Part 15 · Knowledge and Science
Screen Printing
Stretch fine silk on a wooden frame, block the mesh everywhere except the picture, and pull ink through it with a rubber blade. Screen printing puts thick, bright colour on paper, cloth, wood, metal, glass and pottery — posters, signs, labels, flags, instrument dials and patterned cloth — with no press and only a few hours' preparation.
- Difficulty
- ●●●●●
- Time
- A day to build a screen, squeegee and bench; an hour to a day to make a stencil; then a print every 20–30 seconds
- Steps from zero
- 12 prerequisites →
This unlocks
—The full path from nothing — 12 steps before this one
- Fire
- Stone Tools
- Finding and Preparing Clay
- Basic Woodworking
- Pottery
- Charcoal
- Farming from Seed
- Silk
- Lye and Potash
- Ink
- Paper
- Printing
- Screen Printing
Do them roughly in this order. See it on the tech tree →
Why it matters
A wooden printing press (Printing) is the right tool for books: thousands of identical pages of black type on flat paper. Many jobs are different. A village needs 40 posters for a vaccination day (Vaccination), a hundred labels for jars of medicine, a pattern printed down 20 metres of cloth, the scale on a The Thermometer, the name on a glass bottle, a sign on a tin box, or a warning on a metal door. These need thick, bright, opaque colour — often on surfaces that are rough, curved or cannot go under a press.
Screen printing does all of these with a wooden frame, a piece of silk, a rubber blade and a stencil. It needs no type and no press. A single worker can set it up in a day and print two or three copies a minute. The ink film it leaves is ten times thicker than a letterpress print, so white prints solidly on black, colours stay bright, and the same method can lay a glass enamel on a bottle or a protective resist on a copper plate.
How it works
A screen is a fine, even mesh stretched tight on a frame. On its own it lets ink through everywhere. A stencil blocks the mesh except where you want ink.
- The screen sits a few millimetres above the paper — the off-contact gap.
- A pool of ink lies on top of the mesh at one end.
- A squeegee — a straight rubber blade — is pulled across. It presses the mesh down onto the paper in a moving line and shears the ink through the open holes.
- Behind the blade, the stretched mesh springs back up, peeling cleanly away and leaving a sharp film of ink on the paper.
The stencil can be cut paper, painted glue, cut film, or a light-hardened layer made by photography; each is described below. The finer the mesh, the finer the detail and the thinner the ink film.
What you need
| Item | Notes |
|---|---|
| Fine, even silk cloth | Plain or gauze weave, 50–70 threads per cm for paper. Silk, The Loom |
| Softwood battens, 3 × 4 cm | For frames. Basic Woodworking |
| Soft vulcanised rubber strip, 8–10 mm thick | Squeegee blade. Rubber |
| Flat board, hinges or pins, card | Printing bench |
| Hide glue, shellac, beeswax, tallow, soap, lampblack | Stencil fillers and resists. Glues and Adhesives, Pigments, Paints and Varnish |
| Gelatin and potassium dichromate | Photographic stencils (optional) |
| Linseed oil varnish, pigments, turpentine | Oil inks. Pigments, Paints and Varnish, Ether, Acetone and Solvents |
| Alum, madder, starch | Printing on cloth. Dyes and Mordants |
| Powdered coloured glass, a kiln | Printing on glass and pottery. Enamel on Metal, The Kiln |
The printing screen
Mesh
The best natural mesh is silk bolting cloth — the fine, even cloth millers use to sift flour (The Watermill). Silk is strong, springy and smooth, and each thread is round and even. Weave it as gauze (leno weave), in which pairs of warp threads twist round each weft thread and lock it in place, so the holes cannot slide out of square (The Loom). A tight plain weave of fine, hard-twisted silk also works. Fine cotton organdy works for a few dozen prints; fine bronze or steel wire cloth for very long runs.
| Mesh (threads per cm) | Use |
|---|---|
| 30–45 | Cloth — a heavy ink film soaks into the fibres |
| 50–70 | Posters, signs and labels on paper, wood and metal |
| 90–120 | Fine lines and small type; glass and pottery enamels |
Count threads with a magnifying glass (Lenses) over a 1 cm mark. A good cloth has every hole the same size and no thick or thin threads.
Frame
- Wood: straight, dry softwood 3 × 4 cm, corners half-lapped, glued and pegged or screwed (Doors, Windows and Joinery). The frame must lie flat on a table without rocking.
- Size: inside the frame, leave 10 cm beyond the image at each squeegee end (for the pool of ink) and 6–8 cm at each side. A 30 × 40 cm poster needs a frame about 45 × 60 cm inside.
- Seal the wood with two coats of shellac or oil varnish, so it does not swell when washed.
Stretching
The mesh must be drum-tight and even, or prints blur and the stencil shifts.
- Saw a groove 3 mm wide and 6 mm deep all round the top face of the frame, 1 cm in from the inside edge.
- Wet the silk so it is limp, and lay it over the frame with the threads square to the sides and 5 cm extra all round.
- With a blunt chisel, press a 3 mm cord into the groove over the cloth. Start at the middle of one long side, then the middle of the opposite side, then the two short sides; work outwards towards the corners, a few centimetres at a time on each side in turn. The cord drags the cloth into the groove and stretches it.
- Let it dry. Silk shrinks as it dries and tightens further.
Without a groove, pull the wet cloth tight and tack or staple it to the outside of the frame every 2–3 cm, again working from the middles outwards.
Test: flicked with a fingernail, the mesh sounds like a drum. Pressed hard in the middle with a finger, it gives only 3–5 mm and springs straight back. Loose mesh must be re-stretched.
Prepare a new screen by washing it gently with soap and warm water and rinsing well. Never use strong lye: it dissolves silk. Then glue a strip of gummed paper tape (Envelopes, Stamps, Clips and Office Supplies) round the inside edges where mesh meets frame, and coat the tape with shellac, so ink cannot creep under the frame.
The squeegee
The squeegee is a straight rubber blade in a wooden handle.
| Part | Size |
|---|---|
| Blade | Soft vulcanised rubber, 8–10 mm thick, standing 25–30 mm out of the handle |
| Handle | Hardwood 3 × 8 cm, with a slot that grips the blade tightly; glue and a row of small screws |
| Length | The image width plus 2–3 cm at each end, and at least 4 cm shorter than the inside of the frame |
- Mix a firm soft rubber — 100 rubber, 6–8 sulfur, 3 lime, 30 chalk — roll it into a flat sheet between boards with 9 mm spacer strips, and cure it flat (Rubber).
- Cut a strip with a long, wet knife and fit it in the handle.
- Sharpen the edge square: glue coarse sandpaper (Abrasives and Grinding Stones) to a flat board and rub the blade along it, held exactly upright, until the edge is straight and crisp.
A thumbnail should dent the rubber slightly but not deeply. Too soft a blade bends and floods ink; too hard a blade skips. Before rubber, a strip of stiff leather in a wooden handle works, less evenly. Good or bad: a sharp, straight edge prints crisp lines; a rounded or nicked edge prints thick, blurred lines or streaks — re-sharpen it.
The screen-printing bench
- Base: a flat board — glued-up planks planed true, or laminated board — at least 10 cm bigger than the frame all round. It must be flat within about 1 mm.
- Hinge clamps: two hinges screwed to the back of the base, each with a clamp block that grips the frame's back rail, so the frame lifts and lowers in exactly the same place every time. Removable hinge pins let you swap screens.
- Kick leg: a short stick hinged to the side of the frame that drops down to hold it open while you change the paper.
- Off-contact: strips of card 2–4 mm thick under the front corners of the frame, so the mesh only touches the paper under the squeegee.
- Registration guides: three small L-shaped tabs of card glued to the base — two along the bottom edge of the paper, one along the side. Every sheet is pushed against all three, so every print lands in the same place.
For cloth, cover the bench with a layer of felt or blanket under a sheet of oilcloth, and pin the cloth flat. For long lengths, use a long padded table with a rail along one edge and stops spaced at the length of the pattern; the frame is moved from stop to stop, printing every other repeat first and coming back for the gaps once they are dry.
Making the stencil
Method 1: Cut paper
The quickest stencil, good for 20–100 prints of bold shapes.
- Draw the design on thin, strong paper — waxed or oiled paper is best.
- Cut out the parts that should print with a sharp knife.
- Lay the paper on the printing base, lower the screen onto it, and pull the first print. The wet ink glues the paper to the underside of the mesh, and it stays there.
Unlike a cut stencil used on its own, the "islands" — the middle of an O or an A — need no bridges: the ink holds them to the mesh.
Method 2: Block-out
Paint the parts that should not print directly onto the mesh with a filler, using a brush.
- For oil inks, use a water-soluble filler: thin hide glue (1 part glue to 2 parts water, with a little glycerine). Remove it afterwards with warm water.
- For water inks, use shellac in alcohol or oil varnish. Remove it with alcohol or turpentine.
Give two thin coats, the second from the other side. Hold the screen up to the light and touch out every pinhole.
Method 3: Tusche and glue (a drawn resist)
This prints a free drawing with all its brush marks and crayon texture.
- Make tusche, a greasy drawing medium: melt 4 parts beeswax, 2 parts tallow and 2 parts hard soap, stir in 1 part lampblack, and pour into sticks — or thin it with turpentine for a brush.
- Draw the image directly on the mesh, laid over your sketch.
- Squeegee a thin, even coat of hide-glue filler over the whole screen and let it dry. The glue will not stick to the grease.
- Scrub both sides of the drawing gently with a rag and turpentine. The tusche dissolves and lifts the glue above it; everywhere else the glue stays.
The open mesh is now exactly your drawing.
Method 4: Cut film
Hard-edged and lasting for 1,000 prints or more.
- Brush thin, smooth paper with three coats of shellac, drying between coats.
- Lay it over the design, shellac up. Cut through the shellac layer only — not the paper — around each part that should print, and peel those parts away.
- Lay the film under the screen, shellac against the mesh. Dab through the mesh with a rag barely damp with alcohol, a small area at a time (or press with a warm iron through a sheet of paper). The shellac softens and grips the mesh.
- When dry, peel the backing paper off.
Method 5: Photographic stencil
Light makes gelatin mixed with a dichromate salt hard and insoluble. Where light is blocked by the black lines of a drawing, it stays soft and washes away. This gives the finest detail — small type, thin rulings, even photographs broken into dots.
- Make the positive: draw or letter the design in dense black ink on tracing paper (Technical Drawing). It must be truly opaque: hold it to the sky and look for grey lines.
- Mix the coating in dim light: soak 10 g gelatin (the clearest hide glue, Glues and Adhesives) in 100 ml water, melt at about 40 °C, and stir in 1–1.5 g potassium or ammonium dichromate dissolved in 10 ml water. Use it the same day.
- Coat both sides of the screen thinly and evenly, drawing it across with the edge of a straight strip of glass or card. Dry flat in the dark — an hour or two in a warm, dry room.
- Expose: lay the positive, ink side against the mesh on the print side, press it flat under a sheet of glass, with a dark pad behind the screen. Expose to bright sun for 1–4 minutes (find the time with a test strip, as in Photography).
- Wash out with water at about 35–40 °C, sprayed or splashed gently on both sides. The image opens up; the rest stays as a tough, brown, leathery film.
- Dry, look through it against the light, and touch out flaws with block-out.
Later, strip the gelatin off with hot water and a little chlorine bleach (Chlorine and Bleach) to reuse the mesh.
The dichromate is obtained by trade or from a chromate works, which makes it from chromite — heavy black grains found in dark serpentine rock — roasted with potash and saltpeter to yellow potassium chromate, which turns into orange dichromate when acidified with Sulfuric Acid (see Chromium and Its Compounds). It is poisonous; see Dangers.
Inks
Screen inks are thicker than writing ink, about like runny honey: thick enough not to seep through the mesh on their own, thin enough to flow under the blade.
- Oil ink — paper, wood, metal, glass (unfired): grind pigment into boiled linseed oil or oil varnish (Pigments, Paints and Varnish) on a slab with a muller, about 1 part pigment to 1–2 parts varnish, then thin with turpentine. A little chalk or white clay makes it go further and print more transparently. Prints dry in 6–24 hours.
- Water ink — paper: pigment with gum arabic or starch paste. It dries in minutes, so it can clog the screen — print quickly and keep the mesh flooded.
- Cloth: print a mordant paste — 1 part alum stirred into 4 parts thick starch or gum paste, coloured with a little red ochre so you can see it. Let the prints dry for two days, rinse, and dye the cloth in a madder or other mordant dye bath (Dyes and Mordants): the colour fixes only where the paste was printed. Pigment in linseed varnish also prints on cloth and survives washing, but stiffens it.
- Glass and pottery: grind a coloured, low-melting glass (an enamel, Enamel on Metal) to a fine flour and mix it with a fat oil — linseed oil thickened with pine resin — to a smooth paste. Print with a fine mesh, dry, and fire: about 580–620 °C on glass (Glass) and 750–850 °C over a glaze on pottery (Glazes). Curved objects are printed by transfer: print onto paper coated with gum, varnish over the print, soak the film off in water and slide it on.
Step by step: printing
- Set up. Clamp the screen in the hinges, put the off-contact strips in place, and fix the registration guides so the image sits where you want it on the sheet. Tape a few sheets of scrap paper ready.
- Ink. Spoon a line of ink along the near (or far) end of the screen, outside the image, about a finger thick.
- Flood. With the screen lifted on its kick leg, draw the squeegee lightly across, pulling a thin layer of ink over the whole image without pressing it through. This keeps the mesh full and stops it drying.
- Place a sheet against the registration guides and lower the screen.
- Print. Hold the squeegee in both hands, tilted forward at about 70° (60–75°), and pull it across the screen in one steady stroke with firm, even pressure. For cloth, pull twice.
- Lift the screen, flood again, and take the print out by its edges.
- Rack it to dry (below). Check every tenth print for smudges, filling-in and pinholes.
- Clean up the moment you stop: scrape the ink back into its pot, then wash the screen with turpentine (oil ink) or water (water ink) and rags, from both sides, until no colour shows against the light. Ink left to dry in the mesh can ruin a screen.
Several colours
Use one screen for each colour. Print the lightest colour first, let it dry, then each darker one. Put small registration crosses outside the image on every stencil and line them up. Let colours overlap by about 1 mm so no white gaps show if a sheet shifts.
The print drying rack
Wet prints need room. A print drying rack holds 20–40 prints flat without touching:
- Simplest: lines of cord across the room with clothes pegs, for paper and cloth that can hang.
- Better: two wooden uprights 120–150 cm tall with a stack of shelves 5 cm apart, each a light wooden frame strung with a net of cord or thin wire. Each shelf hinges at the back and is held up by a stop. Start with all shelves up; drop the bottom one, lay a print on it, drop the next, and so on to the top.
How to tell it worked
- Edges: look at a printed letter through a magnifier. Edges are sharp, not furry or jagged; counters (the middles of e, a, o) are open.
- Solid areas are even, with no pinholes, streaks or "mesh marks" (a faint grid pattern).
- Registration: 20 sheets stacked and held to the light show the image in the same place, within about 1 mm.
- Durability: after a day, oil prints do not smudge under a rubbing thumb; printed cloth survives five washes; fired enamel does not scratch off with a knife point.
Note Troubleshooting. Blurred or doubled edges → mesh too loose, or no off-contact so the screen sticks and smears; re-stretch, add card strips. Ink bleeds under the stencil → ink too thin, or too much squeegee pressure; thicken with pigment or chalk. Parts of the image don't print → ink drying in the mesh; flood after every print, work faster, add a drop of slow-drying oil. Mesh pattern visible → too little ink or too coarse a mesh; flood more, use finer mesh, or a softer blade. Photo stencil washes away entirely → under-exposed or coating too old; nothing washes out → over-exposed or fogged by light while drying. Pinholes print as dots → touch out with block-out from the ink side.
Dangers
- Turpentine and other solvents catch fire easily and their fumes cause headaches and dizziness. Work in a draught, keep flames away, and store oily rags in a closed metal tin or spread out flat outdoors: rags soaked in linseed oil can heat up and burst into flame on their own if left in a pile.
- Pigments: never use lead white, red lead, chrome yellow or vermilion for textiles, toys, food containers or anything children handle. Glass enamels often contain lead; do not print or fire them on food or drink surfaces.
- Kilns for firing enamels: see The Kiln.
Danger Dichromates are poisonous and cause cancer. Potassium and ammonium dichromate burn and ulcerate the skin, cause lasting skin allergies, and are deadly if swallowed; their dust causes lung cancer. Weigh them wearing gloves, never breathe the dust, keep them locked away from food and children, and wash everything they touch. Never pour dichromate solutions on soil or into water: collect them and turn them harmless by stirring in iron filings and a little acid until the orange colour turns green, then let the green sludge settle and bury it. Ammonium dichromate also burns fiercely if heated dry. Where you can, use cut-film or tusche stencils instead.
What this unlocks
Screen printing labels the products of every workshop — bottles, tins and boxes (Tins, Cans, Drums and Tanks, Sacks, Boxes, Crates and Packaging) — prints scales and dials for instruments (Scientific Instrument Making, The Thermometer), posters and notices for the community, maps on cloth (Maps and Mapmaking), flags and patterned fabrics, and road and railway signs. A screen-printed layer of acid-proof resist on copper-faced board is a quick way to make printed circuits (Building Circuits: Boards, Connectors and Cables), and the light-hardened gelatin stencil is the same idea as the photoresist used to make Integrated Circuits. With Photography, halftone stencils print pictures.
How it was first done
Stencils for printing on cloth are very old in China and Japan. Japanese dyers by the 18th century cut katagami stencils from layers of paper glued together with persimmon juice, and held their loose parts in place with a fine grid of silk threads or human hair between the layers — a direct ancestor of the screen. In 1907 Samuel Simon of Manchester patented printing through silk stretched on a frame, and in the United States around 1914–1918 John Pilsworth of San Francisco developed multicolour printing from one screen. Photographic stencils of light-hardened gelatin followed in the 1910s–1920s, and in 1929 Louis D'Autremont patented a knife-cut film stencil. In the 1930s artists in the United States took up the method for posters and fine prints, which came to be called serigraphs, and in the 1960s Andy Warhol made screen-printed photographs famous. Industry adopted it everywhere: on textiles, bottles, signs, circuit boards and the dials of instruments.
Source: content/entries/knowledge/screen-printing.md