◆ Rebuild

Part 9 · Health and Medicine

Dentistry

Keeping teeth for life with chew sticks, brushes and less sugar; recognising decay, gum disease and the abscess that can kill; pulling a tooth safely; temporary fillings of zinc oxide and clove oil; and making dentures.

Difficulty
●●●●●
Time
Two minutes twice a day to prevent; 15–30 minutes for an extraction; days to make a denture
Steps from zero
7 prerequisites →

You need first

Sterilising Instruments and Dressings

This unlocks

Dental Instruments and Fillings
The full path from nothing — 7 steps before this one
  1. Fire
  2. Finding and Preparing Clay
  3. Sanitation and Germs
  4. Pottery
  5. Fermentation
  6. Distillation
  7. Sterilising Instruments and Dressings
  8. Dentistry

Do them roughly in this order. See it on the tech tree →

Why it matters

Toothache is one of the most disabling pains there is, and in a world without dentists it is common. A rotten tooth stops a person eating, sleeping and working. Worse, the infection at its root can spread into the face and neck and kill within days. People who lose their teeth young cannot chew tough food and become malnourished.

Almost all of this is preventable. Decay is caused mainly by sugar and plaque, and both can be controlled with a stick, a little powder and good habits. When prevention fails, a person trained in this chapter can relieve pain, pull a bad tooth, place a temporary filling, and make false teeth.

How it works

A tooth is a hard crown above the gum and one to three roots below, set in a socket of jawbone and held by a thin elastic ligament.

  • Enamel is the hard white outer shell of the crown — the hardest substance in the body. It has no nerves and cannot heal itself once a hole forms.
  • Dentine, under it, is softer and yellowish, and carries fine channels to the nerve. Decay spreads faster here, and it hurts.
  • Pulp, in the middle, is the living core of nerves and blood vessels, running down the root canals.

Decay. A sticky film of bacteria called plaque builds up on teeth within a day. When you eat sugar or soft starch, the bacteria turn it into acid, which dissolves enamel for 20–40 minutes after each snack. Saliva then slowly repairs the surface. So how often you eat sugar matters far more than how much: sweets sucked all day do far more harm than the same amount eaten with a meal.

Gum disease. Plaque left at the gum line makes the gums red, swollen and bleeding (gingivitis). Over years it hardens into tartar (a yellow-brown crust) and eats away the bone around the roots, until teeth loosen and fall out (periodontitis). Bleeding gums can also mean scurvy — vitamin C deficiency (Nutrition and Deficiency Diseases).

Abscess. When decay reaches the pulp, bacteria kill it and pass down the canal to the root tip. Pus collects in the bone there — a dental abscess.

Enamel Dentine Pulp Root Gum Bone A healthy molar cut in half, set in the jawbone 1 Enamel only no pain; a white or brown spot 2 Into dentine hurts with cold and sweet 3 Pulp dead abscess (yellow) at the root tip HOW DECAY PROGRESSES
Fig. 1 A tooth and the progress of decay. Decay in enamel alone causes no pain; in dentine it hurts with cold and sweet; once it reaches the pulp, the nerve dies and pus collects at the root tip in the bone.

What you need

Item Use Source
Chew sticks or toothbrushes Cleaning See below; Brooms, Brushes and Combs
Tooth powder Polishing Finely ground chalk, a pinch of salt
Silk or fine linen thread Cleaning between teeth Silk, Flax, Hemp and Linen
Mirror and probe Looking Polished metal or Mirrors; a fine steel point
Scaler Scraping tartar A small hooked steel blade (Steel)
Elevator Loosening teeth A narrow steel lever with a rounded, slightly hollowed blade, on a stout handle
Extraction forceps Pulling teeth Two pairs at least: one with straight beaks for upper teeth, one with beaks bent at a right angle for lower teeth. A smith's job (Blacksmithing)
Excavator Scraping out decay A tiny sharp-edged spoon on a handle
Zinc oxide and clove oil Temporary fillings, dressings Zinc and Brass, Distillation
Boiled gauze Stopping bleeding Sterilising Instruments and Dressings
Good light Daylight at a window, or a mirror reflecting sunlight into the mouth

How to forge, harden and finish each of these instruments is in Dental Instruments and Fillings. All instruments are boiled or steamed before every patient (Sterilising Instruments and Dressings): mouths carry hepatitis and other blood-borne infections.

Where to find it

  • Chew stick plants. Twigs of many trees clean teeth well, and several contain mild germ-killers. The best known are arak or miswak (Salvadora persica), a shrub of dry lands from Africa to India; neem (Azadirachta indica) of India and Africa; licorice root; and in cooler lands dogwood, birch and willow twigs. Choose fresh, pencil-thick, fibrous twigs that fray into a brush when chewed, and that are not bitter-poisonous (never oleander, yew or other toxic plants — see Dangerous Plants and Animals).
  • Chalk — soft white limestone (Rocks and Minerals) that marks like a crayon. Ground fine and washed, it makes a gentle tooth powder.
  • Cloves — the dried flower buds of a tropical tree; their oil (eugenol) numbs and soothes. Steam-distil the oil (Distillation).
  • Zinc oxide — the white "smoke" given off when zinc burns, which settles as a fluffy white powder (Zinc and Brass).
  • Beeswax for impressions (Beekeeping); gypsum for plaster models (Gypsum and Plaster of Paris).

Step by step: keeping teeth

fresh twig, pencil-thick bark peeled; chewed until the end splays to a brush chew wire loop pulls a folded tuft of stiff hair through bone or hardwood handle, rows of drilled holes bristles angled into the gum line small strokes gum 1 Chew stick 2 Making a brush 3 Where to clean Twice a day, two minutes, every surface of every tooth. Tooth powder: fine chalk and a pinch of salt — never sand.
Fig. 2 Cleaning teeth. A chew stick is chewed at one end until it frays into a brush. A brush can be made from a bone handle with tufts of stiff hair pulled through drilled holes. Either way, angle the bristles at the gum line and clean every surface.
  1. Make a chew stick: cut a fresh twig 15–20 cm long and as thick as a pencil. Peel the bark from one end and chew it for a minute until the fibres splay into a brush about 1 cm long. Cut off the used end every day or two.
  2. Or make a brush: drill two or three rows of small holes in a flat handle of bone or hardwood; fold small tufts of stiff hog or horse hair in half, pull each through a hole with a loop of fine wire, and glue or wedge them. Trim the tufts level, about 1 cm long.
  3. Clean twice a day, for two minutes, especially before sleep. Hold the bristles at an angle to the gum line, pointing into it, and use short, gentle strokes. Do the outside, inside and biting surface of every tooth, back ones too. Scrubbing hard wears away the gums.
  4. Clean between the teeth once a day with silk or linen thread drawn gently up and down each side of each gap, or with a thin wooden pick.
  5. Tooth powder: chalk, ground to flour and washed, with a pinch of salt. Never use sand, brick dust, crushed shell or coarse charcoal — they scratch away enamel.
  6. Sugar with meals only. Honey, dried fruit, sweet drinks and sticky starches eaten between meals cause the most decay. Rinse the mouth with water after sweet food.
  7. Children: wipe a baby's first teeth with a clean damp cloth daily. Never let a child sleep with a bottle of sweet drink or milk, or a sweetened dummy. Help children brush until they are about 8.
  8. Fluoride. Some natural waters contain fluoride, which hardens enamel against decay. If people who grew up on a water supply have very few cavities, it may be one of these. If they have chalky white or brown mottled teeth, the water has too much fluoride; very high levels damage bones. You cannot easily make fluoride safely — do not try.

Removing tartar (scaling): with good light, slide the hooked scaler gently under the edge of the crust at the gum line and flick it away from the gum. Work tooth by tooth, especially behind the lower front teeth and outside the upper back teeth. Gums bleed at first and then tighten and heal over 1–2 weeks of good cleaning.

What the pain tells you

Symptom Likely cause What to do
Sharp pain with cold or sweet that stops within seconds Decay into dentine, or exposed root Clean well; fill the hole (below)
Pain that lingers after hot or cold; throbbing at night; pain that comes by itself The pulp is dying Extraction (or root treatment by a skilled dentist)
Pain on biting or tapping the tooth; tooth feels "high" Abscess at the root tip Drain it; extract
Swollen gum with a pimple that leaks pus Abscess draining Extract the tooth
Swollen face Spreading abscess Urgent: see the danger box
Bleeding, red gums; loose teeth Gum disease; or scurvy Cleaning, scaling, vitamin C foods

Danger A spreading dental infection can kill within a day or two. Danger signs: swelling under the jaw or tongue, with the tongue pushed up; difficulty swallowing, speaking or breathing; inability to open the mouth; swelling spreading up to the eye; high fever. The swelling can close the airway. The tooth must come out and the pus be drained at once, by the most skilled person available, with antibiotics if any exist (Penicillin). Keep the person sitting up.

For a simple abscess: warm salt-water mouthwashes (a teaspoon of salt in a cup of warm water), held over the tooth for a minute, every 2 hours. If a soft swelling has formed on the gum, a small cut into it with a boiled blade releases the pus and the pain (Basic Surgery). Then remove the tooth: as long as the dead tooth stays, the abscess returns.

Step by step: pulling a tooth

Attempt only teeth that are loose, broken down, or abscessed, and start with the easier ones: front teeth and premolars usually have one root; upper molars have three and lower molars two, set in thick bone. Leave wisdom teeth, deeply broken roots and anyone who bleeds for a long time from small cuts to a skilled person.

FORCEPS ELEVATOR cheek tongue Beaks down under the gum, on the root Bone the socket stretches Gum blade between tooth and bone twist like a key Rock slowly towards the cheek, then the tongue hold each push a second or two; never jerk Loosen first fingers on the jaw to brace
Fig. 3 Pulling a tooth. The elevator first loosens the tooth in its socket. The forceps beaks are pushed down under the gum onto the root, parallel to the tooth. Slow, firm pressure towards the cheek, then towards the tongue, stretches the bone socket until the tooth comes free.
  1. Make sure of the tooth. Count from the middle; tap each suspect tooth with a handle — the bad one hurts most.
  2. Prepare. Sterile instruments, washed hands, a firm chair with the head supported against a wall or headrest, good light. Upper teeth: the patient's mouth at the height of your shoulder; lower teeth: at your elbow.
  3. Numb it if you can. Injected local anaesthetic is best but needs training (Anaesthesia). Without it, a pad of clove oil held on the gum for 5 minutes takes the edge off. Explain that it will hurt for a minute, and work steadily.
  4. Free the gum by running the elevator or a probe all round the neck of the tooth, under the gum edge.
  5. Loosen with the elevator. Push its blade down between the tooth and the bone on the front side of the tooth, hollow side towards the tooth, and twist it like a key, slowly. Brace the hand holding it with your fingers on the jaw, and keep the fingers of your other hand on the gums on either side to feel movement and protect the tongue and cheek. Never lever against a healthy neighbouring tooth.
  6. Apply the forceps. Slide the beaks down under the gum, on the cheek side and the tongue side, as far down the root as you can, parallel to the tooth's long axis. Grip firmly.
  7. Rock slowly. Press steadily towards the cheek and hold for a second or two, then towards the tongue, a little further each time. The bone stretches. For upper front teeth, which have round, cone-shaped roots, add a slow twist. Never jerk — that snaps the root.
  8. Lift it out when it moves freely, usually towards the cheek side.
  9. Check the roots are complete, with smooth, rounded ends. A tiny broken tip in a tooth that was not infected can be left; larger pieces need skill.
  10. Squeeze the socket gently between finger and thumb to press the bone back into shape, then have the patient bite firmly on folded boiled gauze for 30 minutes.

Aftercare: no rinsing, spitting, hot drinks or alcohol for 24 hours — they dislodge the clot that heals the socket. Soft, cool food; chew on the other side. From the next day, warm salt-water rinses after each meal for a week. If it bleeds again, bite on fresh gauze (a damp cloth of strong tea helps) for another 30 minutes.

Fillings — in outline

A temporary filling of zinc oxide and clove oil can stop the pain of a shallow or medium hole and last months:

  1. Scrape out all the soft brown decay with a sharp excavator until the floor of the hole feels hard and scratchy, like the rest of the tooth.
  2. Dry the hole with a twist of cotton.
  3. On a glass or glazed tile, mix zinc oxide powder with clove oil, about 4–6 parts powder to 1 part oil by weight, until it is a stiff putty that does not stick to your fingers.
  4. Press it firmly into the hole and smooth it; have the patient bite gently to check it is not too high. It sets in minutes and hardens over a few hours. The clove oil soothes the pulp.

Permanent fillings were made with gold leaf hammered into the cavity layer by layer — painstaking, but they last decades — or with amalgam, a paste of silver–tin alloy filings and mercury that sets hard. Amalgam works well, but handling mercury (Mercury) poisons the person who mixes it unless it is done with great care and ventilation. Both are skilled work; teeth with deep decay that has reached the pulp cannot be saved by a filling alone.

Dentures

  1. Take an impression. Soften beeswax in warm water, press it into a shallow tray shaped like a horseshoe, and press it over the gums (and any remaining teeth). Let it firm, and ease it out.
  2. Cast a model. Pour plaster of Paris (Gypsum and Plaster of Paris) into the impression; when it has set, warm the wax away. You now have a copy of the mouth.
  3. Make the base on the model: carve it from a dense, fine-grained hardwood such as boxwood, or from bone, or later mould it from vulcanised rubber (Rubber).
  4. Set teeth into it: carved bone, or fired porcelain teeth (Stoneware and Porcelain), fixed in sockets with pins or pegs.
  5. Fit it. A well-fitting upper denture is held by suction; a partial one by small wire clasps around remaining teeth. Mark sore spots with charcoal on the base and scrape them away until it is comfortable.
  6. Clean it daily, and take it out at night.

How to tell it worked

  • Healthy gums are pale pink, firm, and do not bleed when brushed.
  • After an extraction, a dark red clot fills the socket; pain lessens each day and is mostly gone in 3–5 days.
  • A filled tooth stops hurting with cold within a day or two.

Note Troubleshooting. Pain gets worse 2–4 days after an extraction, the socket looks empty and grey and tastes foul → "dry socket": the clot was lost. Rinse gently with warm salt water and lay a small strip of gauze soaked in clove oil loosely in the socket, changed daily. It heals in 1–2 weeks. Root snaps during extraction → stop and judge: leave a small clean tip; refer large or infected pieces. After an upper back tooth, air or fluid passes between mouth and nose → the sinus has been opened. No nose blowing or sucking for 2 weeks; small openings heal by themselves. Temporary filling falls out → the decay was not fully cleaned or the hole was wet; clean, dry and refill.

Dangers

Danger Spreading infection from a tooth can close the airway or reach the brain (see the box above). Heavy bleeding after an extraction that biting on gauze for an hour will not stop needs firm packing of the socket and a skilled person; stitches across the socket may be needed (Basic Surgery).

  • Breaking the jaw: never use great force, especially on lower molars of older people, whose jaws are brittle.
  • Swallowed or inhaled teeth: keep the patient's head upright and have a gauze screen at the back of the mouth.
  • Shared, unsterilised instruments spread hepatitis and HIV. Sterilise everything every time.
  • Mercury: do not make amalgam without proper training and ventilation.

What this unlocks

Good teeth mean better nutrition for life (Nutrition and Deficiency Diseases). Dental work drives fine instrument-making (Steel, Blacksmithing), Anaesthesia (the first public demonstrations of both nitrous oxide and ether were by dentists), and later porcelain, rubber and metal casting for crowns and dentures. Daily cleaning is part of Personal Hygiene.

How it was first done

People in Mehrgarh (in today's Pakistan) drilled holes in living teeth with flint-tipped bow drills between 9,000 and 7,500 years ago, and a 6,500-year-old jaw from Slovenia has a cracked tooth sealed with beeswax. The Etruscans of Italy bound replacement teeth with gold bands around 2,500 years ago. Chew sticks have been used for thousands of years across Africa, the Middle East and Asia, and remain common today. Bristle toothbrushes are recorded in China by the 1400s; in England, William Addis began making bone-handled brushes around 1780. Japanese craftsmen carved full dentures from boxwood by the sixteenth century. The French surgeon Pierre Fauchard, whose 1728 book Le Chirurgien Dentiste described fillings, braces and dentures, is called the father of modern dentistry. Dentists Horace Wells (1844) and William Morton (1846) pioneered anaesthesia. In 1945, Grand Rapids in Michigan became the first city to add fluoride to its water, after the dentist Frederick McKay had noticed, decades earlier, that people with naturally "brown-stained" teeth rarely had decay — a stain later traced to natural fluoride in their water.

Source: content/entries/health/dentistry.md