Part 8 · Chemistry
Lye and Potash
How to turn the ash from your fire into lye — a strong alkali — and then into potash and caustic potash. Lye is the first chemical you can make, and it leads straight to soap, glass, paper and saltpeter.
- Difficulty
- ●●●●●
- Time
- Weeks to save the ash, a day to leach, a day to boil down
- Steps from zero
- 3 prerequisites →
The full path from nothing — 3 steps before this one
- Fire
- Finding and Preparing Clay
- Pottery
- Lye and Potash
Do them roughly in this order. See it on the tech tree →
Why it matters
Every fire you have ever made has left behind a chemical treasure: ash. Pour water through clean wood ash and what drips out is lye — a slippery, bitter, brown liquid that is one of the strongest substances you can make without any equipment. It is an alkali (the chemical opposite of an acid: it feels slippery, tastes bitter and neutralises acids).
With lye you can:
- boil it with fat to make Soap — the cheapest medicine there is;
- melt it with sand to make Glass (it lowers the melting point of sand by hundreds of degrees);
- cook plant fibres soft for Paper;
- turn the crude nitrate salts in old manure heaps into Saltpeter;
- clean grease from wool, cloth and pots, and soften maize for food (see Grain, Flour and Bread);
- feed crops: the potassium in potash is one of the three main plant nutrients (see Compost and Manure).
Boil lye dry and you get potash — the white salt that was, for centuries, one of the most traded chemicals in the world. The name itself comes from the method: ash leached in pots.
How it works
When wood burns, the carbon and hydrogen leave as smoke and gas. What stays behind is the mineral part of the plant: mostly calcium, with potassium, some magnesium, sodium and a little iron. In the heat these minerals combine with carbon dioxide to form carbonates. Calcium carbonate (the same substance as limestone) does not dissolve in water. Potassium carbonate does — very easily.
So when water trickles through ash, it carries the potassium carbonate out with it and leaves the rest behind. This is called leaching — dissolving out the useful part of a solid by letting water flow through it.
The lye you get this way is a solution of potassium carbonate. It is mildly caustic (caustic — able to burn and dissolve living tissue). It makes soft soap slowly and melts glass well. For stronger work you can make it far more caustic by stirring in slaked lime (calcium hydroxide, from Lime):
potassium carbonate + slaked lime → caustic potash (potassium hydroxide) + chalk
The chalk sinks to the bottom as a white mud; the clear liquid above is caustic lye, which turns fat into soap quickly and dissolves feathers, hair and skin.
How much to expect. Burning 100 kg of dry hardwood leaves only about 1 kg of ash (0.5–1.5 %). Good hardwood ash holds roughly 5–10 % of its weight in potash. So 100 kg of ash — about four large sacks, and the leftovers of a whole winter of fires — gives perhaps 5–10 kg of crude potash. This is why potash was precious, and why you should save every scrap of clean ash from now on.
What you need
| Item | Details |
|---|---|
| Wood ash | White or grey, fully burned, kept dry. 20–40 litres for a first batch |
| Leaching vessel | A wooden barrel, a large clay pot (20 litres or more), or a V-shaped wooden hopper — with a small hole near the bottom |
| Catch pot | Glazed clay or wood, placed under the hole |
| Filter | A double handful of fist-sized stones, a layer of pebbles or twigs, and a thick layer of clean straw or dry grass |
| Water | Rainwater is best (see below). About half the volume of the ash |
| Boiling pot | Iron if you have it, otherwise a thick clay pot. Lye slowly eats clay and glaze |
| Slaked lime (for caustic potash only) | From Lime, roughly 6 parts for every 10 parts of potash |
| Test items | A fresh egg or a small potato; a chicken feather |
| Stirring stick | Long — at least 60 cm (an arm's length) — so your hand stays far from splashes |
Rainwater, not hard water. Water from limestone springs and wells is "hard": it carries dissolved calcium which wastes some of your potash by turning it back into chalk. Rainwater or soft stream water from granite and sandstone country works best. If soap curdles in your water instead of lathering, it is hard.
Where to find it
- Which wood. Broad-leaved hardwoods give the most and the best ash. Historically prized: elm, maple, beech, hickory, ash (the tree), and oak. Bark, twigs and leaves are richer in minerals than the heartwood, so do not throw them away. Pine and other conifers give less.
- Other plants. Some non-woody plants are richer still. Bracken fern was cut and burned for glassmakers' potash all over northern Europe. Bean and pea stalks, sunflower stalks, wormwood and tobacco stalks are all good. Burn them in a heap on bare ground and collect the ash.
- Seaweed and salt-marsh plants (kelp, wrack, saltwort, glasswort) give ash rich in soda (sodium carbonate) instead of potash. It does much the same jobs and makes harder soap — see Soda Ash and Baking Soda.
- What good ash looks like. Fine, soft, pale grey to white, with no black lumps of charcoal (those are unburned carbon and do nothing). Ash from a hot fire is better than from a smouldering one. It must never have been rained on — rain is exactly a leaching barrel, and washes the potash away into the ground.
- Keep it dry. Store ash in a covered pot, a lidded basket lined with leaves, or a dry corner under a roof. Never store it in wood or near anything that burns until you are sure it is cold: ash can hide live embers for days.
Step by step
1. Build the leacher
- Make the outlet. Drill or burn a hole about 2 cm across in the side of the barrel or pot, as close to the bottom as you can. Plug it with a twist of straw or a wooden peg with a groove cut down its side, so liquid can seep out slowly.
- Raise it. Stand the vessel on stones or a stump so the catch pot fits underneath the hole. Tilt it very slightly towards the hole.
- Lay the filter. On the bottom put a layer of clean fist-sized stones (5 cm), then pebbles or a criss-cross of sticks (5 cm), then a thick pad of straw or dry grass (10–15 cm), pressed down. This holds the ash back while letting liquid through. (Optional: sprinkle two handfuls of slaked lime on the straw — it makes the lye a little more caustic on the way out.)
- Add the ash. Fill with ash to within 10 cm of the rim, tamping it down every few handfuls with a flat stick. Loose ash lets water rush straight through and you get weak lye. Press a shallow bowl-shaped hollow into the top.
2. Leach
- Wet it slowly. Pour water into the hollow a little at a time — hot water works faster than cold. The ash will drink a great deal before anything comes out: for a 100-litre barrel, expect to add 20–30 litres before the first drip. This can take several hours.
- Wait. Once the ash is soaked through, cover the top and let it stand overnight. The longer the water stays in contact with the ash, the stronger the lye.
- Collect. Pull the plug a little. The first runnings are clear amber to dark brown, like strong tea. Collect them. Keep topping up the water slowly.
- Re-run weak lye. As the ash is exhausted, the lye gets paler and weaker. Test each potful (below). Pour weak lye back through the barrel, or through a second barrel of fresh ash — this is the simplest way to make strong lye without wasting fuel on boiling.
- Finish. When the drips are nearly colourless and feel only slightly slippery between finger and thumb (wash your fingers at once), the ash is spent. Spread it on the garden; it still contains lime that sweetens sour soil.
3. Test the strength
Lye has no colour you can trust, so soapmakers used weight. Strong lye is heavier than water, and things float higher in it.
- Drop a fresh egg or a small potato into a cup of lye.
- Sinks — too weak. Boil it down or run it through fresh ash.
- Floats with a patch about 2–3 cm across showing (the size of a small coin) — right for soapmaking. This is the traditional "soap-strength" lye.
- Floats high, tipped on its side — very strong. Good for boiling down to potash; dilute with water for soap.
The feather test tells you something different — how caustic the lye is. Dip a chicken feather in for a few minutes. In plain ash lye it gets slimy and ragged slowly. In caustic lye (made with lime) the soft vanes dissolve away within minutes, leaving a bare shaft. Use caustic lye for hard soap, and plain lye for glass and saltpeter.
4. Boil down to potash
- Fill the boiling pot no more than two-thirds full with strong lye. Boil it outdoors over a steady fire, topping up with more lye as it shrinks. Ten litres of egg-floating lye gives very roughly 1 kg of salts.
- As it thickens it turns into a dark brown syrup. Lower the fire and stir constantly — this is when it spits. Stand back and use your long stick.
- Keep heating gently until it dries into a hard, dark brown crust. These are black salts — crude potash. Chip them out while still warm and store them in a sealed pot at once.
5. Calcine to pearlash
The brown colour is burned plant matter. To remove it, calcine the salts — bake them hot in air.
- Break the black salts into walnut-sized lumps and spread them in a shallow clay dish or on the floor of a The Kiln.
- Heat to a dull red glow — about 600–700 °C, a red you can see in shade but not in sunlight. Keep it there for 2–4 hours, stirring now and then with an iron or green-wood rake.
- Do not go hotter than a bright orange. Potash melts at about 890 °C, and molten potash eats through a clay dish (that is exactly why it is useful for glass).
- It is done when the lumps are white to pale bluish-grey all through when broken, with no black specks. This purer potash was sold as pearlash.
6. Make caustic potash (optional)
- Dissolve 1 kg of pearlash (or 1.2 kg of black salts) in about 10 litres of water in an iron or thick clay pot. Dilute lye converts better than strong.
- Separately, stir 600 g of slaked lime — or 450 g of quicklime carefully slaked in water first — into a thin "milk of lime".
- Bring the potash solution to the boil and pour in the milk of lime while stirring. Boil gently for 30–60 minutes.
- Check it is finished: take a spoonful, let it settle for a few minutes, and pour a little of the clear top into some vinegar. If it fizzes, there is still carbonate — add more milk of lime and boil again. When it no longer fizzes, the conversion is complete.
- Cover the pot tightly (the carbon dioxide in air slowly turns caustic lye back into carbonate) and let the white chalk settle overnight. Carefully pour or ladle off the clear liquid. That is caustic lye. You can boil it down to make it stronger, but it is far more dangerous to handle when strong.
How to tell it worked
- Slippery. A drop of lye rubbed between finger and thumb feels soapy — because it is turning the oils in your skin into soap. Wash it off immediately.
- Fizzes with acid. Plain lye and potash fizz strongly when vinegar is poured on them (the carbonate releasing carbon dioxide). Caustic lye does not fizz.
- Turns plant colours. Boil a handful of red cabbage, red onion skins or dark berries in water. The purple juice turns green to yellow in lye. (Acids turn it red.)
- Potash drinks water. Leave a lump of potash on a dish in damp weather: within a day it becomes wet and then dissolves into a puddle. Sand, lime and salt don't do that.
- Makes soap. Warm a spoonful of strong lye with a spoonful of fat, stirring for half an hour. It should thicken into a pale, soapy paste that lathers in water. See Soap.
Note Troubleshooting. Lye comes out almost at once and is weak → the ash is packed too loosely, or the water is channelling down the side. Tamp harder, pour more slowly, let it stand longer. Nothing comes out for a day → the plug or straw is clogged with fine ash. Poke a stick up through the hole, or rebuild with more straw. Lye is very weak even from fresh ash → the ash had been rained on, was mostly softwood, or held a lot of charcoal. Try ash from a hotter fire of broad-leaved wood. Pearlash stays grey or brown → not hot enough or not long enough. Calcine again, with more air. Pearlash melted into the dish → too hot. Break it out; it is still usable. Caustic lye keeps fizzing with vinegar → not enough lime, or the lime was old and had turned back to chalk. Use freshly burned lime.
Dangers
Danger Lye can blind you in seconds. A single splash of strong or caustic lye in the eye can destroy the cornea permanently — and unlike acid, alkali keeps soaking deeper into the eye after the first sting. Keep your face well away, shield your eyes with whatever you have (even a thin slatted wooden visor or a strip of cloth with slits helps), and always keep a large pot of clean water within reach before you start. If lye gets in an eye: hold the eye open and pour clean water across it, gently and continuously, for at least 20 minutes, and 30 minutes or more for strong or caustic lye, pouring from the nose side outward. Do not rub it, and never put vinegar in an eye.
Danger Lye looks like water or weak tea. Children and careless adults have died from drinking it. Keep it in a vessel nobody uses for food or drink, mark it clearly (scratch a sign into the clay, tie on a bundle of ash-grey straw — whatever your group agrees means poison), and keep it out of reach. If someone swallows lye, do not make them vomit; rinse the mouth, give a few sips of water or milk and nothing more, and watch the breathing closely: see Emergencies.
- Skin burns. Lye burns do not hurt at first; you feel slipperiness, then stinging. Brush off any dry potash first, then rinse with lots of water for at least 20 minutes (Emergencies). Use water only: do not put vinegar or other acid on the burn.
- Boiling lye spits. Thick boiling lye and molten potash throw droplets far. Wear leather or thick cloth on your arms and hands, stir with a long stick, and never lean over the pot.
- Hot slaking. Quicklime added to water gets hot enough to boil and spatter. Add it slowly and stand back.
- Wrong containers. Lye eats aluminium and zinc, making a flammable gas, and slowly attacks clay, glaze and glass. Store it in iron, thick unglazed stoneware, or well-seasoned wood, with a lid.
What this unlocks
- Soap — the very next step: lye plus fat.
- Glass — potash melted with sand and a little Lime makes "forest glass", the green glass of medieval Europe.
- Saltpeter — potash converts the nitrates leached from old manure heaps into saltpeter.
- Paper — fibres cooked in lye break down into pulp.
- Dyes and Mordants — lye and potash shift dye colours and scour wool clean so dyes take evenly.
- Glazes — wood ash itself, mixed with clay, makes the oldest stoneware glazes in Asia.
- Soda Ash and Baking Soda — the sodium version of potash, from seaweed ash or, later, from salt.
How it was first done
People have used ash and water to clean things since prehistory; a Babylonian clay tablet of about 2200 BC already gives a recipe for soap made from oil and plant-ash alkali. Glassmakers in Mesopotamia and Egypt used plant ash as their flux, and medieval European "forest glass" was made in workshops deep in the woods precisely because of the huge amounts of wood ash they needed.
Potash became big business in the 1600s–1800s. Russia, Scandinavia and then North America burned whole forests to supply Europe's soapmakers, glassmakers and bleachers. Settlers clearing land in New England and Canada burned the felled trees, leached the ash and boiled it in great iron kettles — for many families, potash was their first cash crop. The very first patent of the United States, signed by George Washington in 1790, was granted to Samuel Hopkins for an improved way of making potash and pearlash. The trade faded only after the 1860s, when potassium salts began to be mined from deep deposits in Germany.
Source: content/entries/chemistry/lye.md