Part 6 · Building
Stairs, Floors and Interior Finishes
Turning a frame into rooms — a staircase with risers, landings and a safe banister, boarded and parquet floors that do not squeak, lath-and-plaster ceilings and cornices, skirting boards and wainscot panelling, wallpaper and its paste, and skylights that let light into the roof without letting in rain.
- Difficulty
- ●●●●●
- Time
- A week for a staircase; two to three days to board a room; a week to lath and plaster a ceiling; a day to paper a room
- Steps from zero
- 18 prerequisites →
This unlocks
—The full path from nothing — 18 steps before this one
- Stone Tools
- Fire
- Cordage and Rope
- Finding and Preparing Clay
- Finding and Identifying Ores
- Basic Woodworking
- Hunting and Trapping
- Charcoal
- The Kiln
- Hides and Leather
- Gypsum and Plaster of Paris
- Bellows
- Iron (the Bloomery)
- Blacksmithing
- Steel
- Axes, Chisels, Knives and Planes
- Timber Framing and Log Building
- Doors, Windows and Joinery
- Stairs, Floors and Interior Finishes
Do them roughly in this order. See it on the tech tree →
Why it matters
A frame and a roof (Timber Framing and Log Building, Roofs) give shelter. Finishes make it a house: safe stairs, warm and quiet floors, ceilings, skirting and panelling, paper and paint. Each is a small trade, and they go in order: floors and grounds first, then plaster, then skirting and joinery, then paper and paint.
How it works
- Wood moves across its grain with the seasons (Doors, Windows and Joinery). Floors, panelling and skirting must be fixed so they can shrink without opening ugly gaps — tongues that hide the gap, panels that float, a gap at the wall that the skirting covers.
- A floor is a set of beams. Joists bend under load; too shallow and the floor bounces, cracks the ceiling below, and makes the boards squeak as they rub on the nails. Stiffness rises with the cube of the depth: a joist 25% deeper is nearly twice as stiff.
- Plaster holds on by keys. On a ceiling it is pushed through gaps between thin strips of wood (laths) and sets into hooks behind them called nibs. Hair in the first coat ties it together.
- Stairs follow the stride: twice the rise plus the going = 60–64 cm (Doors, Windows and Joinery), every step within 5 mm of the others.
What you need
| Item | For | See |
|---|---|---|
| Seasoned oak, pine, fir or spruce boards and planks | Stairs, boards, skirting, panelling | Basic Woodworking, Doors, Windows and Joinery |
| Saws, planes (including tongue-and-groove and moulding planes), chisels, brace and bits | All the joinery | Planes, Drawknives and Woodworkers' Tools, Axes, Chisels, Knives and Planes |
| Lathe | Balusters and newel caps | The Lathe |
| Floor brads or cut nails 50–65 mm, lath nails 25–30 mm | Fixing | Nails, Rivets and Wire Fasteners |
| Lime putty, sharp sand, animal hair; plaster of Paris | Ceilings and cornices | Lime, Gypsum and Plaster of Paris |
| Hawk, trowel, wooden float, sheet-iron profile | Plastering, running cornices | Sheet Metal and Rolling |
| Paper, distemper, woodblocks or stencils, wheat flour | Wallpaper and paste | Paper, Printing, Pigments, Paints and Varnish |
| Bitumen or hide glue | Laying parquet | Tar, Pitch and Glue, Glues and Adhesives |
| Glass 6 mm or thicker, sheet lead | Skylights | Window Glass, Lead |
Where to find it: timber as in Doors, Windows and Joinery — oak for treads, handrails and parquet, which take the most wear; pine or fir for joists, boards, laths and skirting. Animal hair for plaster comes from cattle, horses or goats: long, clean hair, teased apart and free of grease. Lime, gypsum and sand are in Lime and Gypsum and Plaster of Paris.
Stairs
Staircase
The basic flight — rise and going, strings, housed treads — is in Doors, Windows and Joinery. A house staircase adds risers, landings and a banister.
Choosing the type:
| Stair | Plan space for a 2.7 m storey | Notes |
|---|---|---|
| Straight flight | about 1 × 4 m | Simplest and safest. A long fall if someone trips at the top. |
| Dog-leg (two flights, turning back on a half landing) | about 2 × 2.5 m | Fits a narrow house; the landing breaks a fall. |
| Quarter turn with a landing or winders | about 2 × 3 m | Winders (wedge-shaped treads round a corner) save space but are the most dangerous part of any stair. |
| Spiral round a central post | about 1.6–2 m across | Steep and narrow; for towers, lofts and second stairs only. |
Sizes: width at least 80–90 cm (two people passing, or carrying furniture: 100 cm); pitch no steeper than 42°; headroom 2 m measured straight up from the line of nosings; a landing at the top and bottom at least as deep as the stair is wide, and no door swinging across a step. A flight of more than about 16 risers needs a landing part-way.
Building a closed-string flight with risers:
- Storey rod. Stand a straight rod on the lower floor and mark the finished upper floor on it. Divide it into equal rises with dividers by trial (Measurement from Scratch) — this is more accurate than arithmetic. Mark the going on a second rod laid across the floor.
- Pitch board. Cut a right-angled triangle of thin board with one side the rise and one the going. Step it along the string to mark every tread and riser, keeping the long side parallel to the string's edge with a fence.
- Housings. Trench each string for the treads and risers 12–15 mm deep, tapering each housing a little wider toward the back so a wedge can be driven in behind each tread and riser.
- Treads 30–40 mm oak or hard pine, with a nosing — the front edge rounded and standing 20–30 mm past the riser below so your heel does not catch. Risers 18–22 mm, tongued into a groove under the tread above and nailed or screwed to the back edge of the tread below.
- Assemble upside down: glue and wedge every tread and riser into both strings. Glue three or four small triangular blocks under the inside corner of each tread and riser; they stop squeaks for a century.
- Wide stairs (over 100 cm) or heavy use: add a carriage — a stout timber under the middle of the treads, notched to fit them.
- Fix the strings to a newel at the bottom, to the trimmer at the top (Timber Framing and Log Building), and to the wall with screws into plugs.
Winders: keep the going at least 5 cm at the narrow end and equal to the straight treads on the walking line, 30–40 cm in from the narrow side. Spiral stair: treads fanned 22–30° apart round a central post 20–25 cm across, their outer ends housed into a curved string or the wall. In stone, each step is one block with its own slice of the central post carved on its narrow end, stacked like coins (Stone Masonry).
Good: you can walk up and down without looking at your feet; no tread moves or creaks; every rise within 5 mm of the others. Bad: a short first or last step, a nosing that catches the toe, or headroom that makes tall people duck.
Banister
The banister (or balustrade) is the guard on the open side of a stair or landing: newel posts at the ends, a handrail along the top and balusters between rail and string.
- Newel post 90–100 mm square oak, at least 1.2 m long, tenoned into the bottom string and carried down through the floor and bolted to a joist. A weak newel is a weak banister.
- Handrail 90 cm above the nosings, measured straight up; 100 cm on landings and any drop over 60 cm. Shape it to fill a hand — 45–65 mm across, round or oval — with no sharp corners. Tenon it into the newels and pull it tight with a handrail bolt (a rod threaded at both ends, with a nut in a hole bored up from underneath) or a drawbored peg. Fit a second, lower rail for children if you can.
- Balusters 32–40 mm square, turned on the The Lathe if you like, set into a groove under the rail and into a capping on the string, with small filler pieces between them. The gap between balusters must not let a 10 cm ball through — a toddler's head. Never use horizontal rails a child can climb like a ladder.
- Wall side: a simple rail on iron brackets screwed into the wall, 5 cm clear of it for the knuckles.
Test it: lean your whole weight sideways on the rail mid-span and at the top newel. Nothing should move. Push each baluster — none should rattle.
Floors
Floorboards
Ground floors and joists are in Foundations and Floors. Upper floors need the same joists (depth in cm ≈ 4 × span in metres + 5, at 40 cm centres), with these additions:
- Openings. Where a joist must stop short — for a stair or a hearth — double the joists each side (trimming joists) and carry the cut ends on a doubled cross-piece (trimmer) jointed into them (Timber Framing and Log Building). Keep all timber at least 20 cm from any flue (Chimneys, Stoves and Heating).
- Strutting. Between joists at mid-span (every 1.8–2.5 m), nail pairs of 50 × 38 mm struts crossing in an X — herringbone strutting. It stops joists twisting and spreads a heavy load to their neighbours: the floor stops bouncing.
- Season the boards indoors for two to four weeks before laying, stacked flat with sticks between, so they reach the house's moisture.
- Boards: 20–25 mm thick, 10–15 cm wide (narrow boards move less), tongued and grooved. Lay them across the joists. Leave a 10–15 mm gap at each wall for swelling; the skirting covers it.
- Cramp them tight. Lay four to six boards loose, then drive them together with a pair of folding wedges (two long wedges laid point to point) between the last board and a batten nailed temporarily to the joists. Tap the wedges toward each other until the joints close.
- Nail two nails per board at each joist, 15 mm from the edges, 2.5 times as long as the board is thick, punched below the surface. For a clean floor, secret-nail: drive one nail at 45° through the root of each tongue, where the next board hides it.
- End joints fall on a joist, and are staggered — never two side by side.
- Finish: plane or scrape down any ridges with a cabinet scraper (Planes, Drawknives and Woodworkers' Tools), then rub in two or three coats of warm linseed oil (Oils and Pressing), a day apart, and polish with beeswax.
Good: no squeak when you walk heel-to-toe across the room; a marble rolls only where you expect (a level floor); no daylight between boards after the first winter. Squeaks come from boards rubbing on loose nails: re-nail beside the old nail with a longer one, or screw down.
Parquet
Small hardwood blocks laid in a pattern on a solid base. Short blocks shrink little, so the floor stays tight, and it uses oak offcuts too short for boards.
- Blocks: oak or another hardwood, about 22–25 mm × 70 × 230–280 mm, all exactly the same size — set the plane against a stop and make them in batches. Tongue and groove them, or cut a groove in every edge and join them with loose tongues.
- The base must be flat, dry and rigid: boards on stiff joists, or a lime concrete floor (Foundations and Floors) dry for at least two months. Damp from below lifts and rots parquet.
- Set out. Snap a chalk line down the middle of the room. A herringbone pattern (blocks at 45°, each end butting the side of the next) is laid out from it in both directions. Leave a border of blocks laid lengthways round the walls, and a 10–15 mm gap at the wall.
- Lay each block into a thin bed of hot bitumen (Tar, Pitch and Glue), pressing and tapping it down — the traditional way; or glue with hide glue in dry rooms (Glues and Adhesives).
- Level the surface with a toothing plane and scraper when the bed has set, then oil and wax as for boards.
Good: every block sounds solid when tapped with a knuckle (a hollow sound means it is not bedded); lines straight across the room.
Ceilings and walls
Ceiling
A ceiling stops dust falling through the boards above, holds a layer of still air and slows fire. Make it 2.4–2.7 m high: lower is warmer, higher is airier in hot climates.
- Boarded ceiling. Tongued and grooved boards 12–15 mm thick, nailed to the underside of the joists. Quick, light, and no plastering skill needed. Bead the edges to hide the joints as they shrink.
- Lath and plaster — the classic ceiling:
- Laths: strips about 25 × 6 mm and 90–120 cm long, riven from straight-grained oak or chestnut or sawn from pine. Soak them in water before fixing so they do not suck the water out of the plaster.
- Nail them across the joists (or ceiling battens at 30–40 cm) with 6–10 mm gaps between them: narrower and the plaster cannot get through; wider and it falls through. Stagger the end joints every eight laths or so, so no long line of joints forms a crack.
- First (scratch) coat: 1 lime putty : 3 sharp sand, with about 0.5 kg of animal hair to every 50 litres of mix, teased in so it is evenly spread. Press it hard up through the laths, 6–10 mm thick over them, so it curls over the back into nibs. Scratch it criss-cross. Let it stiffen for days to a week.
- Second (floating) coat: the same mix with less hair, 8–10 mm, ruled flat with a long straightedge and rubbed with a wooden float.
- Finish (setting) coat: 2–3 mm of fine lime putty mixed with plaster of Paris (Gypsum and Plaster of Paris) or fine sand, trowelled smooth as it stiffens.
- Total about 20–25 mm, weighing 40–50 kg per square metre — the joists and nails must carry it for ever.
Good: flat when you sight along it with a lamp held close; firm when pushed. A bulging, springy patch means the nibs have broken: the plaster is hanging only by its paint. Prop it, then screw it back to the joists with large washers, or take it down and re-lath.
Cornice
A moulded strip of plaster where wall meets ceiling. It hides the crack that always opens at that corner. Run it in place: cut the profile in reverse from sheet iron or zinc, nail it to a wooden horse that slides along a straight batten tacked to the wall, and build the cornice up in coats of plaster of Paris and lime, sliding the horse along after each coat until the profile is full and crisp. Corners are finished by hand with small tools. Small ornaments and a ceiling rose (the round boss round a lamp hook) are cast in plaster moulds (Gypsum and Plaster of Paris) and stuck up with wet plaster.
Skirting board
A board along the foot of every wall that takes kicks and hides the gap between floor and plaster, including the floor's expansion gap.
- Size: 15–22 cm high, 18–25 mm thick, pine or oak, the top edge rounded or moulded.
- Grounds. Before plastering, nail or plug horizontal battens (grounds) to the wall at the skirting's height, as thick as the plaster will be; the plasterer stops the plaster at them. Plugs are wedges of wood driven into raked-out mortar joints.
- Corners: at an outside corner, mitre both boards at 45°. At an inside corner, run one board into the corner and scribe (cope) the other — cut its end to the shape of the first board's face with a coping saw — so the joint stays closed when the wood shrinks.
- Nail to the grounds, punch the nails and fill. Oil or paint before fixing so the back is sealed too.
Wainscot
Wooden panelling on the lower walls — or the whole wall in grand rooms — warm to lean against and proof against knocks from chairs.
- Framed panelling: stiles, rails and floating panels made exactly like a panelled door (Doors, Windows and Joinery), 20–25 mm thick, fixed to grounds at top, middle and bottom.
- Matchboard: cheaper and quicker — tongued and grooved boards 12–15 mm thick, with a small rounded bead run along one edge to hide the joint, set upright and nailed to horizontal battens 40–60 cm apart.
- Dado rail: a moulded rail 5–7 cm deep capping the panelling, at 90–110 cm — about the height of a chair back, which it protects. Many rooms have only the dado rail, with plain plaster below.
- Never fix panelling to a damp wall without an air gap of 2 cm behind it and small vents at top and bottom: still, damp air behind wood breeds dry rot (Rot, Woodworm and Termites).
Wallpaper
Paper on plaster gives colour and pattern cheaply and covers fine cracks.
Making it:
- Paper (Paper): medium weight, rag or wood pulp, made in long sheets or joined end to end with paste into rolls. A practical roll is about 50–55 cm wide and 10 m long — enough for four drops in a 2.4 m room.
- Ground colour: brush on distemper — whiting (ground chalk) mixed with glue size and pigment (Pigments, Paints and Varnish) — and let it dry.
- Pattern: print with carved woodblocks (Printing), one block per colour, each block dipped in distemper colour on a pad and pressed on the paper, with pins on the block's corners to line up the repeats. Or stencil each colour through oiled card.
- Plain lining paper — the same paper with no colour — goes under good paper on rough walls.
Wallpaper paste:
Mix 250 g of wheat flour with cold water to a smooth cream. Pour it into 2 litres of boiling water, stirring hard, and keep stirring over the heat until it thickens and turns translucent, about 5 minutes. Cool, strain through a cloth to remove lumps. Add a teaspoon of alum or borax (Borax and Boric Acid) to keep mould and insects off. Use within two or three days. Glue size — hide glue thinned 1 part to 10 of water (Glues and Adhesives) — brushed on the wall first stops the plaster sucking the paste dry.
Hanging:
- The wall must be dry, smooth and sized; fill cracks first.
- Hang a plumb line near a corner and draw a line: the first drop must be vertical, because walls and corners never are.
- Cut each length 10 cm longer than the wall height, matching the pattern to the previous one.
- Paste the back evenly, fold each end in to the middle, paste to paste, and leave it to soften for 5–10 minutes so it stretches before, not after, it goes on the wall.
- Hang from the top, slide it to the line, and brush out from the centre to push out air. Butt each drop tightly against the last.
- Crease into the ceiling and skirting with the back of the scissors, pull back, cut along the crease, brush back.
Good: no bubbles once dry (small ones shrink flat overnight), seams that you cannot find from 2 m away, the pattern matching across every join. Bad: peeling at the seams (too little paste at the edges) or blisters that stay (paper hung before it had softened).
Light from above
Skylight
A glazed opening in the roof that lights a stairwell, an attic or a deep room. A skylight gives two to three times as much light as a wall window of the same size, but it is the easiest part of a roof to make leak.
- Frame the opening: cut the rafters and carry them on doubled rafters at each side and doubled trimmers across the top and bottom (Roofs). Keep it narrower than about 1 m between rafters unless you trim properly.
- Curb: a box of 50 mm timber standing at least 15 cm above the roof surface, so water running down the roof passes round it, not into it.
- Flashing (Lead): a lead apron dressed down over the covering below the curb; stepped flashings or soakers up the sides, interleaved with each course of slates or tiles; a small lead-lined back gutter above the curb to turn the water to each side.
- Glass: 6 mm or thicker, in bars running down the slope only, with no cross-bars to dam the water. Where panes meet, lap the upper one over the lower by 2–3 cm, like slates, and bed them in putty (Window Glass). A skylight should slope at least 15–20°.
- Condensation gutter: a small channel along the bottom of the curb inside, draining out through a hole or tube, catches the water that runs down the underside of the cold glass.
- Opening skylights hinge at the top and are held by a notched stay — a good way to let hot air out of the top of a stairwell.
- A grille of iron bars or wire under the glass stops broken glass falling into the room, and stops a person falling through.
A roof lantern is a bigger skylight with its own little glazed roof, built like a tiny glasshouse (Cold Frames, Cloches and Greenhouses) on a curb.
Good: no drip after a day of driving rain; the inside stays dry on a frosty morning when the glass streams with condensation.
How to tell it worked
Check each piece against its Good line above. The real test is the first heated winter: skirting, panelling and paper still tight, no new cracks beyond hairlines at the cornice, and the skylight dry through a storm.
Note Troubleshooting. Floor bounces → joists too shallow or no strutting. Add strutting at mid-span, or a beam under the middle. Gaps between boards → laid unseasoned or in a damp season. Lift and re-cramp the boards in summer, adding one; or glue thin slips into the gaps. Stair creaks → loose wedge or missing glue blocks. Drive the wedge home with fresh glue; add blocks from underneath. Plaster fell off in chunks while drying → laths dry when plastered, or gaps too narrow. Soak laths; widen gaps. Skylight drips at the bottom edge → condensation, not a leak, if it drips most on cold mornings. Add the gutter; ventilate the room.
Dangers
Danger Falls on stairs and through roofs. Stairs are among the commonest places for fatal falls in the home, especially for the old and the very young. Uneven steps, a missing handrail, a dark stair or a baluster gap a toddler can squeeze through all kill. And never step on or lean on a skylight from the roof: people falling through roof lights die every year. Board across the roof to work near one.
Danger Arsenic and lead in wallpaper and paint. The bright greens of the 1800s (Scheele's green and Paris green) were copper arsenic compounds; damp rooms papered with them poisoned families with arsenic. Never use arsenic, copper-arsenic or lead pigments in wallpaper or indoor paint. Use earth pigments, chalk, ochres and plant colours (Pigments, Paints and Varnish, Dyes and Mordants).
- Ceiling collapse: old lath-and-plaster ceilings can fall in one piece, 40–50 kg a square metre. Never stand under one you are pulling down; prop sagging ones at once.
- Lime burns eyes and skin (Lime); wear eye protection when plastering overhead, and have clean water at hand.
- Fire: floors and stairs are wood. A ceiling of lath and plaster slows fire well; keep stair enclosures plastered and keep the stair clear — it is the escape route (Firefighting).
Going further
Floorcloths and linoleum are in Linoleum, Oilcloth and Floorcloths, rugs in Blankets, Curtains, Rugs and Towels, plywood panels in Plywood, Veneer and Boards, doors in Doors, Hinges, Handles and Latches, and concrete floors and stairs in Reinforced Concrete. Power planing of boards, tongue-and-groove flooring and mouldings comes with Planers, Thicknessers and Woodworking Machines.
How it was first done
Stone spiral stairs were built in Rome by the 2nd century AD (Trajan's Column has one inside) and became the standard stair of medieval castles; wooden staircases with balustrades and broad landings grew with the large houses of 16th- and 17th-century Europe. Lath and lime plaster ceilings were standard in Europe and its colonies from the 1600s until plasterboard replaced them in the 1900s. Parquet spread from 17th-century France — the Versailles pattern is named after the palace. Wallpaper came from China; block-printed European papers were fashionable by the 1700s, and steam roller printing made them cheap in the mid-1800s, when arsenical greens caused a long public scandal.
Source: content/entries/building/stairs-floors-and-finishes.md