- Burning fat or oil cannot be put out with water — the water sinks, boils instantly and sprays the burning fat everywhere. Smother it with a lid, a wet sack or sand.
- Hot wax and tallow cause deep burns. Melt them in a water bath, never in a pot directly over a high flame: fat heated well past its smoking point catches easily from any nearby flame (above roughly 300 °C) and bursts into flame on its own at about 400 °C.
- Bad air. Many lamps in a small, closed room use up oxygen and give off soot. Leave a vent.
What this unlocks
Light turns long nights into working time and makes Teaching and Schools and reading possible all year. Better candles came from purer fats: stearin (fat split with lime and acid, 1820s), spermaceti, and paraffin wax distilled from shale and crude oil (1850s; see Waxes: Beeswax, Plant Waxes and Paraffin). The chimney lamp led to the gas lamp (burning coal gas, see Lanterns, Gas Lamps and Lighters, Coal and Coke and Biogas and Wood Gas) and the brilliant limelight, and the search for something better still led to the electric arc lamp (Arc Lamps, Neon and Fluorescent Lights) and the The Light Bulb. The same capillary wick drives spirit lamps for Laboratory Glassware work.
How it was first done
People were burning fat in hollowed stones at least 40,000 years ago; over a hundred stone lamps have been found in the painted cave of Lascaux in France, about 17,000 years old. Clay oil lamps appear in Mesopotamia and Egypt by 4000–3000 BC, and the closed, mould-made lamp was produced by the million in the Greek and Roman world. Candles of tallow, dipped round a wick of papyrus or flax, were used by the Romans and Etruscans before 500 BC; in China, early candles used whale fat and later insect wax. Through the Middle Ages beeswax candles were a luxury for churches and the rich, while ordinary people burned smoky tallow dips and rushlights. In 1825–30 the self-trimming plaited wick and stearin candles made candles clean and easy; Argand's lamp (1780) and the kerosene lamp (developed by Ignacy Łukasiewicz and others in the 1850s, using lamp oil first made by Abraham Gesner) made bright light cheap — only a few decades before Edison's light bulb.
Source: content/entries/home/lamps-and-candles.md