◆ Rebuild

Part 2 · Earth and Fire

The Potter's Wheel

A heavy spinning wheel lets one potter make fifty matching cups a day with walls half as thick as hand-built ones. How to build a stick wheel and a kick wheel, then centre, open, pull, shape, trim, add handles and spouts, and throw matching sets — and what changes with an electric wheel.

Difficulty
●●●●●
Time
Two to four days to build a kick wheel; a month of daily practice to centre and throw a decent cup
Steps from zero
16 prerequisites →

You need first

PotteryBearings and Lubrication

This unlocks

Slip Casting, Jiggering and Ceramic Factories
The full path from nothing — 16 steps before this one
  1. Fire
  2. Stone Tools
  3. Cordage and Rope
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Basic Woodworking
  7. Hunting and Trapping
  8. Pottery
  9. Charcoal
  10. Hides and Leather
  11. The Wheel and Axle
  12. Bellows
  13. The Lathe
  14. Copper Smelting
  15. Bronze
  16. Bearings and Lubrication
  17. The Potter's Wheel

Do them roughly in this order. See it on the tech tree →

Why it matters

A hand-built pot (Pottery) takes an hour or more and comes out a little different every time. On a wheel, a practised thrower makes a mug in three minutes, with walls 5 mm thick instead of 10, and the hundredth mug matches the first. That is the difference between a household making its own pots and a workshop supplying a village with cups, bowls, storage jars, drain pipes (Tiles and Clay Pipes), crucibles (Firebrick and Refractories), oil lamps (Lamps and Candles) and chemists' dishes (Burners, Stands and Laboratory Equipment).

Round, even walls dry evenly, crack less and take Glazes evenly. Lids fit because they can be measured. Fine stoneware and porcelain is almost impossible without a wheel.

How it works

The wheel turns the clay so your hands can stay still. A hand held steady against spinning clay touches every point of a circle, so whatever it does — squeeze, lift, push out — it does evenly all the way round.

To keep turning while both hands are busy, a wheel needs a heavy flywheel. The energy it stores grows with its weight and with the square of its speed and radius, so weight at the rim counts far more than weight near the hub. An 80 kg concrete flywheel 80 cm across, kicked to two turns a second, keeps throwing speed for half a minute between kicks; a light wooden disc stops as soon as your hands press on the clay.

Too slow and the hands drag the clay round; too fast and wet walls fling outward and collapse.

Job Turns a minute How it feels
Centring 120–200 Fast; the clay is a blur
Opening and first pull 80–120 Brisk
Later pulls, shaping 50–90 Calm; you can see a mark go round
Finishing a rim, wiring off 30–50 Slow
Trimming 100–150 Fast

The bearings carry two loads: the weight of the wheel pushing down (a footstep at the bottom of the shaft) and the side-push of your hands (a collar near the top). See Bearings and Lubrication.

What you need

Item Size Made from
Throwing clay 5–20 kg to practise Fine, plastic clay (Finding and Preparing Clay), sieved
Flywheel 70–90 cm across, 50–100 kg Concrete, a stone slab, or wood loaded with stone or iron
Shaft 2.5–3 cm iron, or 7–8 cm hardwood; 60–70 cm long Iron (Blacksmithing) or oak
Wheelhead 30–35 cm across, 3–4 cm thick Hardwood, cast iron or concrete
Footstep bearing Hard cup 3–4 cm across Bronze, hardened steel, or a hard pebble with a drilled cup
Collar bearing Split hardwood block or bronze bush Bearings and Lubrication
Frame and seat Posts 8 × 8 cm, plank seat Oak or any sound timber (Doors, Windows and Joinery)
Bats Boards 25–35 cm across Wood, fired clay, or plaster (Gypsum and Plaster of Paris)
Small tools See below Wood, bone, steel strip, wire, sponge

Where to find it

  • Throwing clay must be more plastic than hand-building clay. Roll a pencil-thick coil and wrap it round your finger: it should bend without cracking. Short, sandy clay tears on the wheel; add a quarter to a third of a fatter clay, or settle it again and keep the finest part (Finding and Preparing Clay). Any temper must be fine — sand through a cloth sieve, or grog under 0.5 mm, at 10–20 % — or it tears fingers and walls.
  • The flywheel. Concrete (Mortar and Concrete) cast in a ring of sheet iron or boards is easiest. Otherwise a flat slab of sandstone or limestone pecked round (Quarrying and Cutting Stone), or a solid wooden disc with stones or iron set into its rim.
  • Bearings — hard pebbles (flint, quartzite) for a footstep cup, dense hardwood for collars (Rocks and Minerals).

Method 1: The stick wheel

The simplest fast wheel, used for thousands of years in India, China and Japan, needs no frame and no iron: a heavy wheel lying flat near the ground, spun by a stick, which then coasts while you throw.

  1. Set the pivot. Drive a hardwood post 10 cm thick into the ground until 15–20 cm stands up. Round its top to a blunt point and grease it. A hard stone with a domed top, set in clay, is better.
  2. Make the wheel 90–110 cm across: a hardwood hub 15 cm thick, six or eight spokes, and a rim of bent wood or bamboo (The Wheel and Axle). Plaster the rim with clay mixed with chopped straw or hair, about 10 cm thick, until the wheel weighs 40–60 kg, most of it in the rim.
  3. Fit the socket. Set a hard stone or bronze cup 3 cm across into the underside of the hub, to sit on the pivot. Cover the hub with a flat board 30 cm across to throw on.
  4. Balance it. Spin it slowly; add clay to the rim opposite any side that dips.
  5. Spin it. Put a stick 1–1.2 m long in a thumb-sized notch in the rim and sweep it round for 15–20 seconds. A good heavy wheel keeps working speed for one to three minutes.

Because you must stop to re-spin, throw small pieces off the hump: centre a lump of 3–5 kg, centre only the fist-sized top, throw a cup or lamp from it, cut it off with a wire, and move on. Indian village potters throw hundreds of small pots a day like this.

Method 2: The kick wheel

A kick wheel is a seat, a frame, an upright shaft, a heavy flywheel at foot level and a wheelhead at the top. You kick the flywheel to keep it going and both hands stay on the clay.

KICK WHEEL (SECTION) STICK WHEEL Wheelhead 30–35 cm, true to 1 mm Splash tray catches slurry Seat 10 cm above the head Collar takes the side push Shaft iron, 2.5–3 cm Flywheel 80 cm concrete, ~90 kg Footstep bearing rounded shaft in a hard cup Kick push the rim away Spin with a stick in a notch in the rim Hump of clay one pot from the top Clay-loaded rim 1 m, 40–60 kg Pivot post greased point in a cup under the hub
Fig. 1 A kick wheel in section. The potter sits on the seat and pushes the flywheel round with one foot. The upright shaft turns in a footstep bearing at the bottom and a collar bearing just below the wheelhead; a splash tray catches slurry. Right: the simpler stick wheel.
  1. Frame. A rectangle of heavy timber on the floor about 100 × 70 cm, with two posts at the front carrying a cross-rail for the collar bearing. Brace it with diagonals — a wobbly frame makes a wobbling pot. At the back, a plank seat about 10 cm higher than the wheelhead and 20–30 cm behind it, so you lean over the clay with forearms braced on your thighs. Peg the frame to the floor or weigh it down.
  2. Footstep. In an oak block on the base, set a bronze cup, a hardened steel cup or a drilled hard pebble. Grease it with tallow and a little graphite.
  3. Shaft. Iron, 2.5–3 cm thick and 60–70 cm long, its foot rounded to a blunt cone that sits in the footstep, its top squared to take the wheelhead.
  4. Flywheel. Cast a concrete disc 80 cm across and 8 cm thick (about 90 kg) round an iron hub plate that fits the shaft tightly, 8–12 cm above the floor. Turn the shaft with a stick held near the rim: the gap must stay even. Pack or re-cast until it does.
  5. Collar. A split hardwood block or bronze bush on the cross-rail, 5 cm below the wheelhead, snug but free. Oil it daily.
  6. Wheelhead. A disc of hardwood 30–35 cm across, two layers glued with the grain crossed, fixed 55–60 cm above the floor. Once the wheel turns, true its face with a sharp chisel held on a rest, like a The Lathe. It must not wobble more than 1 mm.
  7. Splash tray. A shallow tray of wood or fired clay round the head, rim 5–8 cm above it, keeps slurry out of the bearings.

Kicking. Push the near side of the flywheel away with the ball of your foot in smooth strokes. Most potters spin anticlockwise seen from above; Japanese potters traditionally spin clockwise. Pick one and keep it.

A treadle wheel replaces the kick with a crank on the shaft and a foot pedal joined to it by a rod (Cranks, Cams and Linkages): a steadier speed, more ironwork.

The small tools

Throwing rib

A thin, stiff blade held against the outside of the wall to smooth, compress and shape it. Cut a kidney shape 8–10 cm long and 3–5 mm thick from hardwood, bone, slate or sheet iron, and round and polish every edge. A good rib leaves the wall glassy; a rough edge drags lines into the clay.

Cutting wire

A wire 40–50 cm long with a wooden toggle at each end, for cutting pots off the wheel and clay from the block. Twist two strands of fine iron or brass wire (Iron and Brass Wire): the twist lets air under the pot so it does not stick. Linen thread or horsehair works without wire.

Trimming tool

A loop of steel strip for shaving leather-hard clay. Bend a strip of spring steel or barrel hoop 6–10 mm wide and about 1 mm thick into a loop 2–3 cm across — round, square or triangular — file its outer edge sharp, bind both ends into a wooden handle 12–15 cm long, and temper it to blue (Steel). A sharpened bamboo strip bent over a flame also works. A good one takes off long clean ribbons; a dull one chatters.

Other tools

A needle tool (a stout needle in a handle) for checking floors and trimming rims; a sponge on a stick for tall pots; calipers of two pinned wooden arms for lids; a gauge — a pointer on a sliding stand — for repeat sizes.

Throwing bat

A removable flat board fixed to the wheelhead, so a wide or floppy pot can be lifted off without being touched. Make it of wood (two layers, grain crossed, oiled), fired clay 2 cm thick, or best of plaster, which drinks water from the base so the pot releases itself. Fix it on a 1 cm pad of soft clay ridged with the fingertips, pressing the damp bat down hard; or with two iron pins in the wheelhead fitting holes in the bat. Throw every plate and large bowl on a bat.

Step by step: throwing a mug

1 Centre cone up, press down, hold till no wobble 2 Open thumbs in the centre, compress the floor 3 Pull fingers in and out, rise together, slowly 4 Shape push out from inside; collar in at the neck 5 Wire off bevel the foot, pull the wire under it floor 8–10 mm walls 5–6 mm wheel slow
Fig. 2 The stages of throwing, in section. Centre the clay; open it, leaving a floor 8–10 mm thick; pull the wall up between fingers inside and out; shape it; undercut and wire it off.
  1. Prepare. Wedge the clay (Finding and Preparing Clay) a little softer than for hand-building: it takes a deep thumbprint but does not stick to a dry palm. Weigh 450–500 g and pat it into a ball.
  2. Fix it. Slap it down in the middle of a clean, dry wheelhead. Wet it.
  3. Centre. Wheel fast. Lock your elbows on your thighs; your arms must not move with the clay. Squeeze it up into a tall cone, then press the cone down with the heel of one hand while the other steadies it, two or three times. Then hold both hands still until there is no wobble at all — it feels like a smooth stone spinning under your palms. Most failures start here: if it is not centred, do it again.
  4. Open. Push your thumbs straight down the exact centre. Stop when the floor is 8–10 mm thick — check by pushing the needle tool to the wheelhead and pinching it at the surface. Draw the opening out to the inside width, and press the floor down hard to compress it; uncompressed floors crack in an S.
  5. Pull. Slow the wheel. Fingertips of one hand inside at the bottom, knuckle of the other outside opposite them. Squeeze until you feel the clay between them, and lift both hands slowly and together — about a finger's width each turn. Ease off at the rim. Two or three pulls, each thinner and taller, to walls 5–6 mm thick top to bottom. Lubricate with slip, not running water; a pot sitting in a puddle goes soft at the base.
  6. Shape. Run the rib up the outside with fingers inside. If the top flares, collar it: ring it with both hands and squeeze gently inward.
  7. Rim. At a slow speed, hold a fold of damp leather lightly over the rim to round and compress it — cracks start at the rim. Trim an uneven rim by holding the needle tool against it as it turns.
  8. Off. Sponge out the floor, bevel the foot with a wooden tool, and pull the taut wire under the pot as the wheel turns slowly. Lift it with dry hands, or slide it onto a wet board.
  9. Cut your first twenty pots in half top to bottom with the wire. The section shows exactly where the wall is thick or thin. Throw them back in the slop bucket.

Shrinkage. Clay shrinks 8–15 % from wet to fired. Draw a 10 cm line on a wet slab, fire it and measure; throw everything that much larger.

Pot Clay Thrown size (wet)
Small cup 300 g 7–8 cm across, 8 cm tall
Mug 450–500 g 9 cm across, 11 cm tall
Bowl 1 kg 18 cm across, 8 cm deep
Dinner plate 1.8–2 kg 30 cm across, on a bat
Teapot body 1 kg 13 cm across, 12 cm tall
Storage jar 3–5 kg 25–35 cm tall; taller ones in two parts, joined

Trimming the foot

TRIMMING A BOWL (SECTION) THROWING TOOLS Wads of soft clay hold the rim down Foot ring 5–6 mm wide, 5–8 mm high Clay removed the thick thrown base Loop tool braced on your hand base as thick as the wall Rib wood, bone or iron, 8–10 cm Cutting wire twisted, 40–50 cm Trimming tools loops of steel strip sharpened outside Needle tool Bat on a pad of soft clay over the wheelhead
Fig. 3 Trimming. A leather-hard bowl is turned upside down on the wheelhead, centred, held with three wads of soft clay and shaved with a loop tool until the base is as thick as the wall and stands on a foot ring.

A thrown pot is always thick at the base. When it is leather-hard — stiff enough to handle without bending, cool to the touch, cut cleanly by a fingernail, usually after half a day to a day under cloth — trim it.

  1. Turn it upside down on a damp wheelhead. Centre it: spin slowly and tap the pot towards the middle as its high side comes round, until a pencil held near it draws an even circle.
  2. Hold it down with three wads of soft clay against the rim.
  3. Wheel fast. Brace the trimming tool on your other hand and shave the base flat, then the outside to follow the inside curve. Tap it: a dull thud means thick; a hollow ring means close to wall thickness.
  4. For a foot ring, leave a ring 5–6 mm wide and 5–8 mm high, set in about a sixth of the pot's width from the edge, and hollow inside it to the wall thickness.
  5. Narrow-necked pots go into a chuck: a thick leather-hard thrown cup on the wheelhead into which the neck fits.

Handles and spouts

Pulled handles. Wet your hand and pull down a carrot of clay (about 100 g for a mug) with long, gentle milking strokes into a strap 1.5–2 cm wide, thinning evenly. Let it stiffen a little, cut it to length, and join it to the leather-hard pot: score both surfaces criss-cross, paint on thick slip, press, and smooth the joint. Leave room for three fingers.

Lips. Wet the rim and stroke it between two fingers of one hand while a finger of the other pulls the lip out and down. A sharp lower edge stops dribbling.

Spouts. Throw a hollow cone off the hump, 10 cm tall, tapering from 4 cm to 1.5 cm. At leather-hard, cut its base to fit the pot. Pierce holes 3–5 mm across in the body behind it; their total area must be larger than the spout's narrowest point. Score, slip and join. The spout tip must be higher than the brim, or the pot spills before it is full. Cut the tip with a sharp bevel so it does not drip.

Lids. Throw the pot with a gallery — a ledge inside the rim — measure it with calipers, and throw the lid to that size from the same clay at the same time, so both shrink together. Fire them together.

Throwing sets

  • Weigh each ball (Balances, Steelyards and Weighing Machines): same clay, same weight.
  • Gauge: set the pointer to the rim height and width of the first good piece, and throw each one to touch it.
  • Same pulls: the same number, the same way, every time.
  • Plates: throw on bats, and compress the floor with the rib four or five times as it spins. Dry slowly, flip onto a board at leather-hard so rim and middle dry together, trim, and finish drying between boards with a light weight on top.

The electric wheel

An The Electric Motor of 250–750 W drives the wheelhead through a belt or friction cone, a foot pedal varying the speed from 0 to about 250 turns a minute. It never slows when you press hard, which makes big lumps easy to centre. A belt from a line shaft driven by a The Waterwheel or engine, through a stepped pulley, does the same. Industrial potteries go further with the jigger and jolley, shaping plates and cups between a spinning plaster mould and a fixed metal profile, so unskilled hands make thousands a day (Slip Casting, Jiggering and Ceramic Factories).

How to tell it worked

  • The wheel: a stick held near the wheelhead rim and face shows an even gap all round. Kicked to speed, a good kick wheel coasts 2–3 minutes; a stick wheel at least one.
  • The pot: cut in half, the wall is even from bottom to rim; after trimming, the floor is no thicker than the wall. Six mugs stand the same height.
  • Fired: a sound pot rings clear when tapped; a dull note means a crack.

Note Troubleshooting. Clay wobbles and will not centre → arms not locked, clay too stiff, or wheel too slow. Pot twists and tears near the base → too little slip, wheel too slow, or gripping too hard. Walls collapse in a spiral → too much water soaked in, walls too thin low down, or wheel too fast. Rim goes wavy → off-centre clay or uneven pulls; trim the rim with the needle tool. S-shaped crack in the floor → floor not compressed, or water left standing in it. Handles crack off → handle wetter than the pot; join at the same dampness, dry slowly under cloth. Plates warp → dried unevenly; dry slowly under boards. Shaft squeals, wheel slows quickly → dry footstep or tight collar; grease, ease, keep slurry out.

Dangers

Warning Clay dust scars the lungs. Dry clay, glaze powder and trimmings contain fine silica; breathing it for years causes silicosis, an incurable scarring of the lungs. Never sweep dry. Clean with a wet mop or damp cloth, keep trimmings damp in a bucket, and never sand dry pots without a wet cloth over mouth and nose.

  • Electric wheels and water. Earth the frame, keep wiring high and dry, and use an earth-leakage breaker (Wiring and Electrical Safety, Motor Starters, Contactors and Protection).
  • Flywheels crush toes and fingers. Wear shoes; never reach under a spinning wheel. Hair, sleeves and apron strings get wound into powered wheels.
  • Backs and wrists. Set the seat at the right height, stand up every half hour, and centre big lumps in stages.

What this unlocks

Fast, cheap, even pots in quantity: tableware (Cutlery and Tableware), storage jars, pipes (Tiles and Clay Pipes), crucibles and retorts (Firebrick and Refractories, Distillation), insulators and laboratory ware (Stoneware and Porcelain). The same steady hand against spinning work carries over to Wood Turning and Treen and the The Lathe.

How it was first done

The first wheels were slow turntables, called tournettes, used in Mesopotamia around 4500 BC to finish coil-built pots. A fast wheel heavy enough to throw from a single lump appears there between about 3500 and 3000 BC and spread to Egypt, the Indus valley and the Mediterranean. In China, potters of the Longshan culture (about 2500 BC) threw black cups with walls under 1 mm thick. The foot-turned kick wheel was in use in the Near East by about 200 BC: the Book of Sirach describes the potter "turning the wheel about with his feet". Stick wheels are still used across India today, and electric wheels became common only in the 20th century.

Source: content/entries/earth/potters-wheel.md